Limitations in Bonding to Dentin and Experimental Strategies to Prevent Bond Degradation
Open accessThe DOI matches its Crossref record; 176 of the 176 references it cites were found in a registry or an index.
Abstract
The limited durability of resin-dentin bonds severely compromises the lifetime of tooth-colored restorations. Bond degradation occurs via hydrolysis of suboptimally polymerized hydrophilic resin components and degradation of water-rich, resin-sparse collagen matrices by matrix metalloproteinases (MMPs) and cysteine cathepsins. This review examined data generated over the past three years on five experimental strategies developed by different research groups for extending the longevity of resin-dentin bonds. They include: (1) increasing the degree of conversion and esterase resistance of hydrophilic adhesives; (2) the use of broad-spectrum inhibitors of collagenolytic enzymes, including novel inhibitor functional groups grafted to methacrylate resins monomers to produce anti-MMP adhesives; (3) the use of cross-linking agents for silencing the activities of MMP and cathepsins that irreversibly alter the 3-D structures of their catalytic/allosteric domains; (4) ethanol wet-bonding with hydrophobic resins to completely replace water from the extrafibrillar and intrafibrillar collagen compartments and immobilize the collagenolytic enzymes; and (5) biomimetic remineralization of the water-filled collagen matrix using analogs of matrix proteins to progressively replace water with intrafibrillar and extrafibrillar apatites to exclude exogenous collagenolytic enzymes and fossilize endogenous collagenolytic enzymes. A combination of several of these strategies should result in overcoming the critical barriers to progress currently encountered in dentin bonding.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“it has been hypothesized that cationic QACs can electrostatically act on the catalytic site of MMPs, thereby inhibiting MMP-catalyzed hydrolysis of the collagen matrix [106], [107].”
From Quaternary ammonium-based biomedical materials: State-of-the-art, toxicological aspects and antimicrobial resistance (2017) · cites this paper as [106]
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Hygroscopic and hydrolytic effects in dental polymer networks
Ferracane, J. L. (2006) · Dental Materials · doi:10.1016/j.dental.2005.05.005 · Cited by 1,505 · cited 1×
“Hydrophilic and ionic resin monomers are vulnerable to hydrolysis, due to the presence of ester linkages (Ferracane, 2006).”
BackgroundControlling Mineral Morphologies and Structures in Biological and Synthetic Systems
Meldrum, F. C., & Cölfen, H. (2008) · Chemical Reviews · doi:10.1021/cr8002856 · Cited by 1,397
Systematic review of the chemical composition of contemporary dental adhesives
Van Landuyt, K. L., Snauwaert, J., De Munck, J., Peumans, M., Yoshida, Y., Poitevin, A., Coutinho, E., Suzuki, K., Lambrechts, P., & Van Meerbeek, B. (2007) · Biomaterials · doi:10.1016/j.biomaterials.2007.04.044 · Cited by 1,397
Dental adhesion review: Aging and stability of the bonded interface
Breschi, L., Mazzoni, A., Ruggeri, A., Cadenaro, M., Di Lenarda, R., & De Stefano Dorigo, E. (2008) · Dental Materials · doi:10.1016/j.dental.2007.02.009 · Cited by 1,276 · cited 4×
“…bond strengths of contemporary adhesives have been shown to be quite high, substantial decreases in resin-dentin bond strength occurred after aging (Breschi et al., 2008), with continuous loss of bonded restorations over time for both etch-and-rinse and self-etch adhesive systems (van Dijken et…”
BackgroundInfluentialSelf-citationNudelman, F., Pieterse, K., George, A., Bomans, P. H. H., Friedrich, H., Brylka, L. J., Hilbers, P. A. J., de With, G., & Sommerdijk, N. A. J. M. (2010) · Nature Materials · doi:10.1038/nmat2875 · Cited by 1,185 · cited 1×
“…al., 2004) was used as a sequestration agent to simulate the aspartic acid and serine-rich mineralization-promoting C-terminal domain (ASARM) of cleaved DMP-1 (Gericke et al., 2010) to stabilize amorphous calcium phosphate into fluidic nanoprecursor particles (Gower, 2008; Nudelman et al., 2010).”
MethodCollagen Degradation by Host-derived Enzymes during Aging
Pashley, D. H., Tay, F. R., Yiu, C., Hashimoto, M., Breschi, L., Carvalho, R. M., & Ito, S. (2004) · Journal of Dental Research · doi:10.1177/154405910408300306 · Cited by 1,123
Self-citationGower, L. B. (2008) · Chemical Reviews · doi:10.1021/cr800443h · Cited by 1,086
Relationship between bond-strength tests and clinical outcomes
Van Meerbeek, B., Peumans, M., Poitevin, A., Mine, A., Van Ende, A., Neves, A., & De Munck, J. (2010) · Dental Materials · doi:10.1016/j.dental.2009.11.148 · Cited by 835
Clinical effectiveness of contemporary adhesives: A systematic review of current clinical trials
Peumans, M., Kanumilli, P., De Munck, J., Van Landuyt, K., Lambrechts, P., & Van Meerbeek, B. (2005) · Dental Materials · doi:10.1016/j.dental.2005.02.003 · Cited by 826
Phosphorylated Proteins and Control over Apatite Nucleation, Crystal Growth, and Inhibition
George, A., & Veis, A. (2008) · Chemical Reviews · doi:10.1021/cr0782729 · Cited by 745 · cited 2×
“Additional acidic matrix phosphoproteins are utilized as templates to induce mineral nucleation and growth within the organic scaffold (George and Veis, 2008).”
