CoChat

Durability of reactive magnesia-activated slag-stabilized low plasticity clay subjected to drying–wetting cycle

Du, Yan-Jun, Bo, Yu-Lin, Jin, Fei, Liu, Chen-Yang · 2016 · European Journal of Environmental and Civil Engineering
Cited by 116

The DOI matches its Crossref record; 2 of the 2 references it cites were found in a registry or an index.

Abstract

The strength characteristics and hydration products of reactive magnesia (MgO)-activated ground-granulated blast-furnace slag (GGBS) cement and concrete have been extensively investigated in previous studies. However, very limited study has comprehensively investigated the impacts of drying–wetting cycle on the engineering properties of GGBS–MgO-stabilised soils. This paper presents details of a study dealing with the influences of drying–wetting cycle on the dry density, pH, unconfined compressive strength (qu) and secant modulus (E50) of GGBS–MgO-stabilised kaolin clay. For the purpose of comparison, the conventional Portland cement (PC)-stabilised kaolin clay is selected as a control sample. Several series of and drying–wetting durability and unconfined compression tests were conducted for the stabilised soils. The variations in dry density, mass loss, pH, qu and E50 with drying–wetting cycle are discussed. The results show that the GGBS–MgO-stabilised kaolin clay display higher dry density (~1–7%) and lower mass loss (~10–30%) than the PC-stabilised kaolin clay. The pH values and qu of the GGBS–MgO-and PC-stabilised kaolin clay decrease with the increase of drying–wetting cycle. When cured for 93–120 days under the controlled temperature of 20 °C and relative humidity of 95%, the GGBS–MgO-stabilised kaolin clay exhibits higher (~1.5 times) qu than the PC-stabilised kaolin clay. However, when the drying–wetting cycle exceeds forth, the GGBS–MgO-stabilised kaolin clay displays lower qu or E50 than the PC-stabilised kaolin clay. The measured soil pH has a good linear relationship with qu of the soils that experienced drying–wetting durability tests. Finally, the mechanisms underneath the gradual loss of qu or E50 with increasing drying–wetting cycle are discussed.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1080/19648189.2015.1030088

Cites

2 of 2 references verified0 citation errors · 0 not checkable

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 2 references

Cited by

See all 116

Metadata

Authors
Du, Y.-J., Bo, Y.-L., Jin, F., & Liu, C.-Y.
Venue
European Journal of Environmental and Civil Engineering
Published
2015-04-13
Volume
20
Issue
2
Pages
215-230
ISSN
  • 1964-8189 (ISSN-L)
  • 2116-7214
OpenAlex
W2000501553
Cited by
116
References
2
FWCI
11.56
Type
journal article
Language
en
Open access
closed

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Durability of reactive magnesia-activated slag-stabilized low plasticity clay subjected to drying–wetting cycle. https://app.cochat.ai/papers/10.1080/19648189.2015.1030088
The paper
Du, Y.-J., Bo, Y.-L., Jin, F., & Liu, C.-Y. (2016). Durability of reactive magnesia-activated slag-stabilized low plasticity clay subjected to drying–wetting cycle. European Journal of Environmental and Civil Engineering. https://doi.org/10.1080/19648189.2015.1030088

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.