Abstract
The limited durability of resin-dentin bonds severely compromises the lifetime of tooth-colored restorations. Bond degradation occurs via hydrolysis of suboptimally polymerized hydrophilic resin components and degradation of water-rich, resin-sparse collagen matrices by matrix metalloproteinases (MMPs) and cysteine cathepsins. This review examined data generated over the past three years on five experimental strategies developed by different research groups for extending the longevity of resin-dentin bonds. They include: (1) increasing the degree of conversion and esterase resistance of hydrophilic adhesives; (2) the use of broad-spectrum inhibitors of collagenolytic enzymes, including novel inhibitor functional groups grafted to methacrylate resins monomers to produce anti-MMP adhesives; (3) the use of cross-linking agents for silencing the activities of MMP and cathepsins that irreversibly alter the 3-D structures of their catalytic/allosteric domains; (4) ethanol wet-bonding with hydrophobic resins to completely replace water from the extrafibrillar and intrafibrillar collagen compartments and immobilize the collagenolytic enzymes; and (5) biomimetic remineralization of the water-filled collagen matrix using analogs of matrix proteins to progressively replace water with intrafibrillar and extrafibrillar apatites to exclude exogenous collagenolytic enzymes and fossilize endogenous collagenolytic enzymes. A combination of several of these strategies should result in overcoming the critical barriers to progress currently encountered in dentin bonding.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“it has been hypothesized that cationic QACs can electrostatically act on the catalytic site of MMPs, thereby inhibiting MMP-catalyzed hydrolysis of the collagen matrix [106], [107].”
From Quaternary ammonium-based biomedical materials: State-of-the-art, toxicological aspects and antimicrobial resistance (2017) · cites this paper as [106]
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Hygroscopic and hydrolytic effects in dental polymer networks
Ferracane, J. L. (2006) · Dental Materials · doi:10.1016/j.dental.2005.05.005 · Cited by 1,505 · cited 1×
“Hydrophilic and ionic resin monomers are vulnerable to hydrolysis, due to the presence of ester linkages (Ferracane, 2006).”
BackgroundControlling Mineral Morphologies and Structures in Biological and Synthetic Systems
Meldrum, F. C., & Cölfen, H. (2008) · Chemical Reviews · doi:10.1021/cr8002856 · Cited by 1,397
Systematic review of the chemical composition of contemporary dental adhesives
Van Landuyt, K. L., Snauwaert, J., De Munck, J., Peumans, M., Yoshida, Y., Poitevin, A., Coutinho, E., Suzuki, K., Lambrechts, P., & Van Meerbeek, B. (2007) · Biomaterials · doi:10.1016/j.biomaterials.2007.04.044 · Cited by 1,397
Dental adhesion review: Aging and stability of the bonded interface
Breschi, L., Mazzoni, A., Ruggeri, A., Cadenaro, M., Di Lenarda, R., & De Stefano Dorigo, E. (2008) · Dental Materials · doi:10.1016/j.dental.2007.02.009 · Cited by 1,276 · cited 4×
“…bond strengths of contemporary adhesives have been shown to be quite high, substantial decreases in resin-dentin bond strength occurred after aging (Breschi et al., 2008), with continuous loss of bonded restorations over time for both etch-and-rinse and self-etch adhesive systems (van Dijken et…”
BackgroundInfluentialSelf-citationNudelman, F., Pieterse, K., George, A., Bomans, P. H. H., Friedrich, H., Brylka, L. J., Hilbers, P. A. J., de With, G., & Sommerdijk, N. A. J. M. (2010) · Nature Materials · doi:10.1038/nmat2875 · Cited by 1,185 · cited 1×
“…al., 2004) was used as a sequestration agent to simulate the aspartic acid and serine-rich mineralization-promoting C-terminal domain (ASARM) of cleaved DMP-1 (Gericke et al., 2010) to stabilize amorphous calcium phosphate into fluidic nanoprecursor particles (Gower, 2008; Nudelman et al., 2010).”
MethodCollagen Degradation by Host-derived Enzymes during Aging
Pashley, D. H., Tay, F. R., Yiu, C., Hashimoto, M., Breschi, L., Carvalho, R. M., & Ito, S. (2004) · Journal of Dental Research · doi:10.1177/154405910408300306 · Cited by 1,123
Self-citationGower, L. B. (2008) · Chemical Reviews · doi:10.1021/cr800443h · Cited by 1,086
Relationship between bond-strength tests and clinical outcomes
Van Meerbeek, B., Peumans, M., Poitevin, A., Mine, A., Van Ende, A., Neves, A., & De Munck, J. (2010) · Dental Materials · doi:10.1016/j.dental.2009.11.148 · Cited by 835
Clinical effectiveness of contemporary adhesives: A systematic review of current clinical trials
Peumans, M., Kanumilli, P., De Munck, J., Van Landuyt, K., Lambrechts, P., & Van Meerbeek, B. (2005) · Dental Materials · doi:10.1016/j.dental.2005.02.003 · Cited by 826
Phosphorylated Proteins and Control over Apatite Nucleation, Crystal Growth, and Inhibition
George, A., & Veis, A. (2008) · Chemical Reviews · doi:10.1021/cr0782729 · Cited by 745 · cited 2×
“Additional acidic matrix phosphoproteins are utilized as templates to induce mineral nucleation and growth within the organic scaffold (George and Veis, 2008).”