BackgroundMethod
Research works printed but not linked: 2
- Scaffa P Barros N Vidal C Tersariol IL Pashley D Tjäderhane L Chlorhexidine inhibits cysteine cathepsins [abstract] J Dent Res 2010 accessed 10/13/2010 (Spec Iss):4554.URL available at: http://iadr.confex.com/iadr/2010barce/webprogramcd/Paper140222.html 22266526
- Xu A-W Ma Y Cölfen H Biomimetic mineralization J Mater Chem 2007 7 415 449
Cited by
Items 301–400 of 694
Chen, L., Chen, W., Yu, Y., Yang, J., Jiang, Q., Wu, W., & Yang, D. (2021) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2021.104625 · Cited by 18
Nagpal, R., Manuja, N., & Pandit, I. K. (2015) · Journal of Clinical Pediatric Dentistry · doi:10.17796/jcpd.39.2.p14u4x3q14272452 · Cited by 18
Pashaev, D., Demırcı, M., Tekçe, N., Tuncer, S., & Baydemır, C. (2017) · Bio-Medical Materials and Engineering · doi:10.3233/bme-171665 · Cited by 18
Role of dentin cross-linking agents in optimizing dentin bond durability
Abu-Nawareg, M. M., Abuelenain, D. A., Elkassas, D. W., Haimed, T. S. A., Al-Dharrab, A. A., Zidan, A. Z., Hassan, A. H., & Pashley, D. H. (2017) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2017.06.009 · Cited by 18
Self-citationSize effect of nano-hydroxyapatite on proliferation of odontoblast-like MDPC-23 cells
Li, N., Wu, G., Hua, Y. A. O., Tang, R., Gu, X., & Tu, C. (2019) · Dental Materials Journal · doi:10.4012/dmj.2018-155 · Cited by 18
Self-citationLonghi, M., Cerroni, L., Sg, C., Ariano, & Pasquantonio, G. (2014) · PubMed · Cited by 17
Liu, Z., Feng, X., Wang, X., Yang, S., Mao, J., & Gong, S. (2021) · Materials · doi:10.3390/ma14051178 · Cited by 17
Self-citationEffect of proanthocyanidin incorporation into dental adhesive on durability of resin–dentin bond
Epasinghe, D. J., Yiu, C. K. Y., & Burrow, M. F. (2015) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2015.09.006 · Cited by 17
Degradation in the fatigue strength of dentin by cutting, etching and adhesive bonding
Lee, H. H., Majd, H., Orrego, S., Majd, B. K., Romberg, E., Mutluay, M. M., & Arola, D. D. (2014) · Dental Materials · doi:10.1016/j.dental.2014.06.005 · Cited by 20
In situ study of the gelatinase activity in demineralized dentin from rat molar teeth
Pessoa, J. I. C., Guimarães, G. N., Viola, N. V., da Silva, W. J., de Souza, A. P., Tjäderhane, L., Line, S. R. P., & Marques, M. R. (2012) · Acta Histochemica · doi:10.1016/j.acthis.2012.07.002 · Cited by 17
Self-citationNagpal, R., Manuja, N., Verma, R., Singh, U., & Tyagi, S. (2013) · Journal of Conservative Dentistry · doi:10.4103/0972-0707.114352 · Cited by 17
“[16] Increase in resin dentin bond longevity achieved by PA cannot be solely explained by augmentation in the cross-linking density.”
Loguércio, A. D., Stanislawczuk, R., Mittelstadt, F. G., Meier, M. M., & Reis, A. (2013) · Journal of Dentistry · doi:10.1016/j.jdent.2013.04.009 · Cited by 17
Wu, S., Gu, L., Huang, Z., Sun, Q., Chen, H., Ling, J., & Mai, S. (2016) · European Journal Of Oral Sciences · doi:10.1111/eos.12319 · Cited by 17
“and increasing the degree of conversion and esterase resistance of hydrophilic adhesives (7).”
