Clinical trials in zirconia: a systematic review
The DOI matches its Crossref record; 63 of the 69 references it cites were found in a registry or an index.
Abstract
Zirconia is unique in its polymorphic crystalline makeup, reported to be sensitive to manufacturing and handling processes, and there is debate about which processing method is least harmful to the final product. Currently, zirconia restorations are manufactured by either soft or hard-milling processes, with the manufacturer of each claiming advantages over the other. Chipping of the veneering porcelain is reported as a common problem and has been labelled as its main clinical setback. The objective of this systematic review is to report on the clinical success of zirconia-based restorations fabricated by both milling processes, in regard to framework fractures and veneering porcelain chipping. A comprehensive review of the literature was completed for in vivo trials on zirconia restorations in MEDLINE and PubMed between 1950 and 2009. A manual hand search of relevant dental journals was also completed. Seventeen clinical trials involving zirconia-based restorations were found, 13 were conducted on fixed partial dentures, two on single crowns and two on zirconia implant abutments, of which 11 were based on soft-milled zirconia and six on hard-milled zirconia. Chipping of the veneering porcelain was a common occurrence, and framework fracture was only observed in soft-milled zirconia. Based on the limited number of short-term in vivo studies, zirconia appears to be suitable for the fabrication of single crowns, and fixed partial dentures and implant abutments providing strict protocols during the manufacturing and delivery process are adhered to. Further long-term prospective studies are necessary to establish the best manufacturing process for zirconia-based restorations.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Citations
Cites
Zirconia as a ceramic biomaterial
Piconi, C., & Maccauro, G. (1999) · Biomaterials · doi:10.1016/s0142-9612(98)00010-6 · Cited by 2,806
State of the art of zirconia for dental applications
Denry, I., & Kelly, J. R. (2008) · Dental Materials · doi:10.1016/j.dental.2007.05.007 · Cited by 2,133
The estimation of cement film thickness by an in vivo technique
McLean, J. W., & von, F. (1971) · British Dental Journal · doi:10.1038/sj.bdj.4802708 · Cited by 1,383
What future for zirconia as a biomaterial?
Chevalier, J. (2006) · Biomaterials · doi:10.1016/j.biomaterials.2005.07.034 · Cited by 1,228
Stabilized zirconia as a structural ceramic: An overview
Kelly, J. R., & Denry, I. (2008) · Dental Materials · doi:10.1016/j.dental.2007.05.005 · Cited by 1,172
Guazzato, M., Albakry, M., Ringer, S. P., & Swain, M. V. (2004) · Dental Materials · doi:10.1016/j.dental.2003.05.002 · Cited by 904
Self-citationFive-year clinical results of zirconia frameworks for posterior fixed partial dentures.
Sailer, I., Fehér, A., Filser, F., Gauckler, L. J., Lüthy, H., & Hämmerle, C. H. F. (2007) · PubMed · Cited by 807
Christel, P., Meunier, A., Heller, M., Torre, J. P., & Peille, C. N. (1989) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820230105 · Cited by 732
Phase change and mechanical properties of ZrO2-Y2O3 solid electrolyte after ageing
Kobayashi, K., KUWAJIMA, H., & Masaki, T. (1981) · Solid State Ionics · doi:10.1016/0167-2738(81)90138-7 · Cited by 661
Swain, M. V. (2009) · Acta Biomaterialia · doi:10.1016/j.actbio.2008.12.016 · Cited by 554
Self-citation
Research works printed but not linked: 1
- Pospiech, 2003, Clinical evaluation of zirconia-based all-ceramic posterior bridges: two-year results, J Dent Res, 82, 114