BackgroundMethod
Research works printed but not linked: 2
- Scaffa P Barros N Vidal C Tersariol IL Pashley D Tjäderhane L Chlorhexidine inhibits cysteine cathepsins [abstract] J Dent Res 2010 accessed 10/13/2010 (Spec Iss):4554.URL available at: http://iadr.confex.com/iadr/2010barce/webprogramcd/Paper140222.html 22266526
- Xu A-W Ma Y Cölfen H Biomimetic mineralization J Mater Chem 2007 7 415 449
Cited by
Items 401–500 of 694
Borgo, G. O., Vieira-Júnior, W. F., Theobaldo, J. D., Aguiar, F. H. B., & Lima, D. A. N. L. (2019) · European Journal of Dentistry · doi:10.1055/s-0039-1694307 · Cited by 8
Effect of tea root-derived proanthocyanidin fractions on protection of dentin collagen
Yang, H., Xie, B., Wang, Y., Cui, Y., Yang, H., Wang, X., Yang, X., & Bao, G. (2019) · Journal of International Medical Research · doi:10.1177/0300060519891303 · Cited by 8
“Because dentin collagen experiences demineralizationinduced instability, collagen cross-linkers have been widely used to improve its stability and durability, thus achieving good performance in dental tissue repair.(10,11) Proanthocyanidins (PAs) are secondary plant metabolites that reportedly have a positive effect o…”
BackgroundAljamhan, A. S., Alhazzaa, S. A., Albakr, A. H., Habib, S. R., & Zafar, M. S. (2021) · Polymers · doi:10.3390/polym13172921 · Cited by 8
“Research studies have shown the bonding to enamel to be more durable, while the bonding to dentin is far more intricate/complicated and can possibly be achieved only if more complicated, and time-consuming techniques are employed [39].”
BackgroundGovil, S., Asthana, G., Khambhala, R., Dhanak, N., Kanodia, S., & Parmar, A. (2021) · Journal of Conservative Dentistry · doi:10.4103/jcd.jcd_607_20 · Cited by 8
“[2] In SEM analysis, we observed the surface topography of mid-coronal dentin treated by wet and dry bonding and with 6.5% proanthocyanidin and 0.1M carbodiimide at ×10,000 and ×30,000 magnification.”
InfluentialThe inhibitory effects of various ions released from S-PRG fillers on dentin protease activity
Salim, I. A., SESEOGULLARI-DIRIHAN, R., Imazato, S., & Tezvergil‐Mutluay, A. (2022) · Dental Materials Journal · doi:10.4012/dmj.2022-141 · Cited by 8
Zhong, Q., Zhou, Q., Xiao, T., Li, X., Wu, X., Li, Y., Tao, Y., Wu, L., Zhou, Z., Wong, H. M., et al. (2023) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.3c07091 · Cited by 8
Effect of Chlorhexidine Application on Bond Durability of a Filled-Adhesive System
Boruziniat, A., Morteza, B., & Gifani, M. (2013) · DOAJ (DOAJ: Directory of Open Access Journals) · doi:10.22038/jdmt.2013.143 · Cited by 8
“So, other alternatives such as application of hydrophobic resin layer (31) or use three step etch and rinse (32), use ethanol-wet bonding (33), MMPs inhibitors (5-6), collagen cross linkers (28) , increasing the degree of conversion and use of esterase resistant adhesive may be helpful (17).”
BackgroundAyar, M. K. (2014) · Journal of Dental Sciences · doi:10.1016/j.jds.2014.06.001 · Cited by 8
“Residual water within interfaces reduces durability of the resinedentin bonding due to hydrolytic and enzymatic degradation of dentin hybrid layer components over time, and thus jeopardizes longevity of adhesive restoration.(5) A novel wet-bonding technique called “ethanol-wet bonding” was recently introduced to impro…”
BackgroundZhang, Z., Beitzel, D., Majd, H., Mutluay, M. M., Tezvergil‐Mutluay, A., Tay, F. R., Pashley, D. H., & Arola, D. D. (2017) · Dental Materials · doi:10.1016/j.dental.2017.08.192 · Cited by 8
Self-citationVallabhdas, A. K., Kabbinale, P., Nayak, R., Rajakumari, M., & Shilpa, T. (2018) · The Journal of Contemporary Dental Practice · doi:10.5005/jp-journals-10024-2211 · Cited by 8
Novel self-bonding composites: resin-dentin interfacial chemistry
Delgado, A. H. S., Almusa, A., Eshmawi, Y. T., Xia, W., Ashley, P. F., & Young, A. M. (2019) · Annals of Medicine · doi:10.1080/07853890.2018.1562698 · Cited by 8
Labban, N. Y., Al-Otaibi, H. N., Binrayes, A., Aljamhan, A. S., Alfouzan, A. F., Taweel, S. M. A., & Assery, M. K. A. (2021) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2021.102975 · Cited by 8
RetractedCruz, J. V. E., Delgado, A. H. S., Félix, S., Brito, J., Gonçalves, L. M. L., & Polido, M. (2022) · Polymers · doi:10.3390/polym14071462 · Cited by 8
“Such differences have been proposed to overcome the drawbacks mentioned above, such as hydrophilicity, limited interdiffusion of resin components and degradation over time, that all contribute to the inevitable failure of the restoration [11,12].”
