Abstract
Erosion of biodegradable parenteral delivery systems (PDS) based on ABA copolymers consisting of poly(L-lactide-co-glycolide) (PLGA) A-blocks attached to polyethylene oxide (PEO) B-blocks, or PLGA is important for the release of macromolecular drugs. The degradation behavior of four types of PDS, namely extruded rods, tablets, films and microspheres, was studied with respect to molecular weight, mass, polymer composition and shape and microstructure of the PDS. For each device the onset time of bulk erosion (t(on)) and the apparent rate of mass loss (k(app)) were calculated. In the case of PLGA, the t(on) was 16.2 days for microspheres, 19.2 days for films and 30.1 days for cylindrical implants and tablets. The k(app) was 0.04 days(-1) for microspheres, 0.09 days(-1) for films, 0.11 days(-1) for implants and 0.10 days(-1) for tablets. The degradation rates were in the same range irrespective of the geometry and the micrographs of eroding PDS demonstrated pore formation; therefore, a complex pore diffusion mechanism seems to control the erosion of PLGA devices. In contrast, PDS based on ABA copolymers showed swelling, followed by a parallel process of molecular weight degradation and polymer erosion, independent of the geometry. The contact angles of ABA films increased either with decreasing PEO content or with increasing chain length of the PEO B-blocks. In summary, the insertion of a hydrophilic B-block leads to an erosion controlled by degradation of ABA copolymers, wherea…
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“The ratio of surface area to volume has shown to be a significant factor for degradation of large devices. Higher surface area ratio leads to higher degradation of the matrix.”
From Poly Lactic-co-Glycolic Acid (PLGA) as Biodegradable Controlled Drug Delivery Carrier (2011) · cites this paper as [86]
Citations
Cites
Hydrolytic degradation of devices based on poly(DL-lactic acid) size-dependence
Grizzi, I., Garreau, H., Li, S., & Vert, M. (1995) · Biomaterials · doi:10.1016/0142-9612(95)93258-f · Cited by 895
Controlled Delivery Systems for Proteins Based on Poly(Lactic/Glycolic Acid) Microspheres
Cohen, S., Yoshioka, T., Lucarelli, M., Hwang, L. H., & Langer, R. (1991) · Pharmaceutical Research · doi:10.1023/a:1015841715384 · Cited by 843
Controlled release of bioactive agents from lactide/glycolide polymers
Lewis, D. H. (1990) · Drugs and the pharmaceutical sciences · Cited by 370
Erosion kinetics of hydrolytically degradable polymers.
Tamada, J. A., & Langer, R. (1993) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.90.2.552 · Cited by 356
Hagan, S. A., Coombes, A. G. A., Garnett, M. C., Dunn, S. E., Davies, M. C., Illum, L., Davis, S. S., Harding, S. E., Purkiss, S., & Gellert, P. R. (1996) · Langmuir · doi:10.1021/la950649v · Cited by 319
Further investigations on the hydrolytic degradation of poly (DL-lactide)
Li, S., & McCarthy, S. (1999) · Biomaterials · doi:10.1016/s0142-9612(97)00226-3 · Cited by 301
Preparation of biodegradable microspheres and microcapsules: 2. Polyactides and related polyesters
Arshady, R. (1991) · Journal of Controlled Release · doi:10.1016/0168-3659(91)90126-x · Cited by 258
Poly (glycolic acid-co-dl-lactic acid): diffusion or degradation controlled drug delivery?
Shah, S. S., Cha, Y., & Pitt, C. G. (1992) · Journal of Controlled Release · doi:10.1016/0168-3659(92)90171-m · Cited by 250
Göpferich, A. (1997) · Macromolecules · doi:10.1021/ma961627y · Cited by 245
Poly(lactide-co-glycolide) decomposition kinetics in vivo and in vitro
Kenley, R. A., Lee, M. O., Mahoney, T. R., & Sanders, L. M. (1987) · Macromolecules · doi:10.1021/ma00176a012 · Cited by 241
Cited by
Poly Lactic-co-Glycolic Acid (PLGA) as Biodegradable Controlled Drug Delivery Carrier
Makadia, H. K., & Siegel, S. J. (2011) · Polymers · doi:10.3390/polym3031377 · Cited by 4,816
“It has also been reported that bulk degradation is faster than pure surface degradation for PLGA, which makes the release of the drug faster from the devices with higher surface area to volume [82,86,87].”
