Abstract
Although Li-ion batteries have emerged as the battery of choice for electric vehicles and large-scale smart grids, significant research efforts are devoted to identifying materials that offer higher energy density, longer cycle life, lower cost, and/or improved safety compared to those of conventional Li-ion batteries based on intercalation electrodes. By moving beyond intercalation chemistry, gravimetric capacities that are 2–5 times higher than that of conventional intercalation materials (e.g., LiCoO2 and graphite) can be achieved. The transition to higher-capacity electrode materials in commercial applications is complicated by several factors. This Review highlights the developments of electrode materials and characterization tools for rechargeable lithium-ion batteries, with a focus on the structural and electrochemical degradation mechanisms that plague these systems.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Sophisticated chemical reactions can result in material loss and structural deformation, causing capacity decrement and resistance increment [3,4].”
From State‐of‐health estimation of lithium‐ion batteries: A comprehensive literature review from cell to pack levels (2024) · cites this paper as [4]
Citations
Cites
Issues and challenges facing rechargeable lithium batteries
Tarascon, J.-M., & Armand, M. (2001) · Nature · doi:10.1038/35104644 · Cited by 21,130
Armand, M., & Tarascon, J.-M. (2008) · Nature · doi:10.1038/451652a · Cited by 19,612
The Li-Ion Rechargeable Battery: A Perspective
Goodenough, J. B., & Park, K.-S. (2013) · Journal of the American Chemical Society · doi:10.1021/ja3091438 · Cited by 9,962
Li-O2 and Li-S batteries with high energy storage
Bruce, P. G., Freunberger, S. A., Hardwick, L. J., & Tarascon, J.-M. (2012) · Nature Materials · doi:10.1038/nmat3191 · Cited by 9,479
Nano-sized transition-metal oxides as negative-electrode materials for lithium-ion batteries
Poizot, P., Laruelle, S., Grugeon, S., Dupont, L., & Tarascon, J.-M. (2000) · Nature · doi:10.1038/35035045 · Cited by 8,041
Phospho‐olivines as Positive‐Electrode Materials for Rechargeable Lithium Batteries
Padhi, A. K., Nanjundaswamy, K. S., & Goodenough, J. B. (1997) · Journal of The Electrochemical Society · doi:10.1149/1.1837571 · Cited by 7,933
Reviving the lithium metal anode for high-energy batteries
Lin, D., Liu, Y., & Cui, Y. (2017) · Nature Nanotechnology · doi:10.1038/nnano.2017.16 · Cited by 6,763
High-performance lithium battery anodes using silicon nanowires
Chan, C. K., Peng, H., Liu, G., McIlwrath, K., Zhang, X. F., Huggins, R. A., & Cui, Y. (2008) · Nature Nanotechnology · doi:10.1038/nnano.2007.411 · Cited by 6,683
Lithium Batteries and Cathode Materials
Whittingham, M. S. (2004) · Chemical Reviews · doi:10.1021/cr020731c · Cited by 6,267
A highly ordered nanostructured carbon–sulphur cathode for lithium–sulphur batteries
Ji, X., Lee, K. T., & Nazar, L. F. (2009) · Nature Materials · doi:10.1038/nmat2460 · Cited by 5,988
Research works printed but not linked: 8
- Li, 2016, Origins of Large Voltage Hysteresis in High-Energy-Density Metal Fluoride Lithium-Ion Battery Conversion Electrodes, J. Am. Chem. Soc., 138, 2838, 10.1021/jacs.6b00061 · DOI · Paper page
- Danuta, 1975, Chemical Investigations of Lithium-Sulfur Cells, 186
- Tan, 2016, Core–Shell Nano-FeS2@N-Doped Graphene as an Advanced Cathode Material for Rechargeable Li-Ion Batteries, Chem. Commun., 52, 986, 10.1039/c5cc08002a · DOI
- Demirocak, 2016, Probing the Aging Effects on Nanomechanical Properties of a Thin Film LiFePO4 Cathode, ECS Trans., 73, 57, 10.1149/07301.0057ecst · DOI