Cited by
Items 301–400 of 586
Sundh, A., Kou, W., & Sjögren, G. (2019) · Operative Dentistry · doi:10.2341/18-071-l · Cited by 8
Ezzat, Y., & Al-Rafee, M. A. (2019) · Saudi Journal of Oral Sciences · doi:10.4103/sjos.sjoralsci_69_18 · Cited by 8
“S J Oral Sci Volume 7 Issue 1 12 January‐April 2020 the veneering material forms a rough, sharp edge that requires readjustment in the form of polishing or repair, and a replacement may be necessary if the fracture affects the tooth’s esthetic appearance or leads to functional impairments.[4-6]”
BackgroundWhite, S. N., Green, C. C., & McMeeking, R. M. (2020) · Journal of Prosthodontic Research · doi:10.1016/j.jpor.2019.11.002 · Cited by 8
Study on PCD Tool Wear in Hard Milling of Fully-Sintered 3Y-TZP Ceramics
Xu, J., Li, L., Ji, M., & Chen, M. (2022) · Journal of Superhard Materials · doi:10.3103/s1063457622040098 · Cited by 8
The Role of Polymer Additives in Enhancing the Response of Calcium Phosphate Cement
Mills, D. K. (2018) · Springer eBooks · doi:10.1007/978-3-319-89542-0_14 · Cited by 10
Berzaghi, A. (2023) · Annali di stomatologia · doi:10.59987/ads/2023.1.17-22 · Cited by 7
Six-year analysis of posterior zirconia crowns with vertical margin preparations
Stack, J., & Millar, B. (2025) · BDJ · doi:10.1038/s41415-024-7951-1 · Cited by 7
Yang, T.-K. K. J.-H. (2013) · Dentistry · doi:10.4172/2161-1122.1000163 · Cited by 7
“Recently, zirconia has been recognized as an alternative solution for this issue, and its clinical application has been widely used [1-5].”
BackgroundElshiyab, S. H., Nawafleh, N., Khan, U., Öchsner, A. Ö., & George, R. (2020) · Bioengineering · doi:10.3390/bioengineering7040117 · Cited by 7
Effect of processing methods on the chipping resistance of veneered zirconia
de Lima, E., Tanaka, C. B., Meira, J. B. C., Santos, K. F., Arashiro, L. L., Cribari, L., Gonzaga, C. C., & Cesar, P. F. (2021) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2021.104995 · Cited by 7
Hammed, M., Abbood, M. A., & Majeed, S. M. (2024) · Annales de Chimie Science des Matériaux · doi:10.18280/acsm.480201 · Cited by 7
“At room temperature, Zirconia in t-form offers the best mechanical characteristics of the three forms, while stabilized oxides, for example, CaO, MgO, and Y 2 O 3 , are utilized to stabilize it in this form [12, 16].”
BackgroundWalczak, K., Rues, S., Wieckiewicz, M. A., Range, U., & Schmitter, M. (2016) · PubMed · doi:10.5277/abb-00529-2015-02 · Cited by 7
“Zirconia ceramics have very good mechanical properties and are biocompatible [1], [13].”
BackgroundSagesen, H. L. E., Sagesen, E. A., & Özcan, M. (2023) · Journal of Prosthodontic Research · doi:10.2186/jpr.jpr_d_22_00316 · Cited by 7
Alumina, Zirconia, and Other Non‐oxide Inert Bioceramics
López, J. P. (2014) · Wiley eBooks · doi:10.1002/9781118406748.ch6 · Cited by 7
Bizo, L., Sabo, K., Barabás, R., Katona, G., Barbu–Tudoran, L., & Berar, A. M. (2020) · Studia Universitatis Babeș-Bolyai Chemia · doi:10.24193/subbchem.2020.1.11 · Cited by 7
Dental Students’ Use of AMSTAR to Critically Appraise Systematic Reviews
Teich, S., Heima, M., & Lang, L. A. (2015) · Journal of Dental Education · doi:10.1002/j.0022-0337.2015.79.9.tb05996.x · Cited by 7
Kong, M.-C., Kim, K.-J., Kwon, T., & Hong, M.-H. (2017) · 대한치과재료학회지 · doi:10.14815/kjdm.2017.44.2.171 · Cited by 7
Ezzat, M. E., Mohsen, C., & Asaad, R. S. (2025) · BMC Oral Health · doi:10.1186/s12903-025-06811-8 · Cited by 6
“It also provides superior light transmission, closely mimicking the natural appearance of tooth enamel, which makes it an ideal choice for anterior restorations where aesthetics are paramount [15, 16].”