BackgroundInteraction of ACP and MDP and its effect on dentin bonding performance
Zhang, L., Wang, W., Wang, C., Li, M., Wang, Z., Su, Z., & Fu, B. (2018) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2018.12.017 · Cited by 17
Rime, S. A., Ahmed, Z., Yamauti, M., Carvalho, R. M., Chowdhury, A. F. M. A., & Sano, H. (2020) · Dental Materials Journal · doi:10.4012/dmj.2019-436 · Cited by 16
Mortazavi, V., Samimi, P., Rafizadeh, M., & Kazemi, S. (2012) · Dental Research Journal · doi:10.4103/1735-3327.104878 · Cited by 16
“[3] In addition to hydrolysis, insuffi cient penetration of resin into the collagen fi brils due to residual water decreases the durability of resin– dentin bond.[1,4] Recent studies have demonstrated that dentin adhesives cannot replace free and loosely bound water from the interfi brillar spaces, even when resin mon…”
Marginal Sealing Durability of Two Contemporary Self-Etch Adhesives
Khoroushi, M., & Mansoori, M. (2012) · ISRN Dentistry · doi:10.5402/2012/204813 · Cited by 16
“The most important challenge for dental adhesives is the production of a durable bond between two materials with different structures [9].”
BackgroundCruz, J. V. E., Polido, M., Brito, J., & Gonçalves, L. M. L. (2020) · Polymers · doi:10.3390/polym12020461 · Cited by 16
“These properties have been considered quite important to the hydrolytic stability of the bonding interface [2,28].”
Prasansuttiporn, T., Thanatvarakorn, O., Mamanee, T., Hosaka, K., Tagami, J., FOXTON, R. M., & Nakajima, M. (2020) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2020.102648 · Cited by 17
Beck, F., & Ilie, N. (2022) · Bioengineering · doi:10.3390/bioengineering9010034 · Cited by 16
Daood, U., & Fawzy, A. (2023) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2023.105737 · Cited by 16
Diniz, A. C. S., Bauer, J. R. D. O., Veloso, S. D. A. R., Abreu‐Pereira, C. A., Carvalho, C. N., Leitão, T. J., Firoozmand, L. M., & Filho, E. M. M. (2023) · Materials · doi:10.3390/ma16051765 · Cited by 16
“Strategies aimed at the preservation of dental structures have been continuously studied, with the remineralization of partially demineralized dentin being verified [1], which can occur in the presence of a healthy pulp.”
BackgroundChai, Y., Lin, H. R., Zheng, G., Zhang, X., Niu, G., & Du, Q. (2015) · Bio-Medical Materials and Engineering · doi:10.3233/bme-151290 · Cited by 16
“Although the bond strength of 2-SE is lower (possibly because its primmer with high viscosity has an adverse effect on the penetration of resinous monomers into the collagen network leading to the non-ideal hybrid layer formation), there is less adhesive infiltration (Figure 5C) and compromising the bond quality, whic…”
ResultEffect of zinc-doping in physicochemical properties of dental adhesives.
Pomacóndor-Hernández, C., Osorio, R., Aguilera, F. S., Cabello, I., De Goes, M., & Toledano, M. (2015) · PubMed · Cited by 16
Toledano, M., Osorio, E., Aguilera, F. S., Cabello, I., Toledano‐Osorio, M., & Osorio, R. (2016) · Journal of Raman Spectroscopy · doi:10.1002/jrs.5055 · Cited by 16
Song, L., Ye, Q., Ge, X., Misra, A. K., Tamerler, C., & Spencer, P. (2017) · Acta Biomaterialia · doi:10.1016/j.actbio.2017.12.001 · Cited by 17
The Effect of SnCl2/AmF Pretreatment on Short- and Long-Term Bond Strength to Eroded Dentin
Zumstein, K., Peutzfeldt, A., Lussi, A., & Flury, S. (2018) · BioMed Research International · doi:10.1155/2018/3895356 · Cited by 16
“Various factors have been held accountable for degradation of the resin-dentin interface such as the hydrophilic monomers incorporated in simplified adhesives, the water concentration in self-etch adhesives [21], inadequate infiltration of resin monomers within the hybrid layer, proteolytic breakdown of exposed collag…”
BackgroundTian, F., Mu, H., Shi, Y., Chen, X., Zou, X., Gao, X., & Wang, X. (2024) · Dental Materials · doi:10.1016/j.dental.2024.05.013 · Cited by 15
Advances in macro-bioactive materials enhancing dentin bonding
Fan, J., Wang, P., Wang, S., Li, R., Yang, Y., Jin, L., Sun, Y., & Li, D. (2025) · Discover Nano · doi:10.1186/s11671-025-04206-w · Cited by 15
The inhibitory effect of a polymerisable cationic monomer on functional matrix metalloproteinases
Liu, N., Li, F., Chen, Y., Zhang, L., Lu, S., Kang, J., & Chen, J. (2013) · Journal of Dentistry · doi:10.1016/j.jdent.2013.08.008 · Cited by 16
Yang, H., Chen, Z., Yan, H.-Y., & Huang, C. (2017) · Dental Materials Journal · doi:10.4012/dmj.2017-006 · Cited by 15
Current Developments on Enamel and Dentin Remineralization
Braga, R. R., & Habelitz, S. (2019) · Current Oral Health Reports · doi:10.1007/s40496-019-00242-5 · Cited by 15
Wu, Q., Shan, T., Zhao, M., Mai, S., & Gu, L. (2019) · Royal Society Open Science · doi:10.1098/rsos.182104 · Cited by 15
“Although integrity of the denuded collagen fibrils can be preserved, the flaccid collagen matrices are susceptible to creep or cyclic fatigue rupture after prolonged function [18].”