- Zhao, 2015, Rechargeable Lithium-Iodine Batteries with Iodine/Nanoporous Carbon Cathode, Nano Lett., 15, 5982, 10.1021/acs.nanolett.5b02116 · DOI · Paper page
- Meng, 2018, Polyiodide-Shuttle Restricting Polymer Cathode for Rechargeable Lithium/Iodine Battery with Ultralong Cycle Life, ACS Appl. Mater. Interfaces, 10, 17933, 10.1021/acsami.8b03212 · DOI
- Arora, 2004, Battery Separators, Chem. Rev., 104, 4419, 10.1021/cr020738u · DOI · Paper page
- Lee, 2015, Fracture of Crystalline Germanium during Electrochemical Lithium Insertion, Extrem. Mech. Lett., 2, 15, 10.1016/j.eml.2015.01.009 · DOI
Cited by
Items 701–800 of 891
Sasmal, S., Roy, S., Gupta, P. K., Ramkumar, K., Biswas, P., Ghorui, B., Saju, S. K., Ajayan, P. M., Valiyaveettil, S., Pala, R. G. S., et al. (2025) · Energy Technology · doi:10.1002/ente.202400531 · Cited by 2
The Effects of Electrode Physical Parameters on the Statistical Life Models of Li-Ion Battery
Mouais, T., Kittaneh, O. A., & Abdulmajid, M. (2021) · IEEE International IOT, Electronics and Mechatronics Conference (IEMTRONICS) · doi:10.1109/iemtronics52119.2021.9422572 · Cited by 2
An Energy Supervisor Architecture for Energy-Harvesting Applications
Saoda, N., Wang, W., Billah, M. F. R. M., & Campbell, B. (2022) · ACM/IEEE International Conference on Information Processing in Sensor Networks (IPSN) · doi:10.1109/ipsn54338.2022.00033 · Cited by 2
“Batteries, due to their limited cycle count [5, 35], potential long recharge times [32, 47], and hazardous nature [25, 29] have become a less attractive option as a power source for applications that require low maintenance and life-long service.”
BackgroundHydrogen Absorption Promoted by Surface Melting: Guidelines for High-Pressure Superhydride SynthesisPreprint
Sato, R., Conway, L. J., Zhang, D., Pickard, C. J., Akagi, K., Sau, K., Hao, L., & Orimo, S. (2024) · ChemRxiv · doi:10.26434/chemrxiv-2024-2v5l6-v2 · Cited by 2
Kumchompoo, J., Kunthadee, P., Laorodphan, N., Kidkhunthod, P., & Puntharod, R. (2023) · Ferroelectrics · doi:10.1080/00150193.2022.2159233 · Cited by 1
A Comprehensive Review of the Li‐Ion Batteries Fast‐Charging Protocols
Mouais, T., & Qaisar, S. M. (2023) · Wiley eBooks · doi:10.1002/9781119872146.ch2 · Cited by 1
Application of Carbonaceous Quantum dots in Energy Storage
Thakur, V., & Sharma, E. (2023) · BENTHAM SCIENCE PUBLISHERS eBooks · doi:10.2174/9789815136265123010012 · Cited by 1
Environmental applications of bioelectrochemical fuel cells
Kumar, A., Sehrawat, S., Priya, Boora, A., Bhavna, Kumar, P., Kumar, S., & Duhan, S. (2024) · Elsevier eBooks · doi:10.1016/b978-0-323-91023-1.00008-9 · Cited by 1
Gorai, S., Ray, A., & Mandal, S. (2024) · Materials Today Communications · doi:10.1016/j.mtcomm.2024.109657 · Cited by 2
Baumann, A. F., Mutter, D., Urban, D. F., & Elsässer, C. (2024) · Physical Review Materials · doi:10.1103/physrevmaterials.8.095401 · Cited by 1
Potassium/sulfur and potassium/selenium battery
Yuan, X., Feng, J., Zhu, B., & Cai, X. (2024) · Elsevier eBooks · doi:10.1016/b978-0-443-13891-1.00011-x · Cited by 1
Babkin, A. V., Drozhzhin, O. A., Kubarkov, A. V., Antipov, E. V., & Sergeyev, V. G. (2024) · Доклады Российской академии наук Химия науки о материалах · doi:10.31857/s2686953524030024 · Cited by 1
Chiu, S., Hong, L.-T., & Louh, R. (2024) · Nanotechnology · doi:10.1088/1361-6528/ad97c3 · Cited by 1
“…energy storage components that are lightweight, compact, stable, and have an extended lifespan, given the rapid development of the information and communication environments ranging from 40 ◦ C to 60 ◦ C [7], (5) exceptionally high charge retention capacity, and (6) durability of the device.”