Recent Modifications of Zirconia in Dentistry
Albarghouti, G., & Sadi, H. (2023) · IntechOpen eBooks · doi:10.5772/intechopen.111891 · Cited by 6
KATADA, H., Inokoshi, M., KAMIJO, S., Liu, H., Xu, K., Kawashita, M., Yokoi, T., Shimabukuro, M., & Minakuchi, S. (2024) · Dental Materials Journal · doi:10.4012/dmj.2023-255 · Cited by 6
Jodha, K. S., Marocho, S. M. S., Mecholsky, J. J., Lirette, S. T., Duan, Y., & Griggs, J. A. (2025) · Dental Materials · doi:10.1016/j.dental.2025.01.002 · Cited by 6
Microstructural Analysis of Terbium Doped Zirconia and Its Biological Studies
Veerachamy, S., & Rajagopal, S. (2022) · Condensed Matter · doi:10.3390/condmat7010020 · Cited by 6
“Zirconia shows tremendous mechanical properties along with physicochemical properties when it exists in the tetragonal phase [16].”
BackgroundPeixoto, R. F., Tonin, B. S. H., Fiamengui, L. M. S. P., de Freitas-Pontes, K. M., Regis, R. R., & de Mattos, M. D. G. C. (2023) · Journal of Prosthodontics · doi:10.1111/jopr.13739 · Cited by 6
Clinical fractures of veneered zirconia single crowns.
Júnior, A. A. A., Chávez, O. F. M., Galvão, B. R., & Adabo, G. L. (2013) · PubMed · Cited by 6
Piascik, J. R., & Swift, E. J. (2012) · Journal of Esthetic and Restorative Dentistry · doi:10.1111/jerd.12004 · Cited by 6
KAYALI, F., & Kahramanoğlu, E. (2020) · Clinical and Experimental Health Sciences · doi:10.33808/clinexphealthsci.783438 · Cited by 6
Roumanas, E. D. (2013) · Journal of Evidence Based Dental Practice · doi:10.1016/j.jebdp.2012.12.004 · Cited by 6
“They both appear to provide clinically acceptable restorations.(1) One study demonstrated a significant problem with marginal adaptation.”
BackgroundResultSelection of dental ceramics in an esthetic area. A case report
de Cali, U. D. V. Y. U. S., Galeano, G. M., Muñoz, L. F. P., del Valle, U., Palomar, L. C. L., & de Cali, U. S. (2017) · Revista Facultad de Odontología Universidad de Antioquia · doi:10.17533/udea.rfo.v29n1a12 · Cited by 6
ZIRCONIA RESIN BONDED BRIDGES: AN INNOVATIVE APPROACH FOR MINIMALLY INVASIVE DENTAL PROSTHESES
Zarbah, M. (2022) · Ceramics - Silikaty · doi:10.13168/cs.2022.0015 · Cited by 6
“Upon cooling, the transformation from a tetragonal phase to a monoclinic phase induces an approximate 4.5 % volume increase which could produce catastrophic failure, so it is stabilised with oxides such as magnesia (MgO), yttria (Y 2 O 3 ), and calcium oxide (CaO) [35].”
BackgroundInfluentialAdhesion between zirconia and indirect composite resin
van Vuuren, W. J., van Vuuren, L. J., Torr, B., & Waddell, J. N. (2016) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2016.03.011 · Cited by 5
Hemdan, S., El-Aziz, S. A., & El-Sharkwy, Z. (2019) · Al-Azhar Dental Journal for Girls · doi:10.21608/adjg.2019.7627.1085 · Cited by 5
“However, the fracture strength of all-ceramic restoration depend on the core as well as the veneer material (8).”
BackgroundSİMANTASYON ÖNCESİ ZİRKONYUM SERAMİKLERE UYGULANAN YÜZEY İŞLEMLERİ
GENÇ, Ö., & Demir, N. (2022) · Selcuk Dental Journal · doi:10.15311/selcukdentj.815274 · Cited by 5
High temperature ionic and electronic conductivity in MgPSZ
Rondão, A. I. B., Grilo, J. P. F., Starykevich, M., Dias, D. M. C., & Marques, F. M. B. (2022) · Solid State Ionics · doi:10.1016/j.ssi.2022.116009 · Cited by 5
Comparison of fracture-load values of cantilevered FDPs
Ohlmann, B., Dittmar, A., Rues, S., & Rammelsberg, P. (2012) · Acta Odontologica Scandinavica · doi:10.3109/00016357.2012.700061 · Cited by 5
“However, although the incidence of zirconia framework fracture has generally been found to be rare, it remains a risk factor for failure of up to 8% for endto-end FDPs [26], although most clinical studies exclude patients with bruxism and high mastication forces.”
