Origin and consequences of silicate glass passivation by surface layers
Open accessAbstract
Silicate glasses are durable materials, but are they sufficiently durable to confine highly radioactive wastes for hundreds of thousands years? Addressing this question requires a thorough understanding of the mechanisms underpinning aqueous corrosion of these materials. Here we show that in silica-saturated solution, a model glass of nuclear interest corrodes but at a rate that dramatically drops as a passivating layer forms. Water ingress into the glass, leading to the congruent release of mobile elements (B, Na and Ca), is followed by in situ repolymerization of the silicate network. This material is at equilibrium with pore and bulk solutions, and acts as a molecular sieve with a cutoff below 1 nm. The low corrosion rate resulting from the formation of this stable passivating layer enables the objective of durability to be met, while progress in the fundamental understanding of corrosion unlocks the potential for optimizing the design of nuclear glass-geological disposal.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Iler, K. (1979) · Medical Entomology and Zoology · Cited by 5,030
A review of focused ion beam milling techniques for TEM specimen preparation
Giannuzzi, L. A., & Stevie, F. A. (1999) · Micron · doi:10.1016/s0968-4328(99)00005-0 · Cited by 1,210
Re-equilibration of Zircon in Aqueous Fluids and Melts
Geisler, T., Schaltegger, U., & Tomaschek, F. (2007) · Elements · doi:10.2113/gselements.3.1.43 · Cited by 856
Chemical weathering rate laws and global geochemical cycles
Lasaga, A. C., Soler, J. M., Ganor, J., Burch, T. E., & Nagy, K. L. (1994) · Geochimica et Cosmochimica Acta · doi:10.1016/0016-7037(94)90016-7 · Cited by 795
Molecular mechanisms for corrosion of silica and silicate glasses
Bunker, B. C. (1994) · Journal of Non-Crystalline Solids · doi:10.1016/0022-3093(94)90708-0 · Cited by 635
An international initiative on long-term behavior of high-level nuclear waste glass
Gin, S., Abdelouas, A., Criscenti, L. J., Ebert, W. L., Ferrand, K., Geisler, T., Harrison, M. T., Inagaki, Y., Mitsui, S., Mueller, K. T., et al. (2013) · Materials Today · doi:10.1016/j.mattod.2013.06.008 · Cited by 546
Self-citationInsight into silicate-glass corrosion mechanisms
Cailleteau, C., Angeli, F., Devreux, F., Gin, S., Jestin, J., Jollivet, P., & Spalla, O. (2008) · Nature Materials · doi:10.1038/nmat2301 · Cited by 488
Self-citationFrugier, P., Gin, S., Minet, Y., Chave, T., Bonin, B., Godon, N., Lartigue, J.-E., Jollivet, P., Ayral, A., De Windt, L., et al. (2008) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2008.06.044 · Cited by 395
Self-citationDaval, D., Sissmann, O., Menguy, N., Saldi, G. D., Guyot, F., Martinez, I., Corvisier, J., Garcia, B., Machouk, I., Knauss, K. G., et al. (2011) · Chemical Geology · doi:10.1016/j.chemgeo.2011.02.021 · Cited by 338
Hellmann, R., Wirth, R., Daval, D., Barnes, J.-P., Penisson, J.-M., Tisserand, D., Epicier, T., Florin, B., & Hervig, R. L. (2012) · Chemical Geology · doi:10.1016/j.chemgeo.2011.12.002 · Cited by 327
Lanford, W. A., Davis, K., LaMarche, P. H., Laursen, T., Groleau, R., & Doremus, R. H. (1979) · Journal of Non-Crystalline Solids · doi:10.1016/0022-3093(79)90053-x · Cited by 315
A General Rate Equation for Nuclear Waste Glass Corrosion
Grambow, B. (1984) · MRS Proceedings · doi:10.1557/proc-44-15 · Cited by 291
Molecular Dynamics Simulations of Water Structure and Diffusion in Silica Nanopores
Bourg, I. C., & Steefel, C. I. (2012) · The Journal of Physical Chemistry C · doi:10.1021/jp301299a · Cited by 286
Vienna, J. D., Ryan, J. V., Gin, S., & Inagaki, Y. (2013) · International Journal of Applied Glass Science · doi:10.1111/ijag.12050 · Cited by 266
Self-citationFirst-order dissolution rate law and the role of surface layers in glass performance assessment
Grambow, B., & Müller, R. (2001) · Journal of Nuclear Materials · doi:10.1016/s0022-3115(01)00619-5 · Cited by 243
Aqueous corrosion of borosilicate glass under acidic conditions: A new corrosion mechanism
Geisler, T., Janssen, A., Scheiter, D., Stephan, T., Berndt, J., & Putnis, A. (2010) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2010.04.033 · Cited by 240
Nuclear Waste Glasses - How Durable?
