Joining of engineering ceramics
The DOI matches its Crossref record; 324 of the 328 references it cites were found in a registry or an index.
Abstract
Engineering ceramics such as alumina, zirconia, silicon nitride and silicon carbide can now be manufactured reliably with reproducible properties. As such, they are of increasing interest to industry, particularly for use in demanding environments, where their thermomechanical performance is of critical importance, with applications ranging from fuel cells to cutting tools. One aspect common to virtually all applications of engineering ceramics is that eventually they must be joined with another material, most usually a metal. The joining of engineering ceramics to metals is not always easy. There are two main considerations. The first consideration is the basic difference in atomic bonding: the ionic or covalent bonding of the ceramic, compared to the metallic bond. The second consideration is the mismatch in the coefficient of thermal expansion. In general, ceramics have a lower coefficient of thermal expansion than metals and, if high tensile forces are produced in the ceramic, either as a consequence of operating conditions or from the joining procedure itself, failure can occur. The plethora of joining processes available will be reviewed in this article, placing them in context from both an academic and commercial perspective. Comment will be made on research reporting advances on known technology, as well as introducing ‘newer’ technologies developed over the last 10 years. Finally, reviews and commentary will be made on the potential applications of the various joining processes in the commercial environment.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Ceramic joining techniques are numerous and technically challenging, and often subject the entire sample to extreme conditions, such as high temperatures and/or vacuums [223].”
From Ultrafast Laser Additive Manufacturing: A Review (2023) · cites this paper as [223]
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Structural Inorganic Chemistry
(1971) · Nature · doi:10.1038/229453c0 · Cited by 5,766
The Superalloys: Fundamentals and Applications
Reed, R. C. (2008) · Cited by 3,725
The Superalloys: Fundamentals and Applications
Reed, R. C. (2006) · Cambridge University Press eBooks · doi:10.1017/cbo9780511541285 · Cited by 2,369
Transformation Toughening in Zirconia‐Containing Ceramics
Hannink, R. H. J., Kelly, P., & Muddle, B. C. (2000) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2000.tb01221.x · Cited by 2,268
Silicon Nitride and Related Materials
Riley, F. L. (2000) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2000.tb01182.x · Cited by 1,566
CRC Materials Science and Engineering Handbook
Shackelford, J. F., Han, Y.-H., Kim, S., & Kwon, S.-H. (2016) · CRC Press eBooks · doi:10.1201/b18971 · Cited by 1,274
Wettability at High Temperatures
(1999) · Pergamon materials series · doi:10.1016/s1470-1804(99)x8001-1 · Cited by 1,042
Current ceramic materials and systems with clinical recommendations: A systematic review
Conrad, H. J., Seong, W.-J., & Pesun, I. J. (2007) · The Journal of Prosthetic Dentistry · doi:10.1016/s0022-3913(07)60124-3 · Cited by 981
The application of the specular reflection of neutrons to the study of surfaces and interfaces
Penfold, J., & Thomas, R. K. (1990) · Journal of Physics Condensed Matter · doi:10.1088/0953-8984/2/6/001 · Cited by 742
Handbook of Ceramic Composites
Bansal, N. P. (2005) · Springer eBooks · doi:10.1007/b104068 · Cited by 654
Research works printed but not linked: 31
- M. F. Ashby: ‘Cambridge engineering selector v4’; 2007, Cambridge, Granta Design Limited.