BackgroundHosseini, M. H., Etemadi, A., & Gorjizadeh, F. (2016) · Iranian Journal of Orthodontics · doi:10.5812/ijo.7267 · Cited by 5
“Zirconia has excellent biocompatibility (2), its color is similar to tooth and its mechanical properties is similar to stainless steel (3).”
BackgroundMete, J. J. (2016) · Advances in Dentistry & Oral Health · doi:10.19080/adoh.2016.02.555581 · Cited by 5
“The comparable mechanical properties and the relative ease and speed of soft Y-TZP blank milling may explain why more operators choose this method to fabricate zirconia restorations, whereas only a small number prefer the hard Y-TZP blanks [24].”
BackgroundKavut, İ., & Külünk, Ş. (2019) · Dentistry and Medical Research · doi:10.4103/dmr.dmr_33_18 · Cited by 5
Swain, M. V., Gee, C., & Li, K. C. (2018) · Acta Biomaterialia · doi:10.1016/j.actbio.2018.04.049 · Cited by 5
Self-citationMicrostructure and Materials Characterization of Sol-Gel Synthesized ZrO2 Systems
Park, S. S., & Shao, G. N. (2019) · Tanzania Journal of Science · doi:10.65085/2507-7961.1708 · Cited by 5
Fracture resistance and failure mode of layered translucent zirconia with different crown designs
AL-QAYSI, S. H., Saleh, A. R., & El-Damanhoury, H. M. (2021) · Dental Materials Journal · doi:10.4012/dmj.2021-051 · Cited by 5
Polymer-zirconia based ceramic composites produced by 3D-printing
Hodásová, Ľ. (2022) · UPCommons institutional repository (Universitat Politècnica de Catalunya) · doi:10.5821/dissertation-2117-380812 · Cited by 5
Fractal analysis in different regions of a fracture surface in a dental glass-ceramic
Jodha, K. S., Marocho, S. M. S., Mecholsky, J. J., Lirette, S. T., Duan, Y., & Griggs, J. A. (2025) · Dental Materials · doi:10.1016/j.dental.2025.06.008 · Cited by 4
Herber, V., Steyer, E., Koller, M., Nassehi, Y., Pichler, A., & Payer, M. (2025) · International Journal of Implant Dentistry · doi:10.1186/s40729-025-00655-1 · Cited by 4
“Ceramic implants made from zirconium dioxide (also known as zirconia) have been proposed as an alternative implant material [7, 8].”
Zhang, Y., Song, X., & Guo, H. (2020) · Surface Topography Metrology and Properties · doi:10.1088/2051-672x/ab8c95 · Cited by 4
Optical Properties of Newly Developed Monolithic CAD/CAM Materials After Aging
ÖZEL, H. B. U., Aslan, Y. U., & Sancaklı, E. (2023) · Clinical and Experimental Health Sciences · doi:10.33808/clinexphealthsci.1185717 · Cited by 4
Nawafleh, N., Mack, F., & Öchsner, A. Ö. (2015) · Advanced structured materials · doi:10.1007/978-3-319-19470-7_11 · Cited by 4
“However, Zirconia is not generally aesthetically-pleasing [8] and the problem of veneer chipping (with or without exposing the underlying core) has been reported as a frequent complication and common cause of failure [3, 9–15].”
BackgroundTreatment outcome of zirconia single crowns and fixed dental prostheses
Pihlaja, J. (2016) · Cited by 4
Nitasnoraset, K., Riddhabhaya, A., Sessirisombat, C., Hotokezaka, H., Yoshida, N., & Sirisoontorn, I. (2024) · Polymers · doi:10.3390/polym16141988 · Cited by 4
“The development of digital technology, particularly CAD/CAM systems, has rev-olutionized dental restorations by enabling precise and efficient digital construction [5], contributing to the rising popularity of monolithic zirconia options for prosthetic restorations.”
