The Electrochemistry of Metallic Nickel: Oxides, Hydroxides, Hydrides and Alkaline Hydrogen Evolution
Open accessAbstract
Ni-based catalysts in aqueous alkaline media are low-cost electrode materials for electrolytic hydrogen generation, a renewable method of producing fuel and industrial feedstock. However, Ni cathodes show a significant decrease in their hydrogen evolution reaction (HER) activity after several hours of electrolysis. Further, industrial electrolysers are often subjected to transient anodic currents, the effects of which on Ni-based catalysts are not well-known. We consider the source of electrode deactivation and the effects of temporary anodic currents on smooth metallic Ni electrodes in alkaline solutions by cyclic voltammetry (CV), galvanostatic and potentiostatic polarization, X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS). Polished surfaces are covered by a bilayer composed of α-Ni(OH) 2 underlaid by non-stoichiometric NiO x . Below the reversible hydrogen electrode (RHE) potential, the air-formed layer mostly reduces to Ni metal and H atoms incorporate deep into the electrode material. Under industrial conditions, i.e., concentrated NaOH/KOH solutions and large cathodic current densities, α-NiH x and β-NiH x can form at the electrode surface. Above the RHE potential, NiO x , α-Ni(OH) 2 , β-Ni(OH) 2 and β-NiOOH form reversibly and mostly reduce back to Ni on subsequent cathodic polarization. However, repeated oxidation and reduction will introduce strain on a catalyst material, which may lead to its mechanical failure.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
X-ray line broadening from filed aluminium and wolfram
Williamson, G. K., & Hall, W. H. (1953) · Acta Metallurgica · doi:10.1016/0001-6160(53)90006-6 · Cited by 10,530
Recent progress in alkaline water electrolysis for hydrogen production and applications
Zeng, K., & Zhang, D. (2010) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2009.11.002 · Cited by 3,611
New interpretations of XPS spectra of nickel metal and oxides
Grosvenor, A. P., Biesinger, M. C., Smart, R. S. C., & McIntyre, N. S. (2006) · Surface Science · doi:10.1016/j.susc.2006.01.041 · Cited by 2,434
Standard Potentials in Aqueous Solution
Bard, A. J., Parsons, R., & Jordan, J. (2017) · Routledge eBooks · doi:10.1201/9780203738764 · Cited by 2,311
Linden, D. (2001) · CERN Document Server (European Organization for Nuclear Research) · Cited by 1,900
Biesinger, M. C., Payne, B. P., Lau, L. W. M., Gerson, A., & Smart, R. S. C. (2009) · Surface and Interface Analysis · doi:10.1002/sia.3026 · Cited by 1,826
Hydrogen futures: toward a sustainable energy system
Dunn, S. (2002) · International Journal of Hydrogen Energy · doi:10.1016/s0360-3199(01)00131-8 · Cited by 1,520
Zur kenntnis der nickelhydroxidelektrode—I.Über das nickel (II)-hydroxidhydrat
Bode, H., Dehmelt, K., & Witte, J. (1966) · Electrochimica Acta · doi:10.1016/0013-4686(66)80045-2 · Cited by 951
Review of the structure and the electrochemistry of nickel hydroxides and oxy-hydroxides
Oliva, P., Leonardi, J., Laurent, J. F., Delmas, C., Braconnier, J. J., Figlarz, M., Fievet, F., & Guibert, A. D. (1982) · Journal of Power Sources · doi:10.1016/0378-7753(82)80057-8 · Cited by 933
Handbook of Aqueous Electrolyte Thermodynamics: Theory & Application
Zemaitis, J. F., Clark, D. M., Rafal, M., & Scrivner, N. C. (1986) · Wiley eBooks · doi:10.1002/9780470938416 · Cited by 686
Hall, D. S., Lockwood, D. J., Poirier, S., Bock, C., & MacDougall, B. R. (2012) · The Journal of Physical Chemistry A · doi:10.1021/jp303546r · Cited by 445
Self-citationKinetics of hydrogen evolution on nickel electrodes
Lasia, A., & Rami, A. (1990) · Journal of Electroanalytical Chemistry and Interfacial Electrochemistry · doi:10.1016/0022-0728(90)87140-f · Cited by 415
In situ studies of the oxidation of nickel electrodes in alkaline solution
Medway, S. L., Lucas, C. A., Kowal, A., Nichols, R. J., & Johnson, D. (2006) · Journal of Electroanalytical Chemistry · doi:10.1016/j.jelechem.2005.11.013 · Cited by 340
Studies concerning charged nickel hydroxide electrodes I. Measurement of reversible potentials
Barnard, R., Randell, C. F., & Tye, F. L. (1980) · Journal of Applied Electrochemistry · doi:10.1007/bf00937345 · Cited by 312
Hahn, F., Beden, B., Croissant, M. J., & Lamy, C. (1986) · Electrochimica Acta · doi:10.1016/0013-4686(86)80087-1 · Cited by 257
The hydrogen evolution reaction on nickel surfaces stabilized by H-absorption