BackgroundDávila‐Sánchez, A., Gutiérrez, M. F., Bermudez, J., Méndez-Bauer, L., Pulido, C., Kiratzc, F., Alegría-Acevedo, L. F., Farago, P. V., Loguércio, A. D., Sauro, S., et al. (2021) · Polymers · doi:10.3390/polym13071145 · Cited by 15
“The bonding interface created by “simplified” adhesive systems is still considered the “Achilles′ heel” of resin-based restorations [1], since it is usually susceptible to severe degradation over time [2,3].”
BackgroundRole of Natural Cross Linkers in Resin–Dentin Bond Durability: A Systematic Review and Meta-Analysis
Anumula, L., Ramesh, S., Kolaparthi, V. S. K., Kirubakaran, R., Karobari, M. I., Arora, S., Saleh, A. A., Aldowah, O., Messina, P., & Scardina, G. A. (2022) · Materials · doi:10.3390/ma15165650 · Cited by 14
“These exposed collagen fibres (incompletely infiltrated) within the hybrid layer may become susceptible to degradation [7].”
BackgroundElectrical properties of resin monomers used in restorative dentistry
Breschi, M., Fabiani, D., Sandrolini, L., Colonna, M., Sisti, L., Vannini, M., Mazzoni, A., Ruggeri, A., Pashley, D. H., & Breschi, L. (2012) · Dental Materials · doi:10.1016/j.dental.2012.05.009 · Cited by 14
“[7] Liu Y, Tjaderhane L, Breschi L, Mazzoni A, Li N, Mao J, et al.”
Self-citationChlorhexidine application to stabilize the adhesive interface: why and how?
Breschi, L. (2013) · PubMed · doi:10.3290/j.jad.a32067 · Cited by 14
Self-citationAl-Khureif, A. A., Mohamed, B. A., Al‐Shehri, A. M., Khan, A. A., & Divakar, D. D. (2020) · Photodiagnosis and Photodynamic Therapy · doi:10.1016/j.pdpdt.2020.101795 · Cited by 14
Almeida, G. S., da Silva, E. M., Guimarães, J. G. A., da Silva, R. N. L., dos Santos, G. B., & Poskus, L. T. (2017) · BioMed Research International · doi:10.1155/2017/5940479 · Cited by 14
“This last one has been proposed as one of the major reasons for the long-term degradation of the hybrid layer and the consequent drop in the resin-dentin bonding [9, 10].”
Guo, X., Cheng, Q., Yu, G., Wang, H., Tian, Z., Shi, Z., Cui, Z., & Zhu, S. (2019) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2019.103471 · Cited by 13
A multi-functional dentine bonding system combining a phosphate monomer with eugenyl methacrylate
Alkattan, R. K., Banerji, S., & Deb, S. (2022) · Dental Materials · doi:10.1016/j.dental.2022.04.005 · Cited by 13
Biochemical and Mechanical Analysis of Occlusal and Proximal Carious Lesions
Al-Shareefi, S., Addie, A. J., & Al-Taee, L. A. (2022) · Diagnostics · doi:10.3390/diagnostics12122944 · Cited by 13
Adhesive Materials with Bioprotective/Biopromoting Functions
Ma, S., Niu, L., Li, F., Fang, M., Zhang, L., Tay, F. R., Imazato, S., & Chen, J. (2014) · Current Oral Health Reports · doi:10.1007/s40496-014-0027-6 · Cited by 14
Self-citationDegradation of resin-dentin bonds of etch-and-rinse adhesive system to primary and permanent teeth
Lenzi, T. L., Soares, F. Z. M., & Rocha, R. D. O. (2012) · Brazilian Oral Research · doi:10.1590/s1806-83242012005000023 · Cited by 13
Alonso, J. R. L., Basso, F. G., Scheffel, D. L. S., Costa, C. A. D. S., & Hebling, J. (2017) · Journal of Prosthetic Dentistry · doi:10.1016/j.prosdent.2017.08.014 · Cited by 15
“The new crosslinks between amino acids within the catalytic site of the enzymes may irreversibly alter the spatial conformation or flexibility of the cleftlike catalytic domain and prevent its optimal recognition and complexing with the collagen substrate.(51,52) A recent study(36) demonstrated that the durability of…”
BackgroundStructure–property relationships for wet dentin adhesive polymers
Parthasarathy, R., Misra, A. K., Song, L., Ye, Q., & Spencer, P. (2018) · Biointerphases · doi:10.1116/1.5058072 · Cited by 13
Peled, Y., Stewart, C. A., Glogauer, M., & Finer, Y. (2023) · Dentistry Journal · doi:10.3390/dj11090217 · Cited by 17
“When incubated with bisGMA monomers (Figure 6), and bisGMA-containing RBC (Figure 7), neutrophils obtain CE-like activities that yield the release of bisHPPP, the degradation derivative of bisGMA, with a reduced bisHPPP release rate after 48 h among the bisGMA-containing RBC [18].”