Chakrabarti, S., & Thakur, A. K. (2025) · Materials Chemistry and Physics · doi:10.1016/j.matchemphys.2025.130655 · Cited by 1
Yoo, S.-Y., Park, J., Park, H.-S., Li, L., & Chun, S. (2025) · Chemical Engineering Journal · doi:10.1016/j.cej.2025.164932 · Cited by 1
Wang, R., Wang, Q., & Bai, Y. (2025) · ACS Applied Engineering Materials · doi:10.1021/acsaenm.5c00341 · Cited by 1
Raman Spectroscopy of Practical LIB Cathodes: A Study of Humidity-Induced Degradation
Mele, C., Ravasio, F., Casalegno, A., Emanuele, E., Rabissi, C., & Bozzini, B. (2025) · Molecules · doi:10.3390/molecules30163448 · Cited by 1
“The SEM micrographs of Figure 7 show a notable impact of humidity exposure on the morphology of NMC-LMO cathodes, in-keeping with the information reported in the literature [16,58–60].”
Li, K., Xu, C., He, Y., Xiang, Y., Ding, Y., Man, S., Liu, H., Liu, W., Xia, Q., Yang, M. J., et al. (2025) · Journal of Power Sources · doi:10.1016/j.jpowsour.2025.238166 · Cited by 1
Zhang, F., Lü, Q., Li, J., Zhang, Q., Yu, H., Wang, Y., Li, J., Ren, H., Liang, H., Shen, F., et al. (2025) · Materials · doi:10.3390/ma18174058 · Cited by 1
Park, C., & Park, K. (2025) · ACS Applied Energy Materials · doi:10.1021/acsaem.5c01764 · Cited by 1
Park, J. S., Kim, G. H., Park, J., Heo, I. B., Kim, J. M., Lim, J., & Jin, H. M. (2025) · Korean Journal of Chemical Engineering · doi:10.1007/s11814-025-00576-0 · Cited by 1
“The performance, longevity, and reliability of rechargeable batteries are closely tied to the nanostructure of each component [1].”
