Shrinkage-reducing measures and mechanisms analysis for alkali-activated coal gangue-slag mortar at room temperature
The DOI matches its Crossref record; 2 of the 2 references it cites were found in a registry or an index.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“The moderate CE is converted into compressive stress acting at the fiber-matrix interface [52], which enhances interfacial bonding and delays crack opening.”
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Freeze–thaw cycle test and damage mechanics models of alkali-activated slag concrete
Fu, Y., Cai, L., & Yonggen, W. (2011) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2010.12.006 · Cited by 279
Preparation and Reaction Mechanism Characterization of Alkali-activated Coal Gangue–Slag Materials
Ma, H., Zhu, H., Yi, C., Fan, J., Chen, H., Xu, X., & Wang, T. (2019) · Materials · doi:10.3390/ma12142250 · Cited by 91
Self-citation
Research works printed but not linked: 36
- Burciaga-Díaz, 2012, Strength and durability in acid media of alkali silicate-activated metakaolin geopolymers, J. Am. Ceram. Soc., 95, 2307, 10.1111/j.1551-2916.2012.05249.x · DOI
- Mobili, 2016, Metakaolin and fly ash alkali-activated mortars compared with cementitious mortars at the same strength class, Cem. Concr. Res., 88, 198, 10.1016/j.cemconres.2016.07.004 · DOI · Paper page
- Yang, 2012, Effect of water–binder ratio on the mechanical properties of calcium hydroxide-based alkali-activated slag concrete, Constr. Build. Mater., 29, 504, 10.1016/j.conbuildmat.2011.10.062 · DOI
- Lancellotti, 2013, Inorganic polymers from alkali activation of metakaolin: effect of setting and curing on structure, J. Solid State Chem., 200, 341, 10.1016/j.jssc.2013.02.003 · DOI
- Lee, 2013, Setting and mechanical properties of alkali-activated fly ash/slag concrete manufactured at room temperature, Constr. Build. Mater., 47, 1201, 10.1016/j.conbuildmat.2013.05.107 · DOI · Paper page
- Zhang, 2017, Durability of alkali-activated materials in aggressive environments: A review on recent studies, Constr. Build. Mater., 152, 598, 10.1016/j.conbuildmat.2017.07.027 · DOI · Paper page
- Arbi, 2016, A review on the durability of alkali-activated fly ash/slag systems: advances, issues, and perspectives, Ind. Eng. Chem. Res., 55, 5439, 10.1021/acs.iecr.6b00559 · DOI · Paper page
- Toniolo, 2017, Boccaccini, Fly ash-based geopolymers containing added silicate waste. A review, Ceram. Int., 43, 14545, 10.1016/j.ceramint.2017.07.221 · DOI
- Lura, 2003, Autogenous shrinkage in high-performance cement paste: an evaluation of basic mechanisms, Cem. Concr. Res., 33, 223, 10.1016/S0008-8846(02)00890-6 · doi:10.1016/s0008-8846(02)00890-6
- Wehbe, 2017, Combined effect of shrinkage reducing admixtures (sra) and superabsorbent polymers (sap) on the autogenous shrinkage, hydration and properties of cementitious materials, Constr. Build. Mater., 138, 151, 10.1016/j.conbuildmat.2016.12.206 · DOI
- Kheradmand, 2017, Shrinkage performance of fly ash alkali-activated cement based binder mortars, KSCE J. Civ. Eng., 22, 1854, 10.1007/s12205-017-1714-3 · DOI
- Cartwright, 2015, Shrinkage characteristics of alkali-activated slag cements, J. Mater. Civ. Eng., 27, B4014007, 10.1061/(ASCE)MT.1943-5533.0001058 · DOI · Paper page
- Collins, 2000, Effect of pore size distribution on drying shrinking of alkali-activated slag concrete, Cem. Concr. Res., 30, 1401, 10.1016/S0008-8846(00)00327-6 · DOI · Paper page
- Fu-Sheng, 2005, Study on modification of the high-strength slag cement material, Cem. Concr. Res., 35, 1344, 10.1016/j.cemconres.2004.10.017 · doi:10.1016/j.cemconres.2004.10.017
- Hardjito, 2004, On the development of fly ash-based geopolymer concrete, ACI Mater. J., 101, 467
- Fernandez-Jimenez, 2006, Engineering properties of alkali-activated fly ash concrete, ACI Mater. J., 103, 106
- Sakulich, 2013, Mitigation of autogenous shrinkage in alkali activated slag mortars by internal curing, Mater. Struct., 46, 1355, 10.1617/s11527-012-9978-z · DOI
- Bakharev, 2000, Effect of admixtures on properties of alkali-activated slag concrete, Cem. Concr. Res., 30, 1367, 10.1016/S0008-8846(00)00349-5 · DOI · Paper page
- Hailong, 2017, Shrinkage mitigation strategies in alkali-activated slag, Cem. Concr. Res., 101, 131, 10.1016/j.cemconres.2017.08.025 · DOI · Paper page
- Yi, 2018, Study on chloride binding capability of coal gangue based cementitious materials, Constr. Build. Mater., 167, 649, 10.1016/j.conbuildmat.2018.02.071 · DOI