BackgroundPark, I.-S., Kim, H., Kwon, J., & Kim, D.-S. (2025) · Journal of Functional Biomaterials · doi:10.3390/jfb16010029 · Cited by 12
“Furthermore, inactive proforms of proteolytic enzymes called matrix metalloproteinases (MMPs) have been identified in both mineralized and demineralized human dentin and exhibit collagenolytic and gelatinolytic activities due to the exposure of collagen fibrils when activated [4,5].”
Seredin, P. V., Goloshchapov, D. L., Кашкаров, В. М., Ippolitov, Y. A., Ippolitov, I. Y., & Vongsvivut, J. P. (2021) · Diagnostics · doi:10.3390/diagnostics11071294 · Cited by 12
“The existing strategies of hybrid layer formation [4,5] are gradually improved.”
BackgroundDental Adhesives—Surface Modifications of Dentin Structure for Stable Bonding
Fronza, B. M., Braga, R. R., & Cadenaro, M. (2022) · Dental Clinics of North America · doi:10.1016/j.cden.2022.05.002 · Cited by 14
The stamp technique for direct restoration in a ICDAS 4 carious lesion: A 4‐year follow‐up
Vertuan, M., Mosquim, V., Guimarães, G. M. D. F., Obeid, A. T., Bombonatti, J. F. S., Ishikiriama, S. K., & Furuse, A. Y. (2022) · Journal of Esthetic and Restorative Dentistry · doi:10.1111/jerd.12963 · Cited by 13
de Oliveira, R. P., de Paula, B. L. F., Alencar, C. D. M., Alves, E. B., & Silva, C. M. (2023) · Journal of Dentistry · doi:10.1016/j.jdent.2022.104407 · Cited by 13
Evaluation of a novel primer containing isocyanate group on dentin bonding durability
Yang, Z., Gao, J., Duan, L.-Y., Luo, M. L., Fan, Y., Xu, R., Zhou, M.-D., Tay, F. R., Niu, L., Zhou, W., et al. (2023) · Dental Materials · doi:10.1016/j.dental.2023.03.008 · Cited by 12
Self-citationMirzaei, K., Ahmadi, E., Rafeie, N., & Abbasi, M. (2023) · BMC Oral Health · doi:10.1186/s12903-023-02913-3 · Cited by 12
Reinke, S. M. G., Lawder, J. A. D. C., Divardin, S. D. F., Raggio, D. P., Reis, A., & Loguércio, A. D. (2012) · Journal of Biomedical Materials Research Part B Applied Biomaterials · doi:10.1002/jbm.b.32708 · Cited by 12
“This shifted the focus of researchers’ investigations for the evaluation of aging mechanisms involved in degradation of the resin-bonded interfaces.(2,3) Most of the knowledge we have about the longevity of dentin bonds are based on in vitro studies, which showed significant reduction on resin–dentin bond strengths va…”
BackgroundInhibitory effect of curcuminoid pretreatments on endogenous dentin proteases
SESEOGULLARI-DIRIHAN, R., Atay, M. T., Pashley, D. H., & Tezvergil‐Mutluay, A. (2018) · Dental Materials Journal · doi:10.4012/dmj.2017-116 · Cited by 13
Self-citationde Souza, M. Y., Jurema, A. L. B., Caneppele, T. M. F., & Bresciani, E. (2019) · Brazilian Oral Research · doi:10.1590/1807-3107bor-2019.vol33.0052 · Cited by 12
AFM study of the effects of collagenase and its inhibitors on dentine collagen fibrils
Zheng, X., Hu, J., Chen, Y., Zhu, Y., & Chen, H. (2011) · Journal of Dentistry · doi:10.1016/j.jdent.2011.12.009 · Cited by 12
Mandava, J., Salagalla, U., Ravi, R., & Nunna, V. (2018) · Journal of Conservative Dentistry · doi:10.4103/jcd.jcd_30_18 · Cited by 12
“[15] The distribution of these matrix metalloproteinases was found to be different with different depths of coronal dentin indicating their different proteolytic potentials.”
Dentine collagen cross-linking using tiopronin-protected Au/EDC nanoparticles formulations
Daood, U., Akram, Z., Matinlinna, J. P., & Fawzy, A. (2019) · Dental Materials · doi:10.1016/j.dental.2019.04.005 · Cited by 13
Effect of grape seed extract-containing phosphoric acid formulations on bonding to enamel and dentin
Paludo, T., Marcondes, M. L., Souto, A. A., Lopes, G. C., Loguércio, A. D., & Spohr, A. M. (2019) · Brazilian Oral Research · doi:10.1590/1807-3107bor-2019.vol33.0098 · Cited by 12
El-Aal, N. H. A., El-Haliem, H. A., & Zaghloul, N. M. (2021) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2021.103073 · Cited by 11
Novel rechargeable nano-calcium phosphate and nano-calcium fluoride resin cements
Alsahafi, R., Mitwalli, H., Alhussein, A., Balhaddad, A. A., Alquria, T., Melo, M. A. S., Lynch, C. D., Oates, T. W., Zhang, K., Xu, H. H. K., et al. (2022) · Journal of Dentistry · doi:10.1016/j.jdent.2022.104312 · Cited by 11
Optimization of direct currents to enhance dentine bonding of simplified one‐step adhesive
Chen, H., Fu, D., Yang, H., Liu, Y., Huang, Y., & Huang, C. (2014) · European Journal Of Oral Sciences · doi:10.1111/eos.12140 · Cited by 11
Self-citationIn vitro remineralization of hybrid layers using biomimetic analogs
Lin, H., Lin, J., Li, J., Xu, J., & Mehl, C. (2016) · Journal of Zhejiang University SCIENCE B · doi:10.1631/jzus.b1600151 · Cited by 14
“Several strategies have been developed to stabilize the bond between composite resin and dentin and thus prevent restoration failure (Liu et al., 2011).”
