The DOI matches its Crossref record.
Review of selective laser melting: Materials and applications
Open accessAbstract
Selective Laser Melting (SLM) is a particular rapid prototyping, 3D printing, or Additive Manufacturing (AM) technique designed to use high power-density laser to melt and fuse metallic powders. A component is built by selectively melting and fusing powders within and between layers. The SLM technique is also commonly known as direct selective laser sintering, LaserCusing, and direct metal laser sintering, and this technique has been proven to produce near net-shape parts up to 99.9% relative density. This enables the process to build near full density functional parts and has viable economic benefits. Recent developments of fibre optics and high-power laser have also enabled SLM to process different metallic materials, such as copper, aluminium, and tungsten. Similarly, this has also opened up research opportunities in SLM of ceramic and composite materials. The review presents the SLM process and some of the common physical phenomena associated with this AM technology. It then focuses on the following areas: (a) applications of SLM materials and (b) mechanical properties of SLM parts achieved in research publications. The review is not meant to put a ceiling on the capabilities of the SLM process but to enable readers to have an overview on the material properties achieved by the SLM process so far. Trends in research of SLM are also elaborated in the last section.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
The source backs part of the claim, not all of it — or backs it for a different population, condition or comparison.
In the citing paper
“The existing AM fatigue literature demonstrates test results that indicate porosity, residual stress and surface roughness are the largest concerns for high cycle fatigue (HCF) and low cycle fatigue (LCF) testing scenarios with overall fatigue properties generally substandard compared to conventional manufacturing processes [34,40,41].”
From Metal additive manufacturing in aerospace: A review (2021) · cites this paper as [41]
Experimental — accuracy not yet measuredThe cited source says what the claim attributes to it.
In the citing paper
“Once the process is optimized, the resulting components produced can boast mechanical properties exceeding those of conventional manufacturing techniques with proper procedures in place [34,41].”
From Metal additive manufacturing in aerospace: A review (2021) · cites this paper as [41]
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
No references could be resolved yet.
Research works printed but not linked: 203
- 2014, 3D Printing and Additive Manufacturing: Principles and Applications, 518
- 2007, Int. J. Mech. Mater. Des., 4, 181, 10.1007/s10999-007-9032-4 · DOI
- 2014, Metall. Mater. Trans. B, 45, 2247, 10.1007/s11663-014-0117-9 · DOI
- 2014, Metall. Mater. Trans. B, 45, 2279, 10.1007/s11663-014-0183-z · DOI
- 2015, Adv. Eng. Mater., 17, 942, 10.1002/adem.201400589 · DOI
- 2015, Metall. Mater. Trans. A, 46, 3864, 10.1007/s11661-015-2912-6 · DOI
- 2011, Int. J. Adv. Manuf. Technol., 59, 1025, 10.1007/s00170-011-3566-1 · DOI
- 2014, Intermetallics, 46, 147, 10.1016/j.intermet.2013.11.012 · DOI
- 2003, Adv. Eng. Mater., 5, 701, 10.1002/adem.200310099 · DOI
- 2000, Rapid Prototyping J., 6, 155, 10.1108/13552540010337029 · DOI
- 2003, Acta Mater., 51, 1651, 10.1016/S1359-6454(02)00567-0 · DOI
- 2002, Int. J. Adv. Manuf. Technol., 19, 351, 10.1007/s001700200024 · DOI
- 2005, Int. J. Heat Mass Transfer, 48, 3423, 10.1016/j.ijheatmasstransfer.2005.01.044 · DOI
- 2014, Virtual Phys. Prototyping, 9, 11, 10.1080/17452759.2013.869608 · DOI
- 2015, Int. J. Heat Mass Transfer, 80, 288, 10.1016/j.ijheatmasstransfer.2014.09.014 · DOI
- 2010, Rapid Prototyping J., 16, 248, 10.1108/13552541011049261 · DOI
- 2011, Rapid Prototyping J., 17, 195, 10.1108/13552541111124770 · DOI
- 2011, International Solid Freeform Fabrication Symposium: An Additive Manufacturing Conference, 227
- 2004, Rapid Prototyping J., 10, 78, 10.1108/13552540410526953 · DOI
- 2004, J. Mater. Process. Technol., 149, 616, 10.1016/j.jmatprotec.2003.11.051 · DOI
- 2015, Virtual Phys. Prototyping, 10, 67, 10.1080/17452759.2015.1026045 · DOI
- 2004, CIRP Ann., 53, 195, 10.1016/S0007-8506(07)60677-5 · DOI
- 2010, Phys. Proc., 5, 587, 10.1016/j.phpro.2010.08.086 · DOI
- 2001, J. Mater. Process. Technol., 111, 210, 10.1016/S0924-0136(01)00522-2 · DOI
- 2005, Manufacture of Stainless Steel Parts by Selective Laser Melting Process, 431
- 2010, Int. J. Adv. Manuf. Technol., 51, 639, 10.1007/s00170-010-2631-5 · DOI
- 2004, CIRP Ann., 53, 191, 10.1016/S0007-8506(07)60676-3 · DOI
- 2005, Proc. Inst. Mech. Eng., Part B, 219, 339, 10.1243/095440505X8109 · DOI
- 2005, Proc. Inst. Mech. Eng., Part B, 219, 379, 10.1243/095440505X32201 · DOI
