Electrode Degradation in Lithium-Ion Batteries
Open accessThe DOI matches its Crossref record; 418 of the 422 references it cites were found in a registry or an index.
Abstract
Although Li-ion batteries have emerged as the battery of choice for electric vehicles and large-scale smart grids, significant research efforts are devoted to identifying materials that offer higher energy density, longer cycle life, lower cost, and/or improved safety compared to those of conventional Li-ion batteries based on intercalation electrodes. By moving beyond intercalation chemistry, gravimetric capacities that are 2–5 times higher than that of conventional intercalation materials (e.g., LiCoO2 and graphite) can be achieved. The transition to higher-capacity electrode materials in commercial applications is complicated by several factors. This Review highlights the developments of electrode materials and characterization tools for rechargeable lithium-ion batteries, with a focus on the structural and electrochemical degradation mechanisms that plague these systems.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Sophisticated chemical reactions can result in material loss and structural deformation, causing capacity decrement and resistance increment [3,4].”
From State‐of‐health estimation of lithium‐ion batteries: A comprehensive literature review from cell to pack levels (2024) · cites this paper as [4]
Citations
Cites
Issues and challenges facing rechargeable lithium batteries
Tarascon, J.-M., & Armand, M. (2001) · Nature · doi:10.1038/35104644 · Cited by 21,130
Armand, M., & Tarascon, J.-M. (2008) · Nature · doi:10.1038/451652a · Cited by 19,612
The Li-Ion Rechargeable Battery: A Perspective
Goodenough, J. B., & Park, K.-S. (2013) · Journal of the American Chemical Society · doi:10.1021/ja3091438 · Cited by 9,962
Li-O2 and Li-S batteries with high energy storage
Bruce, P. G., Freunberger, S. A., Hardwick, L. J., & Tarascon, J.-M. (2012) · Nature Materials · doi:10.1038/nmat3191 · Cited by 9,479
Nano-sized transition-metal oxides as negative-electrode materials for lithium-ion batteries
Poizot, P., Laruelle, S., Grugeon, S., Dupont, L., & Tarascon, J.-M. (2000) · Nature · doi:10.1038/35035045 · Cited by 8,041
Phospho‐olivines as Positive‐Electrode Materials for Rechargeable Lithium Batteries
Padhi, A. K., Nanjundaswamy, K. S., & Goodenough, J. B. (1997) · Journal of The Electrochemical Society · doi:10.1149/1.1837571 · Cited by 7,933
Reviving the lithium metal anode for high-energy batteries
Lin, D., Liu, Y., & Cui, Y. (2017) · Nature Nanotechnology · doi:10.1038/nnano.2017.16 · Cited by 6,763
High-performance lithium battery anodes using silicon nanowires
Chan, C. K., Peng, H., Liu, G., McIlwrath, K., Zhang, X. F., Huggins, R. A., & Cui, Y. (2008) · Nature Nanotechnology · doi:10.1038/nnano.2007.411 · Cited by 6,683
Lithium Batteries and Cathode Materials
Whittingham, M. S. (2004) · Chemical Reviews · doi:10.1021/cr020731c · Cited by 6,267
A highly ordered nanostructured carbon–sulphur cathode for lithium–sulphur batteries
Ji, X., Lee, K. T., & Nazar, L. F. (2009) · Nature Materials · doi:10.1038/nmat2460 · Cited by 5,988
Research works printed but not linked: 8
- Li, 2016, Origins of Large Voltage Hysteresis in High-Energy-Density Metal Fluoride Lithium-Ion Battery Conversion Electrodes, J. Am. Chem. Soc., 138, 2838, 10.1021/jacs.6b00061 · DOI · Paper page
- Danuta, 1975, Chemical Investigations of Lithium-Sulfur Cells, 186
- Tan, 2016, Core–Shell Nano-FeS2@N-Doped Graphene as an Advanced Cathode Material for Rechargeable Li-Ion Batteries, Chem. Commun., 52, 986, 10.1039/c5cc08002a · DOI
- Demirocak, 2016, Probing the Aging Effects on Nanomechanical Properties of a Thin Film LiFePO4 Cathode, ECS Trans., 73, 57, 10.1149/07301.0057ecst · DOI
