Effect of water vapour on the oxidation of Fe–13Cr–5Ni martensitic alloy at 973K
Integrity signals
Registry
Cites
Statistics
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
Previous research focused on the initiation/breakaway event indicates a similar microstructure after the onset of breakaway of Fe-based alloys, seemingly independent of the suggested breakaway reaction.
“Previous research, focused on the initiation/breakaway event, indicate a similar microstructure obtained after the onset of breakaway of Fe-based alloys, seemingly independent of suggested breakaway-reaction [8,20,22,29,31].”
From The influence of Nickel on the corrosion protection of FeCrNi alloys after breakaway corrosion at 600 °C (2024) · cites this paper as [22]
Cites
No references could be resolved yet.
Research works printed but not linked: 25
- Masuyama, 2001, History of power plants and progress in heat resistant steels, ISIJ Int., 41, 612, 10.2355/isijinternational.41.612 · DOI
- Douglass, 1996, International workshop on high-temperature corrosion, Oxid. Met., 45, 529, 10.1007/BF01046850 · DOI
- Essuman, 2008, The effect of water vapor on selective oxidation of Fe–Cr alloys, Oxid. Met., 69, 143, 10.1007/s11085-007-9090-x · DOI
- Żurek, 2005, The effect of water-vapor content and gas flow rate on the oxidation mechanism of a 10% Cr-Ferritic steel in Ar–H2O mixtures, Oxid. Met., 63, 401, 10.1007/s11085-005-4394-1 · DOI
- Mikkelsen, 2003, High temperature oxidation of Fe–Cr alloy in O2–H2-H2O atmospheres; microstructure and kinetics, Mater. Sci. Eng. A, 361, 198, 10.1016/S0921-5093(03)00527-6 · DOI
- Yang, 2005, Effects of water vapor on oxidation behavior of ferritic stainless steels under solid oxide fuel cell interconnect exposure conditions, Solid State Ionics, 176, 1495, 10.1016/j.ssi.2005.03.019 · DOI
- Peng, 2005, Effect of grain refinement on the resistance of 304 stainless steel to breakaway oxidation in wet air, Acta Mater., 53, 5079, 10.1016/j.actamat.2005.07.019 · DOI
- Shen, 1997, High-temperature oxidation of Fe–Cr alloys in wet oxygen, Oxid. Met., 48, 347, 10.1007/BF01670507 · DOI
- Yamauchi, 2003, Evaporation of Cr2O3 in atmospheres containing H2O, Oxid. Met., 59, 517, 10.1023/A:1023671206976 · DOI
- Ehlers, 2006, Enhanced oxidation of the 9% Cr steel P91 in water vapour containing environments, Corros. Sci., 48, 3428, 10.1016/j.corsci.2006.02.002 · DOI
- Asteman, 2002, Evidence for chromium evaporation influencing the oxidation of 304L: the effect of temperature and flow rate, Oxid. Met., 57, 193, 10.1023/A:1014877600235 · DOI
- Norby, 1997, Concentration and transport of protons in oxides, Curr. Opin. Solid State Mater. Sci., 2, 593, 10.1016/S1359-0286(97)80051-4 · DOI
- Rahmel, 1965, Influence of water vapor and carbon dioxide on the oxidation of iron in oxygen at high temperatures, Corros. Sci., 5, 333, 10.1016/S0010-938X(65)90500-7 · DOI
- Hanafi, 2009, The effect of water vapor on high temperature oxidation of Fe–Cr alloys at 1073K, Mater. Trans., JIM, 50, 2656, 10.2320/matertrans.M2009212 · DOI
- Essuman, 2007, Enhanced internal oxidation as trigger for breakaway oxidation of Fe–Cr alloys in gases containing water vapor, Scr. Mater., 57, 845, 10.1016/j.scriptamat.2007.06.058 · DOI
- Otsuka, 1989, Internal–external transition for the oxidation of Fe–Cr–Ni austenitic stainless steels in steam, Oxid. Met., 32, 13, 10.1007/BF00665267 · DOI
