Surface modification of biodegradable magnesium and its alloys for biomedical applications
Open accessThe DOI matches its Crossref record; 125 of the 125 references it cites were found in a registry or an index.
Abstract
Magnesium and its alloys are being paid much attention recently as temporary implants, such as orthopedic implants and cardiovascular stents. However, the rapid degradation of them in physiological environment is a major obstacle preventing their wide applications to date, which will result in rapid mechanical integrity loss or even collapse of magnesium-based implants before injured tissues heal. Moreover, rapid degradation of the magnesium-based implants will also cause some adverse effects to their surrounding environment, such as local gas cavity around the implant, local alkalization and magnesium ion enrichment, which will reduce the integration between implant and tissue. So, in order to obtain better performance of magnesium-based implants in clinical trials, special alloy designs and surface modifications are prerequisite. Actually, when a magnesium-based implant is inserted in vivo, corrosion firstly happens at the implant-tissue interface and the biological response to implant is also determined by the interaction at this interface. So the surface properties, such as corrosion resistance, hemocompatibility and cytocompatibility of the implant, are critical for their in vivo performance. Compared with alloy designs, surface modification is less costly, flexible to construct multi-functional surface and can prevent addition of toxic alloying elements. In this review, we would like to summarize the current investigations of surface modifications of magnesium and its alloys for biomedical application. The advantages/disadvantages of different surface modification methods are also discussed as a suggestion for their utilization.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Figures

![Figure 2. (a) Surface and cross-sectional morphologies of Mg(OH)2 film by NaOH treatment for 3 h [66]. (b) Digital photographs and FE-SEM images of color-tuned surfaces on AZ31 alloy by water treatment [69]. (c) Surface and cross-sectional morphologies of fluoride-treated AZ31 alloy for 72 h. The insert shows the high magnification [71]. (d) Surface and cross-sectional morphologies of the MAO-coated Mg–Zn–Zr alloy [76]. (e) Surface morphologies of Mg–Fe–CO3 LDH layers on pure magnesium by different treatment process [80].](https://figures.cochat.ai/paper-figures/fb34402ec8e346e5a016c65aff5a9cee/surface-modification-of-biodegradable-magnesium-and-its-alloys-for-biomedical-figure-2.jpg)
![Figure 3. (a) Surface morphologies of DCPD, HA and FHA on Mg–Zn alloy by electrodeposition process [87]. (b) Surface morphologies of DCPD [92], β-TCP [94] and HA [96] on magnesium substrate by chemical solution treatment. (c) Surface morphologies of DCPD, DCPD-HA and HA on magnesium substrate by biomimetic process [98].](https://figures.cochat.ai/paper-figures/229369952c4f4c43852a582d0ccc1c6b/surface-modification-of-biodegradable-magnesium-and-its-alloys-for-biomedical-figure-3.jpg)
![Figure 4. (a) Surface morphologies of compact polymer coatings on magnesium substrate [101]. (b) Surface morphologies of porous PCL coatings on AZ91 alloy [35]. (c) Surface morphologies of PEDOT conductive coatings fabricated on magnesium with different processes [104].](https://figures.cochat.ai/paper-figures/12ae3b7073aa4f40a29d2ef03b15e1e8/surface-modification-of-biodegradable-magnesium-and-its-alloys-for-biomedical-figure-4.jpg)
![Figure 5. (a) Surface and sectional morphologies of DCPD/MgF2 and HA/MgF2 composite coatings on Mg–Ca–Zn alloy [108]. (b) Surface morphologies of WE42, WE42-MAO, WE42-MAO/PLLA and corrosion mass loss of WE42, WE42-MAO/PLLA [109]. (c) Surface morphologies and elemental compositions of MAO and calcification MAO coatings, cross-sectional morphology of calcification MAO coating [111].](https://figures.cochat.ai/paper-figures/3c744567a9264dbd9b8bd37b2fbf2a77/surface-modification-of-biodegradable-magnesium-and-its-alloys-for-biomedical-figure-5.jpg)