- Fernie J. A., 1999, Ind Ceram, 19, 172
- Imai H., 2006, JSME Int. J. Ser. A, 49, 450
- Lindner P., 2004, Solid State Technol, 47, 55
- Ito M., 1991, US Patent 5073085
- Duvall D. S., 1974, Weld, 1, 203
- 10.1016/j.ijrmhm.2004.01.003 · doi:10.1016/j.ijrmhm.2004.01.003
- Fernie J. A., 1999, Mater. World, 7, 686
- Loehman R. E., 1989, Am. Ceram. Soc. Bull, 68, 891
- Eustathopoulos N., 1998, Acta Mater, 46, 2319
- Sobczak N., 2005, Curr. Opin. Solid State Mater. Set, 9, 241 — 253
- Derby B., 2004, Interf Set, 12, 29
- Ormston D. R., 2001, ‘The particulate reinforcement of active broze alloys for joining silicon carbide’, Cambridge
- Knowles K. M., 2002, Ceram. Trans, 138, 103
- Nolte H. J., 1954, US Patent 2667432
- Kim J. Y., 2005, J. Electrochem. Soc, 152, J52—J58
- Paulasto M., 1997, Ceram. Trans, 77, 91
- Peteves S. D., 1998, Acta. Mater, 46, 2407
- Reichel U., 1999, Z. Metallkd, 90, 699
- Gasse A., 1997, World Patent WO 9747568
- Chaumat G., 2001, European Patent EP 806402
- Gasse A., 2008, US Patent 7318547
- Pask J. A., 1971, Proc. Porcelain Enamel Inst. Tech. Forum, 33, 1
- Pask J. A., 1987, Am. Ceram. Soc. Bull, 66, 1587
- Ghosh S., 2008, J. Electrochem. Soc, 155, B473—B478
- Kobsiriphat W., 2008, J. Fuel Cell Set Technot, 011002
- Henager C. H., J. Nucl. Mater, 2007, 367
- Appendino P., 1563, J. Nucl. Mater, 2004, 329
- Barabash V., J. Nucl. Mater, 2000, 283
- Ferraris M., 1546, J. Nucl. Mater, 1998, 258
- Suryanarayana C., 2001, Adv. Mater. Processes, 159, 29
Cited by
Items 101–200 of 302
Sun, L., Fang, J., Guo, S., Wen, Y., Liu, C., & Zhang, J. (2021) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2021.09.050 · Cited by 22
Mechanical behavior of reactive air brazed (RAB) Crofer 22 APU-Al2O3 joints at ambient temperature
Tillmann, W., Anar, N. B., & Wojarski, L. (2020) · SN Applied Sciences · doi:10.1007/s42452-020-2622-6 · Cited by 22
Glasses and glass-ceramics as brazing materials for high-temperature applications
Salvo, M., Casalegno, V., Rizzo, S., Smeacetto, F., Ventrella, A., & Ferraris, M. (2013) · Elsevier eBooks · doi:10.1533/9780857096500.3.525 · Cited by 22
Niu, W., Chen, Q., Lin, P., Cui, J., Lin, T., Guo, W., He, P., Ai, C., Zhuang, Y., Chen, L., et al. (2019) · Ceramics International · doi:10.1016/j.ceramint.2019.10.277 · Cited by 22
A comprehensive review on sustainability evaluation of joining methods for engineering materials
Ravichandran, B., & Balasubramanian, M. (2025) · Materials Today Sustainability · doi:10.1016/j.mtsust.2025.101151 · Cited by 21
Advances in reactive air wetting and brazing of engineering ceramics
Zhang, M., Xu, S., Valenza, F., Zhang, X., Liu, G., & Qiao, G. (2024) · Journal of Advanced Ceramics · doi:10.26599/jac.2024.9220997 · Cited by 21
Hadji, Y., Haddad, A., Yahi, M., Benamar, M. E. A., Miroud, D., Sahraoui, T., Hadji, M., & Barsoum, M. W. (2015) · Ceramics International · doi:10.1016/j.ceramint.2015.09.026 · Cited by 21
Luo, D., Xiao, Y., Wang, L., Liu, L., Zeng, X., & Li, M. (2017) · Ceramics International · doi:10.1016/j.ceramint.2017.03.042 · Cited by 21
Zheng, K., Zhang, Q., Wang, J., & Lu, Y. (2020) · Ceramics International · doi:10.1016/j.ceramint.2020.09.129 · Cited by 21
Brazing vs. diffusion welding of graded Fe based matrix composite and yttria stabilized zirconia