BackgroundNovel crosslinking methods to design hydrogels
Hennink, W. E., & van Nostrum, C. F. (2002) · Advanced Drug Delivery Reviews · doi:10.1016/s0169-409x(01)00240-x · Cited by 1,962
Novel crosslinking methods to design hydrogels
Hennink, W. E., & van Nostrum, C. F. (2012) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2012.09.009 · Cited by 1,171
PLGA: a Unique Polymer for Drug Delivery
Kapoor, D. N., Bhatia, A., Kaur, R., Sharma, R., Kaur, G., & Dhawan, S. (2015) · Therapeutic Delivery · doi:10.4155/tde.14.91 · Cited by 609
Alexis, F. (2005) · Polymer International · doi:10.1002/pi.1697 · Cited by 443
Xu, Y., Kim, C., Saylor, D. M., & Koo, D. (2017) · Journal of Biomedical Materials Research Part B: Applied Biomaterials · doi:10.1002/jbm.b.33648 · Cited by 424
“Witt et al.(101) observed that as the surface-to-volume ratio increased, the onset time of erosion decreased in the rank order of rods (30 days)5 tablets (30 days)>films (19 days)>microspheres (16 days) and the rate of erosion decreased in the rank order of rods (0.”
BackgroundInfluentialKissel, T., Li, Y., & Unger, F. (2002) · Advanced Drug Delivery Reviews · doi:10.1016/s0169-409x(01)00244-7 · Cited by 332
Surface characteristics of PLA and PLGA films
Paragkumar N, T., Edith, D., & Six, J.-L. (2006) · Applied Surface Science · doi:10.1016/j.apsusc.2006.05.047 · Cited by 273
Zweers, M. L. T., Engbers, G. H. M., Grijpma, D. W., & Feijen, J. (2004) · Journal of Controlled Release · doi:10.1016/j.jconrel.2004.09.008 · Cited by 162
Modified biopolymer-dextrin based crosslinked hydrogels: application in controlled drug delivery
Das, D., & Pal, S. (2015) · RSC Advances · doi:10.1039/c4ra16103c · Cited by 162
Chen, Y., Zhou, S., & Li, Q. (2010) · Acta Biomaterialia · doi:10.1016/j.actbio.2010.09.038 · Cited by 172
“Thus, autocatalysis plays an important role in the degradation rate and erosion pathway, thereby making the design of synthetic biodegradable matrices size dependent [7–12].”
BackgroundAronin, C. E. P., Sadik, K. W., Lay, A. L., Rion, D. B., Tholpady, S. S., Ogle, R. C., & Botchwey, E. A. (2008) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.32015 · Cited by 97
Virto, M. R., Elorza, B., Torrado, S., Elorza, M., & Frutos, G. (2006) · Biomaterials · doi:10.1016/j.biomaterials.2006.09.045 · Cited by 83
In vitro degradation and erosion behavior of commercial PLGAs used for controlled drug delivery
Walker, J., Albert, J., Liang, D., Sun, J., Schutzman, R., Kumar, R., White, C., Beck‐Broichsitter, M., & Schwendeman, S. P. (2022) · Drug Delivery and Translational Research · doi:10.1007/s13346-022-01177-8 · Cited by 69
Stern, M., Ulrich, K., Geddes, D. M., & Alton, E. W. F. W. (2003) · Gene Therapy · doi:10.1038/sj.gt.3301994 · Cited by 62
Tsuji, H. (2010) · Wiley eBooks · doi:10.1002/9780470649848.ch21 · Cited by 67
The effect of mechanical loads on the degradation of aliphatic biodegradable polyesters
Li, Y., Chu, Z., Li, X., Ding, X., Guo, M., Zhao, H., Yao, J., Wang, L., Cai, Q., & Fan, Y. (2017) · Regenerative Biomaterials · doi:10.1093/rb/rbx009 · Cited by 60
“Similarly, Witt and Kissel [129] compared the degradation rates of microspheres, films, rods and tablets with different dimensions but the same material of PLGA 50/50, and the apparent constant rate of degradation were shown to be 0.”