![Figure 6. (a) XPS depth profile of CO2-PIII-treated AZ31 alloy and polarization curves of untreated and CO2-PIII-treated AZ31 alloy in DMEM and SBF [115]. (b) XPS depth profile, polarization curve in SBF and corrosion in SBF for 18 h of Zn-PIII-treated pure Mg [116]. (c) XPS depth profile, GIXRD pattern and polarization curve in SBF of Al-PIII-treated pure Mg [117].](https://figures.cochat.ai/paper-figures/385b653296cc456e9ac5368cc886b26b/surface-modification-of-biodegradable-magnesium-and-its-alloys-for-biomedical-figure-6.jpg)
![Figure 7. (a) XPS depth profile, polarization curve and EIS spectrum of Al–O dual ion implantation treated WE43 alloy [120]. (b) XPS depth profiles and polarization curves of Ti and Ti–O dual ion implantation treated WE43 alloy [122]. (c) XPS depth profile and polarization curves in SBF and Na2SO4 of Cr–O dual ion implantation treated pure Mg [125].](https://figures.cochat.ai/paper-figures/5209d2478d74464aaddf2a99861eee3c/surface-modification-of-biodegradable-magnesium-and-its-alloys-for-biomedical-figure-7.jpg)
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
The source backs part of the claim, not all of it — or backs it for a different population, condition or comparison.
In the citing paper
“Surface modification of magnesium to overcome these drawbacks is the most effective method for controlling corrosion and enhancing bioactivity [36,37].”
From Functional Surface Modification of Magnesium Implant by Drug-Loaded Biodegradable Polymer Coating (2026) · cites this paper as [37]
Experimental — accuracy not yet measured
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
How useful is SBF in predicting in vivo bone bioactivity?
Kokubo, T., & Takadama, H. (2006) · Biomaterials · doi:10.1016/j.biomaterials.2006.01.017 · Cited by 9,576
Ti based biomaterials, the ultimate choice for orthopaedic implants – A review
Geetha, M., Singh, A. K., Asokamani, R., & Gogia, A. K. (2009) · Progress in Materials Science · doi:10.1016/j.pmatsci.2008.06.004 · Cited by 5,416 · cited 1×
“The early metallic materials used as biomedical implants consist of stainless steel [1, 2], Co–Cr-based alloys [3–6], titanium-based alloys [6–12], zirconium-based alloys [13, 14] and tantalum-based alloys [15, 16].”
BackgroundTitanium alloys in total joint replacement—a materials science perspective
Long, M., & Rack, H. J. (1998) · Biomaterials · doi:10.1016/s0142-9612(97)00146-4 · Cited by 3,510 · cited 1×
“The early metallic materials used as biomedical implants consist of stainless steel [1, 2], Co–Cr-based alloys [3–6], titanium-based alloys [6–12], zirconium-based alloys [13, 14] and tantalum-based alloys [15, 16].”
BackgroundSynthetic biodegradable polymers as orthopedic devices
Middleton, J. C., & Tipton, A. J. (2000) · Biomaterials · doi:10.1016/s0142-9612(00)00101-0 · Cited by 2,741
Biodegradation and biocompatibility of PLA and PLGA microspheres
Anderson, J. M., & Shive, M. S. (1997) · Advanced Drug Delivery Reviews · doi:10.1016/s0169-409x(97)00048-3 · Cited by 2,617 · cited 1×
“the degradation process or the corrosion products can induce local inflammation and the products of inflammation can enhance the degradation process [47, 48].”
BackgroundIn vivo corrosion of four magnesium alloys and the associated bone response
Witte, F., Kaese, V., Haferkamp, H., Switzer, E., Meyer-Lindenberg, A., Wirth, C. J., & Windhagen, H. (2005) · Biomaterials · doi:10.1016/j.biomaterials.2004.09.049 · Cited by 2,395 · cited 1×
“The rapid degradation of magnesium implant in vivo also leads to an accumulation of hydrogen nearby the implant because of limited hydrogen gas adsorption ability of the tissues [27, 44].”