BackgroundPedrosa, V. O., França, F. M. G., Turssi, C. P., do Amaral, F. L. B., Teixeira, L. N., Martinez, E. F., & Basting, R. T. (2018) · Archives of Oral Biology · doi:10.1016/j.archoralbio.2018.06.012 · Cited by 9
Fidalgo, T. K. D. S., Americano, G. C. A., Medina, D., Gonçalves, G. D. S. A., Letieri, A. D. S., & Maia, L. C. (2019) · Brazilian Oral Research · doi:10.1590/1807-3107bor-2019.vol33.0111 · Cited by 8
Zhang, J., Peng, Y., Hu, S., Xu, J., Yu, C., Hua, L., Zhou, S., & Liu, Q. (2025) · AIMS molecular science · doi:10.3934/molsci.2025010 · Cited by 7
Effect of Salvadora persica on resin-dentin bond stability
Abu-Nawareg, M. M., Abouelseoud, H. K., & Zidan, A. Z. (2024) · BMC Oral Health · doi:10.1186/s12903-024-04244-3 · Cited by 8
Pires, P. M., Neves, A. D. A., Farrar, P., Cascales, Á. F., Banerjee, A., Feitosa, V. P., & Sauro, S. (2025) · European Journal of Dentistry · doi:10.1055/s-0045-1804886 · Cited by 7
“8 When collagen fi brils are exposed and notcomplete-ly in fi ltrated by adhesive monomers, 30 they become susceptible to hydrolytic and enzymatic degradation, 20 which compromises the integrity of the resin – dentin bond over time.”
Baz, M. E., & Aboulenien, K. (2018) · Egyptian Dental Journal /Egyptian Dental Journal · doi:10.21608/edj.2018.78470 · Cited by 7
Torkani, M. A. M., Mesbahi, S., & Abdollahi, A. A. (2021) · Frontiers in Dentistry · doi:10.18502/fid.v17i34.5198 · Cited by 7
Wang, D., Wang, P., Xie, N., Yan, X.-Z., Xu, W., Lu-Ming, W. A. N. G., Liu, N., Wang, Y., & Ding, P. (2022) · Dental Materials Journal · doi:10.4012/dmj.2021-215 · Cited by 7
Moradian, M., Saadat, M., Sohrabniya, F., & Afifian, M. (2022) · Clinical and Experimental Dental Research · doi:10.1002/cre2.667 · Cited by 7
“The most rational explanation for these results is the ability of CHX to inhibit MMP‐2,8,9 and cysteine cathepsin enzymes, which play an important role in the degradation of the hybrid layer (Y. Liu et al., 2011).”
BackgroundZhang, T., Deng, W., Zhang, Y., Liu, M., Ling, Y., & Sun, Q. (2022) · FEBS Open Bio · doi:10.1002/2211-5463.13521 · Cited by 7
Hydroxyapatite Affects the Physicochemical Properties of Contemporary One-Step Self-Etch Adhesives
Motoyama, Y., Yamauti, M., Nakajima, M., Ikeda, M., Tagami, J., Shimada, Y., & Hosaka, K. (2022) · Materials · doi:10.3390/ma15228255 · Cited by 7
Boaru, M.-O., Tărăboanţă, I., Stoleriu, S., Andrian, S., Pancu, G., Nica, I., Șufaru, I.-G., & Iovan, G. (2023) · Medicina · doi:10.3390/medicina59020278 · Cited by 7
“On the other hand, when the resin monomers do not fully infiltrate the demineralized dentin, the collagen fibers in the lower area of the HL remain exposed to degrading phenomena [1,15].”
Mao, C., He, H., Chen, C., & Gu, X. (2023) · European Journal Of Oral Sciences · doi:10.1111/eos.12928 · Cited by 7
Fluid flow through dentin–self-etch resin interface during long term in vitro aging
Delannée, M., Grégoire, G., Vergnes, J., & Sharrock, P. (2013) · Materials Science and Engineering C · doi:10.1016/j.msec.2013.05.008 · Cited by 7
Toledano, M., Aguilera, F. S., López‐López, M. T., Osorio, E., Toledano‐Osorio, M., & Osorio, R. (2016) · Microscopy and Microanalysis · doi:10.1017/s1431927616011697 · Cited by 7
“It is important to emphasize that amorphous Ca/P provides a local ion-rich environment, which is considered favorable for in situ generation of prenucleation clusters, succeeding further dentin remineralization (Liu et al., 2011).”
