Use of XPS in the determination of chemical environment and oxidation state of iron and sulfur samples: constitution of a data basis in binding energies for Fe and S reference compounds and applications to the evidence of surface species of an oxidized pyrite in a carbonate medium
The DOI matches its Crossref record; 22 of the 22 references it cites were found in a registry or an index.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Iron oxides in the laboratory: preparation and characterization
(1992) · Choice Reviews Online · doi:10.5860/choice.29-2718 · Cited by 2,259
Acidic mine drainage: the rate-determining step
Singer, P. C., & Stumm, W. (1970) · Science · doi:10.1126/science.167.3921.1121 · Cited by 1,757
Mills, P., & Sullivan, J. L. (1983) · Journal of Physics D: Applied Physics · doi:10.1088/0022-3727/16/5/005 · Cited by 747
Brion, D. (1980) · Applications of Surface Science · doi:10.1016/0378-5963(80)90148-8 · Cited by 603
Oxidation of pyrite in low temperature acidic solutions: Rate laws and surface textures
McKibben, M. A., & Barnes, H. L. (1986) · Geochimica et Cosmochimica Acta · doi:10.1016/0016-7037(86)90325-x · Cited by 553
Evangelou, V. P. (. (2018) · CRC Press eBooks · doi:10.1201/9780203741641 · Cited by 493
An XPS characterization of FeCO3 films from CO2 corrosion
Heuer, J. K., & Stubbins, J. F. (1999) · Corrosion Science · doi:10.1016/s0010-938x(98)00180-2 · Cited by 470
Iron oxides in the laboratory, preparation and characterization
Burstein, G. T. (1992) · Corrosion Science · doi:10.1016/0010-938x(92)90174-2 · Cited by 390
Environmental Geochemistry of Sulfide Oxidation
(1993) · ACS Symposium Series · doi:10.1021/bk-1994-0550 · Cited by 376
Surface Oxidation of Pyrite as a Function of pH
Bonnissel-Gissinger, P., Alnot, M., Ehrhardt, J.-J., & Behra, P. (1998) · Environmental Science & Technology · doi:10.1021/es980213c · Cited by 336
Cited by
He, J., Luo, L., Chen, Y., & Manthiram, A. (2017) · Advanced Materials · doi:10.1002/adma.201702707 · Cited by 521
Iram, M., Guo, C., Guan, Y., Ishfaq, A., & Liu, H. (2010) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2010.05.119 · Cited by 518
Morel, A.-L., Nikitenko, S. I., Gionnet, K., Wattiaux, A., Lai-Kee-Him, J., Labrugere, C., Chevalier, B., Deleris, G., Petibois, C., Brisson, A., et al. (2008) · ACS Nano · doi:10.1021/nn800091q · Cited by 418
Surface reactivity of pyrite and related sulfides
MURPHY, R., & STRONGIN, D. (2009) · Surface Science Reports · doi:10.1016/j.surfrep.2008.09.002 · Cited by 383
Adsorption of sulfur dioxide on hematite and goethite particle surfaces
Baltrusaitis, J., Cwiertny, D. M., & Grassian, V. H. (2007) · Physical Chemistry Chemical Physics · doi:10.1039/b709167b · Cited by 337
Reductive sequestration of chromate by hierarchical FeS@Fe0 particles
Du, J., Bao, J., Lu, C., & Werner, D. (2016) · Water Research · doi:10.1016/j.watres.2016.06.009 · Cited by 337
Guo, L., Chen, F., Fan, X., Cai, W., & Zhang, J. (2010) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2010.02.015 · Cited by 316
Mortazavian, S., An, H., Chun, D., & Moon, J. (2018) · Chemical Engineering Journal · doi:10.1016/j.cej.2018.07.170 · Cited by 277
Revisiting the chemistry of graphite oxides and its effect on ammonia adsorption
Petit, C., Seredych, M., & Bandosz, T. J. (2009) · Journal of Materials Chemistry · doi:10.1039/b916672f · Cited by 269
Ganesan, P., Sivanantham, A., & Shanmugam, S. (2016) · Journal of Materials Chemistry A · doi:10.1039/c6ta04499a · Cited by 265
Chen, Z., Wang, Y., Xia, D., Jiang, X., Fu, D., Shen, L., Wang, H., & Li, Q. B. (2016) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2016.02.069 · Cited by 246
Zhao, J., He, Y., Wang, Y., Wang, W., Yan, L., & Luo, J. (2016) · Tribology International · doi:10.1016/j.triboint.2015.12.006 · Cited by 241
Pyrite dissolution in acidic media