- 2007, Int. J. Mach. Tools Manuf., 47, 779, 10.1016/j.ijmachtools.2006.09.013 · DOI
- 2009, Proc. Inst. Mech. Eng., Part B, 223, 1409, 10.1243/09544054JEM1574 · DOI
- 2005, Digital Manufacturing of Biocompatible Metal Frameworks for Complex Dental Prostheses by Means of SLS/SLM, 139
- 2005, CARS: Computer Assisted Radiology and Surgery, 690
- 2011, Equipment Manufacturing Technology and Automation, 174
- 2012, Rapid Prototyping J., 18, 482, 10.1108/13552541211272027 · DOI
- 2010, J. Mater. Eng. Perform., 19, 666, 10.1007/s11665-009-9535-2 · DOI
- 2009, Rapid Prototyping J., 15, 346, 10.1108/13552540910993879 · DOI
- 2011, Laser-Based Micro- and Nanopackaging and Assembly V
- 2007, J. Nucl. Mater., 362, 189, 10.1016/j.jnucmat.2007.01.078 · DOI
- 2012, Conformal Cooling in Moulds With Special Geometry, p. 409
- 2007, Laser-Based Micro- and Nanopackaging and Assembly, 45911
- 2007, Rapid Prototyping J., 13, 291, 10.1108/13552540710824797 · DOI
- 2007, Proc. Inst. Mech. Eng., Part B, 221, 945, 10.1243/09544054JEM764 · DOI
- 2012, Adv. Mater. Res., 502, 67, 10.4028/www.scientific.net/AMR.502.67 · DOI
- 2012, Mater. Res. Innovations, 16, 321, 10.1179/1433075X11Y.0000000045 · DOI
- 2006, High Performance Structures and Materials III, 481
- 2011, J. Sandwich Struct. Mater., 13, 479, 10.1177/1099636210388983 · DOI
- 2011, J. Sandwich Struct. Mater., 13, 303, 10.1177/1099636210380997 · DOI
- 2012, Shock Compression of Condensed Matter—2011
- 2012, Materials and Manufacturing Technologies XIV, 386
- 2010, J. Sandwich Struct. Mater., 12, 159, 10.1177/1099636209104536 · DOI
- 2013, Int. J. Impact Eng., 60, 120, 10.1016/j.ijimpeng.2013.04.007 · DOI
- 2009, J. Laser Micro Nanoeng., 4, 128, 10.2961/jlmn.2009.02.0010 · DOI
- 2008, Mater. Sci. Technol., 24, 1501, 10.1179/174328408X287691 · DOI
- 2011, Powder Metall., 54, 225, 10.1179/003258909X12450768326947 · DOI
- 2009, J. Sci. Ind. Res., 68, 1038
- 2013, Lasers in Manufacturing, 836
- 2009, Appl. Surf. Sci., 255, 5523, 10.1016/j.apsusc.2008.07.154 · DOI
- 2014, Opt. Laser Technol., 56, 451, 10.1016/j.optlastec.2013.09.017 · DOI
- 2006, CIRP Ann., 55, 187, 10.1016/S0007-8506(07)60395-3 · DOI
- 2012, Surf. Coat. Technol., 206, 4704, 10.1016/j.surfcoat.2012.05.072 · DOI
- 2014, J. Mater. Res., 29, 2036, 10.1557/jmr.2014.131 · DOI
- 2009, Mater. Manuf. Process., 24, 837, 10.1080/10426910902841837 · DOI
- 2009, Mater. Sci. Eng., A, 513–514, 64, 10.1016/j.msea.2009.01.053 · DOI
- 2012, Rapid Prototyping J., 18, 420, 10.1108/13552541211250418 · DOI
- 2011, Rapid Prototyping J., 17, 312, 10.1108/13552541111156450 · DOI
- 2006, Advanced Materials Forum III, 1, 516
- 2013, Mater. Charact., 84, 72, 10.1016/j.matchar.2013.07.010 · DOI
- 2009, J. Strain Anal. Eng. Des., 44, 93, 10.1243/03093247JSA464 · DOI
- 2012, Materialwiss. Werkstofftech., 43, 913, 10.1002/mawe.201200030 · DOI
- 2015, Wohlers Report
- 2013, Mater. Des., 50, 581, 10.1016/j.matdes.2013.03.056 · DOI
- 2013, Int. J. Adv. Manuf. Technol., 69, 1299, 10.1007/s00170-013-5106-7 · DOI
- 2013, Rapid Prototyping J., 19, 88, 10.1108/13552541311302932 · DOI
- 2011, Lasers in Manufacturing 2011: Proceedings of the Sixth International Wlt Conference on Lasers in Manufacturing, 255
- 2012, Int. J. Adv. Manuf. Technol., 60, 601, 10.1007/s00170-011-3643-5 · DOI
- 2013, Int. J. Adv. Manuf. Technol., 69, 1323, 10.1007/s00170-013-5121-8 · DOI
- 2013, Mater. Des., 47, 386, 10.1016/j.matdes.2012.11.062 · DOI
- 2012, Int. J. Adv. Manuf. Technol., 58, 1189, 10.1007/s00170-011-3443-y · DOI
- 2003, Proc. Inst. Mech. Eng., Part C, 217, 119, 10.1243/095440603762554668 · DOI
- 2006, Proc. Inst. Mech. Eng., Part C, 220, 857, 10.1243/09544062JMES133 · DOI
- 2009, J. Biomed. Mater. Res., Part B, 89B, 325, 10.1002/jbm.b.31219 · DOI
- 2009, J. Mater. Sci. Mater. Med., 20, 1839, 10.1007/s10856-009-3763-8 · DOI
- 2007, J. Biomed. Mater. Res., Part A, 83A, 272, 10.1002/jbm.a.31231 · DOI
- 2009, J. Mech. Behav. Biomed. Mater., 2, 20, 10.1016/j.jmbbm.2008.05.004 · DOI
- 2009, Tissue Eng., Part C, 15, 115, 10.1089/ten.tec.2008.0288 · DOI
- 2007, Rapid Prototyping J., 13, 196, 10.1108/13552540710776142 · DOI
- 2013, J. Mater. Sci. Mater. Med., 24, 745, 10.1007/s10856-012-4836-7 · DOI
- 2014, Virtual Phys. Prototyping, 9, 115, 10.1080/17452759.2014.900857 · DOI
- 2011, Mater. Charact., 62, 488, 10.1016/j.matchar.2011.03.006 · DOI
- 2012, Powder Metall., 55, 309, 10.1179/1743290112Y.0000000007 · DOI
- 2013, Titanium Scaffolds for Custom CMF Restorations, 517
- 2013, Acta Bioeng. Biomech., 15, 69, 10.5277/abb130109 · DOI
- 2012, Powder Metallurgy of Titanium: Powder Processing, Consolidation and Metallurgy of Titanium, 226
- 2012, Environmental Degradation of Engineering & Materials Engineering and Technologies, 225
- 2013, First CIRP Conference on Biomanufacturing, 79
- 2010, Mater. Lett., 64, 674, 10.1016/j.matlet.2009.12.035 · DOI