BackgroundDaood, U., Omar, H., Tsoi, J. K. H., & Fawzy, A. (2018) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2018.06.015 · Cited by 7
Surfactin application for a short period (10/20 s) increases the surface wettability of sound dentin
Marcelino, L., Puppin-Rontani, J., Coutte, F., de Miranda, M. T. M., Etchegaray, A., & Puppin‐Rontani, R. M. (2019) · Amino Acids · doi:10.1007/s00726-019-02750-1 · Cited by 7
James, V., Madhubala, M. M., Devarajan, S. S., Mahalaxmi, S., & Sathyakumar, S. (2021) · Frontiers in Dentistry · doi:10.18502/fid.v17i35.5199 · Cited by 8
da Costa, M. B., Delgado, A. H. S., Amorim, T., Proença, L., Ramos, A. S., & Azul, A. M. (2021) · Polymers · doi:10.3390/polym13203562 · Cited by 9
“Not only does this required infiltration pose a challenge in an organic tissue like dentin [14,32,33], recent literature seems to agree that the quality of the adhesive bond becomes even more threatened in erosion [2–4,13,34,35].”
BackgroundResultAwad, M. M., Alradan, M., Alshalan, N., Robaian, A., Alhalabi, F., Abuelqomsan, M. A. S., Rabah, A., & Alrahlah, A. A. (2021) · International Journal of Environmental Research and Public Health · doi:10.3390/ijerph182312408 · Cited by 8
“Such enzymes could markedly deteriorate the resin-dentin bond strength [51].”
Long‐term effect of curcuminoid treatment on resin‐to‐dentin bond strength
Atay, M. T., SESEOGULLARI-DIRIHAN, R., Mutluay, M. M., & Tezvergil‐Mutluay, A. (2021) · European Journal Of Oral Sciences · doi:10.1111/eos.12837 · Cited by 7
Bonding of Bulk Fill versus Contemporary Resin Composites: A Systematic Review and Meta-analysis
Akah, M., Daifalla, L. E., & Yousry, M. M. (2016) · Indian Journal of Science and Technology · doi:10.17485/ijst/2016/v9i20/90525 · Cited by 7
Suppression of hydrolytic degradation in labile polymer networks via integrated styrenic nanogels
Rad, I. Y., Lewis, S. H., Barros, M. D., Kipper, M. J., & Stansbury, J. W. (2021) · Dental Materials · doi:10.1016/j.dental.2021.05.001 · Cited by 7
Li, M., Zheng, H., Xu, Y., Qiu, Y., Wang, Y., Jin, X., Zhang, Z., Zhang, L., & Fu, B. (2024) · BMC Oral Health · doi:10.1186/s12903-024-04756-y · Cited by 6
“This procedure completely demineralizes the superficial dentin, exposes collagen fibrils, and activates the endogenous enzymes, such as matrix metalloproteinases (MMPs) and cysteine cathepsins (CC), in the dentin matrix [6, 7].”
BackgroundThe Remineralization Potential of Resveratrol and Cucurbit[ n ]uril
Li, H., Yang, X., Bai, Z., Lu, Y., Bian, J., Xie, H., Chen, C., & Chen, K. (2025) · Journal of Dental Research · doi:10.1177/00220345251350135 · Cited by 6
“…properties of the collagen matrix and effectively inhibiting the biodegradation of collagen fibers via biomimetic remineralization of the dentin, as well as increasing the inhibition of MMP activity, can improve the durability of the resin–dentin bonding (Kim et al. 2010; Liu et al. 2011).”
Multifunctional Primer for Dentin Bonding via Biomimetic Mineralization
Yang, S., Tian, Z., Wang, H., Sun, D., Qiao, S., Shi, Z., He, X., & Zhu, S. (2025) · Journal of Dental Research · doi:10.1177/00220345251381633 · Cited by 6
“…resin coverage, is highly prone to enzymatic degradation (Breschi et al. 2018), while a water-filled gap zone create a favorable microenvironment for resin hydrolysis, progressively compromising bond integrity and ultimately leading to bonding failure (Kim, Mai, et al. 2010; Liu, Li, et al. 2011).”
Hass, V., Li, Y., Nisar, S., Peng, Z., & Wang, Y. (2022) · Dental Materials · doi:10.1016/j.dental.2022.11.006 · Cited by 6
Zeidan, L. C., Reis, A. F., Cassoni, A., & Rodrigues, J. A. (2016) · The Saudi Journal for Dental Research · doi:10.1016/j.sjdr.2016.06.006 · Cited by 6
Daood, U., Priyadarshini, B. M., Ibrahim, M. A., Pichika, M. R., Mak, K., & Fawzy, A. (2020) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2020.102797 · Cited by 6
“Therefore, bonding to carious dentine produces inferior results irrespective of adhesive system used [6] due to wetness, tubular-occlusion, loss of minerals and degradation of bonded interface by matrix-metalloproteinases [7].”