BackgroundMorphologic Characterization of Ceramic-Ceramic Dental Systems Failure
Miculescu, F., Ciocan, L. T., Meghea, D. M., & Miculescu, M. (2014) · Key engineering materials · doi:10.4028/www.scientific.net/kem.614.140 · Cited by 4
“The morphology investigation at the level of the fractures revealed the defects at the zirconia layer structure that affect the extremely low fatigue resistance of this material [12, 14].”
BackgroundKo, K., Park, C., Cho, L., & Huh, Y. (2020) · The Journal of Advanced Prosthodontics · doi:10.4047/jap.2020.12.4.181 · Cited by 4
Evaluation of Different Zirconia Surface Treatments on their Microhardness
Riyadh, M., & Nayif, M. M. (2020) · Al-Rafidain dental journal/Maǧallaẗ al-rāfidayn li-ṭibb al-asnān · doi:10.33899/rden.2020.166475 · Cited by 4
“Descriptive statistic including the mean and standard deviation (SD) of microhardness values following different treatments were shown in Table(1).”
BackgroundMethodInfluentialBond Strength of Zirconia to Different Core Materials
Torres, C. R. G., Pucci, C. R., Borges, A. B., Frattes, F. C., & de Oliveira, J. S. (2016) · World Journal of Dentistry · doi:10.5005/jp-journals-10015-1389 · Cited by 4
Esthetics using monolithic zirconia and hand-layered zirconia fixed partial denture
Vaishali, S., & Duraisamy, R. (2022) · Bioinformation · doi:10.6026/97320630018651 · Cited by 4
Choi, H., & Hong, M.-H. (2022) · Advances in Materials Science and Engineering · doi:10.1155/2022/1456475 · Cited by 4
Confiabilidade de coroas de dissilicato de lítio com diferentes espessuras sob fadiga
Martins, L. D. M. (2011) · Digital Library of Theses and Dissertations (Universidade de São Paulo) · doi:10.11606/t.25.2011.tde-21032012-160714 · Cited by 4
Gövde uzunlugunun zirkonya alt yapılı sabit parsiyel protezlerin klinik başarısına etkisi
Aydın, S. B. (2013) · Marmara University Open Access System · Cited by 4
Dimitriadis, K., Tulyaganov, D. U., & Agathopoulos, S. (2022) · Wiley eBooks · doi:10.1002/9781119724193.ch18 · Cited by 3
Comparative Analysis of Translucency in Different Thicknesses of Monolithic Zirconia Crowns
Tehrani, A. M., Jalalian, E., Zarbakhsh, A., Farahani, M. M., & Sayyari, M. (2025) · Clinical and Experimental Dental Research · doi:10.1002/cre2.70132 · Cited by 3
Kang, H. S., Shin, Y., Kang, C., & Song, J. S. (2024) · THE JOURNAL OF THE KOREAN ACADEMY OF PEDTATRIC DENTISTRY · doi:10.5933/jkapd.2024.51.1.22 · Cited by 3
“However, zirconia crowns are thicker than SSCs and may be challenging to adjust, which calls for the need for passive sitting[9].”
BackgroundThe Evolution of Dental Zirconia: Advancements and Applications
Yamani, A. E., Soualhi, H., & Alaoui, Y. A. (2025) · CODS Journal of Dentistry · doi:10.5005/jp-journals-10063-0164 · Cited by 3
Roh, K.-W., Yang, D.-S., Jeon, Y., Jeong, C.-M., Yun, M., Lee, S.-H., Choi, J.-W., Lee, J.-J., Bae, E., & Huh, J. (2019) · The Korean Academy of Oral and Maxillofacial Implantology · doi:10.32542/implantology.2019001 · Cited by 3
Rayyan, M. M., Aboushelib, M. N., & Bdeir, M. (2019) · Egyptian Dental Journal /Egyptian Dental Journal · doi:10.21608/edj.2019.73007 · Cited by 3
“(2) Means Fracture resistance in Newton”
BackgroundDoes the glaze application on Y-TZP surface improve the bond strength to pressed veneering ceramic?