Avettand-Fènoël, M.-N., Naji, K., & Pouligny, P. (2019) · Journal of Manufacturing Processes · doi:10.1016/j.jmapro.2019.07.040 · Cited by 21
Wang, M., Hu, X., Xu, X., Yun, Z., Liu, J., Du, H., & Guo, A. (2015) · Materials & Design · doi:10.1016/j.matdes.2015.07.178 · Cited by 21
Copper bonding silicon nitride substrate using atmosphere plasma spray
Liu, G., Wang, D., Xing, Y., Zhong, X., & Pan, W. (2023) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2023.03.009 · Cited by 20
The orientation and morphology of platinum precipitates in sapphire
Santala, M. K., Radmilovic, V. R., Giulian, R., Ridgway, M. C., Gronsky, R., & Glaeser, A. M. (2011) · Acta Materialia · doi:10.1016/j.actamat.2011.04.012 · Cited by 20
Wang, C., Ding, J., Huang, Z., Zhuang, Y., Li, Y., Shi, M., & Qin, Y. F. (2022) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2022.09.034 · Cited by 20
He, Y., Sun, Y., Zhang, J., & Li, X. (2012) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2012.04.004 · Cited by 20
He, Y., Zhang, J., Lv, P., & Liu, C. (2014) · Vacuum · doi:10.1016/j.vacuum.2014.06.027 · Cited by 20
Brazing SiO2-BN diphase ceramic with Nb by using multilayer Ti-Ni composite foils
Yang, J. H., Zhang, L. X., Sun, Z., & Feng, J. C. (2017) · Vacuum · doi:10.1016/j.vacuum.2017.09.022 · Cited by 20
Interfacial microstructures formation mechanism between SiO2 substrate and AgCuTi braze alloys
Xin, C., Li, N., Jia, J., Jinsong, D., & Yan, J. (2018) · Ceramics International · doi:10.1016/j.ceramint.2018.06.246 · Cited by 20
Tunçkan, O., Yurdakul, H., & Turan, S. (2019) · Journal of Advanced Ceramics · doi:10.1007/s40145-019-0330-8 · Cited by 19
Tunçkan, O., Yurdakul, H., & Turan, S. (2012) · Ceramics International · doi:10.1016/j.ceramint.2012.07.031 · Cited by 19
Zhou, Q., Bieler, T. R., & Nicholas, J. D. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.0911910jes · Cited by 19
Sung, H.-W., Kim, Y.-H., & Kim, D. J. (2020) · Ceramics International · doi:10.1016/j.ceramint.2020.08.043 · Cited by 18
Artini, C., Muolo, M. L., Passerone, A., Cacciamani, G., & Valenza, F. (2013) · Journal of Materials Science · doi:10.1007/s10853-013-7290-0 · Cited by 18
Functionally Graded Ceramic Based Materials Using Additive Manufacturing: Review and Progress
Yang, L., Miyanaji, H., Ram, D. J., Zandinejad, A. A., & Zhang, S. (2016) · Ceramic transactions /Ceramic transactions · doi:10.1002/9781119236016.ch5 · Cited by 18
Ultrafast air bonding between SiC ceramic and SnAgTi alloy under the action of ultrasounds
Wu, B., Leng, X., Xiu, Z., & Yan, J. (2018) · Scientific Reports · doi:10.1038/s41598-018-34635-w · Cited by 18
Lin, Y., Qi, X., Niu, G., Sun, Q., Ji, H., Li, M., & Li, Y. (2023) · Journal of Materials Science · doi:10.1007/s10853-023-08604-2 · Cited by 17
Wettability and joining of reaction-bonded silicon carbide (RBSC) by Ti–Si eutectic alloy
Zhao, Z., Liu, Y., Zhou, B., Zhang, H., Liu, X., & Huang, Z. (2024) · Ceramics International · doi:10.1016/j.ceramint.2024.03.227 · Cited by 17
Kassam, T. A., Babu, N. H., Ludford, N., Yan, S., & Howkins, A. (2018) · Scientific Reports · doi:10.1038/s41598-018-20674-w · Cited by 17