BackgroundThe history of biodegradable magnesium implants: A review☆
Witte, F. (2010) · Acta Biomaterialia · doi:10.1016/j.actbio.2010.02.028 · Cited by 1,860 · cited 1×
“However, although most patients experienced subcutaneous gas cavities by rapid degradation of the implants, they had no pain and almost no infections were observed during the postoperative following up in the early clinical cases [45].”
BackgroundInfluentialDegradable biomaterials based on magnesium corrosion
Witte, F., Hort, N., Vogt, C., Cohen, S., Kainer, K. U., Willumeit, R., & Feyerabend, F. (2008) · Current Opinion in Solid State and Materials Science · doi:10.1016/j.cossms.2009.04.001 · Cited by 1,820 · cited 2×
“The rapid degradation of magnesium implant in vivo also leads to an accumulation of hydrogen nearby the implant because of limited hydrogen gas adsorption ability of the tissues [27, 44].”
BackgroundThe development of binary Mg–Ca alloys for use as biodegradable materials within bone
Li, Z., Gu, X., Lou, S., & Zheng, Y. (2008) · Biomaterials · doi:10.1016/j.biomaterials.2007.12.021 · Cited by 1,593 · cited 1×
“Mg–Ca [51, 52], Mg–Zn [53, 54], Mg–Sr [55] and Mg–Ag [56, 57] alloys have been developed by adding single nutrient element or antibacterial element.”
BackgroundSaris, N.-E. L., Mervaala, E., Karppanen, H., Khawaja, J. A., & Lewenstam, A. (2000) · Clinica Chimica Acta · doi:10.1016/s0009-8981(99)00258-2 · Cited by 1,366 · cited 2×
“So the incidence of hyper-magnesium is rare due to the efficient excretion of excess magnesium ions through urine [34].”
Research works printed but not linked: 8
- 2013, Journal of materials science. Materials in medicine, 24, 161, 10.1007/s10856-012-4770-8 · DOI
- 2012, Journal of biomedical materials research. Part A, 101, 1898
- 2013, Journal of materials science. Materials in medicine, 24, 889
- Wang HX Guan SK Wang X In vitro degradation and mechanical integrity of Mg–Zn–Ca alloy coated with Ca-deficient hydroxyapatite by the pulse electrodeposition process.pdf. Acta Biomater 2010; 6: 1743– 8. 20004746 · DOI · Paper page
- 2014, Journal of biomedical materials research. Part A, 102, 429, 10.1002/jbm.a.34718 · DOI
- 2013, Journal of biomedical materials research. Part A, 101, 2340
- 2013, Journal of materials science. Materials in medicine, 24, 85
- 2013, Journal of materials science. Materials in medicine, 24, 307, 10.1007/s10856-012-4796-y · DOI
Cited by
Items 201–232 of 232
Surface analysis of (Ti,Mg)N coated bone fixation devices following the rabbit femur surgery
Sabouni, K., Öztürk, Y., Kaçar, E., Köse, G. T., Kök, F. N., Kazmanlı, K., Ürgen, M., & Önder, S. (2023) · Bio-Medical Materials and Engineering · doi:10.3233/bme-222544
Azizi, S., Ehsani, M. H., Zareidoost, A., Malakpour‐Permlid, A., Boisen, A., & Ajalloueian, F. (2025) · Ceramics International · doi:10.1016/j.ceramint.2025.01.534
Obuz, S., Ozdemir, Ü., Saud, A. N., Koç, E., Elen, L., & Saud, S. (2025) · Canadian Metallurgical Quarterly · doi:10.1080/00084433.2025.2496550
“Additionally, the similarity in elastic modulus and density between Mg and bone tissue makes it particularly suitable for hard tissue engineering, as it helps reduce stress shielding and bone resorption [2,3].”