- Zhao, 2015, Rechargeable Lithium-Iodine Batteries with Iodine/Nanoporous Carbon Cathode, Nano Lett., 15, 5982, 10.1021/acs.nanolett.5b02116 · DOI · Paper page
- Meng, 2018, Polyiodide-Shuttle Restricting Polymer Cathode for Rechargeable Lithium/Iodine Battery with Ultralong Cycle Life, ACS Appl. Mater. Interfaces, 10, 17933, 10.1021/acsami.8b03212 · DOI
- Arora, 2004, Battery Separators, Chem. Rev., 104, 4419, 10.1021/cr020738u · DOI · Paper page
- Lee, 2015, Fracture of Crystalline Germanium during Electrochemical Lithium Insertion, Extrem. Mech. Lett., 2, 15, 10.1016/j.eml.2015.01.009 · DOI
Cited by
Items 101–200 of 891
Pandya, R., Valzania, L., Dorchies, F., Xia, F., Hugh, J. M., Mathieson, A., Tan, H. J., Parton, T. G., Godeffroy, L., Mazloomian, K., et al. (2023) · Nature Nanotechnology · doi:10.1038/s41565-023-01466-4 · Cited by 71
“Propagat-ing the uncertainty in L to one in volume (Supplementary Notes 3 and 4) suggests that changes in the particle volume below ~1.0–1.5% are challenging to unambiguously detect with optical microscopy.”
InfluentialTreatment and recycling of spent lithium-based batteries: a review
Al‐Asheh, S., Aidan, A., Allawi, T., Hammoud, F., Ali, H. A., & Khamiri, M. A. (2023) · Journal of Material Cycles and Waste Management · doi:10.1007/s10163-023-01842-1 · Cited by 75
“For graphite anodes, the majority of the SEI production takes place during the first cycle, which typically results in an irreversible capacity loss of 10% or less [26].”
A Review of Experimental and Numerical Studies of Lithium Ion Battery Fires
Ghiji, M., Edmonds, S., & Moinuddin, K. (2021) · Applied Sciences · doi:10.3390/app11031247 · Cited by 73
A unique co-recovery strategy of cathode and anode from spent LiFePO4 battery
Du, K., Meng, Y., Zhao, X.-X., Wang, X., Luo, X., Zhang, W., & Wu, X. (2021) · Science China Materials · doi:10.1007/s40843-021-1772-6 · Cited by 70
Zhao, G., Mei, Z., Duan, L., An, Q., Yang, Y., Zhang, C., Tan, X., & Guo, H. (2022) · Carbon Energy · doi:10.1002/cey2.248 · Cited by 73
Heo, J., Jung, S., Hwang, I., Cho, S., Eum, D., Park, H., Song, J., Yu, S., Oh, K., Kwon, G., et al. (2022) · Nature Energy · doi:10.1038/s41560-022-01148-w · Cited by 68
Advancements in the development of nanomaterials for lithium-ion batteries: A scientometric review
Poorshakoor, E., & Darab, M. (2023) · Journal of Energy Storage · doi:10.1016/j.est.2023.109638 · Cited by 74
Qiao, D., Wei, X., Zhu, J., Zhang, G., Yang, S., Wang, X., Jiang, B., Lai, X., Zheng, Y., & Dai, H. (2025) · eTransportation · doi:10.1016/j.etran.2025.100450 · Cited by 83
Nazir, G., Rehman, A., Hussain, S., Ikram, M., & Park, S. (2022) · International Journal of Energy Research · doi:10.1002/er.8256 · Cited by 67
“Based on their electrochemical performances, batteries demonstrate high energy density; however low power density accompanied by a short lifetime and unstable cyclic stability over long cycles is observed which is ascribed to physiochemical reactions that occur during the charging/discharging process.(10,11) In additi…”
BackgroundSynthetic Methods and Applications of Carbon Nanodots
Banger, A., Gautam, S., Jadoun, S., Jangid, N. K., Srivastava, A., Pulidindi, I. N., Dwivedi, J., & Srivastava, M. C. (2023) · Catalysts · doi:10.3390/catal13050858 · Cited by 74
Tan, X., Chen, M., Zhang, J., Li, S., Zhang, H., Yang, L., Sun, T. S., Qian, X., & Feng, G. (2024) · Advanced Energy Materials · doi:10.1002/aenm.202400564 · Cited by 72
Sulfur-doped graphene promoted Li4Ti5O12@C nanocrystals for lithium-ion batteries
Huang, Z., Luo, P., Zheng, H., & Lyu, Z. (2022) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2022.164599 · Cited by 64