BackgroundInfluentialSome insight into hydrolytic scission mechanisms in bioerodible polyesters
Alexis, F., Venkatraman, S. S., Rath, S. K., & Gan, L. (2006) · Journal of Applied Polymer Science · doi:10.1002/app.23888 · Cited by 69
In vitro ageing and degradation of PEG-PLA diblock copolymer-based nanoparticles
Stefani, M., Coudane, J., & Vert, M. (2006) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2006.05.009 · Cited by 52
Features of Anisotropic Drug Delivery Systems
Kudryavtseva, V., & Sukhorukov, G. B. (2024) · Advanced Materials · doi:10.1002/adma.202307675 · Cited by 55
Lu, D., Garcia‐Contreras, L., Xu, D., Kurtz, S. L., Liu, J., Braunstein, M., McMurray, D. N., & Hickey, A. J. (2007) · Pharmaceutical Research · doi:10.1007/s11095-007-9302-8 · Cited by 56
Nanomechanical properties of poly(lactic-co-glycolic) acid film during degradation
Shirazi, R. N., Aldabbagh, F., Erxleben, A., Rochev, Y. A., & McHugh, P. E. (2014) · Acta Biomaterialia · doi:10.1016/j.actbio.2014.08.004 · Cited by 61
Schöll, I., Boltz-Nitulescu, G., & Jensen-Jarolim, E. (2005) · Journal of Controlled Release · doi:10.1016/j.jconrel.2004.12.020 · Cited by 51
Wang, P., Zhuo, X., Chu, W., & Tang, X. (2017) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2017.05.069 · Cited by 53
“The drug release from Ms shows a tri-phasic pattern: Phase I is the initial burst release, Phase II is the platform period and Phase III is the terminal rapid release phase (Fredenberg et al., 2011; Kamaly et al., 2016; Luan and Bodmeier, 2006; Schwendeman et al., 2014; Vesna Milacic and Schwendeman, 2014; Witt and Ki…”
BackgroundMonte Carlo Simulation of Degradation of Porous Poly(lactide) Scaffolds, 1: Effect of Porosity on pH
Mohammadi, Y., & Jabbari, E. (2006) · Macromolecular Theory and Simulations · doi:10.1002/mats.200600036 · Cited by 51
Desai, K. G. H., Mallery, S. R., & Schwendeman, S. P. (2008) · European Journal of Pharmaceutics and Biopharmaceutics · doi:10.1016/j.ejpb.2008.03.007 · Cited by 58
Hydrolytic Degradation of Pluronic F127/Poly(lactic acid) Block Copolymer Nanoparticles
Xiong, X. Y., Tam, K. C., & Gan, L. H. (2004) · Macromolecules · doi:10.1021/ma049662p · Cited by 47
Phaechamud, T., Senarat, S., Puyathorn, N., & Praphanwittaya, P. (2018) · International Journal of Biological Macromolecules · doi:10.1016/j.ijbiomac.2018.11.098 · Cited by 40
Biophysical and Transfection Studies of an Amine-Modified Poly(vinyl alcohol) for Gene Delivery
Wittmar, M., Ellis, J. S., Morell, F., Unger, F. T., Schumacher, J. C., Roberts, C. J., Tendler, S. J. B., Davies, M. C., & Kissel, T. (2005) · Bioconjugate Chemistry · doi:10.1021/bc0500995 · Cited by 35
Shirazi, R. N., Ronan, W., Rochev, Y. A., & McHugh, P. E. (2015) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2015.08.030 · Cited by 37
“Some authors have studied the degradation rates for PLGA devices 200 μm to as small as 0.53 μm in size (Dunne et al., 2000; Grayson et al., 2005; Grizzi et al., 1995; Lu et al., 1999; Witt and Kissel, 2001).”