BackgroundBoutsiouki, C., Frankenberger, R., Lücker, S., & Krämer, N. (2023) · PubMed Central · doi:10.3290/j.jad.b3801065 · Cited by 6
Telles, C., Basting, R. T., Bridi, E. C., França, F., do Amaral, F., & Basting, R. T. (2023) · Journal of Clinical and Experimental Dentistry · doi:10.4317/jced.60307 · Cited by 6
“This will compromise the stability of the hybrid layer over time (13,14).”
BackgroundTunable polymer-peptide hybrids for dentin tissue repair
Toledano, M., Fernández-Romero, E., Aguilera, F. S., Osorio, E., Rodríguez-Santana, J. A., Garrido, M., Solís, P. A., García-Godoy, F., & Osorio, R. (2024) · Journal of Dentistry · doi:10.1016/j.jdent.2024.105027 · Cited by 6
“Consequently, this process facilitates further remineralization of dentin [48].”
Macedo, C. L. R., Münchow, E. A., Lima, G. D. S., Zanchi, C. H., Ogliari, F. A., & Piva, E. (2015) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2015.07.001 · Cited by 6
Moncada, G. A., Fonseca, R. G., de Oliveira, O. B., Eduardo Fernandez, G., Martin, J. J., & Vildósola, P. (2014) · Revista clínica de periodoncia implantología y rehabilitación oral · doi:10.1016/j.piro.2014.09.008 · Cited by 6
Biomaterials for catalysed mineralization of dental hard tissues
Osorio, R., & Toledano, M. (2016) · Elsevier eBooks · doi:10.1016/b978-1-78242-338-6.00013-2 · Cited by 6
Resin–Dentin Bonding Interface After Photochemical Surface Treatment
Tonami, K., Sano, K., Ichinose, S., & Araki, K. (2015) · Photomedicine and Laser Surgery · doi:10.1089/pho.2014.3813 · Cited by 6
Effect of Proteolytic Agents on Microleakage of Etch and Rinse Adhesive Systems
Kasraei, S., Yarmohammadi, E., Farhadian, M., & Malek, M. (2017) · Brazilian journal of oral sciences/Brazilian Journal of Oral Sciences · doi:10.20396/bjos.v16i0.8651051 · Cited by 6
Bridi, E. C., Leme-Kraus, A. A., Aydın, B., Basting, R. T., & Bedran‐Russo, A. K. (2018) · Archives of Oral Biology · doi:10.1016/j.archoralbio.2018.04.006 · Cited by 6
The durability of adhesion to Er,Cr:YSGG laser-irradiated enamel
Ayar, M. K. (2018) · LASER THERAPY · doi:10.5978/islsm.18-or-12 · Cited by 6
Gonapa, P., Sajjan, G. S., Bhupathi, A., Podugu, U. K., Sundar, S., Durgabhavani, G., & Rathod, R. T. (2022) · Contemporary Clinical Dentistry · doi:10.4103/ccd.ccd_321_21 · Cited by 6
“com the hybrid layer, which are susceptible to matrix metalloproteinase mediated collagenolytic activity[2,3] b.”
BackgroundWendlinger, M., Cochinski, G. D., Moreira, P. H. D. A., Cardenas, A. F. M., Siqueira, F., Stape, T. H. S., Tezvergil‐Mutluay, A., & Loguércio, A. D. (2025) · Dental Materials · doi:10.1016/j.dental.2025.05.002 · Cited by 5
Chen, Y., Yang, X., Zhang, S., Wang, H., Xie, H., & Chen, C. (2025) · Dental Materials · doi:10.1016/j.dental.2025.09.016 · Cited by 5
Yang, X., Chen, Y., Chen, Y., Xu, J., Yan, H., Luo, Q., Yao, W., & Li, X. (2025) · Dental Materials · doi:10.1016/j.dental.2025.12.009 · Cited by 5
Durability of bond strength to dentin using two universal adhesives in different etching modes
Salem, A., Nassif, M. S. A., & El-Korashy, D. I. (2021) · Brazilian journal of oral sciences/Brazilian Journal of Oral Sciences · doi:10.20396/bjos.v20i00.8660445 · Cited by 5
Bhandari, S., Kondody, R. T., Nair, A. S., Mathew, R. S., Divakar, K. P., & Nambiar, M. K. (2021) · Journal of Conservative Dentistry · doi:10.4103/jcd.jcd_474_21 · Cited by 5
Li, M., Qiu, Y., Wang, Y., Zhang, S., Duan, L., Zhao, W., Shi, Y., Zhang, Z., Tay, F. R., & Fu, B. (2023) · Dental Materials · doi:10.1016/j.dental.2023.11.020 · Cited by 6
Self-citationLi, S., Qi, L., & Liu, Z. (2024) · Frontiers in Materials · doi:10.3389/fmats.2024.1379941 · Cited by 5
Engineering Interfacial Integrity with Hydrolytic-Resistant, Self-Reinforcing Dentin Adhesive
Demirel, E., Korkmaz, B., Chang, Y., Misra, A. K., Tamerler, C., & Spencer, P. (2024) · International Journal of Molecular Sciences · doi:10.3390/ijms25137061 · Cited by 5
Effect of surface treatments and bonding type on elemental composition and bond strength of dentin
Demir, N., Subaşı, M. G., Yavuz, T., KARCI, M., Öztürk, A. N., & Kılıç, H. Ş. (2024) · Scientific Reports · doi:10.1038/s41598-024-75709-2 · Cited by 5
Revista Clínica de Periodoncia, Implantología y Rehabilitación Oral
de Investigación, T., Eduardo Fernandez, G., González, C., Arias, F., de Oliveira, O. B., Fresno, R. C., Casielles, J. M., & Pardo, C. L. (2016) · Cited by 3
Hupa, L., & Fagerlund, S. (2014) · The HKU Scholars Hub (University of Hong Kong) · doi:10.4032/9789814463133 · Cited by 5
Effects of simplified ethanol–wet bonding and hydrophobic coating on resin–dentin bonding properties
Wang, X., Li, H., Chen, L., Wang, Y., Bai, J., Wang, D., & Liu, H. S. (2020) · Journal of Adhesion Science and Technology · doi:10.1080/01694243.2020.1829321 · Cited by 5
“isfactory and poor durability of the bonding interface quality [1].”