Recent advances in NASICON-type oxide electrolytes for solid-state sodium-ion rechargeable batteries
Singh, K., Chakraborty, A., Thirupathi, R., & Omar, S. (2022) · Ionics · doi:10.1007/s11581-022-04765-3 · Cited by 64
A self-healing liquid metal anode for lithium-ion batteries
Qi, Y., Shen, C., Hou, Q., Ren, Z., Jin, T., & Xie, K. (2022) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2022.05.018 · Cited by 63
Li, J., Zhong, W., Deng, Q., Zhang, Q., & Yang, C. (2022) · International Journal of Extreme Manufacturing · doi:10.1088/2631-7990/ac92ef · Cited by 63
“Recently, layered LiNiO2 cathode materials have attracted many interests, as nickel is natural abundance in contrast to cobalt in the earth crust, and a LiNiO2 cathode shows higher capacity than LiCoO2 [5, 6].”
BackgroundInfluentialYu, J., Li, J., Zhang, S., Fan, W., Liu, Y., & Li, J. (2023) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.2217698120 · Cited by 73
“First of all, all spent LIBs need to be fully discharged in a 5% NaCl solution for 24 h to induce the lithium ions in the graphite anode to return to the cathode materials (39).”
MethodEmerging Processes for Sustainable Li‐Ion Battery Cathode Recycling
Bhattacharyya, S., Roy, S., & Vajtai, R. (2024) · Small · doi:10.1002/smll.202400557 · Cited by 65
Carbon coating of electrode materials for lithium-ion batteries
Yaroslavtsev, A. B., & Стенина, И. А. (2020) · Surface Innovations · doi:10.1680/jsuin.20.00044 · Cited by 62
Lee, H. B., Hoang, T. D., Byeon, Y. S., Jung, H., Moon, J., & Park, M. (2022) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.1c19443 · Cited by 62
Eldesoky, A., Bauer, M., Azam, S. M., Zsoldos, E. S., Song, W., Weber, R., Hy, S., Johnson, M. B., Metzger, M., & Dahn, J. R. (2021) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac39fc · Cited by 61
Nano and Battery Anode: A Review
Majdi, H. S., Латипов, З. А., Borisov, V. V., Yuryevna, N. O., Kadhim, M. M., Suksatan, W., Khlewee, I. H., & Kianfar, E. (2021) · Nanoscale Research Letters · doi:10.1186/s11671-021-03631-x · Cited by 60
“Figure 23 shows a number of exchangeable oxide anodes with their reaction and capacity [22, 30, 55].”
BackgroundA Paradox over Electric Vehicles, Mining of Lithium for Car Batteries
Luong, J. H. T., Tran, C., & Ton-That, D. (2022) · Energies · doi:10.3390/en15217997 · Cited by 68
Machine learning-inspired battery material innovation
Ng, M., Sun, Y., & Seh, Z. W. (2023) · Energy Advances · doi:10.1039/d3ya00040k · Cited by 68
Lin, J., Li, W., & Chen, Z. (2025) · ACS Energy Letters · doi:10.1021/acsenergylett.4c03176 · Cited by 66
Tang, L., Cheng, X., Wu, R. F., Cao, T., Lü, J., Zhang, Y., & Zhang, Z. (2021) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2021.07.021 · Cited by 58
Xu, W. M., Welty, C., Peterson, M. R., Read, J. A., & Stadie, N. P. (2022) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac4b87 · Cited by 58
Liu, J., Zhang, Y., Ji, H., Zhang, J., Zhou, P., Cao, Y., Zhou, J., Yan, C., & Qian, T. (2022) · Advanced Science · doi:10.1002/advs.202200390 · Cited by 57
Recycling of electrolyte from spent lithium-ion batteries
Mao, Z., Song, Y., Zhen, A., & Sun, W. (2024) · Next Sustainability · doi:10.1016/j.nxsust.2023.100015 · Cited by 64
Xing, C., Yao, M., & Fei, L. (2024) · Energy storage materials · doi:10.1016/j.ensm.2024.103636 · Cited by 57
Han, S. A., Suh, J. H., Park, M., & Kim, J. H. (2025) · Electrochemical Energy Reviews · doi:10.1007/s41918-025-00240-5 · Cited by 64
“For example, in thick graphite anodes, the formation of thick SEIs and non-uniform electrochemical reactions promote Li plating on graphite near the separator [57], which can cause short circuits that eventually lead to explosion and fire [58].”
