Degradation Mechanism of Ni-Rich Cathode Materials: Focusing on Particle Interior
Abstract
In the development of Li-ion batteries for electric vehicles (EVs), Ni-rich layered oxides are anticipated to be promising cathode materials. However, the rapid capacity fading originating from microcracks has prevented practical applications of Ni-rich cathodes. Herein, we systematically perform post-mortem analyses of Li[Ni x Co y Mn 1- x - y ]O 2 ( x = 0.8 and 0.9) cathodes after long-term cycling, focusing on the particle interior. The results demonstrate that microcracks and the resultant degradation of the secondary particle interior by exposure to the deleterious electrolyte are dominant factors in the deterioration of Ni-rich cathodes. Moreover, cathode degradation significantly decreases the ionic and electrical conductivities, leading to the partial electrochemical insulation inside the cathode particles. This insulation contributes to the kinetic loss of capacity at high C-rates and induces structural inhomogeneity in the cathode. A comprehensive understanding of the degradation mechanism of Ni-rich cathodes suggests guidelines for developing Ni-rich cathode materials that are appropriate for application in EVs.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Commentary: The Materials Project: A materials genome approach to accelerating materials innovation
Jain, A., Ong, S. P., Hautier, G., Chen, W., Richards, W. D., Dacek, S., Cholia, S., Gunter, D., Skinner, D., Ceder, G., et al. (2013) · APL Materials · doi:10.1063/1.4812323 · Cited by 13,094
Ageing mechanisms in lithium-ion batteries
Vetter, J., Novák, P., Wagner, M. R., Veit, C., Möller, K.-C., Besenhard, J. O., Winter, M., Wohlfahrt-Mehrens, M., Vogler, C., & Hammouche, A. (2005) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.01.006 · Cited by 3,987
Noh, H.-J., Youn, S., Yoon, C. S., & Sun, Y.-K. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.01.063 · Cited by 2,302
Self-citationRyu, H.-H., Park, K.-J., Yoon, C. S., & Sun, Y.-K. (2018) · Chemistry of Materials · doi:10.1021/acs.chemmater.7b05269 · Cited by 1,629
Self-citationKondrakov, A. O., Schmidt, A., Xu, J., Geßwein, H., Mönig, R., Hartmann, P., Sommer, H., Brezesinski, T., & Janek, J. (2017) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.6b12885 · Cited by 701
Trevisanello, E., Rueß, R., Conforto, G., Richter, F. H., & Janek, J. (2021) · Advanced Energy Materials · doi:10.1002/aenm.202003400 · Cited by 542
Kim, U.-H., Park, G.-T., Son, B.-K., Nam, G. W., Liu, J., Kuo, L.-Y., Kaghazchi, P., Yoon, C. S., & Sun, Y.-K. (2020) · Nature Energy · doi:10.1038/s41560-020-00693-6 · Cited by 540
Self-citationBeyond Doping and Coating: Prospective Strategies for Stable High-Capacity Layered Ni-Rich Cathodes
Sun, H. H., Ryu, H.-H., Kim, U.-H., Weeks, J. A., Heller, A., Sun, Y.-K., & Mullins, C. B. (2020) · ACS Energy Letters · doi:10.1021/acsenergylett.0c00191 · Cited by 495
Self-citationWatanabe, S., Kinoshita, M., Hosokawa, T., Morigaki, K., & Nakura, K. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.02.018 · Cited by 465
Miller, D. J., Proff, C., Wen, J., Abraham, D. P., & Bareño, J. (2013) · Advanced Energy Materials · doi:10.1002/aenm.201300015 · Cited by 422
de Biasi, L., Kondrakov, A. O., Geßwein, H., Brezesinski, T., Hartmann, P., & Janek, J. (2017) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.7b06363 · Cited by 374
Kim, U., Ryu, H., Kim, J., Mücke, R., Kaghazchi, P., Yoon, C. S., & Sun, Y. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201803902 · Cited by 298
Self-citationA highly stabilized Ni-rich NCA cathode for high-energy lithium-ion batteries
Ryu, H.-H., Park, N.-Y., Seo, J. H., Yu, Y.-S., Sharma, M., Mücke, R., Kaghazchi, P., Yoon, C. S., & Sun, Y.-K. (2020) · Materials Today · doi:10.1016/j.mattod.2020.01.019 · Cited by 264
Self-citationLee, K.-S., Myung, S., Amine, K., Yashiro, H., & Sun, Y. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2769831 · Cited by 212
Self-citationKim, J.-H., Kim, S. J., Yuk, T., et al. (2018) · ACS Energy Letters · doi:10.1021/acsenergylett.8b02043 · Cited by 117
Self-citationStabilization of a Highly Ni-Rich Layered Oxide Cathode through Flower-Petal Grain Arrays
Sun, H. H., Dolocan, A., Weeks, J. A., Heller, A., & Mullins, C. B. (2020) · ACS Nano · doi:10.1021/acsnano.0c06910 · Cited by 90
Rathore, D., Geng, C., Zaker, N., Hamam, I., Liu, Y., Xiao, P., Botton, G. A., Dahn, J. R., & Yang, C. (2021) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac3c26 · Cited by 66
Nanorod Gradient Cathode: Preventing Electrolyte Penetration into Cathode Particles
Sun, H. H., Weeks, J. A., Heller, A., & Mullins, C. B. (2019) · ACS Applied Energy Materials · doi:10.1021/acsaem.9b01116 · Cited by 60
Cited by
Wang, J., Li, D., Zeng, W., Chen, X., Zhang, Y., Zhang, S., Li, Z., Li, C., & Mu, S. (2025) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2024.11.016 · Cited by 62
Metadata
- Authors
- Park, N.-Y., Park, G.-T., Kim, S.-B., Jung, W., Park, B.-C., & Sun, Y.-K.
- Venue
- ACS Energy Letters
- Publisher
- American Chemical Society (ACS)
- Published
- 2022-06-23
- Volume
- 7
- Issue
- 7
- Pages
- 2362-2369
- ISSN
- 2380-8195 (ISSN-L)
- OpenAlex
- W4283359282
- Cited by
- 296
- References
- 18
- FWCI
- 15.93
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.