Mustafa, M. N., Abdah, M. A. A. M., Saidi, N. M., Numan, A., Walvekar, R., & Khalid, M. (2025) · Journal of Energy Storage · doi:10.1016/j.est.2025.118983 · Cited by 2
Starodub, T. N. (2025) · Sustainability · doi:10.3390/su172310612 · Cited by 1
β-Irida-graphene: A new 2D carbon allotrope for sodium-ion battery anodes
Laranjeira, J. A. S., Lima, K. A. L., Martins, N. F., Ribeiro, L. A., Galvao, D. S., Cabral, L. A., & Sambrano, J. R. (2025) · Physica E Low-dimensional Systems and Nanostructures · doi:10.1016/j.physe.2025.116442 · Cited by 3
Effects of Corrosion on the Durability of Battery
Rached, S., Ferraa, N., Mzioud, K., Rehioui, M., Habsaoui, A., & Touhami, M. E. (2025) · IGI Global eBooks · doi:10.4018/979-8-3373-3156-0.ch004 · Cited by 1
A High Capacity‐Long Cycling Concurrent Strategy of Ti 3 C 2 /MgH 2 for Lithium Storage
Xu, T., Li, X., Qu, B., Duan, C., Li, Y., Huang, H., Liu, B., Chen, X., Zeng, H., & Wu, Y. (2025) · Rare Metals · doi:10.1002/rar2.70083 · Cited by 1
Hassan, A. J., Tim, C. K., Pah, L. K., Shah, N. M., Halim, U. A., Noor, N. M., & Razak, W. M. Z. B. A. (2026) · Journal of Materials Science · doi:10.1007/s10853-026-12364-0 · Cited by 1
Lagnoni, M., Quilici, F. G., Cademartori, D., Scarpelli, C., Mithoowani, U. N., Barontini, F., Ruvio, A., Puccini, M., Lutzemberger, G., Carpanese, M. P., et al. (2026) · Advanced Science · doi:10.1002/advs.75306 · Cited by 2
Safety of Lithium Batteries: Mechanistic Gap Analysis from Materials to Large-Format Cells
Kausthubharam, Karmakar, A., Vishnugopi, B. S., Miguel, A. J., Bates, A. M., Hewson, J. C., Johnson, N. B., Preger, Y., Albertus, P. S., Jeevarajan, J. A., et al. (2026) · ACS Energy Letters · doi:10.1021/acsenergylett.6c00637 · Cited by 2
Dual Soft‐Gel Electrodes Enabling Near‐Practical and Deployable Aqueous Batteries
Zhang, K., Yang, S., Xi, H., Yang, Q., Ye, J., & Wu, Y. N. (2026) · Small Methods · doi:10.1002/smtd.70732 · Cited by 1
Namsar, O., Yodbunork, C., Yodying, W., Kunniyom, K., Autthawong, T., Haruta, M., & Sarakonsri, T. (2026) · Biomass and Bioenergy · doi:10.1016/j.biombioe.2026.109516 · Cited by 1
Copper corrosion and capacity fading under overcharge conditions in graphite half cells
Hwang, S., Kim, M., Kim, H.-S., Kim, J., 박현수, & Yoon, W. (2026) · Journal of Electroanalytical Chemistry · doi:10.1016/j.jelechem.2026.120290 · Cited by 1
Hou, Z., Xiao, W., Yang, X., Wang, S., Li, X. B., Zhang, M., Lv, M., Song, X. Y., Qin, J., Yang, H., et al. (2026) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2026.05.027 · Cited by 1
Kim, J., Kang, C., 노은빈, 유준환, Ahmed, A., Chen, W.-H., Hong, S., & Oh, J. (2026) · Chemical Engineering Journal · doi:10.1016/j.cej.2026.178043 · Cited by 1
Coating technologies for battery active materials
Lin, J., Li, F., Ji, Y., Xiao, J., & Chen, Z. (2026) · Nature Reviews Clean Technology · doi:10.1038/s44359-026-00178-x · Cited by 1
“However, achieving these objectives is constrained by the progressive degradation of electrode active materials during repeated cycling and extended storage 2 .”