BackgroundInfluentialHo, M. J., Jeong, H. T., Im, S. H., Kim, H. T., Lee, J. E., Park, J. S., Cho, H. R., Kim, D. Y., Choi, Y. W., Lee, J. W., et al. (2019) · Pharmaceutics · doi:10.3390/pharmaceutics11080419 · Cited by 35
“Although there was marked difference in releas profile depending on the ratio of PLGA and PLA polymer, the drug release pattern f om novel drug microcrystals-loaded MSs were characterized by initial bu st r lease and subseq ent slow release profile, which is con istent with the typi al release pattern of PLGA/PLA base…”
BackgroundResultWittmar, M., Unger, F. T., & Kissel, T. (2006) · Macromolecules · doi:10.1021/ma051837n · Cited by 33
In vitro degradation of poly (D, L‐lactide‐co‐glycolide) nanoparticles loaded with linamarin
Hussein, A. S., Abdullah, N., & Fakhru’l‐Razi, A. (2013) · IET Nanobiotechnology · doi:10.1049/iet-nbt.2012.0012 · Cited by 35
Shen, Y., Wang, J., Li, Y., Tian, Y., Sun, H., Ouahab, A., Tu, J., Wang, B., & Sun, C. (2015) · RSC Advances · doi:10.1039/c5ra03085d · Cited by 31
Qodratnama, R., Serino, L. P., Cox, H. C., Qutachi, O., & White, L. J. (2014) · Materials Science and Engineering C · doi:10.1016/j.msec.2014.11.003 · Cited by 32
Milacic, V., & Schwendeman, S. P. (2013) · Pharmaceutical Research · doi:10.1007/s11095-013-1173-6 · Cited by 27
“Although the initial burst has been commonly thought to primarily occur from the lysozyme molecules released from the external surface and/or adjacent to the surface of the implants (13,17,18), data suggesting peptide and protein release from deep within the polymer from pores originating from preparation and/or initi…”
BackgroundQuaglia, F., Ostacolo, L., Nese, G., Rosa, G. D., Rotonda, M. I. L., Palumbo, R., & Maglio, G. (2005) · Macromolecular Bioscience · doi:10.1002/mabi.200500108 · Cited by 30
Wang, P., li, Y., & Jiang, M. (2018) · Colloids and Surfaces B Biointerfaces · doi:10.1016/j.colsurfb.2018.04.063 · Cited by 26
Polímeros usados como sistemas de transporte de princípios ativos
Severino, P. B., Santana, M. H. A., Malmonge, S. M., & Souto, E. B. (2011) · Polímeros · doi:10.1590/s0104-14282011005000061 · Cited by 38
Microspheres based on poly(3-hydroxy)butyrate for prolonged drug release
Livshits, V. A., Bonartsev, A. P., Иорданский, А. Л., Ivanov, E. A., Makhina, T. A., Мышкина, В. Л., & Bonartseva, G. A. (2009) · Polymer Science Series B · doi:10.1134/s1560090409070082 · Cited by 22
Protein release from dihydroxyacetone-based poly(carbonate ester) matrices
Weiser, J. R., Yueh, A., & Putnam, D. A. (2013) · Acta Biomaterialia · doi:10.1016/j.actbio.2013.05.020 · Cited by 24
van Dijkhuizen-Radersma, R., Roosma, J., Sohier, J., Péters, F. L. A. M. A., Doel, M., van Blitterswijk, C., de Groot, K., & Bezemer, J. M. (2004) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.30136 · Cited by 22
Biodegradable polymers: emerging excipients for the pharmaceutical and medical device industries
Patel, B. B., & Chakraborty, S. (2016) · International Journal of Pharmaceutical Excipients · doi:10.66617/001c.1010 · Cited by 23
RhBMP-2-Loaded PLGA/Titanium Nanotube Delivery System Synergistically Enhances Osseointegration
Zhang, Y., Hu, L., Lin, M. S., Cao, S., Feng, Y., & Sun, S. (2021) · ACS Omega · doi:10.1021/acsomega.1c00851 · Cited by 18
Tsuji, H. (2022) · Wiley eBooks · doi:10.1002/9781119767480.ch21 · Cited by 23
Terriza, A., Vilches-Pérez, J. I., de la Orden, E., Yubero, F., González-Caballero, J. L., González-Elipe, A. R., Vilches, J., & Salido, M. (2014) · BioMed Research International · doi:10.1155/2014/253590 · Cited by 16
Accelerated degradation testing impacts the degradation processes in 3D printed amorphous PLLA
Malone, L. P., Best, S. M., & Cameron, R. E. (2024) · Frontiers in Bioengineering and Biotechnology · doi:10.3389/fbioe.2024.1419654 · Cited by 18
Delivery Systems and Dosing for Antipsychotics
Rabin, C. R., & Siegel, S. J. (2012) · Handbook of experimental pharmacology · doi:10.1007/978-3-642-25761-2_11 · Cited by 18
“film) does not have a significant effect on release rate independent of surface area, it does affect the induction time for drug release (Witt and Kissel 2001; Witt et al. 2000).”
BackgroundMethodTorrés-Lagares, D., Castellanos‐Cosano, L., Serrera‐Figallo, M., García-García, F. J., López‐Santos, C., Barranco, Á., González-Elipe, A. R., Rivera-Jiménez, C., & Pérez, J. L. G. (2017) · Polymers · doi:10.3390/polym9090410 · Cited by 13
“5% dichloromethane was prepared by evaporation of the solvent on a Teflon plate for 48 h in air at room temperature obtaining a film of suitable consistency and a thickness of about 50 μm [16].”