- Cheng, 2006, Effect of water vapor on annealing scale formation on 316 SS, Corros. Sci., 48, 634, 10.1016/j.corsci.2005.02.014 · DOI
- Ericsson, 1970, Stratified oxide scale growth on two Cr–Ni steels oxidized in high-pressure steam at 800°C, Oxid. Met., 2, 173, 10.1007/BF00603656 · DOI
- Peraldi, 2004, Effect of Cr and Ni contents on the oxidation behavior of ferritic and austenitic model alloys in air with water vapor, Oxid. Met., 61, 463, 10.1023/B:OXID.0000032334.75463.da · DOI · Paper page
- Oikawa, 1982, Review on lattice diffusion of substitutional impurities in iron. A summary report, Technol. Reports Tohoku Univ., 47, 215
- de Faria, 1997, Raman microspectroscopy of some iron oxides and oxyhydroxides, J. Raman Spectrosc., 28, 873, 10.1002/(SICI)1097-4555(199711)28:11<873::AID-JRS177>3.0.CO;2-B · DOI
- Setiawan, 2010, Oxygen permeability through internal oxidation zone in Fe–Cr alloys under dry and humid conditions at 973 and 1073K, ISIJ Int., 50, 259, 10.2355/isijinternational.50.259 · DOI
- Wagner, 1959, Reaction types during oxidation of alloys, Z. Electrochem., 63, 772
- M. Hanafi, PhD Thesis, Tokyo Institute of Technology, 2009.
- Swisher, 1967, Solubility, permeability, and diffusivity of oxygen in solid iron, Trans. Met. Soc. AIME, 239, 426
Cited by
Sorted by citations
Jonsson, T., Karlsson, S., Hooshyar, H., Sattari, M., Liske, J., Svensson, J.-E., & Johansson, L.-G. (2016) · Oxidation of Metals · doi:10.1007/s11085-016-9610-7 · Cited by 103 · see citing works
Eklund, J., Jönsson, B., Persdotter, A., Liske, J., Svensson, J.-E., & Jonsson, T. (2018) · Corrosion Science · doi:10.1016/j.corsci.2018.09.004 · Cited by 55 · see citing works
Persdotter, A., Eklund, J., Liske, J., & Jonsson, T. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108961 · Cited by 44 · see citing works
Jiang, C., Feng, M., Chen, M., Chen, K., Geng, S., & Wang, F. (2021) · Corrosion Science · doi:10.1016/j.corsci.2021.109484 · Cited by 42 · see citing works
Persdotter, A., Larsson, H., Eklund, J., Bigdeli, S., & Jonsson, T. (2024) · Corrosion Science · doi:10.1016/j.corsci.2024.112473 · Cited by 1 · see citing works
- Authors
- Liu, L., Yang, Z.-G., Zhang, C., Ueda, M., Kawamura, K., & Maruyama, T.
- Affiliations
- Tsinghua University (CN)
- Tokyo Institute of Technology (JP)
- Corresponding author
- Yang, Z.-G.
- Venue
- Corrosion Science
- Publisher
- Elsevier BV
- Published
- 2012-07
- Volume
- 60
- Pages
- 90-97
- ISSN
- 0010-938X (ISSN-L)
- OpenAlex
- W2041922549
- Cited by
- 28
- References
- 0
- Citations by year
- 2026: 1 · 2025: 2 · 2024: 4 · 2023: 1 · 2021: 2 · 2020: 2 · 2019: 2 · 2018: 3 · 2016: 2 · 2015: 3 · 2014: 3 · 2013: 3
- FWCI
- 4.84
- Type
- journal article
- Language
- en
- Open access
- closed
- Locations
- Corrosion Science (publishedVersion)
- Tokyo Tech Research Repository (Tokyo Institute of Technology) (submittedVersion)
- Funders
- National Natural Science Foundation of China
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Materials Science › Materials Chemistry › Nuclear Materials and Properties
- Physical Sciences › Materials Science › Metals and Alloys › Hydrogen embrittlement and corrosion behaviors in metals
- Keywords
- water vapor, high-temperature oxidation, duplex oxide scale, Fe2O3, magnetite
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›