Rodrigues, V. A., Paradella, T. C., Coelho, A. V. P., Souza, K. B., Bottıno, M. A., de Melo, R. M., Özcan, M., & Souza, R. O. D. A. E. (2020) · Journal of Adhesion Science and Technology · doi:10.1080/01694243.2020.1846898 · Cited by 3
“Such failures are reported as common regardless of the trademark of the zirconia used, occurring even when the ceramic coating was specifically indicated by the manufacturer [20].”
BackgroundRizky, N. S., Rikmasari, R., & Bonifacius, S. (2022) · Key engineering materials · doi:10.4028/p-46wccw · Cited by 3
“Mechanical treatment is carried out by grinding, sandblasting, or laser, while chemical treatment applies silane or etching [7-9].”
Alsafi, M. S., & Abed, I. J. (2023) · Revue des composites et des matériaux avancés · doi:10.18280/rcma.330405 · Cited by 3
“The hard machining (milling) refers to milling the restorations or the framework directly to the required dimensions from sintered high density, strength and homogenous zirconia blanks in which they have been hot isostatic pressed as shown in the Table 1 [4].”
Genotoxicity Test of Self-Renovated Ceramics in Primary Human Peripheral Lymphocytes
Hua, N., Zhu, H., Zhuang, J., & Chen, L. (2014) · Cell Biochemistry and Biophysics · doi:10.1007/s12013-014-0127-x · Cited by 3
Vafaee, F., Firooz, F., Heidari, B., Khoshhal, M., Fotovat, F., & Allahbakhshi, H. (2016) · Scholars Journal of Dental Sciences · doi:10.21276/sjds.2016.3.7.5 · Cited by 3
“However, chipping of the bi-layered all-ceramic restorations [2,14] and bulk fracture of monolithic all-ceramic restorations, still demonstrate the most commonly reported laboratory and clinical complications [15-17].”
BackgroundFerracane, J. L., Lohbauer, U., & Palin, W. M. (2016) · Elsevier eBooks · doi:10.1016/b978-0-08-100330-5.00005-4 · Cited by 3
A review of biocompatibility of zirconia: In vitro experiment
Suh, D. H., Kim, Y., & Yi, Y. (2018) · The Journal of Korean Academy of Prosthodontics · doi:10.4047/jkap.2018.56.4.391 · Cited by 3
“지르코니아는 장기간 방치되거나, 수분에 노출될 경우 aging 이 발생하여 정방정에서 단사정으로의 상전이가 발생한다.(1,2) Garvie 등(8)은 이러한 지르코니아의 aging이 생체조건하에서 발 생하는 지에 대해 연구하였다.”
Zahran, M. (2013) · TSpace (University of Toronto) · Cited by 3
Bilkhair, A. (2014) · FreiDok plus (Universitätsbibliothek Freiburg) · Cited by 3
Ezmek, B., & Sipahi, C. (2023) · Journal of Adhesion Science and Technology · doi:10.1080/01694243.2023.2180820 · Cited by 2
Graiff, L., Savio, G., Fiore, A. D., Meneghello, R., & Uccheddu, F. (2023) · International Journal on Interactive Design and Manufacturing (IJIDeM) · doi:10.1007/s12008-023-01438-x · Cited by 2
“Chipping or flaking of ceramic coatings on zirconia-ceramic prosthe-ses have been identified as a complication that can occur over time with this type of material [23].”
BackgroundEvaluating mechanical and optical patterns of translucent zirconia ceramics
Gupta, N. K., Tripathi, S., Tripathi, S., Singhraul, P. K., Shah, M., Bhargava, A., & Mehta, M. (2025) · Bioinformation · doi:10.6026/973206300212811 · Cited by 2
Mohd, M. S. N., Tan, K. B. C., Teoh, K. H., Quek, C. E. Y., & Lee, F. K. F. (2025) · Journal of Prosthetic Dentistry · doi:10.1016/j.prosdent.2025.10.019 · Cited by 2
Gulmez, O., & Kul, E. (2025) · BMC Oral Health · doi:10.1186/s12903-025-07225-2 · Cited by 2
“Stresses between the core material and feldspathic porcelain may cause cohesive fractures in the veneered zirconia restorations [3, 4].”