- 2013, Mater. Des., 49, 545, 10.1016/j.matdes.2013.01.038 · DOI
- 2011, Mater. Sci. Eng., A, 528, 7962, 10.1016/j.msea.2011.07.026 · DOI
- 2013, J. Mater. Process. Technol., 213, 1558, 10.1016/j.jmatprotec.2013.03.013 · DOI
- 2013, Biomed. Mater. Eng., 23, 433, 10.3233/BME-130765 · DOI
- 1999, Mater. Des., 20, 115, 10.1016/S0261-3069(99)00017-5 · DOI
- 2009, Single Part Microwave Filters Made From Selective Laser Melting, 1421
- 2012, Mater. Des., 41, 226, 10.1016/j.matdes.2012.05.017 · DOI
- 2004, Proc. Inst. Mech. Eng., Part C, 218, 711, 10.1243/0954406041319545 · DOI
- 2012, Acta Mater., 60, 3849, 10.1016/j.actamat.2012.04.006 · DOI
- 2013, Vacuum, 95, 25, 10.1016/j.vacuum.2013.02.003 · DOI
- 2011, Scr. Mater., 65, 21, 10.1016/j.scriptamat.2011.03.024 · DOI
- 2015, Virtual Phys. Prototyping, 10, 13, 10.1080/17452759.2015.1008643 · DOI
- 2012, J. Mech. Behav. Biomed. Mater., 9, 34, 10.1016/j.jmbbm.2012.01.008 · DOI
- 2010, Mater. Des., 31, 3982, 10.1016/j.matdes.2010.02.050 · DOI
- 2010, Selective Laser Melting of NiTi Shape Memory Components, 233
- 2012, Structural and Functional Properties of NiTi Shape Memory Alloys Produced by Selective Laser Melting, 291
- 2012, Acta Mater., 60, 2229, 10.1016/j.actamat.2011.12.032 · DOI
- 2012, J. Alloys Compd., 513, 518, 10.1016/j.jallcom.2011.10.107 · DOI
- 2013, Virtual Phys. Prototyping, 8, 87, 10.1080/17452759.2013.790600 · DOI
- 2011, Mater. Sci. Technol., 27, 344, 10.1179/026708309X12578491814591 · DOI
- 2012, Mater. Sci. Eng., A, 534, 446, 10.1016/j.msea.2011.11.092 · DOI
- 2013, Rapid Prototyping J., 19, 282, 10.1108/13552541311323281 · DOI
- 2006, Int. J. Mach. Tools Manuf., 46, 1188, 10.1016/j.ijmachtools.2006.01.024 · DOI
- 2013, Mater. Sci. Eng.,: C, 33, 419, 10.1016/j.msec.2012.09.008 · DOI
- 1998, Rapid Prototyping J., 4, 112, 10.1108/13552549810222939 · DOI
- 1998, J. Miner. Met. Mater. Soc., 50, 17, 10.1007/s11837-998-0299-1 · DOI
- 2013, J. Mater. Process. Technol., 213, 2126, 10.1016/j.jmatprotec.2013.06.013 · DOI
- 2011, Int. J. Adv. Manuf. Technol., 58, 545, 10.1007/s00170-011-3423-2 · DOI
- 2010, J. Mater. Process. Technol., 210, 1624, 10.1016/j.jmatprotec.2010.05.010 · DOI
- 2009, Rapid Prototyping J., 15, 96, 10.1108/13552540910943397 · DOI
- Process optimization and microstructural analysis for selective laser melting of AlSi10Mg, 484
- 2006, Powder Metall., 49, 258, 10.1179/174329006X95662 · DOI
- 2010, Virtual Phys. Prototyping, 5, 13, 10.1080/17452751003718629 · DOI
- 2012, Mater. Manuf. Process., 27, 1267, 10.1080/10426914.2012.663119 · DOI
- 2014, Int. J. Refract. Met. Hard Mater., 45, 15, 10.1016/j.ijrmhm.2014.02.007 · DOI
- 2013, Mater. Today, 16, 37, 10.1016/j.mattod.2013.01.018 · DOI
- S. P. Faure, L. Mercier, P. Didier, R. Roux, J. F. Coulon, and S. Garel, Laser Sintering Process Analysis: Application to Chromium-Cobalt Alloys For Dental Prosthesis Production (ASME, 2012), pp. 9–15. · DOI
- 2011, Virtual Phys. Prototyping, 6, 179, 10.1080/17452759.2011.619083 · DOI
- 2012, Odontology, 100, 249, 10.1007/s10266-011-0050-1 · DOI
- 2013, Dental Mater., 29, E91, 10.1016/j.dental.2013.04.007 · DOI
- 2013, J. Adv. Prosthodontics, 5, 471, 10.4047/jap.2013.5.4.471 · DOI
- 2011, Rapid Prototyping J., 17, 479, 10.1108/13552541111184206 · DOI
- 2003, Rapid Prototyping J., 9, 334, 10.1108/13552540310502239 · DOI · Paper page
- 2013, Appl. Therm. Eng., 52, 498, 10.1016/j.applthermaleng.2012.12.011 · DOI
- 2013, Metall. Italiana, 10, 15
- 2010, J. Mater. Eng. Perform., 20, 1049, 10.1007/s11665-010-9720-3 · DOI
- 2013, Med. Phys., 40, 012501, 10.1118/1.4769122 · DOI
- 2012, Rapid Prototyping J., 18, 81, 10.1108/13552541211193520 · DOI
- 2011, Gold Bull., 44, 113, 10.1007/s13404-011-0017-6 · DOI
- 2007, J. Mater. Process. Technol., 182, 564, 10.1016/j.jmatprotec.2006.09.026 · DOI
- 2007, Chin. Opt. Lett., 5, 37
- 2009, Mater. Des., 30, 2099, 10.1016/j.matdes.2008.08.036 · DOI
- 2014, Selective Laser Melting: On The Study of Microstructure of K220, 176
- 2012, Mater. Des., 34, 753, 10.1016/j.matdes.2011.06.061 · DOI
- 2010, Gold Bull., 43, 8, 10.1007/bf03214976 · DOI
- 2013, Int. J. Adv. Manuf. Technol., 67, 2743, 10.1007/s00170-012-4688-9 · DOI
- 2010, Selective Laser Melting of Magnesium for Future Applications in Medicine
- 2013, High Value Manufacturing: Advanced Research in Virtual and Rapid Prototyping: Proceedings of the 6th International Conference on Advanced Research in Virtual and Rapid Prototyping, Leiria, Portugal, 1–5 October 2013, 261
- 2013, High Value Manufacturing: Advanced Research in Virtual and Rapid Prototyping: Proceedings of the 6th International Conference on Advanced Research in Virtual and Rapid Prototyping, Leiria, Portugal, 1–5 October 2013, 267
- 2013, Rapid Prototyping J., 19, 51, 10.1108/13552541311292736 · DOI
- 2011, in SFF Symposium
- 2012, J. Sol-Gel Sci. Technol., 64, 704, 10.1007/s10971-012-2905-5 · DOI