Heugel, P., Märkle, W., Deich, T., von Kessel, O., & Tübke, J. (2022) · Journal of Energy Storage · doi:10.1016/j.est.2022.105101 · Cited by 59
Yang, T., Li, S., Wang, W., Lü, J., Fan, W., Zuo, X., & Nan, J. (2021) · Journal of Power Sources · doi:10.1016/j.jpowsour.2021.230055 · Cited by 57
Ibrahim, I. A., Zheng, S. Q., Foo, C. Y., Huang, N. M., & Lim, . N. (2021) · Journal of Energy Storage · doi:10.1016/j.est.2021.103304 · Cited by 56
Farahmandjou, M., Zhao, S., Lai, W., Sun, B., Notten, P. H. L., & Wang, G. (2022) · Nano Materials Science · doi:10.1016/j.nanoms.2022.03.004 · Cited by 55
Fu, X., Zhou, Y., Huang, J., Feng, L., Yu, P., Zhang, Q., Yang, W. M., & Wang, Y. (2023) · Advanced Energy Materials · doi:10.1002/aenm.202301385 · Cited by 55
Zhang, Y., Jiang, Q., Peng, L., Yuan, N., & Tang, J. (2020) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2020.156580 · Cited by 55
Two-dimensional (2D) materials for 3D printed micro-supercapacitors and micro-batteries
Saeed, G., Kang, T., Byun, J. S., Min, D., Kim, J. S., Sadavar, S. V., & Park, H. S. (2024) · Energy Materials · doi:10.20517/energymater.2023.81 · Cited by 57
Wei-xing, H., Gu, T., Xu, X., Zuo, S., Shen, J., Liu, J., & Zhu, M. H. (2022) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.2c11313 · Cited by 54
High entropy fluorides as conversion cathodes with tailorable electrochemical performance
Cui, Y., Sukkurji, P. A., Wang, K., Azmi, R., Nunn, A. M., Hahn, H., Breitung, B., Ting, Y., Kowalski, P. M., Kaghazchi, P., et al. (2022) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2022.05.032 · Cited by 56
Santos, D. A., Rezaei, S., Zhang, D., Luo, Y., Lin, B., Balakrishna, A. R., Xu, B., & Banerjee, S. (2022) · Chemical Science · doi:10.1039/d2sc04157j · Cited by 59
Fischer, M., Brand, M. J., Karger, A., Gomez, M. R., Rehm, M., Natterer, J., & Jossen, A. (2025) · Journal of Power Sources · doi:10.1016/j.jpowsour.2025.237921 · Cited by 53
Hallot, M., Caja-Muñoz, B., Leviel, C., Lebedev, O. I., Retoux, R., Avila, J., Roussel, P., Asensio, M. C., & Lethien, C. (2021) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.0c21961 · Cited by 53
Rechargeable Potassium–Selenium Batteries
Huang, X., Guo, Z., Dou, S. X., & Wang, Z. (2021) · Advanced Functional Materials · doi:10.1002/adfm.202102326 · Cited by 52
Sakthivel, P., Babu, G. A., Karuppiah, M., Asaithambi, S., Balaji, V., Pandian, M. S., Ramasamy, P., Mohammed, M. K. A., Navaneethan, N., & Ravi, G. (2021) · Ceramics International · doi:10.1016/j.ceramint.2021.11.155 · Cited by 52
Ren, H., Li, H., Barry, P., Wang, Z., Campos, A. R., Takeuchi, E. S., Marschilok, A. C., Yan, S., Takeuchi, K. J., & Reichmanis, E. (2024) · Chemistry of Materials · doi:10.1021/acs.chemmater.4c02013 · Cited by 56
Chen, Y.-S., Dominko, R., Marczewski, M., & Wieczorek, W. (2024) · Applied Physics A · doi:10.1007/s00339-024-07897-7 · Cited by 54
“Although single-crystal NMC cathodes were developed to address the significant problems caused by intergranular 35, 36].”