The Evolution of High-Strength Ceramics: the Role of Microstructure and Manufacturing
Badarneh, A., Choi, J. J. E., Ratnayake, J. T., Lyons, K. M., Waddell, J. N., Li, K. C., & Khurshid, Z. (2026) · European Journal of General Dentistry · doi:10.1055/s-0046-1815915 · Cited by 2
“48 The fi rst is the high incidence of veneering porcelain fracture, manifesting clinically as chipping fractures, 49 – 51 and the second is an inherent tetragonal to monoclinic phase transformation (ageing) problem that has been identi fi ed to occur in zirconia in the presence of water.”
Self-citationLee, S., Yi, Y., & Jo, D. (2017) · The Journal of Korean Academy of Prosthodontics · doi:10.4047/jkap.2017.55.4.410 · Cited by 2
“임상적 편의성이나 이차우식 예방의 관점 에서는술자의숙련도에민감한레진시멘트보다레진강화형 글라스아이오노머 시멘트(RMGI)가 더 유용할 수 있다.(15) 형성 된 치아의 치관 길이나 폭이 적절하고 기계적 유지와 저항 형 태가확보된다면, 지르코니아수복물에레진시멘트를이용한 것보다 RMGI가 더 나은 결합력을 보였다는 연구결과도 보고 된바있다.”
Kalecik, S., Yılmaz, D., Gürol, A., ÖZDOĞAN, A., & Kurucu, Y. (2024) · Physica Scripta · doi:10.1088/1402-4896/ad3ff3 · Cited by 2
Effect of Veneering Techniques on Ceramic Fracture of Zirconia Restoration
Hung, C., & Huang, Y.-S. (2012) · Cited by 2
Zirkonyum Oksit Altyapı ve Veneer Seramik Bağlantı Mekanizması ve Bağlantıyı Etkileyen Faktörler
Yıldırak, M. K., Türker, Ş. B., & Özkan, Y. (2019) · Marmara Dental Journal · doi:10.35333/erd.2019.15 · Cited by 2
Tosun, B., & YANIKOĞLU, N. (2020) · Atatürk Üniversitesi Diş Hekimliği Fakültesi Dergisi · doi:10.17567/ataunidfd.674142 · Cited by 2
Consideraciones mecánicas y biológicas sobre el envejecimiento del óxido de circonio odontológico
Molina, I. C., Volpato, C. Â. M., García, M. A. J. S., Luna, M. D. P., & de Vasconcellos, D. K. (2014) · Revista internacional de prótesis estomatológica · Cited by 2
Surface Treatment Prior to Cementation of Y-TZP Based
Della, P., Sperandio, M., Ghizoni, S., de Paula, V. G., Lorenzoni, F. C., & Pereira (2014) · Cited by 2
BONDING ORTHODONTIC RESIN CEMENT TO ZIRCONIUM OXIDE UNDER ORTHODONTICS LOAD AND THERMOCYCLING EFFECT
Hussein, H. S., Abdulhameed, N. F., Shen, C., Dolce, C., & Roulet, J. (2018) · STOMATOLOGY EDU JOURNAL · doi:10.25241/stomaeduj.2018.5(2).art.4 · Cited by 2
“shorter because of the delamination and chipping of veneering ceramic; to overcome this problem, the monolithic zirconium oxide (MZ) was introduced to the dental market [1,2,4,7].”
