Factor analysis of selective laser melting process parameters and geometrical characteristics of synthesized single tracks
The DOI matches its Crossref record; 11 of the 11 references it cites were found in a registry or an index.
Abstract
Purpose: Properties of the parts manufactured by selective laser melting (SLM) depend strongly on the each single laser‐melted track and each single layer, as well as the strength of the connections between them. The purpose of this paper to establish links between the principal SLM parameters (laser power density, scanning speed, layer thickness), properties of the powder and geometrical characteristics of single tracks. This study will provide a theoretical and technical basis for production of parts from metal powders. Design/methodology/approach: This paper discusses the SLM parameters affecting on geometrical characteristics of the synthesized single tracks. Granulomorphometric characteristics of powders were studied in detail. A Greco‐Latin square design was used to control geometrical characteristics of the tracks. Analysis of variance (ANOVA) permitted to establish a statistically significant influence of the SLM process parameters on geometry of the single laser‐melted track. Findings: The behavior of individual tracks and their geometric characteristics depend on the process parameters, and physical‐chemical and granulomorphometrical properties of the powder. Each powder shows peculiar behavior in the process of single track formation. For stainless steel grade 904L powders with different particle size it was found that the most influencing parameter is the laser power (the following values were applied: 25, 37.5, 50 W), and then, in order of decreasing importance, are the powder layer thickness (60, 90, 120 μm), the scanning speed (0.05, 0.10, 0.15 m/s), and, finally, the particle size. Originality/value: The proposed hierarchy of the process parameters is a new systematic study presented by the authors, developed for selective laser melting. Obtained data can be used in surface structuring and micro‐manufacturing characterized by a small number of layers within a part and, thus, sensible to the geometric dimensions and shape of the individual tracks.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Binding mechanisms in selective laser sintering and selective laser melting
Kruth, J., Mercelis, P., Van Vaerenbergh, J., Froyen, L., & Rombouts, M. (2005) · Rapid Prototyping Journal · doi:10.1108/13552540510573365 · Cited by 1,383
Single track formation in selective laser melting of metal powders
Yadroitsev, I., Gusarov, A., Yadroitsava, I., & Smurov, I. (2010) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2010.05.010 · Cited by 827
Self-citationParametric analysis of the selective laser melting process
Yadroitsev, I., Bertrand, P., & Smurov, I. (2007) · Applied Surface Science · doi:10.1016/j.apsusc.2007.02.088 · Cited by 650
Self-citationDirect laser sintering of metal powders: Mechanism, kinetics and microstructural features
Simchi, A. (2006) · Materials Science and Engineering: A · doi:10.1016/j.msea.2006.04.117 · Cited by 590
Yadroitsev, I., & Smurov, I. (2010) · Physics Procedia · doi:10.1016/j.phpro.2010.08.083 · Cited by 339
Self-citationThe thermal conductivity of aggregates of several phases, including porous materials
Brailsford, A. D., & Major, K. G. (1964) · British Journal of Applied Physics · doi:10.1088/0508-3443/15/3/311 · Cited by 274
Characteristics of laser aided direct metal/material deposition process for tool steel
Choi, J. R., & Chang, Y. (2004) · International Journal of Machine Tools and Manufacture · doi:10.1016/j.ijmachtools.2004.08.014 · Cited by 209
Contact thermal conductivity of a powder bed in selective laser sintering
Gusarov, A. V., Laoui, T., Froyen, L., & Titov, V. I. (2003) · International Journal of Heat and Mass Transfer · doi:10.1016/s0017-9310(02)00370-8 · Cited by 195
Balling phenomena during direct laser sintering of multi-component Cu-based metal powder
Gu, D., & Shen, Y. (2007) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2006.06.011 · Cited by 178
Photopyroelectric measurement of thermal conductivity of metallic powders