- 2003, Int. J. Adv. Manuf. Technol., 21, 1015, 10.1007/s00170-002-1424-x · DOI
- 2007, Appl. Surf. Sci., 254, 989, 10.1016/j.apsusc.2007.08.085 · DOI
- 2007, Appl. Surf. Sci., 254, 966, 10.1016/j.apsusc.2007.09.001 · DOI
- 2007, Interceramics, 56, 420
- 2003, Mater. Des., 24, 623, 10.1016/S0261-3069(03)00126-2 · DOI
- 2012, Int. J. Adv. Manuf. Technol., 64, 239, 10.1007/s00170-012-3994-6 · DOI
- 1998, Mater. Manuf. Process., 13, 241, 10.1080/10426919808935239 · DOI
- 2009, Mater. Lett., 63, 1577, 10.1016/j.matlet.2009.04.010 · DOI
- 2007, J. Mater. Sci., 42, 7647, 10.1007/s10853-007-1661-3 · DOI
- 2009, J. Mater. Process. Technol., 209, 5793, 10.1016/j.jmatprotec.2009.06.012 · DOI
- 2011, J. Biomed. Mater. Res., Part A, 97, 466, 10.1002/jbm.a.33058 · DOI
- 2011, Surf. Coat. Technol., 205, 3285, 10.1016/j.surfcoat.2010.11.051 · DOI
- 2011, Powder Metall. Metal Ceram., 50, 275, 10.1007/s11106-011-9329-6 · DOI
- 2012, Virtual Phys. Prototyping, 7, 107, 10.1080/17452759.2012.687911 · DOI
- 2000, Mater. Des., 21, 63, 10.1016/S0261-3069(99)00057-6 · DOI
- 2012, Powder Technol., 231, 112, 10.1016/j.powtec.2012.07.061 · DOI
- 2009, Mater. Lett., 63, 2536, 10.1016/j.matlet.2009.08.043 · DOI
- 2010, Acta Metall. Sin., 46, 761, 10.3724/SP.J.1037.2010.00761 · DOI
- 2009, Appl. Surf. Sci., 255, 9230, 10.1016/j.apsusc.2009.07.008 · DOI
- 2011, Compos. Sci. Technol., 71, 1612, 10.1016/j.compscitech.2011.07.010 · DOI
- 2010, Mater. Sci. Eng., A, 527, 7585, 10.1016/j.msea.2010.08.075 · DOI
- 2009, Int. J. Adv. Manuf. Technol., 48, 597, 10.1007/s00170-009-2304-4 · DOI
- 2006, J. Alloys Compd., 421, 166, 10.1016/j.jallcom.2005.09.084 · DOI
- 2011, Adv. Compos. Mater., 20, 277, 10.1163/092430410X547092 · DOI
- 2008, Appl. Surf. Sci., 254, 3971, 10.1016/j.apsusc.2007.12.028 · DOI
- 2009, J. Mater. Res., 24, 3397, 10.1557/jmr.2009.0419 · DOI
- 2012, J. Alloys Compd., 541, 328, 10.1016/j.jallcom.2012.06.097 · DOI
- 2012, Scr. Mater., 67, 185, 10.1016/j.scriptamat.2012.04.013 · DOI
- 2012, Metall. Mater. Trans. A, 43A, 697, 10.1007/s11661-011-0876-8 · DOI
- 2013, J. Alloys Compd., 579, 415, 10.1016/j.jallcom.2013.06.087 · DOI
- 2002, Solid Freeform Fabrication Symposium, 224
- 2003, CIRP Ann., 52, 173, 10.1016/S0007-8506(07)60558-7 · DOI
- 2006, Mater. Sci. Eng., A, 435–436, 54, 10.1016/j.msea.2006.07.105 · DOI
- 2013, Virtual Phys. Prototyping, 8, 11, 10.1080/17452759.2013.772319 · DOI
- 2007, Mater. Sci. Eng., A, 445–446, 316, 10.1016/j.msea.2006.09.057 · DOI
- 2010, Rapid Prototyping J., 16, 258, 10.1108/13552541011049270 · DOI
- 2011, Mater. Des., 32, 139, 10.1016/j.matdes.2010.06.020 · DOI
- 2013, Virtual Phys. Prototyping, 8, 19, 10.1080/17452759.2013.778175 · DOI
- 2014, Mater. Charact., 94, 116, 10.1016/j.matchar.2014.05.001 · DOI
- 2013, J. Mater. Process. Technol., 213, 1019, 10.1016/j.jmatprotec.2013.01.020 · DOI · Paper page
- 2014, Virtual Phys. Prototyping, 9, 213, 10.1080/17452759.2014.949406 · DOI
200 of 203 shown
Cited by
Sorted by citations
Items 401–500 of 1,007
Borges, D. J. A., Souza, A. M., & da Silva, E. J. (2023) · Machining Science and Technology · doi:10.1080/10910344.2023.2253027 · Cited by 14
“According to Tian et al. (2019a), diamond abrasive grains do not generally melt during the SLM process; however, depending on the laser energy density some grains may burn, resulting in surface graphitization of diamond, thus decreasing the holding strength (given by the binder agent) of abrasives in the metal matrix.”
BackgroundInfluentialTusher, M. M. H., & Ince, A. (2023) · Materials Performance and Characterization · doi:10.1520/mpc20220088 · Cited by 15
SLM Additive Manufacturing of Oscillating Heat Pipe
Chen, K.-L., Luo, K., Gupta, P., & Kang, S.-W. (2023) · Sustainability · doi:10.3390/su15097538 · Cited by 13
Ultrasonic-based surface patterning and interfacial reaction of ZrO2 ceramics
Dong, H.-J., Li, Z.-L., Song, X., Feng, J.-C., Wei, S.-J., Fu, J.-H., & Shi, Y. (2023) · Journal of Materials Science & Technology · doi:10.1016/j.jmst.2022.11.067 · Cited by 13
Leban, M. B., Hren, M., & Kosec, T. (2023) · Scientific Reports · doi:10.1038/s41598-023-28971-9 · Cited by 13
Lin, Z., Zhu, M.-P., Song, C., Liu, T.-B., Yin, C., Zeng, T., & Shao, J.-D. (2023) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2023.169443 · Cited by 13
Recent Developments in Additive-Manufactured Intermetallic Compounds for Bio-Implant Applications
Yeh, P.-Y., Huang, J. C., Jang, J. S., Pan, C.-T., Chen, C.-H., & Lin, C.-H. (2022) · Journal of Medical and Biological Engineering · doi:10.1007/s40846-022-00753-0 · Cited by 13
Corrosion of nickel-based alloys fabricated through additive manufacturing: a review
Mehta, S., Jha, S., & Liang, H. (2022) · Progress in Additive Manufacturing · doi:10.1007/s40964-022-00298-3 · Cited by 13
“Adapted with permission from reference [69].”