BackgroundY-TZP surface treatments and their effects on the bond strength to resin cement
May, M. M., Marchionatti, A. M. E., Valandro, L. F., Foletto, E. L., Dorneles, L. S., & May, L. G. (2019) · Brazilian journal of oral sciences/Brazilian Journal of Oral Sciences · doi:10.20396/bjos.v18i0.8655141 · Cited by 2
Zirkonyum Destekli Sabit Protetik Restorasyonlarda Klinik Başarı Değerlendirme Kriterleri
ÖZYER, E. K., Kahramanoğlu, E., Akmansoy, Ş. C., & Özkan, Y. (2019) · Marmara Dental Journal · doi:10.35333/erd.2019.14 · Cited by 2
Mosharraf, M., Azizi, A., Naziri, B., & Abolhasani, M. (2020) · Brazilian Dental Science · doi:10.14295/bds.2021.v24i1.1968 · Cited by 2
Bae, G.-H., Bae, J.-H., Huh, J., & Choi, J.-W. (2020) · Journal of Korean Acedemy of Dental Technology · doi:10.14347/jtd.2020.42.4.326 · Cited by 2
Daou, E. E. (2021) · The International Journal of Prosthodontics · doi:10.11607/ijp.6873 · Cited by 2
Limmer, B. (2012) · Carolina Digital Repository (University of North Carolina at Chapel Hill) · doi:10.17615/ax62-m141 · Cited by 2
Tanaka, C. B. (2016) · Digital Library of Theses and Dissertations (Universidade de São Paulo) · doi:10.11606/t.23.2016.tde-19012016-164834 · Cited by 2
Heikamp, F. (2012) · bonndoc (University of Bonn) · Cited by 2
10-year clinical outcomes of fixed dental prostheses with zirconia frameworks
Sax, C. (2011) · Zurich Open Repository and Archive (University of Zurich) · doi:10.5167/uzh-63986 · Cited by 2
Mechanical Behavior and Reliability of Engineering Ceramics
Saâdaoui, M. (2026) · Ceramics · doi:10.3390/ceramics9040041 · Cited by 2
Kim, W.-Y., Chung, I.-S., & Jeon, B.-W. (2016) · Journal of Korean Acedemy of Dental Technology · doi:10.14347/kadt.2016.38.4.255 · Cited by 1
BORGES, H. C. P. (2019) · Portuguese National Funding Agency for Science, Research and Technology (RCAAP Project by FCT) · Cited by 1
Imaemporn, S., Angwaravong, O., & Angwarawong, T. (2025) · The Journal of Advanced Prosthodontics · doi:10.4047/jap.2025.17.6.354 · Cited by 1
Elkady, M. A., Taymour, M., & Anwar, E. M. (2026) · The Journal of Contemporary Dental Practice · doi:10.5005/jp-journals-10024-4020 · Cited by 1
Naumann, M., Hohmann, C., Happe, A., Beuer, F., Frankenberger, R., Seemann, R., & Rosentritt, M. (2012) · Clinical Oral Investigations · doi:10.1007/s00784-012-0866-2 · Cited by 1
Metadata
- Authors
- AL-AMLEH, B., LYONS, K., & SWAIN, M.
- Affiliations
- University of Otago (NZ)
- Venue
- Journal of Oral Rehabilitation
- Publisher
- Wiley
- Published
- 2010-04
- Volume
- 37
- Issue
- 8
- Pages
- 641-652
- ISSN
- 0305-182X (ISSN-L)
- 1365-2842
- OpenAlex
- W2076537850
- Cited by
- 587
- References
- 69
- Citations by year
- 2026: 12 · 2025: 23 · 2024: 17 · 2023: 26 · 2022: 37 · 2021: 37 · 2020: 39 · 2019: 53 · 2018: 38 · 2017: 29 · 2016: 56 · 2015: 46 · 2014: 47 · 2013: 54 · 2012: 43
- FWCI
- 5.12
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- doi.wiley.com/10.1002/tdm_license_1.1 (tdm, 1979 d)
- Locations
- Journal of Oral Rehabilitation (publishedVersion)
- PubMed (publishedVersion)
- Topics
- Health Sciences › Dentistry › General Dentistry › Dental materials and restorations
- Health Sciences › Dentistry › Oral Surgery › Dental Implant Techniques and Outcomes
- Health Sciences › Dentistry › Oral Surgery › Endodontics and Root Canal Treatments
- Keywords
- zirconia, zirconia restorations, hard milling, framework fracture, fixed partial dentures, single crowns, zirconia abutments
- MeSH terms
- Dental Abutments, Clinical Trials as Topic, Crowns, Dental Materials, Dental Porcelain, Denture, Partial, Fixed, Humans, Yttrium, Zirconium, Dental Implants
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.