Oxidation After Breakdown of the Chromium-Rich Scale on Stainless Steels at High Temperature: Internal Oxidation

Open access

Abstract

Breakaway oxidation of alloy 304L at 600 °C was studied in four environments (O2 + H2O + KCl, O2 + H2O + SO2 + KCl, H2 + H2O + Ar, O2 + K2CO3) for up to 168 h. The resulting scales were investigated by FIB/SEM, SEM/EDX, STEM/EELS, STEM/EDS and oxidation was elucidated by thermodynamic calculations (Thermo-Calc). The initial thin protective scale broke down in all cases. After breakaway, the scale consisted of two layers, i.e. an inward growing spinel/reaction zone and an outward growing iron-rich layer. The general features and microstructure of the scales after breakaway were similar in all environments and were explained in terms of: (1) Different diffusivities of Cr3+ and Fe2+ in the spinel oxide. (2) The appearance of a miscibility gap in the FeCr and FeCrNi spinel oxides. (3) The equilibrium composition of the spinel (at low pO2 Ni is not present in the spinel).

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1007/s11085-016-9610-7

Cites

42 of 42 references verified0 citation errors · 0 not checkable

Statistics

Figures

Image 1
CC-BY · From the PDF
Image 2
CC-BY · From the PDF
Image 3
CC-BY · From the PDF
Image 4
CC-BY · From the PDF
Fig. 5 a BSE image of a BIB cross-section through the oxide scale and into the alloy on the 304L (18Cr10Ni) samples exposed for 168 h at 600 ° C in 5%O2 ? 40%H2O ? KCl. A magnified image of the marked region close to the right hand side of the micrograph is shown in ( b ) and the SEM/EDX elemental maps from the central marked region is shown in ( d ). b BSE image of the marked area in ( a ). The inward growing oxide scale can be divided into darker areas (fully oxidized regions) and brighter areas , i.e. mixed oxide and metal (reaction zone). A TEM sample was taken from a similar region as indicated in the marked region. c HAADF image of a region similar to the marked region in ( b ). The inward growing oxide scale can be divided into a region of mixed oxide and metal, i.e. a reaction zone, and darker fully oxidized regions. At the alloy grain boundary a Fe-Cr oxide could be found. CBED patterns from the oxides are inseted in the image. The oxide at the grain boundary was indexed as a spinel structure (M3O4) with the zone axis [001] (i). The small oxide precipitates were also indexed as a spinel structure (M3O4) with the zone axis [001] (ii). d SEM/EDX elemental maps from the marked area in ( a ) of the sample exposed for 168 h in 5%O2 ? 40%H2O ? KCl
Fig. 5 a BSE image of a BIB cross-section through the oxide scale and into the alloy on the 304L (18Cr10Ni) samples exposed for 168 h at 600 ° C in 5%O2 ? 40%H2O ? KCl. A magnified image of the marked region close to the right hand side of the micrograph is shown in ( b ) and the SEM/EDX elemental maps from the central marked region is shown in ( d ). b BSE image of the marked area in ( a ). The inward growing oxide scale can be divided into darker areas (fully oxidized regions) and brighter areas , i.e. mixed oxide and metal (reaction zone). A TEM sample was taken from a similar region as indicated in the marked region. c HAADF image of a region similar to the marked region in ( b ). The inward growing oxide scale can be divided into a region of mixed oxide and metal, i.e. a reaction zone, and darker fully oxidized regions. At the alloy grain boundary a Fe-Cr oxide could be found. CBED patterns from the oxides are inseted in the image. The oxide at the grain boundary was indexed as a spinel structure (M3O4) with the zone axis [001] (i). The small oxide precipitates were also indexed as a spinel structure (M3O4) with the zone axis [001] (ii). d SEM/EDX elemental maps from the marked area in ( a ) of the sample exposed for 168 h in 5%O2 ? 40%H2O ? KClCC-BY · From the PDF
Fig. 5 continued
Fig. 5 continuedCC-BY · From the PDF
Fig. 6 a BSE image of a BIB cross-section of the 304L (18Cr-10Ni) sample exposed for 168 h in presence of SO2 at 600 ° C in 5%O2 ? 40% H2O ? KCl. The marked area is shown in higher magnification in ( b , c ). b , c HAADF image of a region similar to the marked region in ( a ). The inward growing oxide scale can be divided into a region of mixed oxide and metal, i.e. a reaction zone, and darker fully oxidized regions. c The marked region in ( b ) shown with higher magnification
Fig. 6 a BSE image of a BIB cross-section of the 304L (18Cr-10Ni) sample exposed for 168 h in presence of SO2 at 600 ° C in 5%O2 ? 40% H2O ? KCl. The marked area is shown in higher magnification in ( b , c ). b , c HAADF image of a region similar to the marked region in ( a ). The inward growing oxide scale can be divided into a region of mixed oxide and metal, i.e. a reaction zone, and darker fully oxidized regions. c The marked region in ( b ) shown with higher magnificationCC-BY · From the PDF
Fig. 7 a BSE image of a polished cross-section of the 304L (18Cr-8Ni) sample exposed for 72 h in 10%H2-20%H2O-Ar. The marked areas are shown in higher magnification in b , c . b HAADF image of a region similar to the marked area in ( a ). The inward growing oxide scale can be divided into a region of mixed oxide and metal, i.e. a reaction zone, and darker fully oxidized regions. c The marked region in ( a ) covering an alloy grain boundary region shown with higher magnification
Fig. 7 a BSE image of a polished cross-section of the 304L (18Cr-8Ni) sample exposed for 72 h in 10%H2-20%H2O-Ar. The marked areas are shown in higher magnification in b , c . b HAADF image of a region similar to the marked area in ( a ). The inward growing oxide scale can be divided into a region of mixed oxide and metal, i.e. a reaction zone, and darker fully oxidized regions. c The marked region in ( a ) covering an alloy grain boundary region shown with higher magnificationCC-BY · From the PDF
Fig. 8 BSE image of an ion milled cross-section of the 304L (18Cr-10Ni) sample exposed for 168 h at 600 ° C in O2 ? K2CO3. The scale can be divided into an outward growing part consisting of iron oxide and an inward growing more complex oxide (FeCrNi oxide)
Fig. 8 BSE image of an ion milled cross-section of the 304L (18Cr-10Ni) sample exposed for 168 h at 600 ° C in O2 ? K2CO3. The scale can be divided into an outward growing part consisting of iron oxide and an inward growing more complex oxide (FeCrNi oxide)CC-BY · From the PDF
Fig. 9 Oxygen activity versus mole fraction of all components of 304L alloy (18-10) in the spinel type structure (M3O4) at 600 ° C calculated using the THERMO-CALC program with the database TCFE7
Fig. 9 Oxygen activity versus mole fraction of all components of 304L alloy (18-10) in the spinel type structure (M3O4) at 600 ° C calculated using the THERMO-CALC program with the database TCFE7CC-BY · From the PDF
Fig. 10 A schematic drawing summarizing the different stages of propagation following breakaway oxidation of Fe, Cr, (Ni) alloys in both high and low PO2. First stage of propagation after breakaway: (high PO2 environments) the new scale formed immediately below the original metal/oxide interface is always fully oxidized, consisting of FeCrNi spinel. (low PO2 environments) Ni 2 ? did not enter the corresponding ''first inward oxide layer'' and internal oxidation is promoted. After longer exposure times the composition of the internal oxide (RZ) is similar in all environments studied and on both 304L grades
Fig. 10 A schematic drawing summarizing the different stages of propagation following breakaway oxidation of Fe, Cr, (Ni) alloys in both high and low PO2. First stage of propagation after breakaway: (high PO2 environments) the new scale formed immediately below the original metal/oxide interface is always fully oxidized, consisting of FeCrNi spinel. (low PO2 environments) Ni 2 ? did not enter the corresponding ''first inward oxide layer'' and internal oxidation is promoted. After longer exposure times the composition of the internal oxide (RZ) is similar in all environments studied and on both 304L gradesCC-BY · From the PDF