Erskine, K. M., Meier, A. M., Joshi, V. V., & Pilgrim, S. M. (2014) · Advanced Engineering Materials · doi:10.1002/adem.201400128 · Cited by 17
Joining Alumina to Titanium Alloys Using Ag-Cu Sputter-Coated Ti Brazing Filler
Emadinia, O., Guedes, A., Tavares, C. J., & Simões, S. (2020) · Materials · doi:10.3390/ma13214802 · Cited by 16
Ultrasonic-based surface patterning and interfacial reaction of ZrO2 ceramics
Dong, H., Li, Z., Song, X., Feng, J., Wei, S., Fu, J. H., & Shi, Y. (2023) · Journal of Material Science and Technology · doi:10.1016/j.jmst.2022.11.067 · Cited by 15
Liu, G., Zhong, X., Xing, Y., Li, T., & Pan, W. (2020) · Journal of the American Ceramic Society · doi:10.1111/jace.17522 · Cited by 15
Compound connection mechanism of Al2O3 ceramic and TC4 Ti alloy with different joining modes
Zhang, Y., Chen, Y., Zhou, J., Sun, D., & Li, H. (2021) · Scientific Reports · doi:10.1038/s41598-021-00815-4 · Cited by 15
A heat-resistant organic adhesive for joining Al2O3 ceramics in air and argon atmospheres
Wang, X., Wang, J., & Wang, H. (2017) · Journal of Manufacturing Processes · doi:10.1016/j.jmapro.2017.01.014 · Cited by 15
The application of Lu-Al-Si-O-N oxynitride glass in transparent AlON ceramics joining
Liang, H., Guo, H., Yin, J., Zuo, K., Xia, Y., Yao, D., Zhang, J., Zeng, Y., & Wang, S. (2018) · Ceramics International · doi:10.1016/j.ceramint.2018.10.193 · Cited by 15
Deng, N., Zhao, J., Yang, L., & Zheng, Z. (2021) · Frontiers in Materials · doi:10.3389/fmats.2020.580938 · Cited by 15
Habibi, F., Samadi, A., & Nouri, M. (2025) · International Journal of Refractory Metals and Hard Materials · doi:10.1016/j.ijrmhm.2025.107359 · Cited by 14
Flash joining of Y2O3 transparent ceramic to titanium alloy
Zhang, K., Li, T., Zhao, Z., Huang, Z., & Liu, Y. (2023) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2023.08.054 · Cited by 14
Sun, Y., Zhang, J., Zhang, H., Fan, G., & He, Y. (2011) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2011.05.101 · Cited by 14
Microwave-assisted brazing of alumina ceramics for electron tube applications
Shukla, M., Ghosh, S., Dandapat, N., Mandal, A. K., & Balla, V. K. (2016) · Bulletin of Materials Science · doi:10.1007/s12034-016-1167-1 · Cited by 14
Wang, X., Wang, J., & Wang, H. (2018) · The Journal of Adhesion · doi:10.1080/00218464.2017.1396897 · Cited by 14
Investigation on brazing of zirconia ceramic with Bi2O3-B2O3-Al2O3 glass
Guo, W., Gao, L., An, B., Hao, D., Xiong, J., & Li, J. (2022) · Materials Characterization · doi:10.1016/j.matchar.2022.112604 · Cited by 13
Evolution of the interfacial phases in Al2O3–Kovar® joints brazed using a Ag–Cu–Ti-based alloy
Ali, M., Knowles, K. M., Mallinson, P. M., & Fernie, J. A. (2017) · The Philosophical Magazine A Journal of Theoretical Experimental and Applied Physics · doi:10.1080/14786435.2016.1275868 · Cited by 13
Self-citationMicrostructure and mechanical properties of MoSi2–MoSi2 joints brazed by Ag–Cu–Zr interlayer
Ramsheh, H. H., Sani, M. A. F., & Kokabi, A. H. (2013) · Materials & Design (1980-2015) · doi:10.1016/j.matdes.2013.01.027 · Cited by 13
Sinnamon, K. E., Meier, A. M., & Joshi, V. V. (2014) · Advanced Engineering Materials · doi:10.1002/adem.201400104 · Cited by 13
Joining of ceramic to metal by friction welding process: A review
