Durability of PEFCs at High Humidity Conditions
Open accessAbstract
This work addresses issues of long-term durability of hydrogen-air polymer electrolyte fuel cells (PEFCs). The chromium in a binary alloy catalyst has been found to migrate from cathode to anode during the course of life testing when operating within the oversaturated, or high-humidity, gas feed regime (one or both inlet feeds with a dew point equal to or higher than cell operating temperature) above current density. Other major factors such as membrane degradation, dissolution of catalyst-layer recast ionomer, catalyst oxidation, and catalyst agglomeration/growth have been identified as simultaneous, gradual processes that can lead to long-term PEFC failure. In situ cyclic voltammetry measurement of electrochemically active catalyst surface area shows a continuous decrease, revealing that catalyst agglomeration and/or growth may be a major cause of membrane electrode assembly degradation during middle-term life tests ( i.e. , operation times up to about 2000 h) under high-humidity conditions. Membrane and/or recast ionomer degradation was confirmed by the presence of fluoride and sulfate anions in the cathode outlet water. Scanning and transmission electron microscopy observation of a tested MEA suggest the loss of carbon-supported catalyst clusters and possible dissolution of recast Nafion ionomer. © 2004 The Electrochemical Society. All rights reserved.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Modern Aspects of Electrochemistry
(2002) · Modern Aspects of Electrochemistry · doi:10.1007/b114168 · Cited by 5,949
Polymer Electrolyte Fuel Cell Model
Springer, T. E., Zawodzinski, T. A., & Gottesfeld, S. (1991) · Journal of The Electrochemical Society · doi:10.1149/1.2085971 · Cited by 3,528
Self-citationCarbon: Electrochemical and Physicochemical Properties
Kinoshita, K. (1988) · Medical Entomology and Zoology · Cited by 1,367
Thin-film catalyst layers for polymer electrolyte fuel cell electrodes
Wilson, M. S., & Gottesfeld, S. (1992) · Journal of Applied Electrochemistry · doi:10.1007/bf01093004 · Cited by 871
Characterization of Polymer Electrolyte Fuel Cells Using AC Impedance Spectroscopy
Springer, T. E., Zawodzinski, T. A., Wilson, M. S., & Gottesfeld, S. (1996) · Journal of The Electrochemical Society · doi:10.1149/1.1836485 · Cited by 711
Self-citationKinetic Model of Platinum Dissolution in PEMFCs
Darling, R. M., & Meyers, J. P. (2003) · Journal of The Electrochemical Society · doi:10.1149/1.1613669 · Cited by 688
High Performance Catalyzed Membranes of Ultra‐low Pt Loadings for Polymer Electrolyte Fuel Cells
Wilson, M. S., & Gottesfeld, S. (1992) · Journal of The Electrochemical Society · doi:10.1149/1.2069277 · Cited by 510
Wilson, M. S., Valerio, J. A., & Gottesfeld, S. (1995) · Electrochimica Acta · doi:10.1016/0013-4686(94)00272-3 · Cited by 476
Surface Area Loss of Supported Platinum in Polymer Electrolyte Fuel Cells
Wilson, M. S., Garzon, F. H., Sickafus, K. E., & Gottesfeld, S. (1993) · Journal of The Electrochemical Society · doi:10.1149/1.2220925 · Cited by 411
Ionic Conductivity of PEMFC Electrodes
Li, G., & Pickup, P. G. (2003) · Journal of The Electrochemical Society · doi:10.1149/1.1611493 · Cited by 273
Cited by
Wang, Y., Chen, K. S., Mishler, J., Cho, S. C., & Adroher, X. C. (2011) · Applied Energy · doi:10.1016/j.apenergy.2010.09.030 · Cited by 3,329
Review of the proton exchange membranes for fuel cell applications
Peighambardoust, S. J., Rowshanzamir, S., & Amjadi, M. (2010) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2010.05.017 · Cited by 2,186
A review of PEM fuel cell durability: Degradation mechanisms and mitigation strategies
Wu, J., Yuan, X. Z., Martin, J. J., Wang, H., Zhang, J., Shen, J., Wu, S., & Merida, W. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.06.006 · Cited by 1,587