Somo, T. R., Mabokela, T. E., Teffu, D. M., Sekgobela, T. K., Ramogayana, B., Hato, M. J., & Modibane, K. D. (2021) · Coatings · doi:10.3390/coatings11070744 · Cited by 52
Preparation and application of 0D-2D nanomaterial hybrid heterostructures for energy applications
Sinha, S., Kim, H., & Robertson, A. W. (2021) · Materials Today Advances · doi:10.1016/j.mtadv.2021.100169 · Cited by 54
“Designing suitable electrodes that support and are robust toward these reversible chemistries is one of the core materials challenges in this research [429].”
BackgroundCross-Linked Gel Electrolytes with Self-Healing Functionalities for Smart Lithium Batteries
Davino, S., Callegari, D., Pasini, D., Thomas, M., Nicotera, I., Bonizzoni, S., Mustarelli, P., & Quartarone, E. (2022) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.2c15011 · Cited by 51
Observation of Zn Dendrite Growth via Operando Digital Microscopy and Time-Lapse Tomography
Du, W., Zhang, Z., Iacoviello, F., Zhou, S., Owen, R. E., Jervis, R., Brett, D. J. L., & Shearing, P. R. (2023) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.2c19895 · Cited by 51
Atchudan, R., Perumal, S., Edison, T. N. J. I., Albasher, G. I., Sundramoorthy, A. K., Vinodh, R., & Lee, Y. R. (2022) · Environmental Research · doi:10.1016/j.envres.2022.113910 · Cited by 50
Engineering d-p orbital hybridization for high-stable lithium manganate cathode
Zhang, S., Fang, S., Chen, J., Ni, L., Deng, W., Zou, G., Hou, H., & Ji, X. (2022) · Chemical Engineering Journal · doi:10.1016/j.cej.2022.138511 · Cited by 60
Wang, S., Hu, L., Li, X. F., Qiu, S., Qiu, S., Zhou, Q., Deng, W., Lu, X., Yang, Z., Qiu, M., et al. (2023) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2023.12.005 · Cited by 50
Self-rechargeable energizers for sustainability
Ling, J., Kunwar, R., Li, L., Peng, S., Misnon, I. I., Rahim, M. H. A., Yang, C., & Jose, R. (2022) · eScience · doi:10.1016/j.esci.2022.07.002 · Cited by 50
Aqueous Rechargeable Zinc–Metal Batteries: A Critical Analysis
Sambandam, B., Mathew, V., Fahri, A. N., Kim, S., Song, M., & Kim, J. (2024) · ACS Energy Letters · doi:10.1021/acsenergylett.4c00792 · Cited by 49
Malavekar, D. B., Pawar, D. C., Bagde, A. G., Khot, S. D., Sankapal, S. R., Bachankar, S., Patil, S. S., Lokhande, C. D., & Kim, J. H. (2024) · Chemical Engineering Journal · doi:10.1016/j.cej.2024.157533 · Cited by 49
Novel synthesis and electrochemical investigations of ZnO/C composites for lithium-ion batteries
Thauer, E., Zakharova, G. S., Андрейков, Е. И., Adam, V., Wegener, S. A., Nölke, J. H., Singer, L., Ottmann, A., Asyuda, A., Zharnikov, M., et al. (2021) · Journal of Materials Science · doi:10.1007/s10853-021-06125-4 · Cited by 49
“[44] Pender JP, Jha G, Youn DH, Ziegler JM, Andoni I, Choi EJ,”
BackgroundPMMA-LiTFSI based gel polymer electrolyte for lithium-oxygen cell application
Kufian, M. Z., Ramesh, S., & Arof, A. K. (2021) · Optical Materials · doi:10.1016/j.optmat.2021.111418 · Cited by 49