BackgroundAl-Ani, A. A. S. S., Salim, I. A., SESEOGULLARI-DIRIHAN, R., Mutluay, M., Tjäderhane, L., & Tezvergil‐Mutluay, A. (2021) · European Journal Of Oral Sciences · doi:10.1111/eos.12756 · Cited by 11
Self-citationRosa‐e‐Silva, V. L., da Silva, F. A. S., dos Santos, G. N. A., de Assis, H. C., Souza‐Gabriel, A. E., Silva‐Sousa, Y. T. C., Lopes‐Olhê, F. C., Sousa‐Neto, M. D., & Mazzi‐Chaves, J. F. (2022) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2022.105486 · Cited by 11
Influence of EDC on Dentin-Resin Shear Bond Strength and Demineralized Dentin Thermal Properties
Tang, L., Zhang, Y., Liu, Y., & Zhou, Y. (2016) · Materials · doi:10.3390/ma9110920 · Cited by 11
Self-citationEndogenous Enzymatic Activity in Dentin Treated with a Chitosan Primer
Maravić, T., Baena, E., Mazzitelli, C., Josić, U., Mancuso, E., Checchi, V., Generali, L., Ceballos, L., Breschi, L., & Mazzoni, A. (2021) · International Journal of Molecular Sciences · doi:10.3390/ijms22168852 · Cited by 11
“There are two main trends under investigation, MMPs inhibitors and cross-linking agents [5,7,8].”
BackgroundSelf-citationNisar, S., Hass, V., & Wang, Y. (2025) · Dental Materials · doi:10.1016/j.dental.2025.03.005 · Cited by 11
Inhibitory effect of natural polyphenols on recombinant and endogenous dentinal proteases
Liu, Y., Yang, H., Qiu, K., Li, K., Yu, J. L., Yao, C., & Huang, C. (2025) · Journal of Dentistry · doi:10.1016/j.jdent.2025.105895 · Cited by 10
Self-citationReher, T. P. V. V. (2015) · JBR Journal of Interdisciplinary Medicine and Dental Science · doi:10.4172/2376-032x.1000166 · Cited by 10
“It is well documented that dentin and dentinal fluid can act as a peroxide and oxygen reservoir [20] which may be present at the bonding interface, inhibiting the polymerization reaction and reducing bond strength.”
BackgroundEffect of the use of bromelain associated with bioactive glass-ceramic on dentin/adhesive interface
Vivanco, R. G., Sousa, A. B. S., Oliveira, V. D. C., Sinhoreti, M. A. C., & Pires‐de‐Souza, F. D. C. P. (2024) · Clinical Oral Investigations · doi:10.1007/s00784-024-05496-7 · Cited by 12
“MMPs and cysteine cathepsins (CTs) display optimal proteolytic activity at acidic pH [48, 49], like that induced by the universal adhesive system used in this study (pH = 2.7) [48].”
InfluentialEffect of chitosan on resin-dentin interface durability: A 2 year in-vitro study
Zidan, A. Z. (2019) · Egyptian Dental Journal /Egyptian Dental Journal · doi:10.21608/edj.2019.72691 · Cited by 10
“TABLE (2) The mean, standard deviation (SD) values and results of two-way ANOVA test for comparison between nanoleakage (”
BackgroundMethodInfluentialWang, X., Li, Q., Lu, H., Liu, Z., Wu, Y., Mao, J., & Gong, S. (2022) · Polymers · doi:10.3390/polym14153166 · Cited by 13
Self-citationNanoleakage and Durability of Resin/Dentin Bonds
Hashimoto, M., Yamaguchi, S., & Imazato, S. (2015) · Current Oral Health Reports · doi:10.1007/s40496-015-0059-6 · Cited by 11
da Fonseca, B. M., Pleffken, P. R., Balducci, I., Tay, F. R., Pucci, C. R., & de Araújo, M. A. M. (2013) · Brazilian Dental Science · doi:10.14295/bds.2013.v16i3.876 · Cited by 16
Self-citationFuture Perspectives of Biomimetics in Restorative Dentistry
Basheer, N., Madhubala, M. M., & Mahalaxmi, S. (2020) · Journal of Pharmaceutical Research International · doi:10.9734/jpri/2020/v32i2530820 · Cited by 10
Bin-Shuwaish, M. S., & Aljamhan, A. S. (2020) · The Journal of Contemporary Dental Practice · doi:10.5005/jp-journals-10024-2948 · Cited by 10
“Photomed Laser Surg 2007;25(2):118–123.”