Zhu, X., Li, X., & Wang, L. (2026) · Materials Horizons · doi:10.1039/d6mh00816j · Cited by 1
Hasani, A., Salminen, A., Joshi, S. V., Makowska, M. G., Chameh, B., Lehto, V., Vinay, G., Goel, S., Angervo, I., & Ganvir, A. (2026) · Materials & Design · doi:10.1016/j.matdes.2026.116414 · Cited by 2
Liu, Z., Liu, H., Lu, F., Liu, Y., Pan, G., & Xiao, Y. (2026) · Journal of Energy Storage · doi:10.1016/j.est.2026.123208 · Cited by 1
Gong, S. M., Song, S. W., Kim, Y., Yoon, J., Kang, J. H., Jung, Y., Kim, T., Yang, S. J., & Kim, J. H. (2026) · Energy & environment materials · doi:10.1002/eem2.70466 · Cited by 1
Jang, J., Kim, J.-H., Park, D., Kim, M.-C., Moon, S., Kim, W., Ahn, S.-Y., & Park, K. (2026) · Journal of Energy Storage · doi:10.1016/j.est.2026.123759 · Cited by 1
Batool, K., Nazir, S., Rubab, R., Li, W., & Liu, G. G. (2026) · Journal of Energy Storage · doi:10.1016/j.est.2026.124022 · Cited by 1
Ruan, G., Zhu, Y., Chen, Q., Kong, X., Guo, H., Yang, Q., Cai, Y., & Yuan, W. (2026) · Energies · doi:10.3390/en19153704 · Cited by 1
Feng, C., Hou, C., Ma, X., Meng, Y., Gou, N., Xu, D., & Zhang, D. (2026) · Journal of Energy Storage · doi:10.1016/j.est.2026.124008 · Cited by 1
Vargas-Arana, C., & Leal-Perez, J. E. (2026) · Journal of Materials Science Materials in Energy · doi:10.1007/s44308-026-00041-2 · Cited by 1
Stress-coupled lithium transport in all-solid-state batteries
Kim, H., Kim, D., Nam, C., Kim, J. T., Hwang, Y., Hwang, S., Jo, S., Seo, S., You, H., Choi, E., et al. (2026) · Joule · doi:10.1016/j.joule.2026.102680 · Cited by 1
Self-citationPark, T. W., Kang, Y. L., Lee, S. H., No, G. W., Park, E.-S., Park, C., Lee, J., & Park, W. I. (2021) · Materials · doi:10.3390/ma14071585 · Cited by 1
Developments in Dilatometry for Characterisation of Electrochemical Devices
Michael, H., Jervis, R., Brett, D. J. L., & Shearing, P. R. (2021) · Batteries & Supercaps · doi:10.1002/batt.202100200 · Cited by 1
Boron-induced metamorphosis of graphitic structures - a new form of mesoscopic carbon
Echeverría, E., Austin, A. J., Dice, N., Kalkan, A. K., Zhang, L., Weng, B., Meyer, D., & Mcllroy, D. N. (2020) · Carbon Trends · doi:10.1016/j.cartre.2020.100012 · Cited by 1
Samantara, A. K., & Ratha, S. (2020) · SpringerBriefs in energy · doi:10.1007/978-3-030-60812-5_1 · Cited by 1
Basa, A., Gajko, E., Goclon, J., Wilczewska, A. Z., & Winkler, K. (2022) · ChemElectroChem · doi:10.1002/celc.202200174 · Cited by 1
Phase evolution, electrical properties, and conductivity mechanism in LiNbWO6
Wu, S., Li, C., Wei, H., Song, X., Liu, L., & Xu, J. (2022) · Materials Today Communications · doi:10.1016/j.mtcomm.2022.104492 · Cited by 1
Shi, J., Li, X., Wang, Y., Wang, Z. M., Liu, S., & Li, H. (2023) · Lecture notes in electrical engineering · doi:10.1007/978-981-99-1027-4_1 · Cited by 1
Suo, Y., Xiao, J., & He, Z. (2023) · Mechanics of Solids · doi:10.3103/s0025654423600265 · Cited by 1
“Some experiments have indicated that the cycling-induced changes of the structure can lead to the structural damage [15, 16].”
BackgroundYan, H., Liu, Z., Chen, S., Fu, Y., Zhang, Y., Zhang, B., & Chen, Y. (2023) · Journal of Physics and Chemistry of Solids · doi:10.1016/j.jpcs.2023.111603 · Cited by 1
Kim, K. M., Kim, C., Kwon, S., Choi, W. S., & Kang, H. (2023) · Journal of Electrical Engineering and Technology · doi:10.1007/s42835-023-01580-2 · Cited by 1
Kim, T. (2023) · Colloids and Surfaces A Physicochemical and Engineering Aspects · doi:10.1016/j.colsurfa.2023.132937 · Cited by 1
Magnetic Force Dilatometry for Operando Coin Cell Electrochemical Dilation Measurements
Osad, W., Reese, C. W., Sayed, S. Y., Galant, A., & Balogh, M. P. (2024) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ad4a10 · Cited by 1
Zhao, Z., Liu, W., Qi, Y., & Bai, Y. (2024) · Ionics · doi:10.1007/s11581-024-05718-8 · Cited by 1
“Natural graphite (NG) as a general anode material for Li-ion batteries (LIBs) reveals a high theoretical specific capacity, good electrical conductivity, and low price [3, 4].”