MethodDegradation of Polymer Films on Surfaces: A Model Study with Poly(sebacic anhydride)
Deng, Z., Schweigerdt, A., Norow, A., & Lienkamp, K. (2019) · Macromolecular Chemistry and Physics · doi:10.1002/macp.201900121 · Cited by 11
Controlled-release implant system formulated using biodegradable hemostatic gauze as scaffold
Xu, L., Wu, F., Yuan, W., & Jin, T. (2007) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2007.12.019 · Cited by 11
Ehrenfried, L. M., Farrar, D. F., & Cameron, R. E. (2010) · Journal of The Royal Society Interface · doi:10.1098/rsif.2010.0014.focus · Cited by 9
“The formation of a porous surface of degrading polyester microspheres was also reported in the literature (Witt & Kissel 2001).”
BackgroundKumar, S., Singh, S., Quadir, S. S., Joshi, G., Chouhan, M., Puri, D., & Choudhary, D. K. (2024) · Elsevier eBooks · doi:10.1016/b978-0-443-18915-9.00004-5 · Cited by 11
Santoveña-Estévez, A., Fariña, J. B., Llabrés, M., Zhu, Y.-L., & Dannies, P. S. (2010) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2009.12.054 · Cited by 7
Caffeic Acid-PLGA Conjugate to Design Protein Drug Delivery Systems Stable to Irradiation
Selmin, F., Puoci, F., Parisi, O. I., Franzè, S., Musazzi, U. M., & Cilurzo, F. (2015) · Journal of Functional Biomaterials · doi:10.3390/jfb6010001 · Cited by 8
“For instance, Witt and Kissel observed that in the case of microspheres, the high surface to volume ratio led to a shorter onset time of erosion; meanwhile in the case of rods a bulk erosion kinetic was observed [14].”
BackgroundGadad, A. P., Vannuruswamy, G., Sharath Chandra, P., Dandagi, P. M., & Mastiholimath, V. S. (2012) · INDIAN DRUGS · doi:10.53879/id.49.12.p0005 · Cited by 11
Assali, M., Zaid, A. N., Bani-Odeh, M., Faroun, M., Muzaffar, R., & Sawalha, H. (2017) · International Journal of Polymeric Materials · doi:10.1080/00914037.2016.1263951 · Cited by 7
Antipsychotic Dosing and Drug Delivery
Rabin, C. R., & Siegel, S. J. (2010) · Current topics in behavioral neurosciences · doi:10.1007/7854_2010_46 · Cited by 8
“film) does not have a significant effect on release rate independent of surface area, it does affect the induction time for drug release (Witt and Kissel 2001; Witt et al. 2000).”
BackgroundMethodSchliecker, G., Schmidt, C., Fuchs, S., & Kissel, T. (2004) · Journal of Controlled Release · doi:10.1016/j.jconrel.2004.03.035 · Cited by 7
Cyclic Swelling as a Phenomenon Inherent to Biodegradable Polyesters
Dittrich, M., & Šnejdrová, E. (2014) · Journal of Pharmaceutical Sciences · doi:10.1002/jps.24146 · Cited by 6
Sibambo, S. R., Pillay, V., Choonara, Y. E., Khan, R. A., & Sweet, J. L. (2007) · Biomaterials · doi:10.1016/j.biomaterials.2007.04.045 · Cited by 5
Bunjes, H., & Kuntsche, J. (2016) · Advances in delivery science and technology · doi:10.1007/978-1-4939-4029-5_16 · Cited by 6
Applications of Nanometre Scale Particles as Pharmaceutical Delivery Vehicles in Medicine
Le, X. T., Poinern, G. E. J., Sadhasivam, S., & Fawcett, D. (2015) · Murdoch University Research Portal · Cited by 5
Mathematical Modeling of Polymer Biodegradation and Erosion
Chen, Y. H., & Li, Q. (2010) · Materials science forum · doi:10.4028/www.scientific.net/msf.654-656.2071 · Cited by 3
Du, H., Wang, L., Wu, X.-H., Liu, X.-A., Huo, M.-W., Huang, X., Shi, L.-Z., Liu, Y., Tang, M., Shi, L., et al. (2024) · Current Drug Delivery · doi:10.2174/0115672018302129240603052316 · Cited by 2
Ertan, G., Karasulu, E., Özgüney, I., Karasulu, H. Y., Apaydın, Ş., Kantarcı, G., Yurdasiper, A., & Ege, M. A. (2011) · European Journal of Drug Metabolism and Pharmacokinetics · doi:10.1007/s13318-011-0049-6 · Cited by 2
“…Pharmacy, Ege University, Bornova, 35100 Izmir, Turkey dosage forms (Harrison et al. 1993; Karasulu et al. 2003) and 1–5 months for some biodegradable implants containing antibiotics, antineoplastics, enzymes or antiinflammatories and etc. (Witt and Kissel 2001; Woo et al. 2001; Zhang et al. 2003).”