Zhao, J.-C., Liu, J.-B., Huang, L.-Y., Ren, K., & Cao, Y. (2026) · Journal of Manufacturing Processes · doi:10.1016/j.jmapro.2026.02.064 · Cited by 12
Xue, X.-Y., Bao, J.-G., Wu, Z.-K., Zhao, Y., Da, R., Yang, D.-B., Wu, S.-C., Burnett, T. L., & Withers, P. J. (2026) · Materials science & engineering. R, Reports · doi:10.1016/j.mser.2026.101197 · Cited by 12
Comparative study of LPBF Ta–Ti alloy: microstructural evolution and deformation behavior
Yang, Z.-Y., Qiu, Y., Zhu, J.-Q., Huang, Z.-F., Dai, S.-B., Yang, W.-H., Liu, M., Wang, G., Yan, X.-C., & Huang, W. (2025) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2025.08.165 · Cited by 12
Kadavath, J. K., Krishnan, B., Pelaes, R. F. C., Guzman, S. S., García-Gomez, N. A., Avellaneda, D., & Shaji, S. (2025) · Microchemical journal (Print) · doi:10.1016/j.microc.2025.114537 · Cited by 12
Tekdir, H., Yetim, A., Yıldız, F., Kaymaz, I., & Korkmaz, I. H. (2025) · Fatigue & Fracture of Engineering Materials & Structures · doi:10.1111/ffe.14676 · Cited by 12
Gadlegaonkar, N., Bansod, P., Lakshmikanthan, A., Bhole, K., C., M., & Linul, E. (2025) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2025.04.039 · Cited by 12
Anisotropic creep and stress rupture behaviour of laser powder bed fusion processed Hastelloy X
Agrawal, S., Kumar, C., Avadhani, G. S., Heilmaier, M., & Suwas, S. (2025) · Materials Science & Engineering: A · doi:10.1016/j.msea.2025.148342 · Cited by 12
Liu, Y., Liu, X., Lu, J.-Z., Zhang, Z.-Y., Luo, K.-Y., Huang, S., Lu, H.-F., Xu, G., Dai, G.-Q., & Zhou, S.-Y. (2025) · Virtual and Physical Prototyping · doi:10.1080/17452759.2024.2430328 · Cited by 12
“AM had been widely used in the manufacturing of various titanium alloy components [8].”
Petousis, M., Nasikas, N. K., Papadakis, V. M., Valsamos, I., Gkagkanatsiou, K., Mountakis, N., Argyros, A., Dimitriou, E., Michailidis, N., & Vidakis, N. (2025) · Polymers · doi:10.3390/polym17030410 · Cited by 12
“The latter is also the reason why AM is frequently termed three-dimensional printing or just 3D printing (3DP) [4–6].”
Deformation Behavior of Inconel 625 Alloy with TPMS Structure
Xu, K., Cao, J.-H., Zheng, Z.-W., Zhao, R., Xu, G., Wang, H., Wang, J., Hur, B., & Yue, X.-Z. (2025) · Materials · doi:10.3390/ma18020396 · Cited by 12
Horňas, J., Materna, A., Glinz, J., Yosifov, M., & Senck, S. (2024) · Engineering Fracture Mechanics · doi:10.1016/j.engfracmech.2024.110756 · Cited by 14
Chen, S., Chu, S.-J., & Mao, B. (2024) · Acta Metallurgica Sinica · doi:10.1007/s40195-024-01758-1 · Cited by 12
Jeong, J.-U., Lee, K.-K., Ahn, D.-G., & Lee, J.-W. (2024) · Journal of Mechanical Science and Technology · doi:10.1007/s12206-024-2412-y · Cited by 12
Kim, C., & Jang, I. (2024) · Journal of Physics Energy · doi:10.1088/2515-7655/ad5fbb · Cited by 11
Hatos, I., Hargitai, H., Fekete, G., & Fekete, I. (2024) · Materials · doi:10.3390/ma17143432 · Cited by 12
“The main parameters include the layer thickness, scanning speed, laser power, hatch spacing, scanning direction, and strategy [10].”
BackgroundJuri, A., Arachchige, Y., Nguyen, P., Ryszawa, M., Tran, B., Rapagna, S., Perilli, E., Labrinidis, A., & Yin, L. (2024) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2024.07.029 · Cited by 12
Model-Based Sensitivity Analysis of the Temperature in Laser Powder Bed Fusion
Yang, Z., Zhang, S.-T., Ji, X., & Liang, S. Y. (2024) · Materials · doi:10.3390/ma17112565 · Cited by 12
Hu, Q.-J., Luo, D., Guo, J., & Qiu, W.-B. (2023) · ACS Applied Materials and Interfaces · doi:10.1021/acsami.3c08116 · Cited by 12
Kumar, N., Kumar, M., Kumar, V. V., & Sharma, A. (2023) · JOM · doi:10.1007/s11837-023-05756-z · Cited by 12
Electrochemical Anisotropy of Hastelloy X Fabricated by Selective Laser Melting in a NaNO3 Solution
Zhang, S.-L., Shi, Y., Zhang, Y.-P., Guo, P.-F., Li, X., & Luo, K. (2023) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2023.169947 · Cited by 12
Staroń, S., Macioł, P., Dubiel, B., Gola, K., & Falkus, J. (2023) · Archives of Civil and Mechanical Engineering · doi:10.1007/s43452-023-00626-6 · Cited by 12
“, in aerospace, energy, and chemical industries [2].”
BackgroundXia, J., Xin, D., Chen, X.-Z., & Xin, H. (2022) · Journal of Materials Science · doi:10.1007/s10853-022-07792-7 · Cited by 12
Evaluation of microstructure and porosity for 3D printed stainless steel
Aripin, M. A., Sajuri, Z., Syarif, J., Baghdadi, A., & Mohamed, I. F. (2022) · Materials Today: Proceedings · doi:10.1016/j.matpr.2022.07.396 · Cited by 12
Assi, M., Favre, J., Fraczkiewicz, A., & Tancret, F. (2022) · Journal of Materials Science · doi:10.1007/s10853-022-07441-z · Cited by 12
Laser induced keyhole reshaping in laser powder bed fusion of aluminum alloy
Hua, S., Pan, Y., Guo, Q.-H., Zhang, G., Dong, F., Zhang, C., & Liu, S. (2025) · Additive Manufacturing · doi:10.1016/j.addma.2025.104993 · Cited by 11
High-temperature oxidation behavior of gas-atomized CoCrFeNiCu high-entropy alloy powders
Ren, M.-Z., Ren, L., Ma, Y.-F., Yang, Z., Xu, Y., Li, Q.-M., Gong, P., Deng, L., Jin, J.-S., Tang, X., et al. (2025) · Applications of Surface Science · doi:10.1016/j.apsusc.2025.162561 · Cited by 11
Investigating Melt Pool Dimensions in Laser Powder Bed Fusion of Nitinol: An Analytical Approach
Rangaswamy, S., Bourke, D., Monu, M., Healy, P., Gu, H.-S., Ahad, I., & Brabazon, D. (2024) · Advanced Engineering Materials · doi:10.1002/adem.202401636 · Cited by 11
Influence of porous titanium-based jaw implant structure on osseointegration mechanisms.