Carbon Nanomaterials for Advanced Energy Conversion and Storage
Dai, L., Chang, D. W., Baek, J., & Lu, W. (2012) · Small · doi:10.1002/smll.201101594 · Cited by 1,546
Instability of Pt∕C Electrocatalysts in Proton Exchange Membrane Fuel Cells
Ferreira, P. J., la O’, G. J., Shao-Horn, Y., Morgan, D., Makharia, R., Kocha, S., & Gasteiger, H. A. (2005) · Journal of The Electrochemical Society · doi:10.1149/1.2050347 · Cited by 1,491
Materials, technological status, and fundamentals of PEM fuel cells – A review
Wang, Y., Ruiz Diaz, D. F., Chen, K. S., Wang, Z., & Adroher, X. C. (2020) · Materials Today · doi:10.1016/j.mattod.2019.06.005 · Cited by 1,419
High temperature proton exchange membranes based on polybenzimidazoles for fuel cells
Li, Q., Jensen, J. O., Savinell, R. F., & Bjerrum, N. J. (2009) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2008.12.003 · Cited by 1,323
Understanding and approaches for the durability issues of Pt-based catalysts for PEM fuel cell
Shao, Y., Yin, G., & Gao, Y. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.07.004 · Cited by 1,197
Recent advances in activity and durability enhancement of Pt/C catalytic cathode in PEMFC
Yu, X., & Ye, S. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.07.048 · Cited by 1,098
Review: Durability and Degradation Issues of PEM Fuel Cell Components
de Bruijn, F. A., Dam, V. A. T., & Janssen, G. J. M. (2008) · Fuel Cells · doi:10.1002/fuce.200700053 · Cited by 1,001
Instability of Supported Platinum Nanoparticles in Low-Temperature Fuel Cells
Shao-Horn, Y., Sheng, W. C., Chen, S., Ferreira, P. J., Holby, E. F., & Morgan, D. (2007) · Topics in Catalysis · doi:10.1007/s11244-007-9000-0 · Cited by 939
Bose, S., Kuila, T., Nguyen, T. X. H., Kim, N. H., Lau, K.-T., & Lee, J. H. (2011) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2011.01.003 · Cited by 934
Supportless Pt and PtPd Nanotubes as Electrocatalysts for Oxygen‐Reduction Reactions
Chen, Z., Waje, M., Li, W., & Yan, Y. (2007) · Angewandte Chemie International Edition · doi:10.1002/anie.200700894 · Cited by 838
A review of platinum-based catalyst layer degradation in proton exchange membrane fuel cells
Zhang, S., Yuan, X.-Z., Hin, J. N. C., Wang, H., Friedrich, K. A., & Schulze, M. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.06.073 · Cited by 661
Wang, X., Li, W., Chen, Z., Waje, M., & Yan, Y. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.09.039 · Cited by 630
Pei, P., & Chen, H. (2014) · Applied Energy · doi:10.1016/j.apenergy.2014.03.048 · Cited by 616
Gas crossover and membrane degradation in polymer electrolyte fuel cells
Inaba, M., Kinumoto, T., Kiriake, M., Umebayashi, R., Tasaka, A., & Ogumi, Z. (2006) · Electrochimica Acta · doi:10.1016/j.electacta.2006.03.008 · Cited by 611
Proton exchange membrane fuel cell from low temperature to high temperature: Material challenges
Shao, Y., Yin, G., Wang, Z., & Gao, Y. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.02.065 · Cited by 571
Degradation of polymer electrolyte membranes
COLLIER, A., WANG, H., ZIYUAN, X., ZHANG, J., & WILKINSON, D. (2006) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2006.05.006 · Cited by 538
A review of accelerated stress tests of MEA durability in PEM fuel cells
ZHANG, S., YUAN, X., WANG, H., MERIDA, W., ZHU, H., SHEN, J., WU, S., & ZHANG, J. (2009) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2008.10.012 · Cited by 525
A quick evaluating method for automotive fuel cell lifetime
PEI, P., CHANG, Q., & TANG, T. (2008) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2008.04.048 · Cited by 518
Antolini, E., Salgado, J. R. C., & Gonzalez, E. R. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.03.006 · Cited by 503
