The DOI matches its Crossref record; 45 of the 45 references it cites were found in a registry or an index.
Characterization of Vulcan Electrochemically Oxidized under Simulated PEM Fuel Cell Conditions
Open accessAbstract
Electrochemical surface oxidation of Vulcan XC-72, a carbon black commonly used in proton exchange membrane (PEM) fuel cells, was studied following potentiostatic treatments up to 120 h at potentials from 0.6 to 1.2 V at room temperature and 65°C. Surface oxidation was followed using cyclic voltammetry (CV), thermal gravimetric analysis coupled to on-line mass spectrometry (TGA-MS), X-ray photoelectron spectroscopy (XPS), and contact angle measurements. The analytical techniques all indicate significant surface oxidation occurred during the first 16 h of 1.2 V potential holds at room temperature and a slow increase in surface oxide formation thereafter. An identification of ether, carbonyl, and carboxyl surface oxide species was made by deconvolution of XPS spectra and assigning these functional groups to the observed TGA-MS evolution peaks (150-750°C). An increase in CO evolution (>800°C) determined by TGA-MS was consistent with electrochemical CV data, which detected electroactive hydroquinone/quinone species; these electrochemically detected species were a minor fraction of the electrochemically generated surface oxides. Potential holds at 1.0 V at room temperature only resulted in slight oxidation of Vulcan XC-72. However, experiments at 65°C showed clear signs of surface oxidation after only 16 h at potentials ⩾0.8 V, verifying that surface oxides can be generated under simulated PEM fuel cell conditions. Overall, these results suggest that changes in component hydrophobicity, driven by carbon surface oxidation, are an important factor in determining long-term PEM performance instability and decay. © 2004 The Electrochemical Society. All rights reserved.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Modification of the surface chemistry of activated carbons
Figueiredo, J. L., Pereira, M. F. R., Freitas, M. M. A., & Órfão, J. J. M. (1999) · Carbon · doi:10.1016/s0008-6223(98)00333-9 · Cited by 2,935
The characterization of activated carbons with oxygen and nitrogen surface groups
Biniak, S., Szymański, G., Siedlewski, J., & Świątkowski, A. (1997) · Carbon · doi:10.1016/s0008-6223(97)00096-1 · Cited by 1,513
Carbon: Electrochemical and Physicochemical Properties
Kinoshita, K. (1988) · Medical Entomology and Zoology · Cited by 1,367
Surface-oxidized carbon fibers: I. Surface structure and chemistry
Zielke, U., Hüttinger, K. J., & Hoffman, W. P. (1996) · Carbon · doi:10.1016/0008-6223(96)00032-2 · Cited by 788
Surface characterization of electrochemically oxidized carbon fibers
Yue, Z. R., Jiang, W., Wang, L., Gardner, S. D., & Pittman, C. U. (1999) · Carbon · doi:10.1016/s0008-6223(99)00047-0 · Cited by 647
A DRIFTS study of the formation of surface groups on carbon by oxidation
Fanning, P. E., & Vannice, M. A. (1993) · Carbon · doi:10.1016/0008-6223(93)90009-y · Cited by 644
Otake, Y., & Jenkins, R. G. (1993) · Carbon · doi:10.1016/0008-6223(93)90163-5 · Cited by 446
Dekanski, A. B., Stevanović, J., Stevanović, R. M., Nikolić, B., & Jovanović, V. M. (2001) · Carbon · doi:10.1016/s0008-6223(00)00228-1 · Cited by 403
Brennan, J. K., Bandosz, T. J., Thomson, K. T., & Gubbins, K. E. (2001) · Colloids and Surfaces A: Physicochemical and Engineering Aspects · doi:10.1016/s0927-7757(01)00644-6 · Cited by 401
Surface Oxidation of Carbon Nanofibres
Ros, T. G., van Dillen, A. J., Geus, J. W., & Koningsberger, D. C. (2002) · Chemistry - A European Journal · Cited by 322
Cited by
Scientific Aspects of Polymer Electrolyte Fuel Cell Durability and Degradation
Borup, R., Meyers, J., Pivovar, B., Kim, Y. S., Mukundan, R., Garland, N., Myers, D., Wilson, M., Garzon, F., Wood, D., et al. (2007) · Chemical Reviews · doi:10.1021/cr050182l · Cited by 3,402
A review of PEM fuel cell durability: Degradation mechanisms and mitigation strategies