Toròs, P., Ramos, P. P., Reina, F. D., & Lasorsa, C. A. (2025) · Información tecnológica · doi:10.4067/s0718-07642025000400011
Hashemi, T. S., Çelikin, M., McCarthy, H. O., Levingstone, T. J., & Dunne, N. (2025) · Surfaces and Interfaces · doi:10.1016/j.surfin.2025.107941
Chemical bioadaptability of biodegradable metals
Zheng, Y. (2025) · Elsevier eBooks · doi:10.1016/b978-0-443-22133-0.00005-9
Аналіз поверхні сплавів після плазмової електрооксидації
Олешко, О. М., Олешко, А. Н., Oleshko, O. M., Дейнека, В. М., Дейнека, В. Н., Deineka, V. M., Линдін, М. С., Лындин, Н. С., Lyndin, M. S., Гусак, Є. В., et al. (2020) · Electronic Sumy State University Institutional Repository (Sumy State University)
Електрохімічні особливості методу плазмової електрооксидації
Муквич, В. Ю. (2024) · Electronic Sumy State University Institutional Repository (Sumy State University)
Получение и исследование свойств микродуговых силикатных покрытий
Угодчикова, А. В. (2019) · Электронный научный архив ТПУ: Главная страница (Tomsk Polytechnic University)
Sadat Hashemi, T. (2025) · Dublin City University Open Access Institutional Repository (Dublin City University)
Mousavian, S. M. H., & Bautin, V. A. (2026) · Annals of Biomedical Engineering · doi:10.1007/s10439-026-04001-3 · Cited by 2
“Polymer coatings like PLGA regulate degradation, reducing H 2 production in Mg-Zn alloys in mice by up to 70% over 14 days, though polymer degradation products may acidify the environment [24, 98].”
Zamel, H. H., Salih, A.-E., & Abbass, M. K. (2026) · AIP conference proceedings · doi:10.1063/5.0305829
Mäkinen, L. (2024) · Tampere University Institutional Repository (Tampere University)
Rahaman, K. A., Jung, Y., Hasan, M. L., Robby, A. I., Uddin, S., & Han, H. (2026) · Journal of Materials Chemistry B · doi:10.1039/d6tb00116e
Balu, D., Nouri, A., Shirvan, A. R., & Yousefi, S. (2026) · Smart Materials in Manufacturing · doi:10.1016/j.smmf.2026.100135
Magnesium-based biodegradable materials : from surface functionalization to cellular evaluation
Román, L. C. C. (2016) · theses.fr (ABES) · doi:10.70675/d4cf14d9zef62z4376z8e1bzaf7a2ab67cf3
“In 2014, Tian and Liu [129] made a critical review on surface modifications of Mg alloys.”
BackgroundInfluentialHydroxylated/graphene-oxide surface modification of Mg-based alloy for nerve regenerationPreprint
Malvestiti, L., de la Hoz, F. T., Fioravanti, F., Lacconi, G. I., Setton-Avruj, C. P., Katunar, M. R., Usach, V., & Ceré, S. (2026) · SSRN Electronic Journal · doi:10.2139/ssrn.6560246
Ahmadi, N., Naffakh-Moosavy, H., Varnosfaderani, N. G., Bagheri, F., & Hadavi, S. M. M. (2026) · Results in Engineering · doi:10.1016/j.rineng.2026.110761
Kudva, S. A., Anne, G., Mathapati, M., Ramesh, S., Kumar, P., & Prabhu, A. (2026) · Materials Research Express · doi:10.1088/2053-1591/ae67e1
“…surfaces of Mg alloys for implant applications as they are normally developed as a separate layer thereby preserving the substrate composition [29], however, their bonding strength with the substrate has always been a challenge and any compromise would lead to peeling off post implantation [30].”
張, 穎., & Ying, Z. (2023) · Saitama Institute of Technology Academic Collections
Wu, Z., Cheng, P. M., & Liu, J. (2026) · Industrial Lubrication and Tribology · doi:10.1108/ilt-02-2026-0057
Villada, Y. A. E., Ferreira, M. O. A., Gelamo, R. V., Obata, M. M. S., da Silva, M. V., Koga, G. Y., Barreto, R. R., de Siervo, A., Schmitz, T. C., Kopp, A., et al. (2026) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2026.133732 · Cited by 1
Clinical Evaluation of a Magnesium-based Barrier Membrane for Guided Bone Regeneration
Franke, T., KOLLBACH, M., Barbeck, M., & Koržinskas, T. (2026) · In Vivo · doi:10.21873/invivo.14370
雷华昌, Liu, X., Hui, Y., Jia, Y., Sun, H., Jia, Y., Liu, M., Sun, K., & Wang, G. (2026) · Journal of Materials Chemistry B · doi:10.1039/d6tb00619a
Self-citationMagnesium‐Based Transient Bioelectronics, Bio‐Optics and Bio‐Scaffolds
Mariello, M., & Leterrier, Y. (2026) · Advanced Functional Materials · doi:10.1002/adfm.77034
“Ensuring uniform dissolution without generating excessive gas (e.g., hydrogen evolution) or causing localized alkalinity is critical [121].”