Yousfi-Steiner, N., Moçotéguy, P., Candusso, D., & Hissel, D. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.03.060 · Cited by 431
Zhao, J., & Li, X. (2019) · Energy Conversion and Management · doi:10.1016/j.enconman.2019.112022 · Cited by 430
Durability Study of Pt∕C and Pt∕CNTs Catalysts under Simulated PEM Fuel Cell Conditions
Shao, Y., Yin, G., Gao, Y., & Shi, P. (2006) · Journal of The Electrochemical Society · doi:10.1149/1.2191147 · Cited by 411
Yan, Q., Toghiani, H., & Causey, H. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.03.077 · Cited by 391
Rodgers, M. P., Bonville, L. J., Kunz, H. R., Slattery, D. K., & Fenton, J. M. (2012) · Chemical Reviews · doi:10.1021/cr200424d · Cited by 383
Durability of perfluorinated ionomer membrane against hydrogen peroxide
Kinumoto, T., Inaba, M., Nakayama, Y., Ogata, K., Umebayashi, R., Tasaka, A., Iriyama, Y., Abe, T., & Ogumi, Z. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.10.043 · Cited by 354
Wen, Z., Liu, J., & Li, J. (2008) · Advanced Materials · doi:10.1002/adma.200701578 · Cited by 325
Mechanical response of fuel cell membranes subjected to a hygro-thermal cycle
Kusoglu, A., Karlsson, A. M., Santare, M. H., Cleghorn, S., & Johnson, W. B. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.05.020 · Cited by 323
Yu, Y., Li, H., Wang, H., Yuan, X.-Z., Wang, G., & Pan, M. (2012) · Journal of Power Sources · doi:10.1016/j.jpowsour.2012.01.059 · Cited by 313
Kusoglu, A., Karlsson, A. M., Santare, M. H., Cleghorn, S., & Johnson, W. B. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.03.063 · Cited by 274
Morphological features (defects) in fuel cell membrane electrode assemblies
Kundu, S., Fowler, M. W., Simon, L. C., & Grot, S. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.12.027 · Cited by 244
Understanding Pt Nanoparticle Anchoring on Graphene Supports through Surface Functionalization
Xin, L., Yang, F., Rasouli, S., Qiu, Y., Li, Z.-F., Uzunoglu, A., Sun, C.-J., Liu, Y., Ferreira, P., Li, W., et al. (2016) · ACS Catalysis · doi:10.1021/acscatal.5b02722 · Cited by 209
Self-citationQiu, D., Peng, L., Lai, X., Ni, M., & Lehnert, W. (2019) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2019.109289 · Cited by 208
Shah, A. A., Ralph, T. R., & Walsh, F. C. (2009) · Journal of The Electrochemical Society · doi:10.1149/1.3077573 · Cited by 149
Zhang, L., & Mukerjee, S. (2006) · Journal of The Electrochemical Society · doi:10.1149/1.2180715 · Cited by 137
Wang, W., Chen, S., Li, J., & Wang, W. (2015) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2015.02.027 · Cited by 115
A highly durable fuel cell electrocatalyst based on double-polymer-coated carbon nanotubes
Berber, M. R., Hafez, I. H., Fujigaya, T., & Nakashima, N. (2015) · Scientific Reports · doi:10.1038/srep16711 · Cited by 55
Okaya, K., Yano, H., Kakinuma, K., Watanabe, M., & Uchida, H. (2012) · ACS Applied Materials & Interfaces · doi:10.1021/am302224n · Cited by 36
Modeling an ordered nanostructured cathode catalyst layer for proton exchange membrane fuel cells
Hussain, M. M., Song, D., Liu, Z.-S., & Xie, Z. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.10.111 · Cited by 35
The Model of Stress Distribution in Polymer Electrolyte Membrane
Atrazhev, V. V., Astakhova, T. Y., Dmitriev, D. V., Erikhman, N. S., Sultanov, V. I., Patterson, T., & Burlatsky, S. F. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.079310jes · Cited by 16
Metadata
- Authors
- Xie, J., Wood, D. L., Wayne, D. M., Zawodzinski, T. A., Atanassov, P., & Borup, R. L.
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 2005
- Volume
- 152
- Issue
- 1
- Pages
- A104
- ISSN
- 0013-4651 (ISSN-L)
- OpenAlex
- W2004742529
- Cited by
- 382
- References
- 22
- FWCI
- 19.29
- Type
- journal article
- Language
- en
- Open access
- bronze
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.