Wu, J., Yuan, X. Z., Martin, J. J., Wang, H., Zhang, J., Shen, J., Wu, S., & Merida, W. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.06.006 · Cited by 1,587
Carbon Nanomaterials for Advanced Energy Conversion and Storage
Dai, L., Chang, D. W., Baek, J., & Lu, W. (2012) · Small · doi:10.1002/smll.201101594 · Cited by 1,546
Understanding and approaches for the durability issues of Pt-based catalysts for PEM fuel cell
Shao, Y., Yin, G., & Gao, Y. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.07.004 · Cited by 1,197
Tjong, S. C. (2013) · Materials Science and Engineering: R: Reports · doi:10.1016/j.mser.2013.08.001 · Cited by 1,155
Recent advances in activity and durability enhancement of Pt/C catalytic cathode in PEMFC
Yu, X., & Ye, S. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.07.048 · Cited by 1,098
Review: Durability and Degradation Issues of PEM Fuel Cell Components
de Bruijn, F. A., Dam, V. A. T., & Janssen, G. J. M. (2008) · Fuel Cells · doi:10.1002/fuce.200700053 · Cited by 1,001
Facile and controllable electrochemical reduction of graphene oxide and its applications
Shao, Y., Wang, J., Engelhard, M., Wang, C., & Lin, Y. (2010) · J. Mater. Chem. · doi:10.1039/b917975e · Cited by 879
High-Temperature PEM Fuel Cells
Zhang, J., Zhang, H., Wu, J., & Zhang, J. (2013) · Pem Fuel Cell Testing and Diagnosis · doi:10.1016/b978-0-444-53688-4.00010-3 · Cited by 809
Effects of oxygen-containing functional groups on carbon materials in supercapacitors: A review
Qiu, C., Jiang, L., Gao, Y., & Sheng, L. (2023) · Materials & Design · doi:10.1016/j.matdes.2023.111952 · Cited by 761
Carbon support oxidation in PEM fuel cell cathodes
Maass, S., Finsterwalder, F., Frank, G., Hartmann, R., & Merten, C. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.08.053 · Cited by 740
Ren, P., Pei, P., Li, Y., Wu, Z., Chen, D., & Huang, S. (2020) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2020.100859 · Cited by 737
Durability challenges of anion exchange membrane fuel cells
Mustain, W. E., Chatenet, M., Page, M., & Kim, Y. S. (2020) · Energy & Environmental Science · doi:10.1039/d0ee01133a · Cited by 677
A review of platinum-based catalyst layer degradation in proton exchange membrane fuel cells
Zhang, S., Yuan, X.-Z., Hin, J. N. C., Wang, H., Friedrich, K. A., & Schulze, M. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.06.073 · Cited by 661
Wang, X., Li, W., Chen, Z., Waje, M., & Yan, Y. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.09.039 · Cited by 630
Flexible Zn– and Li–air batteries: recent advances, challenges, and future perspectives
Tan, P., Chen, B., Xu, H., Zhang, H., Cai, W., Ni, M., Liu, M., & Shao, Z. (2017) · Energy Environ. Sci. · doi:10.1039/c7ee01913k · Cited by 583
A review of accelerated stress tests of MEA durability in PEM fuel cells
ZHANG, S., YUAN, X., WANG, H., MERIDA, W., ZHU, H., SHEN, J., WU, S., & ZHANG, J. (2009) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2008.10.012 · Cited by 525
Carbon as catalyst and support for electrochemical energy conversion
Trogadas, P., Fuller, T. F., & Strasser, P. (2014) · Carbon · doi:10.1016/j.carbon.2014.04.005 · Cited by 522
Antolini, E., Salgado, J. R. C., & Gonzalez, E. R. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.03.006 · Cited by 503
Bezerra, C. W. B., Zhang, L., Liu, H., Lee, K., Marques, A. L. B., Marques, E. P., Wang, H., & Zhang, J. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.08.028 · Cited by 439
Effect of carbon black support corrosion on the durability of Pt/C catalyst
Wang, J., Yin, G., Shao, Y., Zhang, S., Wang, Z., & Gao, Y. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.06.084 · Cited by 441
Oh, H.-S., Nong, H. N., Reier, T., Gliech, M., & Strasser, P. (2015) · Chemical Science · doi:10.1039/c5sc00518c · Cited by 423
Zhang, J., Yuan, Y., Gao, L., Zeng, G., Li, M., & Huang, H. (2021) · Advanced Materials · doi:10.1002/adma.202006494 · Cited by 420
Zhang, T., Wang, P., Chen, H., & Pei, P. (2018) · Applied Energy · doi:10.1016/j.apenergy.2018.04.049 · Cited by 416
