Radical (HO•, H• and HOO•) Formation and Ionomer Degradation in Polymer Electrolyte Fuel Cells

Open access
Gubler, Lorenz, Dockheer, Sindy M., Koppenol, Willem H.·2011·Journal of The Electrochemical Society

Abstract

Formation of radicals, such as HO•, H• and HOO•, in the membrane of the polymer electrolyte fuel cell and their attack on perfluoroalkylsulfonic acid (PFSA) and poly(styrenesulfonic acid) (PSSA) ionomers was simulated based on a kinetic framework with H 2 O 2 as “parent” molecule and with contaminating Fe as parameter. Analysis under quasi-steady state conditions yielded radical concentrations of around 10−19 M for H•, 10−16 M for HO• and 10−10 M for HOO•. H• is formed via the reaction of HO• with H 2 dissolved in the membrane. The attack of the PFSA ionomer was assumed to proceed via weak carboxylic end-groups. The corresponding calculated fluoride emission rate (FER) showed good agreement with experimental data under ex situ Fenton test conditions. The predicted FER under fuel cell operating conditions was underestimated by 2–3 orders of magnitude. It is likely that degradation via side-chain attack is prevalent during open circuit voltage hold tests. The oxidative degradation of PSSA ionomer follows an entirely different pathway, because, in addition to α-hydrogen abstraction by HO•, the aromatic ring effectively scavenges HO• to form an OH-adduct. Follow-up reactions lead to chain scission and formation of a stable hydroxylated degradation product.

Overview

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1149/1.3581040

Cites

95 of 95 references verified0 citation errors · 0 not checkable

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 95 references

Cited by

See all 336

Metadata

Authors
Gubler, L., Dockheer, S. M., & Koppenol, W. H.
Venue
Journal of The Electrochemical Society
Published
2011-04-27
Volume
158
Issue
7
Pages
B755-B769
ISSN
  • 0013-4651 (ISSN-L)
  • 1945-7111
OpenAlex
W1990485402
Cited by
336
References
95
FWCI
8.24
Type
journal article
Language
en
Open access
bronze

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Radical (HO•, H• and HOO•) Formation and Ionomer Degradation in Polymer Electrolyte Fuel Cells. https://app.cochat.ai/papers/10.1149/1.3581040
The paper
Gubler, L., Dockheer, S. M., & Koppenol, W. H. (2011). Radical (HO•, H• and HOO•) Formation and Ionomer Degradation in Polymer Electrolyte Fuel Cells. Journal of The Electrochemical Society. https://doi.org/10.1149/1.3581040

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.