Ghazvehi, K., Saffarpour, A., & Habibzadeh, S. (2022) · Clinical and Experimental Dental Research · doi:10.1002/cre2.569 · Cited by 10
“diimide (EDC), is another MMP inhibitor, recently introduced as a nonspecific protein cross‐linker with low toxicity (Liu et al., 2011; Scheffel et al., 2015).”
BackgroundYehia, Y. H., Ibrahim, A. H., Abouauf, E. A., & ElZoghbi, A. (2022) · Open Access Macedonian Journal of Medical Sciences · doi:10.3889/oamjms.2022.7952 · Cited by 9
“The esterases enzymes can break covalent bonds between the polymers by the addition of water to the ester bonds [21].”
BackgroundNew Monomer Capable of Dual Chemical Binding with Dentin to Improve Bonding Durability
Wang, H., Li, K., Tian, Z., Zhu, Y., Liu, X. Y., Yang, S. H., Qiao, S., Zhu, S., & Shi, Z. (2024) · Journal of Dental Research · doi:10.1177/00220345241253526 · Cited by 9
“In addition, researchers have synthesized collagen crosslinking agents or endogenous enzyme inhibitors that enhance the resistance of collagen fibers in dentin against enzymatic degradation (Liu et al. 2011; Xu et al. 2019; Yu et al. 2022).”
Amelogenin-Derived Peptide-Modified Poly(amidoamine) Dendrimers for Root Caries Prevention
Cai, X., Chen, Y., Wu, J., Wang, A., & Wang, X. (2025) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.4c20204 · Cited by 9
Luo, Q., Zhang, Z., Chen, Y., Shu, C., Cheng, Y., Lu, Y., Xu, J., & Li, X. (2025) · Chemical Engineering Journal · doi:10.1016/j.cej.2025.167575 · Cited by 9
Effect of Collagen-Reactive Functional Monomer on Etch-and-Rinse Adhesives
Yu, S. Y., He, X., Tian, Z., Li, K. X., Chen, H., Wang, H. M., Shi, Z., Zhu, S., & Cui, Z. (2022) · Journal of Dental Research · doi:10.1177/00220345221134278 · Cited by 9
“However, such improvements in bond stability require coordination with ethanol wet bonding techniques, and the application of a primer increases the clinical steps and processing time involved (Liu et al. 2011).”
BackgroundTang, W., Li, Q., Sui, Y., Dong, X., Nie, R., & Meng, X. (2023) · Journal of Dentistry · doi:10.1016/j.jdent.2023.104733 · Cited by 10
Understanding the chemistry and improving the durability of dental resin–dentin bonded interface
Li, F., Zhang, L., Weir, M. D., Cheng, L., Zhang, K., & Xu, H. H. K. (2016) · Elsevier eBooks · doi:10.1016/b978-0-08-100330-5.00006-6 · Cited by 11
Madhubala, M. M., Mahalaxmi, S., Jayaraman, M., & Sathyakumar, S. (2016) · Indian Journal of Dental Research · doi:10.4103/0970-9290.199585 · Cited by 9
Influence of grape seed extract in adhesion on dentin surfaces conditioned with Er,Cr:YSGG laser
da Silva, A. C. M., Melo, P., Ferreira, J. P. M., Arantes‐Oliveira, S., & Gutknecht, N. (2019) · Lasers in Medical Science · doi:10.1007/s10103-019-02749-w · Cited by 9
Effect of polydopamine incorporated dentin adhesives on bond durability
Devarajan, S. S., Madhubala, M. M., Rajkumar, K., James, V., Narasimhan, S., Mahalaxmi, S., & Sathyakumar, S. (2020) · Journal of Adhesion Science and Technology · doi:10.1080/01694243.2020.1792136 · Cited by 10
Li, M. X., Duan, L., Chen, M. L., Tian, F. C., & Fu, B. (2021) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2021.105038 · Cited by 9
Ebrahimi, M., Majidinia, S., & Sarraf, A. (2023) · Frontiers in Dentistry · doi:10.18502/fid.v19i39.11749 · Cited by 9
Luo, Y. F., Si, R., Yuan, H., Wang, M., Yu, Y., Huang, X., Huang, R., Huang, Y., Luo, Y., Jin, W., et al. (2023) · BMC Oral Health · doi:10.1186/s12903-023-02841-2 · Cited by 9
“Although cross-linker can maintain the integrity of the mineral-denuded collagen matrices, the waterfilled, resin-sparse and flaccid collagen fibrils are prone to cyclic fatigue breakdown after repetitive loads [8].”