Durability Study of Pt∕C and Pt∕CNTs Catalysts under Simulated PEM Fuel Cell Conditions
Shao, Y., Yin, G., Gao, Y., & Shi, P. (2006) · Journal of The Electrochemical Society · doi:10.1149/1.2191147 · Cited by 411
Song, Z., Ding, J., Liu, B., Liu, X., Han, X., Deng, Y., Hu, W., & Zhong, C. (2020) · Advanced Materials · doi:10.1002/adma.201908127 · Cited by 351
Carbon Corrosion in PEM Fuel Cells and the Development of Accelerated Stress Tests
Macauley, N., Papadias, D. D., Fairweather, J., Spernjak, D., Langlois, D., Ahluwalia, R., More, K. L., Mukundan, R., & Borup, R. L. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0061806jes · Cited by 341
Shao, Y., Yin, G., Zhang, J., & Gao, Y. (2006) · Electrochimica Acta · doi:10.1016/j.electacta.2006.03.021 · Cited by 322
Dong, W., Xie, M., Zhao, S., Qin, Q., & Huang, F. (2023) · Materials Science and Engineering: R: Reports · doi:10.1016/j.mser.2022.100713 · Cited by 319
Avasarala, B., & Haldar, P. (2010) · Electrochimica Acta · doi:10.1016/j.electacta.2010.08.035 · Cited by 317
Advanced Extremely Durable 3D Bifunctional Air Electrodes for Rechargeable Zinc‐Air Batteries
Lee, D. U., Choi, J., Feng, K., Park, H. W., & Chen, Z. (2014) · Advanced Energy Materials · doi:10.1002/aenm.201301389 · Cited by 312
Durability Studies of PBI‐based High Temperature PEMFCs
Yu, S., Xiao, L., & Benicewicz, B. C. (2008) · Fuel Cells · doi:10.1002/fuce.200800024 · Cited by 310
Ioroi, T., Siroma, Z., Fujiwara, N., Yamazaki, S.-I., & Yasuda, K. (2005) · Electrochemistry Communications · doi:10.1016/j.elecom.2004.12.007 · Cited by 300
Bhowmik, T., Kundu, M. K., & Barman, S. (2016) · ACS Catalysis · doi:10.1021/acscatal.5b02485 · Cited by 299
Ceramic materials as supports for low-temperature fuel cell catalysts
Antolini, E., & Gonzalez, E. R. (2009) · Solid State Ionics · doi:10.1016/j.ssi.2009.03.007 · Cited by 283
Castanheira, L., Dubau, L., Mermoux, M., Berthomé, G., Caqué, N., Rossinot, E., Chatenet, M., & Maillard, F. (2014) · ACS Catalysis · doi:10.1021/cs500449q · Cited by 280
Zhang, G., Chenitz, R., Lefèvre, M., Sun, S., & Dodelet, J.-P. (2016) · Nano Energy · doi:10.1016/j.nanoen.2016.02.038 · Cited by 278
Jayasayee, K., Veen, J. A. R. V., Manivasagam, T. G., Celebi, S., Hensen, E. J. M., & de Bruijn, F. A. (2012) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2011.11.003 · Cited by 204
Molecular Dynamics Study of Ionomer Adsorption at a Carbon Surface in Catalyst Ink
Mashio, T., Ohma, A., & Tokumasu, T. (2016) · Electrochimica Acta · doi:10.1016/j.electacta.2016.04.004 · Cited by 84
Hu, J., Sui, P. C., Kumar, S., & Djilali, N. (2009) · Electrochimica Acta · doi:10.1016/j.electacta.2009.04.073 · Cited by 61
Yoshii, K., Yamaji, K., Tsuda, T., Matsumoto, H., Sato, T., Izumi, R., Torimoto, T., & Kuwabata, S. (2016) · Journal of Materials Chemistry A · doi:10.1039/c6ta04859e · Cited by 53
Sheng, W., Lee, S. W., Crumlin, E. J., Chen, S., & Shao-Horn, Y. (2011) · Journal of The Electrochemical Society · doi:10.1149/2.066111jes · Cited by 39
Modeling an ordered nanostructured cathode catalyst layer for proton exchange membrane fuel cells
Hussain, M. M., Song, D., Liu, Z.-S., & Xie, Z. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.10.111 · Cited by 35
Selvaganesh, S. V., Sridhar, P., Pitchumani, S., & Shukla, A. K. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.051301jes · Cited by 28
Carbon nanotubes as catalyst support in a glucose microfluidic fuel cell in basic media
Guerra-Balcázar, M., Cuevas-Muñiz, F. M., Castaneda, F., Ortega, R., Álvarez-Contreras, L., Ledesma-García, J., & Arriaga, L. G. (2011) · Electrochimica Acta · doi:10.1016/j.electacta.2011.07.099 · Cited by 26
Metadata
- Authors
- Kangasniemi, K. H., Condit, D. A., & Jarvi, T. D.
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 2004
- Volume
- 151
- Issue
- 4
- Pages
- E125
- ISSN
- 0013-4651 (ISSN-L)
- OpenAlex
- W2057639036
- Cited by
- 599
- References
- 45
- FWCI
- 13.41
- Type
- journal article
- Language
- en
- Open access
- bronze
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.