Didwal, P. N., Verma, R., Nguyen, A., Ramasamy, H. V., Lee, G., & Park, C. (2022) · Advanced Science · doi:10.1002/advs.202105448 · Cited by 49
Meng, Y., Liang, C., Jiang, D., Zhang, Y., Su, J., Xu, X., & Lü, M. (2023) · Journal of Energy Storage · doi:10.1016/j.est.2023.109105 · Cited by 49
Passivation and corrosion of Al current collectors in lithium-ion batteries
Du, P., Wan, J., Qu, J., Xie, H., Wang, D., & Yin, H. (2024) · npj Materials Degradation · doi:10.1038/s41529-024-00453-x · Cited by 48
Er-Rami, F.-E., Duffiet, M., Hinkle, S., Auvergniot, J., Blangero, M., Cabelguen, P., Song, K., Weill, F., Delmas, C., & Carlier, D. (2022) · Chemistry of Materials · doi:10.1021/acs.chemmater.1c04338 · Cited by 47
Fault prognosis of Li-ion batteries in electric vehicles: Recent progress, challenges and prospects
Li, H., Kaleem, M. B., Liu, K., Wu, Y., Liu, W., & Peng, Q. (2025) · Journal of Energy Storage · doi:10.1016/j.est.2025.116002 · Cited by 52
Influence of Al2O3 Coatings on HF Induced Transition Metal Dissolution from Lithium-Ion Cathodes
Tesfamhret, Y., Younesi, R., & Berg, E. J. (2022) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac4ab1 · Cited by 48
Mei, P., Zhang, Y., & Zhang, W. (2022) · Nanoscale · doi:10.1039/d2nr06294a · Cited by 46
Shen, P., Zhang, B., Wang, Y., Liu, X., Yu, C., Xu, T., Mofarah, S. S., Yu, Y., Liu, Y., Sun, H., et al. (2020) · Journal of nanostructure in chemistry · doi:10.1007/s40097-020-00367-5 · Cited by 46
Dual-Site Doping Strategy for Enhancing the Structural Stability of Lithium-Rich Layered Oxides
Tang, W. X., Duan, J., Xie, J., Qian, Y., Li, J., & Zhang, Y. (2021) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.1c02020 · Cited by 46
Aligned Carbon‐Based Electrodes for Fast‐Charging Batteries: A Review
Huang, Q., Ni, S., Jiao, M., Zhong, X., Zhou, G., & Cheng, H. (2021) · Small · doi:10.1002/smll.202007676 · Cited by 46
Multiscale modeling for enhanced battery health analysis: Pathways to longevity
Yang, K., Zhang, L., Wang, W., Long, C., Yang, S., Zhu, T., & Liu, X. (2024) · Carbon Neutralization · doi:10.1002/cnl2.124 · Cited by 47
State-of-the-art review of degradation mechanisms of commercial lithium-ion batteries
Jeon, D. H., Kim, S., & Hempelmann, R. (2025) · Journal of Power Sources · doi:10.1016/j.jpowsour.2025.237242 · Cited by 51
Fang, Z., Confer, M. P., Wang, Y., Wang, Q., Kunz, M. R., Dufek, E. J., Liaw, B. Y., Klein, T. M., Dixon, D. A., & Fushimi, R. (2021) · Journal of the American Chemical Society · doi:10.1021/jacs.1c03812 · Cited by 45
Chen, K., Uthirakumar, P., Dao, D. V., Cao, Y., Yadav, S., & Lee, I.-H. (2025) · Advanced Composites and Hybrid Materials · doi:10.1007/s42114-025-01474-z · Cited by 48
Lai, D., Ling, L., Su, M., Kang, Q., Gao, F., & Lu, Q. (2023) · Chemical Science · doi:10.1039/d2sc04900g · Cited by 44