Pulse-Induced Energy Gains in Electrochemical Systems
Kerrow Energetics, S. J., & Perry, J. A. (2024) · Journal of Electrical Electronics Engineering · doi:10.33140/jeee.03.04.05 · Cited by 1
Petit, J., Heugel, P., Geiger, S., Klein, F., & Tübke, J. (2024) · Batteries · doi:10.3390/batteries10120445 · Cited by 1
“In particular, the degradation of electrodes, especially the anode, plays a pivotal role in determining the efficiency and safety of lithium-ion batteries and was investigated in detail by many researchers [4–6].”
Zhang, P. (2025) · Polymer Testing · doi:10.1016/j.polymertesting.2025.108821 · Cited by 1
Breaking structural symmetry to facilitate fast reaction kinetics
Min, W., Lee, S., Hwang, J., Yoon, S., & Kim, D. (2025) · Journal of Materials Chemistry A · doi:10.1039/d5ta02769a · Cited by 1
Cho, H., Kang, S., Tag, K., Cho, H., Gong, H.-W., Kim, H., Kim, H., & Ahn, J. (2023) · Microscopy and Microanalysis · doi:10.1093/micmic/ozad067.911 · Cited by 1
Development of nonaqueous zinc-ion battery based on manganese dioxide cathode
Kao‐ian, W. (2021) · Chula Digiverse · doi:10.58837/chula.the.2021.57 · Cited by 1
A Comprehensive Review of EV Lithium-Ion Battery DegradationPreprint
Júnior, C. A. R., Sanseverino, E. R., Gallo, P., Amaral, M. M., Koch, D., Kotak, Y., Diel, S., Walter, G., Schweiger, H., & Zanin, H. (2023) · Preprints.org · doi:10.20944/preprints202306.0228.v2 · Cited by 4
Gupta, P. (2023) · KTH Publication Database DiVA (KTH Royal Institute of Technology) · Cited by 1
Krupp, A. (2023) · elib (German Aerospace Center) · Cited by 2
Evaluation of LFP battery performed by high-resolution neutron diffraction technique
Putra, T. Y. S. P., Insani, A., Mugirahardjo, H., Kamila, R., Purwamargapratala, Y., Sudaryanto, S., & Honggowiranto, W. (2021) · AIP conference proceedings · doi:10.1063/5.0059998
Liu, Z. Y., & Zhu, Z. (2022) · SSRN Electronic Journal · doi:10.2139/ssrn.4096080
Armazenamento de energia em eletrólitos altamente concentrados: um estudo interfacial
Obana, T. T. (2021) · Digital Library of Theses and Dissertations (Universidade de São Paulo) · doi:10.11606/t.46.2021.tde-07012022-161536
Du, S., Zhang, H., Kuai, P., Guo, B., & Weng, Z. (2022) · Russian Journal of Physical Chemistry A · doi:10.1134/s0036024422050272
Chiochan, P., Jangsan, C., Anansuksawat, N., Homlamai, K., Phattharasupakun, N., & Sawangphruk, M. (2021) · SSRN Electronic Journal · doi:10.2139/ssrn.3983712
Quérel, E., & Aguadero, A. (2022) · Wiley eBooks · doi:10.1002/9783527825769.ch20
Polymer‐Containing Batteries *
Newkome, G. R., Schubert, U. S., & Winter, A. (2023) · Wiley eBooks · doi:10.1002/9783527843466.ch2
Fundamental understanding of working batteries by in situ and operando Raman spectroelectrochemistry
Radtke, M., Heber, M., & Hess, C. (2023) · Elsevier eBooks · doi:10.1016/b978-0-323-85669-0.00100-8
