Achieving high strength and high electrical conductivity in Cu-Cr-Zr alloy by modifying shear banding during rolling
The DOI matches its Crossref record; the references it cites are not checked yet.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
The citation lists haven’t been fetched yet
Cited by 42
Research works printed but not linked: 25
- Lu, 2004, Ultrahigh strength and gigh electrical conductivity in copper, Science, 304, 422, 10.1126/science.1092905 · DOI · Paper page
- Han, 2021, Alloy design strategies to increase strength and its trade-offs together, Prog. Mater. Sci., 117, 10.1016/j.pmatsci.2020.100720 · DOI
- Lai, 2022, Heterogeneous microstructure enables a synergy of strength, ductility and electrical conductivity in copper alloys, J. Alloy. Compd., 902, 10.1016/j.jallcom.2022.163646 · DOI · Paper page
- Li, 2021, Study on the variation of properties of Cu–Cr–Zr alloy by different rolling and aging sequence, Mater. Sci. Eng., A, 802, 10.1016/j.msea.2020.140413 · doi:10.1016/j.msea.2020.140413
- Li, 2021, Microstructure evolution and properties of a Cu–Cr–Zr alloy with high strength and high conductivity, Mater. Sci. Eng., A, 819, 10.1016/j.msea.2021.141464 · doi:10.1016/j.msea.2021.141464
- Cheng, 2014, Solute clusters and chemistry in a Cu–Cr–Zr–Mg alloy during the early stage of aging, Mater. Lett., 115, 201, 10.1016/j.matlet.2013.10.055 · doi:10.1016/j.matlet.2013.10.055
- Wang, 2022, Effects of Si addition on properties and microstructure of CuCrZr, Alloy., J. Alloy. Compd., 906
- Pang, 2014, Effects of Zr and (Ni, Si) additions on properties and microstructure of Cu-Cr, Alloy., J. Alloy. Compd., 582, 786, 10.1016/j.jallcom.2013.08.146 · doi:10.1016/j.jallcom.2013.08.146
- Huang, 2019, Optimizing the strength, ductility and electrical conductivity of a Cu-Cr-Zr alloy by rotary swaging and aging treatment, Mater. Sci. Eng., A, 746, 211, 10.1016/j.msea.2019.01.002 · doi:10.1016/j.msea.2019.01.002
- Hatakeyama, 2008, Nanostructural evolution of Cr-rich precipitates in a Cu-Cr-Zr alloy during heat treatment studied by 3 dimensional atom probe, Mater. Trans., 49, 518, 10.2320/matertrans.MBW200736 · doi:10.2320/matertrans.mbw200736
- Chen, 2019, Contribution of Zr to strength and grain refinement in CuCrZr alloy, Mater. Sci. Eng., A, 756, 464, 10.1016/j.msea.2019.04.053 · doi:10.1016/j.msea.2019.04.053
- Wang, 2018, Retaining meta-stable fcc-Cr phase by restraining nucleation of equilibrium bcc-Cr phase in CuCrZrTi, Alloy. Ageing, J. Alloy. Compd., 749, 140, 10.1016/j.jallcom.2018.03.238 · doi:10.1016/j.jallcom.2018.03.238
- Shangina, 2017, Effect of chromium and zirconium content on structure, strength and electrical conductivity of Cu-Cr-Zr alloys after high pressure torsion, Mater. Lett., 199, 46, 10.1016/j.matlet.2017.04.039 · doi:10.1016/j.matlet.2017.04.039
- Zhang, 2017, A high strength and high electrical conductivity Cu-Cr-Zr alloy fabricated by cryorolling and intermediate aging treatment, Mater. Sci. Eng., A, 680, 108, 10.1016/j.msea.2016.10.087 · DOI · Paper page
- Wang, 2022, Improved strength with good conductivity in Cu–Cr–Zr alloys: determinant effect of under-aging treatment before rolling and aging, Mater. Sci. Eng., A, 848, 10.1016/j.msea.2022.143395 · doi:10.1016/j.msea.2022.143395