BackgroundSubmicron-to-nanoscale structure characterization and organization of crystals in dentin bioapatites
Toledano, M., Aguilera, F. S., Osorio, E., López‐López, M. T., Cabello, I., Toledano‐Osorio, M., & Osorio, R. (2016) · RSC Advances · doi:10.1039/c6ra02373h · Cited by 9
Microleakage of Lithium Disilicate Crown Margins Finished on Direct Restorative Materials
Metz, M. J., Durski, M. T., Chou, J., Crim, G. A., Harris, B. T., & Lin, W.-S. (2016) · Operative Dentistry · doi:10.2341/15-225-l · Cited by 9
Mohammadi, R., Kaplan, S. A., Harmankaya, A., & Gönder, H. Y. (2025) · Materials · doi:10.3390/ma18163888 · Cited by 8
“Recent advances in restorative dentistry have largely focused on perfecting the bonding process and adhesive interfaces [10].”
Yang, Y., Inoue, G., Hosaka, K., Tichý, A., Ikeda, M., Tagami, J., & Shimada, Y. (2023) · Operative Dentistry · doi:10.2341/23-005-l · Cited by 10
Enhancing dentin bonding quality through Acetone wet-bonding technique: a promising approach
Zhao, S., Zhu, Z., Yu, J. L., Yao, C., Yu, M., Yang, H., & Huang, C. (2023) · Frontiers in Bioengineering and Biotechnology · doi:10.3389/fbioe.2023.1309503 · Cited by 8
“After acid etching of dentin surfaces, the collagen left unprotected would be degraded by enzymes, resulting in poor dentin bonding durability (Liu et al., 2011).”
BackgroundRadiographic, antibacterial and bond-strength effects of radiopaque caries tagging
Umwali, A., Askar, H., Paris, S., & Schwendicke, F. (2016) · Scientific Reports · doi:10.1038/srep27319 · Cited by 8
Topbaş, C., Adıgüzel, Ö., & Çölgeçen, Ö. (2019) · International Dental Research · doi:10.5577/intdentres.2019.vol9.no1.4 · Cited by 8
“The increase in surface roughness can be of clinical benefit as restorative dentistry also increases the bond strength of resin-containing fillers (29, 46).”
Background
Metadata
- Authors
- Liu, Y., Tjäderhane, L., Breschi, L., Mazzoni, A., Li, N., Mao, J., Pashley, D. H., & Tay, F. R.
- Affiliations
- Tongji Hospital (CN)
- Oulu University Hospital (FI)
- University of Trieste (IT)
- University of Bologna (IT)
- Fujian University of Traditional Chinese Medicine (CN)
- Department of Oral Biology
- Augusta University (US)
- Corresponding author
- Mao, J.
- Tay, F.R.
- Venue
- Journal of Dental Research
- Publisher
- SAGE Publications
- Published
- 2011-01-10
- Volume
- 90
- Issue
- 8
- Pages
- 953-968
- ISSN
- 0022-0345 (ISSN-L)
- 1544-0591
- PMC
- PMC3148178
- OpenAlex
- W2135724989
- Semantic Scholar
- fe5dcc58cb3bed23576b1db47776e8d76d4cd6a2
- Cited by
- 665
- References
- 176
- Citations by year
- 2026: 23 · 2025: 25 · 2024: 24 · 2023: 35 · 2022: 47 · 2021: 54 · 2020: 56 · 2019: 55 · 2018: 54 · 2017: 57 · 2016: 59 · 2015: 58 · 2014: 40 · 2013: 43 · 2012: 26
- FWCI
- 6.61
- Type
- journal article
- Language
- en
- Open access
- green
- www.ncbi.nlm.nih.gov
- Licence
- journals.sagepub.com/page/policies/text-and-data-mining-license (tdm)
- Locations
- Journal of Dental Research (publishedVersion)
- PubMed Central (publishedVersion)
- PubMed (publishedVersion)
- ArTS Archivio della ricerca di Trieste (University of Trieste https://www.units.it/) (submittedVersion)
- Archivio istituzionale della ricerca (Alma Mater Studiorum Università di Bologna) (submittedVersion)
- Funders
- National Institute of Dental and Craniofacial Research (R21DE019213, R01DE015306)
- Topics
- Health Sciences › Dentistry › General Dentistry › Dental materials and restorations
- Health Sciences › Dentistry › Oral Surgery › Endodontics and Root Canal Treatments
- Physical Sciences › Materials Science › General Materials Science › Material Properties and Applications
- Keywords
- dentin bonding, bond degradation, matrix metalloproteinases, cathepsins, collagenolytic enzymes, degree of conversion, collagenase inhibitors, crosslinking agents, ethanol-wet bonding, hydrophobic resin, biomimetic remineralization, collagen matrix, tooth-colored restorations
- MeSH terms
- Dental Bonding, Cathepsins, Collagen, Composite Resins, Cross-Linking Reagents, Dentin, Esterases, Humans, Hydrolysis, Tooth Remineralization, Dentin-Bonding Agents, Resin Cements, Hydrophobic and Hydrophilic Interactions, Polymerization, Matrix Metalloproteinase Inhibitors
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.