- Yi, 2018, Preparation and characterization of coal gangue geopolymers, Constr. Build. Mater., 187, 18
- Rajabipour, 2008, Interactions between shrinkage reducing admixtures (SRA) and cement paste’s pore solution, Cem. Concr. Res., 38, 606, 10.1016/j.cemconres.2007.12.005 · doi:10.1016/j.cemconres.2007.12.005
- Palacios, 2007, Effect of shrinkage-reducing admixtures on the properties of alkali-activated slag mortars and pastes, Cem. Concr. Res., 37, 691, 10.1016/j.cemconres.2006.11.021 · DOI · Paper page
- Ma, 2018, Property and cementation mechanism of alkali-activated coal gangue-slag cementitious materials, Chin. J. Mater. Res., 32, 898
- Ma, 2019, Study on the drying shrinkage of alkali-activated coal gangue-slag mortar and its mechanisms, Constr. Build. Mater., 225, 204, 10.1016/j.conbuildmat.2019.07.258 · doi:10.1016/j.conbuildmat.2019.07.258
- Folliard, 1997, Properties of high performance concrete containing shrinkage reducing admixture, Cem. Concr. Res., 27, 1357, 10.1016/S0008-8846(97)00135-X · doi:10.1016/s0008-8846(97)00135-x
- Neto, 2008, Drying and autogenous shrinkage of pastes and mortars with activated slag cement, Cem. Concr. Res., 38, 565, 10.1016/j.cemconres.2007.11.002 · DOI · Paper page
- Ye, 2017, Radlińska Aleksandra, Understanding the drying shrinkage performance of alkali-activated slag mortars, Cem. Concr. Compos., 76, 13, 10.1016/j.cemconcomp.2016.11.010 · DOI · Paper page
- Mastali, 2018, Drying shrinkage in alkali-activated binders–a critical review, Constr. Build. Mater., 190, 533, 10.1016/j.conbuildmat.2018.09.125 · DOI · Paper page
- Ma, 2015, The shrinkage of alkali activated fly ash, Cem. Concr. Res., 68, 75, 10.1016/j.cemconres.2014.10.024 · DOI · Paper page
- Thomas, 2006, A colloidal interpretation of chemical aging of the c-s-h gel and its effects on the properties of cement paste, Cem. Concr. Res., 36, 30, 10.1016/j.cemconres.2004.10.022 · DOI
- Hou, 2011, Influence of permeability of hcsa expansive agent on high volume fly ash concrete, Key Eng. Mater., 477, 354, 10.4028/www.scientific.net/KEM.477.354 · doi:10.4028/www.scientific.net/kem.477.354
- Wei, 2015, Impact on splitting tensile properties of the early age shrinkage-compensating steel fiber reinforced concrete, Bull. Chin. Ceram. Soc., 34, 3004
- Ye, 2016, Radlińska Aleksandra, Shrinkage mechanisms of alkali-activated slag, Cem. Concr. Res., 88, 126, 10.1016/j.cemconres.2016.07.001 · DOI · Paper page
- Gong, 2018, Influence of shrinkage-reducing agent and polypropylene fiber on shrinkage of ceramsite concrete, Constr. Build. Mater., 159, 155, 10.1016/j.conbuildmat.2017.10.064 · DOI
- Izaguirre, 2011, Characterization of aerial lime-based mortars modified by the addition of two different water-retaining agents, Cem. Concr. Comp., 33, 309, 10.1016/j.cemconcomp.2010.09.008 · DOI
Cited by
Zhang, B., Zhu, H., Cheng, Y., Huseien, G. F., & Shah, K. W. (2022) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.125993 · Cited by 258
Self-citationZhang, B., Zhu, H., Feng, P., & Zhang, P. (2022) · Journal of Building Engineering · doi:10.1016/j.jobe.2022.104056 · Cited by 192
Self-citationLu, S., Liu, J., Fantilli, A. P., Sun, X., Gan, L., Lacidogna, G., Tang, J., Ma, Y., Wang, T., Lu, Y., et al. (2026) · Case Studies in Construction Materials · doi:10.1016/j.cscm.2026.e06462
“The moderate CE is converted into compressive stress acting at the fiber-matrix interface [52], which enhances interfacial bonding and delays crack opening.”
Metadata
- Authors
- Ma, H., Zhu, H., Chen, H., Ni, Y., Xu, X., & Huo, Q.
- Venue
- Construction and Building Materials
- Publisher
- Elsevier BV
- Published
- 2020-08
- Volume
- 252
- Pages
- 119001
- ISSN
- 0950-0618
- Cited by
- 47
- References
- 2
- Language
- en
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- www.elsevier.com/legal/tdmrep-license (tdm)
- Funders
- China Scholarship Council
- National Natural Science Foundation of China
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Shrinkage-reducing measures and mechanisms analysis for alkali-activated coal gangue-slag mortar at room temperature. https://app.cochat.ai/papers/10.1016/j.conbuildmat.2020.119001
- The paper
- Ma, H., Zhu, H., Chen, H., Ni, Y., Xu, X., & Huo, Q. (2020). Shrinkage-reducing measures and mechanisms analysis for alkali-activated coal gangue-slag mortar at room temperature. Construction and Building Materials. https://doi.org/10.1016/j.conbuildmat.2020.119001
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.