- Wang, 2022, Nucleation and growth of nanoscale precipitates and the effect on properties during secondary isothermal aging in thin-band of Cu-0.8Cr-0.1Zr alloy, Materialia, 23, 10.1016/j.mtla.2022.101452 · doi:10.1016/j.mtla.2022.101452
- Purcek, 2016, Optimization of strength, ductility and electrical conductivity of Cu-Cr-Zr alloy by combining multi-route ECAP and aging, Mater. Sci. Eng., A, 649, 114, 10.1016/j.msea.2015.09.111 · DOI
- Yan, 2021, Shear localization in metallic materials at high strain rates, Prog. Mater. Sci., 119, 10.1016/j.pmatsci.2020.100755 · DOI · Paper page
- Boakye Yiadom, 2014, Effect of microstructure on the nucleation and initiation of adiabatic shear bands (ASBs) during impact, Mater. Sci. Eng., A, 615, 373, 10.1016/j.msea.2014.07.095 · doi:10.1016/j.msea.2014.07.095
- Xie, 2021, Microstructural evolution and strengthening mechanisms in cold-rolled Cu–Ag alloys, J. Alloy. Compd., 851, 10.1016/j.jallcom.2020.156893 · doi:10.1016/j.jallcom.2020.156893
- Williamson, 1956, III. Dislocation densities in some annealed and cold-worked metals from measurements on the X-ray debye-scherrer spectrum, Philos. Mag., 1, 34, 10.1080/14786435608238074 · DOI · Paper page
- Li, 2019, The roles of Hf element in optimizing strength, ductility and electrical conductivity of copper alloys, Mater. Sci. Eng., A, 758, 130, 10.1016/j.msea.2019.04.110 · DOI
- Zhu, 2023, Heterostructured materials, Prog. Mater. Sci., 131, 10.1016/j.pmatsci.2022.101019 · DOI · Paper page
- Wang, 2019, Heterostructure induced dispersive shear bands in heterostructured Cu, Scr. Mater., 170, 76, 10.1016/j.scriptamat.2019.05.036 · doi:10.1016/j.scriptamat.2019.05.036
- Wang, 2022, Activating dispersed strain bands in tensioned nanostructure layer for high ductility: the effects of microstructure inhomogeneity, Int. J. Plast., 149, 10.1016/j.ijplas.2021.103159 · doi:10.1016/j.ijplas.2021.103159
Metadata
- Authors
- Lai, Z., Peng, K., Gao, B., Mai, Y., & Jie, X.
- Venue
- Journal of Alloys and Compounds
- Publisher
- Elsevier BV
- Published
- 2023-10
- Volume
- 958
- Pages
- 170402
- ISSN
- 0925-8388
- Cited by
- 42
- Language
- en
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- www.elsevier.com/legal/tdmrep-license (tdm)
- doi.org/10.15223/policy-017 (stm-asf)
- doi.org/10.15223/policy-037 (stm-asf)
- doi.org/10.15223/policy-012 (stm-asf)
- doi.org/10.15223/policy-029 (stm-asf)
- doi.org/10.15223/policy-004 (stm-asf)
- Funders
- Guangzhou Municipal Science and Technology Project (201904010406)
- Guangdong University of Technology
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Achieving high strength and high electrical conductivity in Cu-Cr-Zr alloy by modifying shear banding during rolling. https://app.cochat.ai/papers/10.1016/j.jallcom.2023.170402
- The paper
- Lai, Z., Peng, K., Gao, B., Mai, Y., & Jie, X. (2023). Achieving high strength and high electrical conductivity in Cu-Cr-Zr alloy by modifying shear banding during rolling. Journal of Alloys and Compounds. https://doi.org/10.1016/j.jallcom.2023.170402
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.