Liu, L., Yan, X., Xu, Y., Zhang, D., & Xue, K. (2026) · Coatings · doi:10.3390/coatings16080887
Shanaghi, A., Souri, A., Naseri, M., Ghotbi, M. Y., Okulov, A. V., & Iusupova, O. (2026) · Science Progress · doi:10.1177/00368504261488152
“For example, in a study by Tian et al., 114 the degradation of a magnesium alloy implant coating led to a local inflammatory response and an increased risk of infection.”
Metal scaffolds for bone tissue engineering: materials, challenges, and clinical prospects
Kim, H., Lee, J., Hyun, C., Kim, I., Ferguson, S. J., & Lee, S. S. (2026) · Materials & Design · doi:10.1016/j.matdes.2026.117027
Kumar, R., Kapil, S., & Rajput, A. (2026) · Elsevier eBooks · doi:10.1016/b978-0-443-33889-2.00005-4
Hou, Z., Jin, Y. Q., Hua, L., Du, J., & Fan, H. (2026) · Composite Structures · doi:10.1016/j.compstruct.2026.121061
Arunnellaiappan, T., Arun, S., Mohankumar, N., Pavanan, V. V., Nagumothu, R., Durairaj, M., & Ramaswamy, K. (2026) · Next Materials · doi:10.1016/j.nxmate.2026.103933
Cellulose nanofiber-enabled MXene textronics for wearable therapeutic applications
El-Sayyad, G. S., Alrabghi, G., Siddiq, A., & Ghobashy, M. M. (2026) · RSC Advances · doi:10.1039/d6ra05144h
Metadata
- Authors
- Tian, P., & Liu, X.
- Affiliations
- Chinese Academy of Sciences (CN)
- Corresponding author
- Liu, X.
- ORCID
- Tian, P.
- Venue
- Regenerative Biomaterials
- Publisher
- Oxford University Press (OUP)
- Published
- 2014-11-27
- Volume
- 2
- Issue
- 2
- Pages
- 135-151
- ISSN
- 2056-3418 (ISSN-L)
- 2056-3426
- PMC
- PMC4669019
- OpenAlex
- W1971085544
- Semantic Scholar
- 7eb87072668a371340f5c86266b38187c0e8fcb8
- Cited by
- 218
- References
- 124
- Citations by year
- 2026: 23 · 2025: 23 · 2024: 22 · 2023: 15 · 2022: 23 · 2021: 28 · 2020: 26 · 2019: 22 · 2018: 19 · 2017: 6 · 2016: 8 · 2015: 3
- FWCI
- 0.39
- Type
- journal article
- Language
- en
- Open access
- gold
- doi.org
- Licence
- cc-by
- Locations
- Regenerative Biomaterials (publishedVersion, cc-by)
- PubMed Central (publishedVersion, cc-by)
- PubMed (publishedVersion)
- Funders
- National Natural Science Foundation of China (973 Program, 2012CB933600, 81271704)
- National Key Research and Development Program of China (973 Program, 2012CB933600, 2012CB933600)
- Topics
- Physical Sciences › Materials Science › Biomaterials › Magnesium Alloys: Properties and Applications
- Physical Sciences › Materials Science › Materials Chemistry › Titanium Alloys Microstructure and Properties
- Physical Sciences › Engineering › Mechanical Engineering › Surface Treatment and Coatings
- Keywords
- magnesium alloys, biodegradable implants, surface modification, corrosion resistance, hemocompatibility, cytocompatibility, implant-tissue interface, temporary implants, orthopedic implants, cardiovascular stents, magnesium ion release, biodegradation
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.