Machado, S. A. S., & Avaca, L. A. (1994) · Electrochimica Acta · doi:10.1016/0013-4686(94)e0003-i · Cited by 239
Electrochemical oxidation of nickel in alkaline solutions: a voltammetric study and modelling
Seghiouer, A., Chevalet, J., Barhoun, A., & Lantelme, F. (1998) · Journal of Electroanalytical Chemistry · doi:10.1016/s0022-0728(97)00498-1 · Cited by 199
The Apparent Constant-Phase-Element Behavior of a Disk Electrode with Faradaic Reactions
Huang, V. M.-W., Vivier, V., Orazem, M. E., Pébère, N., & Tribollet, B. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2398894 · Cited by 185
Soares, D. M., Teschke, O., & Torriani, I. L. (1992) · Journal of The Electrochemical Society · doi:10.1149/1.2069207 · Cited by 178
Interfacial electrochemistry: An experimental approach
Gileadi, E., Kirowa‐Eisner, E., & Penciner, J. (1975) · Cited by 167
Conway, B. E., Angerstein‐Kozlowska, H., Sattar, M. A., & Tilak, B. V. K. S. R. A. (1983) · Journal of The Electrochemical Society · doi:10.1149/1.2120106 · Cited by 138
Alsabet, M., Grdeń, M., & Jerkiewicz, G. (2011) · Electrocatalysis · doi:10.1007/s12678-011-0067-9 · Cited by 137
Voltammetry and anodic stability of a hydrous oxide film on a nickel electrode in alkaline solution
Vukovìć, M. (1994) · Journal of Applied Electrochemistry · doi:10.1007/bf00348775 · Cited by 121
Electrochemical studies of a nickel electrode for the hydrogen evolution reaction
Kibria, A. K. M. F. (1995) · International Journal of Hydrogen Energy · doi:10.1016/0360-3199(94)00073-9 · Cited by 94
Voltammetric behaviour of nickel in base with particular reference to thick oxide growth
Burke, L. D., & Twomey, T. A. M. (1984) · Journal of Electroanalytical Chemistry · doi:10.1016/s0022-0728(84)80158-8 · Cited by 93
A comparison of cathodes for zero gap alkaline water electrolysers for hydrogen production
Pletcher, D., Li, X., & Wang, S. (2012) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2012.02.013 · Cited by 93
Melendres, C. A., & Pankuch, M. (1992) · Journal of Electroanalytical Chemistry · doi:10.1016/0022-0728(92)80384-g · Cited by 78
Abouatallah, R., Kirk, D. W., Thorpe, S. J., & Graydon, J. W. (2001) · Electrochimica Acta · doi:10.1016/s0013-4686(01)00777-0 · Cited by 70
Beden, B., Floner, D., ́GER, J.-M. L., & Lamy, C. (1985) · Surface Science · doi:10.1016/0039-6028(85)90985-9 · Cited by 70
Heats of Formation of Nickel and Cobalt Oxides (NiO and CoO) of Combustion Calorimetry
Boyle, B. J., King, E. G., & Conway, K. C. (1954) · Journal of the American Chemical Society · doi:10.1021/ja01643a072 · Cited by 69
The Role of Absorbed Hydrogen on the Voltage‐Time Behavior of Nickel Cathodes in Hydrogen Evolution
Rommal, H. E. G., & Morgan, P. J. (1988) · Journal of The Electrochemical Society · doi:10.1149/1.2095612 · Cited by 68
Time‐Dependent Energy Efficiency Losses at Nickel Cathodes in Alkaline Water Electrolysis Systems
Rommal, H. E. G., & Moran, P. J. (1985) · Journal of The Electrochemical Society · doi:10.1149/1.2113831 · Cited by 68
Cited by
Anion-Exchange Membrane Water Electrolyzers
Du, N., Roy, C., Peach, R., Turnbull, M., Thiele, S., & Bock, C. (2022) · Chemical Reviews · doi:10.1021/acs.chemrev.1c00854 · Cited by 1,075
Self-citationNickel hydroxides and related materials: a review of their structures, synthesis and properties
Hall, D. S., Lockwood, D. J., Bock, C., & MacDougall, B. R. (2015) · Proceedings of the Royal Society A: Mathematical, Physical and Engineering Sciences · doi:10.1098/rspa.2014.0792 · Cited by 1,043
Self-citationLedendecker, M., Krick Calderón, S., Papp, C., Steinrück, H., Antonietti, M., & Shalom, M. (2015) · Angewandte Chemie International Edition · doi:10.1002/anie.201502438 · Cited by 858
Electrocatalysts for the generation of hydrogen, oxygen and synthesis gas
Sapountzi, F. M., Gracia, J. M., Weststrate, C. J. (.-J., Fredriksson, H. O. A., & Niemantsverdriet, J. W. (. (2017) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2016.09.001 · Cited by 765
Zheng, X., Xu, J., Yan, K., Wang, H., Wang, Z., & Yang, S. (2014) · Chemistry of Materials · doi:10.1021/cm500347r · Cited by 671
Metadata
- Authors
- Hall, D. S., Bock, C., & MacDougall, B. R.
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 2013
- Volume
- 160
- Issue
- 3
- Pages
- F235-F243
- ISSN
- 0013-4651 (ISSN-L)
- 1945-7111
- OpenAlex
- W2138425634
- Cited by
- 330
- References
- 32
- FWCI
- 4.93
- Type
- journal article
- Language
- en
- Open access
- green
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.