BackgroundSharafeddin, F., & Moraveji, P. (2022) · PubMed Central · doi:10.30476/dentjods.2021.88737.1355 · Cited by 5
“Bromelain enzyme can eliminate organic component and collagen from the surface of the dentin and increase resin penetration into dentin structure, improve the hybrid layer, and decrease microleakage [20].”
Backgroundde Assis, H. C., Bertolini, G. R., Sousa‐Neto, M. D., & Lopes‐Olhê, F. C. (2023) · Journal of Biomedical Materials Research Part B Applied Biomaterials · doi:10.1002/jbm.b.35289 · Cited by 5
Application of modified aldehyde compounds in self-etching bonding of dentin
Chen, H., Hou, Y., Lin, Q., Yu, S., Bai, T., Cui, Z., & Zhu, S. (2023) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2023.106087 · Cited by 5
Nagpal, R., Tyagi, S., Manuja, N., & Sharma, P. (2015) · Journal of Conservative Dentistry · doi:10.4103/0972-0707.159751 · Cited by 5
“[19] To overcome this obstacle, clinically relevant simplified dehydration protocol with single-step 1 min application of 100% ethanol has been developed.”
The Effect of Viscosity and Application Mode of Phosphoric Acid on Bond Strength of GlassFiber Post
Scholz, M. F. C., de Almeida, R. A. M., Scholz, N., Gómes, O. M. M., Masson, M. J., Loguércio, A. D., Reis, A., & Bandéca, M. C. (2020) · Clinical Cosmetic and Investigational Dentistry · doi:10.2147/ccide.s230134 · Cited by 5
“In fact, it has previously been demonstrated that host-derived proteases play a role in the degradation of resin–dentin interfaces.(29) Therefore, it will be expected that a decrease in the bond strength values after long-term water storage when sonic application was applied associated with phosphoric acid.”
BackgroundThe effect of additional chlorhexidine and/or ethanol on the bond strength of universal adhesives
Kaynar, Z. B., Kazak, M., Dönmez, N., & Dalkılıç, E. E. (2020) · Journal of Adhesion Science and Technology · doi:10.1080/01694243.2020.1804723 · Cited by 5
Hosaka, K., Tichý, A., Araoka, D., Wurihan, W., Shibata, Y., Ikeda, M., Klein-Júnior, C. A., Tagami, J., & Nakajima, M. (2021) · PubMed · doi:10.3290/j.jad.b1999815 · Cited by 5
Trivedi, R., Gautam, D., Kehe, G. M., Escobedo, H. D., Patel, K. R., Stansbury, J. W., Schurr, M. J., & Nair, D. P. (2021) · European Journal Of Oral Sciences · doi:10.1111/eos.12832 · Cited by 4
Bond strength of composite resin to enamel: assessment of two ethanol wet-bonding techniques.
Khoroushi, M., Rafizadeh, M., & Samimi, P. (2014) · PubMed Central · Cited by 4
Keerthipriya, G., Ravikumar, N., & Mahalaxmi, S. (2021) · Applied Adhesion Science · doi:10.1186/s40563-021-00135-w · Cited by 5
Influence of chlorhexidine, propolis, pulpal pressure simulation, and aging on dentin bond strength
Perote, L. C. C. C., Barcellos, D. C., Matuda, A. G. N., Campos, R. P., Rosetti, E. P., & Pucci, C. R. (2022) · Microscopy Research and Technique · doi:10.1002/jemt.24150 · Cited by 4
Comba, A., Baldi, A., Pucci, R., Rolando, C., Alovisi, M., Pasqualini, D., & Scotti, N. (2024) · Journal of Clinical Medicine · doi:10.3390/jcm13092474 · Cited by 4
“Longer observation times are needed to validate these in vitro results and better clarify the role of extended etching time on radicular dentin adhesion.”