Ionic liquid applications for capacitor and charge storage devices
Thomas, P., Lai, C. W., Johan, M. R., & Chowdhury, Z. Z. (2023) · Elsevier eBooks · doi:10.1016/b978-0-323-95931-5.00017-8
Measuring Battery Health - Secondary cell dynamics and electrochemistryPreprint
Perry, J. A. (2023) · OSF Preprints (OSF Preprints) · doi:10.31219/osf.io/y5swg
Aida, M. N. (2022) · Chula Digiverse · doi:10.58837/chula.the.2022.261 · Cited by 1
Electrospun Tio2-Bi@C Nanofibers with Excellent Potassium Storage PerformancePreprint
Luo, J., Liu, L., Liu, S., Zhou, L., Yang, J., Huang, Z., & Hu, H. R. (2024) · SSRN Electronic Journal · doi:10.2139/ssrn.4813289
Analytical design of electrode particle debonding for battery applications
Mitra, A. S., Anapolsky, A., & García, R. E. (2024) · Modelling and Simulation in Materials Science and Engineering · doi:10.1088/1361-651x/ad5f49
An, Q., Zhang, W., Ma, Z., Guo, S., Wang, Y., Yao, Y., Dong, L., Xia, W., Cai, R., & Wang, H. (2024) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.4c12707
Fundamental insights of electrochemistry and reaction mechanisms of lithium-ion batteries
Sunil, K., Chacko, E., Lal, H. M., Uthaman, A., & Thomas, S. (2024) · Elsevier eBooks · doi:10.1016/b978-0-443-13338-1.00011-3
Exfoliation and cracking in MoS2 following in-situ lithiation
Ghosh, C. K., Singh, M. K., Dongare, A. M., & Carter, C. B. (2024) · Journal of Materials Science · doi:10.1007/s10853-024-10399-9
“…directly linked to the possible failure of the electrochemical storage cells during operation or especially during the charging cycle [1]; this is a major concern of the present battery technology and is associated with the degradation of the electrode materials interacting with the Li-ions [2–5].”
Liu, D., Jiang, M., Potter, K. D., & Harris, P. J. F. (2024) · Royal Society of Chemistry eBooks · doi:10.1039/9781839169984-00001 · Cited by 3
Battery Cells and Materials Performance Evaluation
Maher, K., & Boumaiza, A. (2024) · International Conference on Renewable Energy and Power Engineering (REPE) · doi:10.1109/repe62578.2024.10809978
Putra, S. E. M., Habibi, F. A. N., Simatupang, D. H., & Mustaqim, A. (2024) · Greensusmater · doi:10.62755/greensusmater.2024.1.2.57-62
“Based on these battery types, lithium batteries show good performance compared to other battery types [8, 9, 10].”
Rexhausen, W., Parsons, C., Garg, U., Qu, D., & Guptasarma, P. (2024) · arXiv (Cornell University) · doi:10.48550/arxiv.2408.01595
“…have also been found to be attributable to the filling of oxygen and transition metal vacancies in the bulk by ions migrating from the surface, reactions stemming from degradation of the electrolyte, and the nature of the redox reaction when cycling at higher voltage [29], [30], [31], [32].”