Descostes, M., Vitorge, P., & Beaucaire, C. (2004) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2004.04.012 · Cited by 223
Self-citationPalanivel, B., Mudisoodum perumal, S. D., Maiyalagan, T., Jayarman, V., Ayyappan, C., & Alagiri, M. (2019) · Applied Surface Science · doi:10.1016/j.apsusc.2019.143807 · Cited by 216
Al-Anazi, A., Abdelraheem, W. H., Han, C., Nadagouda, M. N., Sygellou, L., Arfanis, M. K., Falaras, P., Sharma, V. K., & Dionysiou, D. D. (2018) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2017.08.054 · Cited by 202
Gong, L., Chng, X. Y. E., Du, Y., Xi, S., & Yeo, B. S. (2018) · ACS Catalysis · doi:10.1021/acscatal.7b03509 · Cited by 201
Fan, D., Anitori, R. P., Tebo, B. M., Tratnyek, P. G., Lezama Pacheco, J. S., Kukkadapu, R. K., Engelhard, M. H., Bowden, M. E., Kovarik, L., & Arey, B. W. (2013) · Environmental Science & Technology · doi:10.1021/es304829z · Cited by 201
Yan, S., Shi, Y., Tao, Y., & Zhang, H. (2019) · Chemical Engineering Journal · doi:10.1016/j.cej.2018.11.093 · Cited by 197
Treatment of Organic Compounds by Activated Persulfate Using Nanoscale Zerovalent Iron
Al-Shamsi, M. A., & Thomson, N. R. (2013) · Industrial & Engineering Chemistry Research · doi:10.1021/ie400387p · Cited by 194
Sun, H., Xie, G., He, D., & Zhang, L. (2020) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2019.118383 · Cited by 194
XPS and FTIR spectroscopic study on microwave treated high phosphorus iron ore
Omran, M., Fabritius, T., Elmahdy, A. M., Abdel-Khalek, N. A., El-Aref, M., & Elmanawi, A. E.-H. (2015) · Applied Surface Science · doi:10.1016/j.apsusc.2015.03.209 · Cited by 192
Grewe, T., Deng, X., Weidenthaler, C., Schüth, F., & Tüysüz, H. (2013) · Chemistry of Materials · doi:10.1021/cm403153u · Cited by 191
Candelaria, S. L., Bedford, N. M., Woehl, T. J., Rentz, N. S., Showalter, A. R., Pylypenko, S., Bunker, B. A., Lee, S., Reinhart, B., Ren, Y., et al. (2017) · ACS Catalysis · doi:10.1021/acscatal.6b02552 · Cited by 185
Pyrite Oxidation Mechanism by Oxygen in Aqueous Medium
Dos Santos, E. C., de Mendonça Silva, J. C., & Duarte, H. A. (2016) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.5b10949 · Cited by 177
Degradation of organic dyes by a new heterogeneous Fenton reagent - Fe2GeS4 nanoparticle
Shi, X., Tian, A., You, J., Yang, H., Wang, Y., & Xue, X. (2018) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2018.04.018 · Cited by 172
Jourshabani, M., Lee, B.-K., & Shariatinia, Z. (2020) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2020.119157 · Cited by 172
Wang, Y., Zhao, G., Chai, S., Zhao, H., & Wang, Y. (2013) · ACS Applied Materials & Interfaces · doi:10.1021/am302437a · Cited by 162
Persulfate activation by magnetic γ-Fe2O3/Mn3O4 nanocomposites for degradation of organic pollutants
Ma, Q., Zhang, X., Guo, R., Zhang, H., Cheng, Q., Xie, M., & Cheng, X. (2019) · Separation and Purification Technology · doi:10.1016/j.seppur.2018.06.060 · Cited by 162
Yao, T., Guo, S., Zeng, C., Wang, C., & Zhang, L. (2015) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2015.03.014 · Cited by 160
The role of sulfur-containing groups in ammonia retention on activated carbons
Petit, C., Kante, K., & Bandosz, T. J. (2010) · Carbon · doi:10.1016/j.carbon.2009.10.007 · Cited by 108
Tomatis, M., Turci, F., Ceschino, R., Riganti, C., Gazzano, E., Martra, G., Ghigo, D., & Fubini, B. (2010) · Inhalation Toxicology · doi:10.3109/08958378.2010.504243 · Cited by 53
Metadata
- Authors
- Descostes, M., Mercier, F., Thromat, N., Beaucaire, C., & Gautier-Soyer, M.
- Venue
- Applied Surface Science
- Publisher
- Elsevier BV
- Published
- 2000-10
- Volume
- 165
- Issue
- 4
- Pages
- 288-302
- ISSN
- 0169-4332 (ISSN-L)
- OpenAlex
- W1982335964
- Cited by
- 791
- References
- 22
- FWCI
- 3.36
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.