Rombouts, M., Froyen, L., Gusarov, A. V., Bentefour, E. H., & Glorieux, C. (2005) · Journal of Applied Physics · doi:10.1063/1.1832740 · Cited by 170
Cited by
Additive manufacturing of metallic components – Process, structure and properties
DebRoy, T., Wei, H. L., Zuback, J. S., Mukherjee, T., Elmer, J. W., Milewski, J. O., Beese, A. M., Wilson-Heid, A., De, A., & Zhang, W. (2018) · Progress in Materials Science · doi:10.1016/j.pmatsci.2017.10.001 · Cited by 8,805
“There is an abundance of literature reporting densities lower than theoretical densities owing to porosity for aluminum alloys [35,148,179,189,270,548,555,640–650], steels [651–657], nickel base alloys [180,368,378,401,494,503,507,509,658,659], stainless steels [33,205,267,312,357,468,469,485,660,661] and titanium all…”
BackgroundOn the limitations of Volumetric Energy Density as a design parameter for Selective Laser Melting
Scipioni Bertoli, U., Wolfer, A. J., Matthews, M. J., Delplanque, J.-P. R., & Schoenung, J. M. (2017) · Materials & Design · doi:10.1016/j.matdes.2016.10.037 · Cited by 796
An overview of residual stresses in metal powder bed fusion
Bartlett, J. L., & Li, X. (2019) · Additive Manufacturing · doi:10.1016/j.addma.2019.02.020 · Cited by 616
du Plessis, A., Yadroitsev, I., Yadroitsava, I., & Le Roux, S. G. (2018) · 3D Printing and Additive Manufacturing · doi:10.1089/3dp.2018.0060 · Cited by 550
Self-citationTrevisan, F., Calignano, F., Lorusso, M., Pakkanen, J., Aversa, A., Ambrosio, E., Lombardi, M., Fino, P., & Manfredi, D. (2017) · Materials · doi:10.3390/ma10010076 · Cited by 502
Yadroitsev, I., Krakhmalev, P., Yadroitsava, I., Johansson, S., & Smurov, I. (2013) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2012.11.014 · Cited by 471
Self-citationIs the energy density a reliable parameter for materials synthesis by selective laser melting?
Prashanth, K. G., Scudino, S., Maity, T., Das, J., & Eckert, J. (2017) · Materials Research Letters · doi:10.1080/21663831.2017.1299808 · Cited by 418
Yadroitsev, I., & Yadroitsava, I. (2015) · Virtual and Physical Prototyping · doi:10.1080/17452759.2015.1026045 · Cited by 349
Self-citationSeede, R., Shoukr, D., Zhang, B., Whitt, A., Gibbons, S., Flater, P., Elwany, A., Arroyave, R., & Karaman, I. (2020) · Acta Materialia · doi:10.1016/j.actamat.2019.12.037 · Cited by 301
Effects of process parameters on porosity in laser powder bed fusion revealed by X-ray tomography
du Plessis, A. (2019) · Additive Manufacturing · doi:10.1016/j.addma.2019.100871 · Cited by 264
Singh, N., Hameed, P., Ummethala, R., Manivasagam, G., Prashanth, K. G., & Eckert, J. (2020) · Materials Today Advances · doi:10.1016/j.mtadv.2020.100097 · Cited by 229
Process monitoring and inspection systems in metal additive manufacturing: Status and applications
Chua, Z. Y., Ahn, I. H., & Moon, S. K. (2017) · International Journal of Precision Engineering and Manufacturing-Green Technology · doi:10.1007/s40684-017-0029-7 · Cited by 207
The Effect of Layer Thickness at Selective Laser Melting
Sufiiarov, V. S., Popovich, A. A., Borisov, E. V., Polozov, I. A., Masaylo, D. V., & Orlov, A. V. (2017) · Procedia Engineering · doi:10.1016/j.proeng.2017.01.179 · Cited by 200
Laser additive manufacturing of steels
Yin, Y., Tan, Q., Bermingham, M., Mo, N., Zhang, J., & Zhang, M.-X. (2022) · International Materials Reviews · doi:10.1080/09506608.2021.1983351 · Cited by 173
Hitzler, L., Merkel, M., Hall, W., & Öchsner, A. (2018) · Advanced Engineering Materials · doi:10.1002/adem.201700658 · Cited by 171
Dejene, N. D., & Lemu, H. G. (2023) · Metals · doi:10.3390/met13020424 · Cited by 165
“, distortions and cracking are irreversible by post-processing techniques such as stress relief heat treatment [116,117].”
BackgroundMethod
Metadata
- Authors
- Yadroitsev, I., Yadroitsava, I., Bertrand, P., & Smurov, I.
- Venue
- Rapid Prototyping Journal
- Publisher
- Emerald
- Published
- 2012-04-20
- Volume
- 18
- Issue
- 3
- Pages
- 201-208
- ISSN
- 1355-2546 (ISSN-L)
- OpenAlex
- W1975822745
- Cited by
- 221
- References
- 11
- FWCI
- 8.82
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.