Xu, W., Li, Q., Sui, F., Guo, S., Qi, R., Yan, C., Chen, L., Xia, S., Guo, J., Li, Z., et al. (2023) · Applied Surface Science · doi:10.1016/j.apsusc.2023.157142 · Cited by 44
Weisenberger, C., Harrison, D. K., Zhou, C., & Knoblauch, V. (2023) · Electrochimica Acta · doi:10.1016/j.electacta.2023.142629 · Cited by 44
Selvam, T., Durgalakshmi, D., Balakumar, S., & Rakkesh, R. A. (2023) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.3c05835 · Cited by 43
Huu, H. T., & Im, W. B. (2020) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.0c11862 · Cited by 43
Iron-chalcogenide-based electrode materials for electrochemical energy storage
Wang, X., Wei, Q., Li, H., Sun, J., Li, H., He, Y., & Liu, Z. (2022) · Journal of Materials Chemistry A · doi:10.1039/d1ta10930h · Cited by 43
Yang, C., Li, Y., Zhang, X., Xiao, J., Xiong, H., Li, W., Guo, P., Yang, Z., & Xie, M. (2022) · Ionics · doi:10.1007/s11581-022-04691-4 · Cited by 43
Design of Ti4+-doped Li3V2(PO4)3/C fibers for lithium energy storage
Huang, Z., Luo, P., & Zheng, H. (2021) · Ceramics International · doi:10.1016/j.ceramint.2021.12.037 · Cited by 42
Tarek, Y. A., Shakil, R., Reaz, A. H., Roy, C. K., Barai, H. R., & Firoz, S. H. (2022) · ACS Omega · doi:10.1021/acsomega.2c01986 · Cited by 43
Abdollahi, A., Abnavi, A., Ghasemi, F., Ghasemi, S., Sanaee, Z., & Mohajerzadeh, S. (2021) · Electrochimica Acta · doi:10.1016/j.electacta.2021.138826 · Cited by 42
Feng, M., Pan, J., & Qi, Y. (2021) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.1c03186 · Cited by 44
N/S co-doped carbon nanosheet bundles as high-capacity anode for potassium-ion battery
Cao, J., Zhong, J., Xu, H., Li, S., Deng, H., Wang, T., Fan, L., Wang, X., Wang, L., Zhu, J., et al. (2021) · Nano Research · doi:10.1007/s12274-021-3773-5 · Cited by 42
Gribble, D. A., Li, Z., Özdoğru, B., McCulfor, E., Çapraz, Ö. Ö., & Pol, V. G. (2022) · Advanced Energy Materials · doi:10.1002/aenm.202103439 · Cited by 43
Han, J. Y., & Jung, S. (2022) · Batteries · doi:10.3390/batteries8070061 · Cited by 42
Sahu, S., & Foster, J. M. (2023) · Journal of Energy Storage · doi:10.1016/j.est.2022.106516 · Cited by 42
Wu, S., Wang, C., Li, S., & Weng, J. (2024) · Materials Chemistry Frontiers · doi:10.1039/d4qm00219a · Cited by 41
Majid, M. A., Charles Rajesh Kumar., J., & Ahmed, A. (2024) · e-Prime - Advances in Electrical Engineering Electronics and Energy · doi:10.1016/j.prime.2024.100753 · Cited by 61
First 18650-format Na-ion cells aging investigation: A degradation mechanism study
Nguyen, L. H. B., Camacho, P. S., Fondard, J., Carlier, D., Croguennec, L., Palacín, M. R., Ponrouch, A., Courrèges, C., Dedryvère, R., Trad, K., et al. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2022.231253 · Cited by 41
“Indeed, degradation mechanisms observed at the positive electrode in LIBs are commonly classified into (i) loss of Li+ ions that are no longer available to shuttle between the two electrodes and (ii) loss of active material in the electrode [1,3,4,6,51].”