BackgroundRole of Metalloproteinases in Adhesion to Radicular Dentin: A Literature Review
Valdez-Montoya, M., Avendaño-Félix, M. M., Basurto-Flores, J. C., Ramírez-Álvarez, M., Cázarez-Camacho, M. D. R., Santana, M. Á. C., Zavala-Alonso, N. V., Sarmiento-Hernández, S. N., Silva-Benítez, E. D. L., & Soto-Sainz, J. E. (2024) · Materials · doi:10.3390/ma17225674 · Cited by 4
“…[80,115], showing a significant reduction after pulp tissue removal and canal filling with synthetic materials through endodontic therapy; in addition, in vitro, a low cytotoxicity reaction has been reported; although, so far no removal problems of the inhibitors have been reported [116–118].”
Shafıei, F., Memarpour, M., Vafamand, N., & Mohammadi, M. (2017) · Journal of Clinical and Experimental Dentistry · doi:10.4317/jced.53992 · Cited by 4
“A rapid degradation process might have occurred following rapid water diffusion through the small surface area of the adhesive interface (22).”
BackgroundEffect of carbodiimide on the bond strength and durability of resin-dentin interface
Paulose, N. E., & Fawzy, A. (2017) · Journal of Adhesion Science and Technology · doi:10.1080/01694243.2017.1393927 · Cited by 4
“Thus, the degradation of collagen fibrils and the resin can lead to destruction of the hybrid layer in the long term [9].”
BackgroundTawfic, H., Niazy, M. A., & El-Sharkawy, D. (2017) · Al-Azhar Dental Journal for Girls · doi:10.21608/adjg.2017.5269 · Cited by 4
Effect of duration of Er,Cr:YSGG laser etching on dentin morphology: an in vitro study
Mahdisiar, F., Mirzaei, A., Fallah, A., Gutknecht, N., & Akhoundan, S. (2018) · Lasers in Dental Science · doi:10.1007/s41547-018-0038-z · Cited by 4
“Otherwise, cysteine cathepsins, which can be activated in mildly acidic environments, may also activate matrix-bound matrix metalloproteinases and destabilize the hybrid layer in long term [10, 11].”
BackgroundKasraei, S., Mojtahedi, M., Goodarzi, M. T., Azarsina, M., & Khamverdi, Z. (2019) · Dental and Medical Problems · doi:10.17219/dmp/105408 · Cited by 4
Nanoindentation Mapping and Bond Strength Study of Adhesive–Dentin Interfaces
Yao, C., Wang, Z., Yu, J. L., Liu, P., Wang, Y., Ahmed, M. H., MEERBEEK, B. V., & Huang, C. (2022) · Advanced Materials Interfaces · doi:10.1002/admi.202101327 · Cited by 4
Budnicka, M., Sobiech, M., Sieczko, K., & Luliński, P. (2024) · Macromolecules · doi:10.1021/acs.macromol.4c00695 · Cited by 4
Alhamdan, M. M., Knowles, J. C., & McDonald, A. V. (2018) · The International Journal of Prosthodontics · doi:10.11607/ijp.6044 · Cited by 4
Donovan, T. E., Anderson, M., Becker, W., Cagna, D. R., Hilton, T. J., McKee, J. R., & Metz, J. E. (2012) · Journal of Prosthetic Dentistry · doi:10.1016/s0022-3913(12)60104-8 · Cited by 6
Ngai, K. (2020) · TSpace (University of Toronto) · Cited by 5
Fahmy, S., Fahmy, O., El‐Korashy, S. A., & Labib, M. E. M. (2025) · Dental and Medical Problems · doi:10.17219/dmp/183841 · Cited by 3
Quero, I. B., Dias, P. C., Paula‐Silva, F. W. G., Magalhães, N. L., Faraoni, J. J., & Palma‐Dibb, R. G. (2025) · Dental Materials · doi:10.1016/j.dental.2025.08.006 · Cited by 3
Daood, U., Daood, S. A., Liit, N. M., Zain, E., Seow, L. L., Matinlinna, J. P., Sauro, S., Peters, O. A., Tezvergil‐Mutluay, A., Yiu, C. K. Y., et al. (2025) · Journal of Dentistry · doi:10.1016/j.jdent.2025.106198 · Cited by 3
Redistribution Effect of Demineralized Dentin on Hydrophobic Monomers
Xu, J., Lei, Y., Pan, M., Li, Z., Lao, W., Luo, Q., & Li, X. (2026) · Journal of Dental Research · doi:10.1177/00220345251408838 · Cited by 3
“Insufficient infiltration of BisGMA-based adhesives into 3-dimensional (3D) porous demineralized dentin matrix (DDM; Nakabayashi et al 1982) creates structurally defective hybrid layers (Spencer and Swafford 1999; Pashley et al 2004; Breschi et al 2008; Liu et al 2011).”