BackgroundGreener Alternative Materials for Batteries
Sardar, S., Kasilingam, R., & Kapgate, B. P. (2023) · Encyclopedia of Green Materials · doi:10.1007/978-981-16-4921-9_209-1
Sadiq, M., Nasiruddeen, A., & Abdul, A. (2025) · SSRN Electronic Journal · doi:10.2139/ssrn.5253576
Asiri, M., Kedhim, M., Jain, V. D., Ballal, S., Singh, A., Kavitha, V. S. N. P., Ibragimovna, K. N., & Nourizadeh, M. (2025) · SSRN Electronic Journal · doi:10.2139/ssrn.5270222 · Cited by 1
Applications in Energy Systems
Phogat, P., Sharma, S., Rai, S., & Thakur, J. (2025) · Engineering materials · doi:10.1007/978-981-96-6767-3_8
Study And Application of Nanotechnology in Lithium Batteries
Zeng, Y. (2025) · Highlights in Science Engineering and Technology · doi:10.54097/h19wrh82
Zheng, Y., Li, Y., Zhou, Y., Huang, W., He, S., & Chen, Z. (2025) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2025.184616
Structure design and future development of lithium ion sieve bulk adsorbents
Zhang, R., Li, C., & Wang, M. (2025) · Journal of environmental chemical engineering · doi:10.1016/j.jece.2025.119933 · Cited by 3
Makki, S. K., & Al‐Saadi, T. M. (2025) · Ibn AL- Haitham Journal For Pure and Applied Science · doi:10.30526/38.4.4175
“Therefore, the slight decrease in density reflects a balance between the effect of the atomic mass of the copper ions on the one hand, and the increase in the crystal lattice size and the redistribution of cations on the other (23).”
Chaturvedi, P., Mishra, S. M., & Choi, D. S. (2025) · Journal of Electroanalytical Chemistry · doi:10.1016/j.jelechem.2025.119622
Latif, C., Maulana, T. A. J., Yogianto, M. F. I., & Adziimaa, A. F. (2025) · Journal of Energy Material and Instrumentation Technology · doi:10.23960/jemit.379
Study of materials and interphases for electrochemical energy storage from renewable sources
Lacarbonara, G. (2023) · AMS Dottorato Institutional Doctoral Theses Repository (University of Bologna) · doi:10.48676/unibo/amsdottorato/10682
Foo, C. (2022) · Oxford University Research Archive (ORA) (University of Oxford) · doi:10.5287/ora-2neyzqvyw
Mechanistic studies and applications of oxygen activation for energy conversion and storage
Tran, L. K. (2024) · Library, Museums and Press - UDSpace (University of Delaware) · doi:10.58088/da4m-ky05
Metadata
- Authors
- Pender, J. P., Jha, G., Youn, D. H., Ziegler, J. M., Andoni, I., Choi, E. J., Heller, A., Dunn, B. S., Weiss, P. S., Penner, R. M., & Mullins, C. B.
- Affiliations
- The University of Texas at Austin (US)
- University of California, Irvine (US)
- Kangwon National University (KR)
- University of California, Los Angeles (US)
- California NanoSystems Institute (US)
- Corresponding author
- Penner, Reginald M.
- Mullins, C. Buddie
- ORCID
- Venue
- ACS Nano
- Publisher
- American Chemical Society (ACS)
- Published
- 2020-01-02
- Volume
- 14
- Issue
- 2
- Pages
- 1243-1295
- ISSN
- 1936-0851 (ISSN-L)
- 1936-086X
- OpenAlex
- W2996908450
- Cited by
- 873
- References
- 422
- Citations by year
- 2026: 121 · 2025: 145 · 2024: 125 · 2023: 145 · 2022: 180 · 2021: 124 · 2020: 33
- FWCI
- 41.35
- Type
- journal article
- Language
- en
- Open access
- hybrid
- doi.org
- Locations
- ACS Nano (publishedVersion, other-oa)
- PubMed (publishedVersion)
- OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) (submittedVersion)
- Funders
- Division of Chemical, Bioengineering, Environmental, and Transport Systems (CBET-1603491)
- Welch Foundation (F-1131, F-1436)
- Basic Energy Sciences (DESC0001160)
- Topics
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advancements in Battery Materials
- Physical Sciences › Engineering › Automotive Engineering › Battery Modeling and Management
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advanced Battery Materials and Technologies
- Keywords
- lithium-ion batteries, electrode degradation, structural deterioration, electrochemical degradation, gravimetric capacity, cycle life, battery safety
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.