Kilina, P., Kuchumov, A., Sirotenko, L., Vassilouk, V., Golovin, S., Drozdov, A., & Sadyrin, E. (2024) · Journal of The Mechanical Behavior of Biomedical Materials · doi:10.1016/j.jmbbm.2024.106724 · Cited by 11
Feng, Y.-J., Wang, H.-F., Zhao, Z.-X., Chen, D.-H., Peng, Y.-W., Gong, J.-M., & Somers, M. A. J. (2024) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2024.09.165 · Cited by 11
Kumar, M. S., Jeyaprakash, N., & Yang, C.-H. (2024) · Engineering Failure Analysis · doi:10.1016/j.engfailanal.2024.108206 · Cited by 11
Chen, J., Zheng, Z., Wang, D., Bi, G.-J., & Bai, Y.-C. (2024) · Additive Manufacturing Frontiers · doi:10.1016/j.amf.2024.200150 · Cited by 11
Interpenetrating microstructure in laser powder-bed fusion parts using selective rescanning
Ravichander, B., Jagdale, S. H., & Kumar, G. (2024) · Additive Manufacturing Letters · doi:10.1016/j.addlet.2024.100221 · Cited by 11
Li, Y., Xu, J., Liu, B., Gao, Y.-B., Xue, S., Hu, Y., Ding, Y.-T., Zhang, D., & Lu, S.-J. (2024) · Materials Science & Engineering: A · doi:10.1016/j.msea.2024.146412 · Cited by 11
Self-citationZhao, G., Wang, R.-K., Li, F.-Y., & Liu, J. (2024) · Virtual and Physical Prototyping · doi:10.1080/17452759.2024.2324429 · Cited by 11
“Laser powder bed fusion (LPBF) [11] is a powder-based layer-by-layer metal AM process, that can produce high-density metal parts with complex shapes and precise microstructures [12 – 14].”
Effects of Preheating on Thermal Behavior in Inconel 718 Processed by Additive Manufacturing
Chowdhury, H. T., Naidu, P. T., Kakuta, N., & Kakehi, K. (2024) · Thermo · doi:10.3390/thermo4010005 · Cited by 11
“Some SLM machines can provide preheating to the building chamber or the substrate plate [1].”
BackgroundInfluentialOpportunities and limitations of metal additive manufacturing of structured catalytic converters
Mehdipour, F., Delrieux, T., Maurer, F., Grunwaldt, J., Klahn, C., & Dittmeyer, R. (2024) · Catalysis Communications · doi:10.1016/j.catcom.2024.106873 · Cited by 17
“To protect LB-PBF manufacturing against oxidation of the metals, the construction chamber is filled with an inert gas like argon or nitrogen [67,74 – 76].”
Gallab, M., Le, P. T. M., Shintani, S. A., Takadama, H., Ito, M., Kitagaki, H., Matsushita, T., Honda, S., Okuzu, Y., Fujibayashi, S., et al. (2024) · Biomaterials Advances · doi:10.1016/j.bioadv.2024.213781 · Cited by 11
Polyzos, E., Pulju, H., Mackel, P., Hinderdael, M., Ertveldt, J., Hemelrijck, D. V., & Pyl, L. (2023) · Materials · doi:10.3390/ma16041444 · Cited by 11
“Laser applications have become increasingly prominent in recent years, with applications being found in a variety of fields, such as additive manufacturing [1].”
Liu, W., Lee, M.-H., Guo, R., & Yao, J.-Y. (2023) · Inorganic Chemistry · doi:10.1021/acs.inorgchem.2c04499 · Cited by 11
Caprio, L., Demir, A., & Previtali, B. (2022) · Journal of Physics D: Applied Physics · doi:10.1088/1361-6463/ac984c · Cited by 11
Batalha, W. C., Batalha, R., Kosiba, K., Kiminami, C., & Gargarella, P. (2022) · Journal of Materials Research · doi:10.1557/s43578-022-00735-7 · Cited by 11
Zeng, S.-J., He, W., Wang, J., Xu, M., & Wei, T.-P. (2022) · Journal of materials engineering and performance (Print) · doi:10.1007/s11665-022-07377-0 · Cited by 11
Yang, J.-L., Li, C.-W., Yuan, Y., Huang, Y., Zhang, H., Yang, X.-D., & Gu, J.-F. (2025) · Materials Science & Engineering: A · doi:10.1016/j.msea.2025.148919 · Cited by 10
Huang, Y.-J. X., Li, X.-R., Chen, H.-Y., Ren, K., Guo, H., & Qi, H. (2025) · Materials · doi:10.3390/ma18112605 · Cited by 10
“These challenges stem from zirconia’s intrinsic properties, including a high melting point, limited ductility, and poor thermal shock resistance [32–34].”
Law, W. K., Wang, H.-L., Song, C., Wong, K., Lim, C. S., & Sun, Z. (2025) · International journal of plasticity · doi:10.1016/j.ijplas.2025.104400 · Cited by 10
AlMgScZr alloys for laser powder bed fusion additive manufacturing. A review
González-Rovira, L., Cabrera-Correa, L., López-Castro, J. D. D., Ojeda-López, A., & Botana, F. J. (2025) · Materials & Design · doi:10.1016/j.matdes.2025.114080 · Cited by 10
Daniel, S., & Anand, P. (2025) · Proceedings of the Institution of mechanical engineers. Part E, journal of process mechanical engineering · doi:10.1177/09544089251317120 · Cited by 10
Hu, M.-J., Chi, Q., Ji, L.-K., Li, W.-W., Yan, S., & Cheng, F. (2024) · Materials · doi:10.3390/ma17215376 · Cited by 10
Wu, W.-Z., Tang, X., Guo, J.-Y., Wang, J., Zhang, X., & Zhao, C.-H. (2024) · Journal of Applied Electrochemistry · doi:10.1007/s10800-024-02181-1 · Cited by 10
“In the field of manufacturing metal 3D structures, the widely used additive manufacturing (AM) method are high-energy beam-driven technologies, such as selective laser melting (SLM) or sintering (SLS) [7, 8].”