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

2 more claims about this paper

Create a free account to see every claim other papers make about this one.

See all claims — free account

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 43 references

Research works printed but not linked: 2

  1. H. Asteman, J.-E. Svensson, M. Norell and L.-G. Johansson, Oxidition of Metals 54, 11 (2000). · DOI · Paper page
  2. B. Pujilaksono, T. Jonsson, H. Heidari, M. Halvarsson, J. E. Svensson and L. G. Johansson, Oxidation of Metals 75, 183 (2011). · DOI · Paper page

Cited by

See all 110

Metadata

Authors
Jonsson, T., Karlsson, S., Hooshyar, H., Sattari, M., Liske, J., Svensson, J.-E., & Johansson, L.-G.
Affiliations
Chalmers University of Technology (SE)
Corresponding author
Jonsson, T.
Venue
Oxidation of Metals
Published
2016-01-20
Volume
85
Issue
5-6
Pages
509-536
ISSN
  • 0030-770X (ISSN-L)
  • 1573-4889
OpenAlex
W2287046081
Cited by
103
References
43
Citations by year
2026: 16 · 2025: 10 · 2024: 9 · 2023: 7 · 2022: 7 · 2021: 11 · 2020: 12 · 2019: 9 · 2018: 12 · 2017: 6 · 2016: 4
FWCI
12.62
Type
journal article
Language
en
Open access
Locations
  • Oxidation of Metals (publishedVersion, cc-by)
  • Chalmers Research (Chalmers University of Technology) (submittedVersion)
Funders
Chalmers Tekniska Högskola
Topics
  • Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
  • Physical Sciences › Materials Science › Metals and Alloys › Hydrogen embrittlement and corrosion behaviors in metals
  • Physical Sciences › Materials Science › Materials Chemistry › Advancements in Solid Oxide Fuel Cells
Keywords
breakaway oxidation, internal oxidation, high-temperature oxidation, spinel oxides, miscibility gap, scale microstructure, thermodynamic calculation

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Oxidation After Breakdown of the Chromium-Rich Scale on Stainless Steels at High Temperature: Internal Oxidation. https://app.cochat.ai/papers/10.1007/s11085-016-9610-7
The paper
Jonsson, T., Karlsson, S., Hooshyar, H., Sattari, M., Liske, J., Svensson, J.-E., & Johansson, L.-G. (2016). Oxidation After Breakdown of the Chromium-Rich Scale on Stainless Steels at High Temperature: Internal Oxidation. Oxidation of Metals. https://doi.org/10.1007/s11085-016-9610-7

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.