Grambow, B. (2006) · Elements · doi:10.2113/gselements.2.6.357 · Cited by 194
The structure of Na2O–Al2O3–SiO2 glass: impact on sodium ion exchange in H2O and D2O
McGrail, B. P., Icenhower, J. P., Shuh, D. K., Liu, P., Darab, J. G., Baer, D. R., Thevuthasen, S., Shutthanandan, V., Engelhard, M. H., Booth, C. H., et al. (2001) · Journal of Non-Crystalline Solids · doi:10.1016/s0022-3093(01)00890-0 · Cited by 173
Kinetic aspects of basaltic glass dissolution at 90°C: role of aqueous silicon and aluminium
Daux, V., Guy, C., Advocat, T., Crovisier, J.-L., & Stille, P. (1997) · Chemical Geology · doi:10.1016/s0009-2541(97)00079-x · Cited by 164
Crovisier, J. L., Advocat, T., & Dussossoy, J. (2003) · Journal of Nuclear Materials · doi:10.1016/s0022-3115(03)00206-x · Cited by 160
Wang, Y. (2014) · Chemical Geology · doi:10.1016/j.chemgeo.2014.04.007 · Cited by 152
Nuclear Glass Durability: New Insight into Alteration Layer Properties
Gin, S., Guittonneau, C., Godon, N., Neff, D., Rébiscoul, D., Cabié, M., & Mostefaoui, S. (2011) · The Journal of Physical Chemistry C · doi:10.1021/jp205477q · Cited by 146
Self-citationCurti, E., Crovisier, J. L., Morvan, G., & Karpoff, A. M. (2006) · Applied Geochemistry · doi:10.1016/j.apgeochem.2006.03.010 · Cited by 143
Leaching of mineral and glass surfaces during dissolution
Casey, W. H., & Bunker, B. C. (1990) · Reviews in Mineralogy and Geochemistry · Cited by 141
Elemental and isotopic (29Si and 18O) tracing of glass alteration mechanisms
Valle, N., Verney‐Carron, A., Sterpenich, J., Libourel, G., Deloule, É., & Jollivet, P. (2010) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2010.03.028 · Cited by 139
Self-citationGin, S., Ryan, J. V., Schreiber, D. K., Neeway, J. J., & Cabié, M. (2013) · Chemical Geology · doi:10.1016/j.chemgeo.2013.04.001 · Cited by 133
Self-citationLeaching of borosilicate glasses. I. Experiments
Ledieu, A., Devreux, F., Barboux, P., et al. (2004) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2004.06.006 · Cited by 125
Schneider, J., Mastelaro, V. R., Zanotto, E. D., Shakhmatkin, B. A., Vedishcheva, N. M., Wright, A. C., & Panepucci, H. C. (2003) · Journal of Non-Crystalline Solids · doi:10.1016/s0022-3093(03)00332-6 · Cited by 118
Sissmann, O. J., Brunet, F., Martinez, I., Guyot, F., Verlaguet, A., Pinquier, Y., & Daval, D. (2014) · Environmental Science & Technology · doi:10.1021/es405508a · Cited by 109
Bourcier, W. L., Peiffer, D. W., Knauss, K. G., McKeegan, K. D., & Smith, D. K. (1989) · MRS Proceedings · doi:10.1557/proc-176-209 · Cited by 105
Cho, H., Felmy, A. R., Craciun, R., Keenum, J. P., Shah, N., & Dixon, D. A. (2006) · Journal of the American Chemical Society · doi:10.1021/ja0559202 · Cited by 92
Investigation of gel porosity clogging during glass leaching
Jollivet, P., Angeli, F., Cailleteau, C., Devreux, F., Frugier, P., & Gin, S. (2008) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2008.07.023 · Cited by 91
Self-citationBriman, I. M., Rébiscoul, D., Diat, O., et al. (2012) · The Journal of Physical Chemistry C · doi:10.1021/jp3001898 · Cited by 73
Munier, I., Crovisier, J. L., Grambow, B., Fritz, B., & Clément, A. (2003) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2003.08.033 · Cited by 37
Cited by
A comparative review of the aqueous corrosion of glasses, crystalline ceramics, and metals
Frankel, G. S., Vienna, J. D., Lian, J., Scully, J. R., Gin, S., Ryan, J. V., Wang, J., Kim, S. H., Windl, W., & Du, J. (2018) · npj Materials Degradation · doi:10.1038/s41529-018-0037-2 · Cited by 276
Self-citationThe Nanoscale Basis of CO2 Trapping for Geologic Storage
Bourg, I. C., Beckingham, L. E., & DePaolo, D. J. (2015) · Environmental Science & Technology · doi:10.1021/acs.est.5b03003 · Cited by 163
Daval, D., Calvaruso, C., Guyot, F., & Turpault, M.-P. (2018) · Earth and Planetary Science Letters · doi:10.1016/j.epsl.2018.06.035 · Cited by 49
Miller, Q. R. S., Kaszuba, J. P., Kerisit, S. N., Schaef, H. T., Bowden, M. E., McGrail, B. P., & Rosso, K. M. (2020) · Environmental Science: Nano · doi:10.1039/c9en01382b · Cited by 41
Dynamics of altered surface layer formation on dissolving silicates
Daval, D., Bernard, S., Rémusat, L., Wild, B., Guyot, F., Micha, J. S., Rieutord, F., Magnin, V., & Fernandez-Martinez, A. (2017) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2017.04.010 · Cited by 39
Metadata
- Authors
- Gin, S., Jollivet, P., Fournier, M., Angeli, F., Frugier, P., & Charpentier, T.
- Venue
- Nature Communications
- Published
- 2015-02-19
- Volume
- 6
- Issue
- 1
- Pages
- 6360-6360
- ISSN
- 2041-1723 (ISSN-L)
- OpenAlex
- W2049027197
- Cited by
- 303
- References
- 34
- FWCI
- 27.97
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.