BackgroundWang, H., Roof, M., Burgher, K., Pham, C. V., Samuels, E. R., He, Y., Jian, H., & Wang, T. (2024) · Journal of Pharmaceutical Sciences · doi:10.1016/j.xphs.2024.08.028 · Cited by 1
Shu, Y., Pang, H., Wu, Y., Wang, Y., Huang, G., Zhang, C., & Han, F. Y. (2024) · Journal of Polymer Science · doi:10.1002/pol.20240238 · Cited by 3
Preparation of Microspheres and Incorporation of Lipid Hydroperoxide for Sustained Release Studies
Armstrong, D., Kimura, H., Tamai, K., Yasukawa, T., Afzal, M., & Browne, R. W. (2003) · Humana Press eBooks · doi:10.1385/1-59259-274-0:313 · Cited by 1
Biodegradable multiblock copolymers for drug delivery applications
van Dijkhuizen-Radersma, R. (2004) · University of Twente Research Information
Armentano, I., Latterini, L., Rescignano, N., Tarpani, L., Fortunati, E., & Kenny, J. M. (2015) · Wiley eBooks · doi:10.1002/9781119041450.ch17
Xiong, X. (2005) · DR-NTU (Nanyang Technological University) · doi:10.32657/10356/5426
Biodegradable ocular implant for sustained drug delivery
Peng, Y. (2011) · DR-NTU (Nanyang Technological University) · doi:10.32657/10356/50365
“This is in agreement with literature [94, 95] for similar types of biodegradable polymers.”
BackgroundResultProgramming Degradation and Drug Release Through Micropatterning of PLGA Films
Guerriero, I., Pesce, C., Spanò, R., Sganga, S., Tirelli, N., Palange, A. L., Mascolo, D. D., & Decuzzi, P. (2026) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.6c04044 · Cited by 2
Lin, Y., Wang, L., Lin, Y., Lv, J., Hu, H., Liu, A., Luo, Z., 贾赤宇, Wu, Y.-L., & Yang, B. (2026) · Precision medicine and engineering. · doi:10.1016/j.preme.2026.100082
Zhao, J., Pan, Y., Yang, S., Gao, M., & Zhang, J. (2026) · Journal of environmental chemical engineering · doi:10.1016/j.jece.2026.125375
Metadata
- Authors
- Witt, C.
- Affiliations
- Philipps University of Marburg (DE)
- Corresponding author
- Witt, C
- Venue
- European Journal of Pharmaceutics and Biopharmaceutics
- Publisher
- Elsevier BV
- Published
- 2001-05
- Volume
- 51
- Issue
- 3
- Pages
- 171-181
- ISSN
- 0939-6411 (ISSN-L)
- OpenAlex
- W2000124984
- Cited by
- 77
- References
- 28
- Citations by year
- 2026: 3 · 2024: 5 · 2023: 1 · 2022: 2 · 2021: 1 · 2019: 3 · 2018: 2 · 2017: 4 · 2016: 3 · 2015: 7 · 2014: 4 · 2013: 3 · 2012: 3
- FWCI
- 3.19
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- Locations
- European Journal of Pharmaceutics and Biopharmaceutics (publishedVersion)
- PubMed (publishedVersion)
- Topics
- Life Sciences › Pharmacology, Toxicology and Pharmaceutics › Pharmaceutical Science › Advanced Drug Delivery Systems
- Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
- Physical Sciences › Materials Science › Biomaterials › Nanoparticle-Based Drug Delivery
- Keywords
- poly(lactic-co-glycolic acid), ABA triblock copolymers, poly(ethylene oxide), bulk erosion, drug release, intraparticle diffusion, polymer swelling, molecular weight degradation, microspheres, cinema, implants, contact angle
- MeSH terms
- Biodegradation, Environmental, Diffusion, Microscopy, Electron, Scanning, Microspheres, Motion Pictures, Polyglactin 910, Prostheses and Implants
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.