Ismail, O., Hassanein, O. E., Hafez, R. M., & Mamdouh, M. (2024) · Journal of international oral health · doi:10.4103/jioh.jioh_11_24 · Cited by 3
Effect of solvent pretreatments on intraradicular bond strength of bioactive cements
Salim, I. A., Al-Ani, A. A. S. S., Stape, T. H. S., Mutluay, M. M., & Tezvergil‐Mutluay, A. (2025) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2025.103952 · Cited by 3
Chaves, L. V. D. F., Chaves, V. S. D. F., Felix, M. D. D. S., Borges, B. C. D., da Costa, G. D. F. A., & Geraldeli, S. (2016) · Journal of Adhesion Science and Technology · doi:10.1080/01694243.2016.1174521 · Cited by 3
“Bond degradation occurs via hydrolysis of suboptimally polymerized hydrophilic resin components and degradation of water-rich, resin-sparse collagen matrices by matrix metalloproteinases and cysteine cathepsins.[12] The use of NaOCl storage to degrade dentin interfaces was previously proposed in an attempt to perform…”
BackgroundCaries-resistant bonding layer in dentin
Zhou, W., Niu, L., Hu, L., Jiao, K., Chang, G., Shen, L.-J., Tay, F. R., & Chen, J. (2016) · Scientific Reports · doi:10.1038/srep32740 · Cited by 3
Self-citationAkram, Z., Aati, S. Y., Shrestha, B., Clode, P. L., Saunders, M., Ngo, H. C., & Fawzy, A. (2021) · Biomaterials Science · doi:10.1039/d1bm01408k · Cited by 3
Nathan, S., Reddy, B. N., Subramani, S. K., Govindarajan, J., Hemasathya, B. A., & Sankar, S. (2023) · The Journal of Contemporary Dental Practice · doi:10.5005/jp-journals-10024-3439 · Cited by 3
Effect of limonene associated with bioactive glass‐ceramic on dentin/adhesive interface
Pinto, A. H. G., Vivanco, R. G., & Pires‐de‐Souza, F. D. C. P. (2023) · European Journal Of Oral Sciences · doi:10.1111/eos.12947 · Cited by 3
Lobão, S. R. C., Nonato, R. D. F., Moreira, P. H. D. A., Mendonça, A. M. S., Trovão, M. M. A., Wendlinger, M., Oliveira, B. E. C., da Silva, L. C. N., Gonçalves, L. M., Cardenas, A. F. M., et al. (2024) · PubMed Central · doi:10.3290/j.jad.b5199073 · Cited by 3
Metadata
- Authors
- Liu, Y., Tjäderhane, L., Breschi, L., Mazzoni, A., Li, N., Mao, J., Pashley, D. H., & Tay, F. R.
- Affiliations
- Tongji Hospital (CN)
- Oulu University Hospital (FI)
- University of Trieste (IT)
- University of Bologna (IT)
- Fujian University of Traditional Chinese Medicine (CN)
- Department of Oral Biology
- Augusta University (US)
- Corresponding author
- Mao, J.
- Tay, F.R.
- Venue
- Journal of Dental Research
- Publisher
- SAGE Publications
- Published
- 2011-01-10
- Volume
- 90
- Issue
- 8
- Pages
- 953-968
- ISSN
- 0022-0345 (ISSN-L)
- 1544-0591
- PMC
- PMC3148178
- OpenAlex
- W2135724989
- Semantic Scholar
- fe5dcc58cb3bed23576b1db47776e8d76d4cd6a2
- Cited by
- 665
- References
- 176
- Citations by year
- 2026: 23 · 2025: 25 · 2024: 24 · 2023: 35 · 2022: 47 · 2021: 54 · 2020: 56 · 2019: 55 · 2018: 54 · 2017: 57 · 2016: 59 · 2015: 58 · 2014: 40 · 2013: 43 · 2012: 26
- FWCI
- 6.61
- Type
- journal article
- Language
- en
- Open access
- green
- www.ncbi.nlm.nih.gov
- Licence
- journals.sagepub.com/page/policies/text-and-data-mining-license (tdm)
- Locations
- Journal of Dental Research (publishedVersion)
- PubMed Central (publishedVersion)
- PubMed (publishedVersion)
- ArTS Archivio della ricerca di Trieste (University of Trieste https://www.units.it/) (submittedVersion)
- Archivio istituzionale della ricerca (Alma Mater Studiorum Università di Bologna) (submittedVersion)
- Funders
- National Institute of Dental and Craniofacial Research (R21DE019213, R01DE015306)
- Topics
- Health Sciences › Dentistry › General Dentistry › Dental materials and restorations
- Health Sciences › Dentistry › Oral Surgery › Endodontics and Root Canal Treatments
- Physical Sciences › Materials Science › General Materials Science › Material Properties and Applications
- Keywords
- dentin bonding, bond degradation, matrix metalloproteinases, cathepsins, collagenolytic enzymes, degree of conversion, collagenase inhibitors, crosslinking agents, ethanol-wet bonding, hydrophobic resin, biomimetic remineralization, collagen matrix, tooth-colored restorations
- MeSH terms
- Dental Bonding, Cathepsins, Collagen, Composite Resins, Cross-Linking Reagents, Dentin, Esterases, Humans, Hydrolysis, Tooth Remineralization, Dentin-Bonding Agents, Resin Cements, Hydrophobic and Hydrophilic Interactions, Polymerization, Matrix Metalloproteinase Inhibitors
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.