BackgroundJang, J.-H., Lee, M., Park, S.-H., Oh, J., Park, J. K., & Paek, S. (2023) · Journal of Materials Chemistry A · doi:10.1039/d3ta01537h · Cited by 42
Peng, C., Liang, S., Yu, Y., Cao, L., Yang, C., Liu, X., Guo, K., Müller‐Buschbaum, P., Cheng, Y., & Wang, C. (2024) · Carbon Neutralization · doi:10.1002/cnl2.177 · Cited by 41
Mücke, R., Finsterbusch, M., Kaghazchi, P., Fattakhova‐Rohlfing, D., & Guillon, O. (2021) · Journal of Power Sources · doi:10.1016/j.jpowsour.2020.229430 · Cited by 39
Chi, P., Paul, T., Su, Y.-H., Su, K.-H., Su, C.-Y., Wu, P. M., Wang, S., & Wu, M. (2022) · Scientific Reports · doi:10.1038/s41598-022-08584-4 · Cited by 39
Matras, D., Ashton, T. E., Dong, H., Mirolo, M., Martens, I., Drnec, J., Darr, J. A., Quinn, P. D., Jacques, S. D. M., Beale, A. M., et al. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2022.231589 · Cited by 39
Setta, J., Lecocq, A., Desprez, P., Origuchi, M., Destriau, L., Marlair, G., Carlier, D., Croguennec, L., & Bordes, A. (2025) · Journal of Power Sources · doi:10.1016/j.jpowsour.2025.238265 · Cited by 41
Improving Thermodynamic Stability of nano-LiMn2O4 for Li-Ion Battery Cathode
Nakajima, K., Souza, F. L., Freitas, A. L. M., Thron, A. M., & Castro, R. H. R. (2021) · Chemistry of Materials · doi:10.1021/acs.chemmater.0c04305 · Cited by 38
Modeling NCA/C6-Si battery ageing
Chen, Z., Danilov, D. L., Zhang, Q., Jiang, M. Z., Zhou, J., Eichel, R., & Notten, P. H. L. (2022) · Electrochimica Acta · doi:10.1016/j.electacta.2022.141077 · Cited by 39
Kong, J., Zhou, S., He, T., Gu, S., & Yu, J. (2023) · Green Chemistry · doi:10.1039/d3gc00171g · Cited by 38
Kim, K., Kim, P. J., Chowdhury, R. A., Kantharaj, R., Candadai, A. A., Marconnet, A. M., Pol, V. G., & Youngblood, J. P. (2020) · Chemical Engineering Journal · doi:10.1016/j.cej.2020.128128 · Cited by 37
Metadata
- Authors
- Pender, J. P., Jha, G., Youn, D. H., Ziegler, J. M., Andoni, I., Choi, E. J., Heller, A., Dunn, B. S., Weiss, P. S., Penner, R. M., & Mullins, C. B.
- Affiliations
- The University of Texas at Austin (US)
- University of California, Irvine (US)
- Kangwon National University (KR)
- University of California, Los Angeles (US)
- California NanoSystems Institute (US)
- Corresponding author
- Penner, Reginald M.
- Mullins, C. Buddie
- ORCID
- Venue
- ACS Nano
- Publisher
- American Chemical Society (ACS)
- Published
- 2020-01-02
- Volume
- 14
- Issue
- 2
- Pages
- 1243-1295
- ISSN
- 1936-0851 (ISSN-L)
- 1936-086X
- OpenAlex
- W2996908450
- Cited by
- 873
- References
- 422
- Citations by year
- 2026: 121 · 2025: 145 · 2024: 125 · 2023: 145 · 2022: 180 · 2021: 124 · 2020: 33
- FWCI
- 41.35
- Type
- journal article
- Language
- en
- Open access
- hybrid
- doi.org
- Locations
- ACS Nano (publishedVersion, other-oa)
- PubMed (publishedVersion)
- OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) (submittedVersion)
- Funders
- Division of Chemical, Bioengineering, Environmental, and Transport Systems (CBET-1603491)
- Welch Foundation (F-1131, F-1436)
- Basic Energy Sciences (DESC0001160)
- Topics
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advancements in Battery Materials
- Physical Sciences › Engineering › Automotive Engineering › Battery Modeling and Management
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advanced Battery Materials and Technologies
- Keywords
- lithium-ion batteries, electrode degradation, structural deterioration, electrochemical degradation, gravimetric capacity, cycle life, battery safety
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.