Estrada-Díaz, J. A., Elías-Zúñiga, A., Martínez-Romero, O., Palacios-Pineda, L. M., Guzmán-Nogales, R., Cedeño-Viveros, L. D., & Olvera-Trejo, D. (2024) · International Journal of Sustainable Engineering · doi:10.1080/19397038.2024.2327386 · Cited by 10
“Conversely, excessively large energetic input conditions lead to issues such as delamination, porosity caused by gas entrapment, and balling phenomena, among others (Yap et al. 2015).”
InfluentialNumerical simulation of thermal processes in cold metal transfer-based additive manufacturing
Li, L., Jiang, Y.-N., Xiao, Y.-C., Chen, H.-R., & Shi, L. (2024) · The International Journal of Advanced Manufacturing Technology · doi:10.1007/s00170-024-13019-7 · Cited by 10
“Depending on the employed heat source and the material, metal additive manufacturing technology can be divided into electron beam selective melting (EBSM) [3], selective laser melting (SLM) [4], laser engineered net shaping (LENS) [5], wire arc additive manufacturing (WAAN)[6] and so on.”
Tardelli, J., Valente, M. L. D. C., Otani, L., Batalha, R., Alves, F., Pereira-da-Siva, M. A., Bagnato, V., Dibb, R., Gargarella, P., Bolfarini, C., et al. (2023) · Ceramics International · doi:10.1016/j.ceramint.2023.11.008 · Cited by 10
Yuan, X.-Y., Li, W.-B., & Deng, M.-X. (2023) · Measurement science and technology · doi:10.1088/1361-6501/ad0707 · Cited by 10
A lattice structure coupon sample for build quality control in metal additive manufacturing
Park, M., Venter, M., & du Plessis, A. (2023) · Materials & Design · doi:10.1016/j.matdes.2023.112436 · Cited by 10
Towards Selective Laser Melting of High-Density Tungsten
Zhang, H.-P., Wang, D.-K., Li, X.-Y., Yin, F.-S., Zhang, L., Li, X.-D., & Qu, X. (2023) · Metals · doi:10.3390/met13081431 · Cited by 10
Feng, Y.-J., Duan, H., Zhao, Z., Liu, Z., Peng, Y.-W., Gong, J., & Somers, M. W. (2023) · Surface & Coatings Technology · doi:10.1016/j.surfcoat.2023.129874 · Cited by 10
Self-citationA short review on SLM-processed Ti6Al4V composites
Kathiresan, M., KARTHIKEYAN, M., & Immanuel, R. J. (2023) · Proceedings of the Institution of Mechanical Engineers Part E Journal of Process Mechanical Engineering · doi:10.1177/09544089231169380 · Cited by 11
“34,35 32, 34 Other features associated associated with the SLM process include a”
Yan, Y., Lu, C., Chen, Z., Zhuo, Y., Wang, C.-Y., & Jia, Q. (2023) · Metals · doi:10.3390/met13040788 · Cited by 10
Gorey, T., Stull, J., Hackenberg, R., Clark, C., & Hooks, D. (2022) · JOM · doi:10.1007/s11837-022-05558-9 · Cited by 10
Laser printing: trends and perspectives
Chichkov, B. (2022) · Applied Physics A · doi:10.1007/s00339-022-06158-9 · Cited by 10
Zhou, Z.-L., He, D., Tan, Z., Wang, Y., Shao, W., Guo, X.-Y., Zhou, Z., Wu, X., Cui, L., Wang, B.-P., et al. (2022) · Journal of Manufacturing Processes · doi:10.1016/j.jmapro.2022.08.005 · Cited by 10
Bittner, F., Thielsch, J., & Drossel, W. (2022) · IEEE transactions on magnetics · doi:10.1109/tmag.2022.3167246 · Cited by 10
Hein, M., Dias, N. F. L., Kokalj, D., Stangier, D., Hoyer, K., Tillmann, W., & Schaper, M. (2022) · International Journal of Fatigue · doi:10.1016/j.ijfatigue.2022.107235 · Cited by 10
Wang, S.-H., Qu, H.-Y., Yu, S., & Zhang, S.-X. (2022) · Materials Today: Proceedings · doi:10.1016/j.matpr.2022.08.559 · Cited by 10
Li, F.-Y., Wang, R.-K., Zheng, Z.-J., & Liu, J. (2022) · Virtual and Physical Prototyping · doi:10.1080/17452759.2022.2074196 · Cited by 10
“Selective laser melting (SLM) is a famous metal AM that can produce highdensity and complex shape metal parts with fine microstructures, which are difficult or even impossible to achieve with traditional manufacturing techniques (Kumar et al. 2021; Nagarajan et al. 2019; Yap et al. 2015; Zhu et al. 2021).”
BackgroundAdditive Manufacturing feasibility of WC-17Co cermet parts by Laser Powder Bed Fusion
Papy, K., Sova, A., Borbély, A., Staerk, J.-M., Favre, J., Roulon, Z., Sijobert, J., & Bertrand, P. (2022) · Procedia CIRP · doi:10.1016/j.procir.2022.08.049 · Cited by 10
Mussatto, A., Groarke, R., Vijayaraghavan, R. K., Obeidi, M., Macloughlin, R., McNally, P., Nicolosi, V., Delaure, Y., & Brabazon, D. (2022) · Materials Chemistry and Physics · doi:10.1016/j.matchemphys.2022.126245 · Cited by 10
Łach, Ł., & Svyetlichnyy, D. S. (2026) · Materials · doi:10.3390/ma19020426 · Cited by 13
Yang, B., Liu, Y.-G., Qi, Y., Wei, K.-W., Gong, J.-Q., Wang, Y.-S., & Zeng, X.-Y. (2025) · Materials Science & Engineering: A · doi:10.1016/j.msea.2025.149084 · Cited by 9
A Review of Selective Laser Sintering/Melting Techniques for Lunar Construction
Agapkin, I. A., & Slyuta, E. (2025) · Acta Astronautica · doi:10.1016/j.actaastro.2025.08.047 · Cited by 9
Gao, Z.-J., Li, H., Ma, T., Yang, H., Wang, W., Wei, W., Huang, H., Wen, S.-P., & Nie, Z.-R. (2025) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2025.07.186 · Cited by 9
Additive Manufacturing of Vapor Chambers
Chen, K., Hsu, S.-C., & Kang, S.-W. (2025) · Materials · doi:10.3390/ma18050979 · Cited by 9
“Components are built by selectively melting and fusing the powder within and between layers [24].”
