Single [0001]-oriented zinc metal anode enables sustainable zinc batteries
Open accessThe DOI matches its Crossref record; 31 of the 31 references it cites were found in a registry or an index.
Abstract
The optimization of crystalline orientation of a Zn metal substrate to expose more Zn(0002) planes has been recognized as an effective strategy in pursuit of highly reversible Zn metal anodes. However, the lattice mismatch between substrate and overgrowth crystals has hampered the epitaxial sustainability of Zn metal. Herein, we discover that the presence of crystal grains deviating from [0001] orientation within a Zn(0002) metal anode leads to the failure of epitaxial mechanism. The electrodeposited [0001]-uniaxial oriented Zn metal anodes with a single (0002) texture fundamentally eliminate the lattice mismatch and achieve ultra-sustainable homoepitaxial growth. Using high-angle angular dark-filed scanning transmission electron microscopy, we elucidate the homoepitaxial growth of the deposited Zn following the “~ABABAB~” arrangement on the Zn(0002) metal from an atomic-level perspective. Such consistently epitaxial behavior of Zn metal retards dendrite formation and enables improved cycling, even in Zn||NH 4 V 4 O 10 pouch cells, with a high capacity of 220 mAh g−1 for over 450 cycles. The insights gained from this work on the [0001]-oriented Zn metal anode and its persistently homoepitaxial mechanism pave the way for other metal electrodes with high reversibility.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Scientific Challenges for the Implementation of Zn-Ion Batteries
Blanc, L. E., Kundu, D., & Nazar, L. F. (2020) · Joule · doi:10.1016/j.joule.2020.03.002 · Cited by 2,113
Reversible epitaxial electrodeposition of metals in battery anodes
Zheng, J., Zhao, Q., Tang, T., Yin, J., Quilty, C. D., Renderos, G. D., Liu, X., Deng, Y., Wang, L., Bock, D. C., et al. (2019) · Science · doi:10.1126/science.aax6873 · Cited by 1,877 · cited 2×
“Additionally, the residual stresses of Zn(0002) metal (14.8MPa) were found to be lower than that of com-Zn metal (22.8 MPa), indicating minimal lattice strain and mis fi t dislocations 9,39 .”
InfluentialJia, X., Liu, C., Neale, Z. G., Yang, J., & Cao, G. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.9b00628 · Cited by 1,791
Design principles for electrolytes and interfaces for stable lithium-metal batteries
Tikekar, M. D., Choudhury, S., Tu, Z., & Archer, L. A. (2016) · Nature Energy · doi:10.1038/nenergy.2016.114 · Cited by 1,765
Nanoscale Nucleation and Growth of Electrodeposited Lithium Metal
Pei, A., Zheng, G., Shi, F., Li, Y., & Cui, Y. (2017) · Nano Letters · doi:10.1021/acs.nanolett.6b04755 · Cited by 1,726 · cited 1×
“The Zn plating process canbedivided into two stages: nucleation and continuous growth, which are in fl u-enced by the current density in accordance with the Bulter-Volmer electrode kinetics relationship 46 .”
Atomic structure of sensitive battery materials and interfaces revealed by cryo–electron microscopy
Li, Y., Li, Y., Pei, A., Yan, K., Sun, Y., Wu, C.-L., Joubert, L.-M., Chin, R., Koh, A. L., Yu, Y., et al. (2017) · Science · doi:10.1126/science.aam6014 · Cited by 1,547
Surface‐Preferred Crystal Plane for a Stable and Reversible Zinc Anode
Zhou, M., Guo, S., Li, J., Luo, X., Liu, Z., Zhang, T., Cao, X., Long, M., Lu, B., Pan, A., et al. (2021) · Advanced Materials · doi:10.1002/adma.202100187 · Cited by 1,044 · cited 1×
“%) with the Zn(0002) plane 9,10 , optimizing the electrolyte to direct the generation of an optimum dense surface 11 , and reconstructing Zn metal matrix to regulate its crystallographic orientation 12 – 14 .”
Self-citationShape-Controlled Synthesis of Colloidal Metal Nanocrystals: Thermodynamic versus Kinetic Products
Xia, Y., Xia, X., & Peng, H.-C. (2015) · Journal of the American Chemical Society · doi:10.1021/jacs.5b04641 · Cited by 969
Wang, S., Ran, Q., Yao, R., Shi, H., Wen, Z., Zhao, M., Lang, X., & Jiang, Q. (2020) · Nature Communications · doi:10.1038/s41467-020-15478-4 · Cited by 833
Cryo-STEM mapping of solid–liquid interfaces and dendrites in lithium-metal batteries
Zachman, M. J., Tu, Z., Choudhury, S., Archer, L. A., & Kourkoutis, L. F. (2018) · Nature · doi:10.1038/s41586-018-0397-3 · Cited by 823 · cited 1×
“Zn metal shows a preference for forming disordered and nonplanar platelet electrodeposits at liquid-solid interfaces due to its lower thermodynamic free energy 41 – 45 .”
Cited by
Interfacial Biomacromolecular Engineering Toward Stable Ah‐Level Aqueous Zinc Batteries
Huang, J., Zhong, Y., Fu, H., Zhao, Y., Li, S., Xie, Y., Zhang, H., Lu, B., Chen, L., Liang, S., et al. (2024) · Advanced Materials · doi:10.1002/adma.202406257 · Cited by 192
Self-citation
Metadata
- Authors
- Zhang, X., Li, J., Liu, Y., Lu, B., Liang, S., & Zhou, J.
- Venue
- Nature Communications
- Published
- 2024-03-28
- Volume
- 15
- Issue
- 1
- Pages
- 2735-2735
- ISSN
- 2041-1723 (ISSN-L)
- OpenAlex
- W4393279922
- Cited by
- 232
- References
- 31
- FWCI
- 23.93
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Single [0001]-oriented zinc metal anode enables sustainable zinc batteries. https://app.cochat.ai/papers/10.1038/s41467-024-47101-1
- The paper
- Zhang, X., Li, J., Liu, Y., Lu, B., Liang, S., & Zhou, J. (2024). Single [0001]-oriented zinc metal anode enables sustainable zinc batteries. Nature Communications. https://doi.org/10.1038/s41467-024-47101-1
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.