Tinajero, C., Palmara, G., Zanatta, M., & Sans, V. (2025) · Chemical Engineering Journal · doi:10.1016/j.cej.2025.159442 · Cited by 9
Processing of pure copper by powder bed fusion with infrared laser
Calignano, F., Bove, A., & Pavese, M. (2025) · Results in Engineering · doi:10.1016/j.rineng.2025.104497 · Cited by 9
Deng, X., Hu, Y.-N., Yi, Y., Kan, Q.-H., & Kang, G.-Z. (2025) · Engineering Failure Analysis · doi:10.1016/j.engfailanal.2025.109367 · Cited by 9
Giarmas, E., Tsakalos, V., Tzimtzimis, E., Kladovasilakis, N., Kostavelis, I., Tzovaras, D., & Tzetzis, D. (2024) · The International Journal of Advanced Manufacturing Technology · doi:10.1007/s00170-024-14007-7 · Cited by 9
Strakošová, A., Roudnická, M., Šafka, J., Ackermann, M., Dvorský, D., Školáková, A., Vronka, M., Svora, P., Drahokoupil, J., Pinc, J., et al. (2024) · Additive Manufacturing · doi:10.1016/j.addma.2024.104264 · Cited by 9
Aronne, M., Bertana, V., Schimmenti, F., Roppolo, I., Chiappone, A., Cocuzza, M., Marasso, S., Scaltrito, L., & Ferrero, S. (2024) · Micromachines · doi:10.3390/mi15060678 · Cited by 9
“…parameters, SLM can produce a complete, dense, near-net-shaped part, with a one-step process, without the need of intense post-processing treatments and without the need for binders, improving the printed object quality, the time for the process, and reproducibility of the printing process [28].”
BackgroundSasnauskas, A., Coban, A., Zhang, W.-Y., Abbot, W. M., Babu, R., Pham, M.-S., & Lupoi, R. (2024) · CIRP annals · doi:10.1016/j.cirp.2024.04.066 · Cited by 9
Cakmak, O., Chung, S., Lee, S.-H., Koo, J.-H., Yeom, H., & Cho, J.-W. (2024) · Additive Manufacturing Letters · doi:10.1016/j.addlet.2024.100219 · Cited by 9
Sanchez, S., Zafari, A., Caprio, L., Demir, A., & Jafari, D. (2024) · Lasers in Manufacturing and Materials Processing · doi:10.1007/s40516-023-00244-3 · Cited by 9
“However, limits in LPBF feature resolution (~ 100 μm) [4] result in pores of ~ 100–200 μm diameter, which are too large for these applications.”
Ayalew, A., Han, X., Suzuki, K., Yoshida, S., & Sakairi, M. (2023) · Materials Today Communications · doi:10.1016/j.mtcomm.2023.107069 · Cited by 9
Additive manufacturing of biomaterials: A review
Jayanth, N., Roshan, M. V., Balaji, S. S., Karthik, P. D., Barathwaj, A., & Rishiyadhav, G. (2023) · Materials Today Proceedings · doi:10.1016/j.matpr.2023.09.190 · Cited by 15
Numerical and Experimental Characterization of Melt Pool in Laser Powder Bed Fusion of SS316l
Khan, A., Jaffery, S. I., Hussain, S., Anwar, Z., & Dilawar, S. (2023) · Integrating Materials and Manufacturing Innovation · doi:10.1007/s40192-023-00302-w · Cited by 9
Yan, R.-H., & Liu, Z. (2023) · Coatings · doi:10.3390/coatings13050845 · Cited by 9
Self-citationA Short and Technical Review on Lattice Structures Produced by Additive Manufacturing
Özdemir, M. T., & Korkmaz, M. (2023) · Prabha Materials Science Letters · doi:10.33889/pmsl.2023.2.1.005 · Cited by 9
“SLM process is used for materials such as titanium and alloys, nickel superalloys (Inconel 625/718, Hastelloy X), copper alloys, valuable mines (gold, silver), cobalt chrome alloys, aluminum alloys, stainless and tool steels (Yap et al., 2015).”
Dezső, G., Szigeti, F., & Varga, G. (2022) · Periodica Polytechnica: Mechanical Engineering · doi:10.3311/ppme.21124 · Cited by 9
“Direct metal selective laser melting (DMSLM, or here referred as SLM) today widely applied for manufacturing metallic parts [2, 3].”
BackgroundZhang, J.-H., Lyu, T., Hua, Y., Shen, Z., Sun, Q., Rong, Y., & Zou, Y. (2022) · Integrating Materials and Manufacturing Innovation · doi:10.1007/s40192-022-00272-5 · Cited by 9
Cao, Y.-F., Moumni, Z., Zhu, J.-H., Gu, X.-J., & Zhang, W.-H. (2022) · Materials Science & Engineering: A · doi:10.1016/j.msea.2022.143598 · Cited by 9
He, M.-R., Banerjee, A., Marvel, C., Price, S., McCue, I., Schwalbach, E., & Hemker, K. (2022) · Metallurgical and Materials Transactions. A · doi:10.1007/s11661-022-06715-0 · Cited by 9
Advanced ceramic coatings on aluminum by laser treatment of filled organosilazane-based composites
Horcher, A., Tangermann-Gerk, K., Krenkel, W., Schafföner, S., & Motz, G. (2022) · Ceramics International · doi:10.1016/j.ceramint.2022.04.314 · Cited by 9
Metadata
- Authors
- Yap, C. Y., Chua, C. K., Dong, Z. L., Liu, Z. H., Zhang, D. Q., Loh, L. E., & Sing, S. L.
- Affiliations
- Nanyang Technological University (SG)
- Venue
- Applied Physics Reviews
- Publisher
- AIP Publishing
- Published
- 2015-12-01
- Volume
- 2
- Issue
- 4
- ISSN
- 1931-9401 (ISSN-L)
- OpenAlex
- W2192772080
- Cited by
- 2,353
- References
- 0
- Citations by year
- 2026: 170 · 2025: 269 · 2024: 262 · 2023: 296 · 2022: 341 · 2021: 325 · 2020: 262 · 2019: 190 · 2018: 130 · 2017: 77 · 2016: 31
- FWCI
- 77.93
- Type
- journal article
- Language
- en
- Open access
- bronze
- doi.org
- Locations
- Applied Physics Reviews (publishedVersion)
- DR-NTU (Nanyang Technological University) (submittedVersion)
- Funders
- Nanyang Technological University
- Topics
- Physical Sciences › Engineering › Mechanical Engineering › Additive Manufacturing Materials and Processes
- Physical Sciences › Engineering › Industrial and Manufacturing Engineering › Additive Manufacturing and 3D Printing Technologies
- Physical Sciences › Engineering › Mechanical Engineering › Powder Metallurgy Techniques and Materials
- Keywords
- laser powder bed fusion, additive manufacturing, direct metal laser sintering, near-net-shape parts, relative density, copper, aluminum, tungsten, fiber optics, high-power lasers
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review