Ahmed, S. A., Hasanabadi, M. F., & Kumar, A. V. (2021) · Proceedings of the Institution of Mechanical Engineers Part L Journal of Materials Design and Applications · doi:10.1177/14644207211001080 · Cited by 13
Field-assisted sintering: Overview of thermo-electro-mechanical coupling effects
Liu, D., Shao, G., Tai, X., Li, X., Jeon, S.-C., Guo, J., Lin, M., Ji, W., Xiong, Y., Chen, S., et al. (2026) · Journal of Advanced Ceramics · doi:10.26599/jac.2026.9221276 · Cited by 12
Joining of alumina using magnesium- or calcium-aluminosilicate glass–ceramic fillers
Salman, M., Bae, H.-M., & Yoon, D. (2022) · Ceramics International · doi:10.1016/j.ceramint.2022.04.122 · Cited by 12
Ji, F., Li, Y., Dong, W., & Chen, H. (2024) · Optics & Laser Technology · doi:10.1016/j.optlastec.2024.111377 · Cited by 12
Prevost, E., DeMarco, A. J., MacMichael, B., Joshi, V. V., Meier, A. M., Hoffman, J. W., & Walker, W. J. J. (2014) · Advanced Engineering Materials · doi:10.1002/adem.201400140 · Cited by 12
Properties of −O–Cu–O– Bridged Copper Phosphate-Based Thermal Insulation Materials
Zhan, Z., Sun, W., Zhang, Z., Xiong, X., Xu, Y., Zeng, Y., & Yin, J. (2019) · ACS Omega · doi:10.1021/acsomega.9b02914 · Cited by 12
Surface synthesis of aluminum borate whiskers on the ZTA ceramics and its application to joining
Cao, J. H., Yang, B., Li, C., Si, X., Wang, Z., Lin, T., Su, S., Qi, J., & Feng, J. (2020) · Ceramics International · doi:10.1016/j.ceramint.2020.12.252 · Cited by 12
Active Brazing for Energy Devices Sealing
Feng, J. X., Herrmann, M., Reinecke, A.-M., & Hurtado, A. (2024) · Journal of Experimental and Theoretical Analyses · doi:10.3390/jeta2010001 · Cited by 11
Singh, M., Martínez-Fernández, J., Asthana, R., Ramirez‐Rico, J., & Valera-Feria, F. M. (2022) · International Journal of Applied Ceramic Technology · doi:10.1111/ijac.14266 · Cited by 11
Liu, Y., Zhang, K., Tianyu, L. I., Zhou, B., Xuejian, L. I. U., & HUANG, Z. (2022) · Journal of Inorganic Materials · doi:10.15541/jim20220400 · Cited by 11
Pietrzak, K., Olesińska, W., Kaliński, D., & Strojny‐Nędza, A. (2014) · Bulletin of the Polish Academy of Sciences Technical Sciences · doi:10.2478/bpasts-2014-0003 · Cited by 11
Zu, Y., Wang, K., Lv, S., Chen, G., Fu, X., & Zhou, W. (2020) · Materials Science and Engineering A · doi:10.1016/j.msea.2020.139121 · Cited by 11
Advances in Transient-Liquid-Phase Bonding of Ultra-high Temperature ZrC Ceramics
Sciti, D., Silvestroni, L., Esposito, L., Nakashima, K., Saito, N., Yamaoka, Y., & Glaeser, A. M. (2012) · High Temperature Materials and Processes · doi:10.1515/htmp-2012-0087 · Cited by 11
Aguilar-Elguezabal, A., Reyes-Rojas, A., Esparza-Ponce, H. E., Lardizábal‐Gutiérrez, D., & Bocanegra-Bernal, M. H. (2026) · Ceramics · doi:10.3390/ceramics9040039 · Cited by 10
Liu, J., Ji, X., Hu, Z., Wang, Y., Li, J., Qi, C., Gao, Z., Wan, Y., Xiao, B., & Wang, M. (2025) · Ceramics International · doi:10.1016/j.ceramint.2025.04.105 · Cited by 10
Park, S., Joo, S., Song, J. S., Eom, J., Cheong, H. N., & Yoon, D. (2025) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2025.117269 · Cited by 10
Zhao, Z., Liu, Y., Zhou, B., Zhang, K., Liu, X., & Huang, Z. (2024) · Ceramics International · doi:10.1016/j.ceramint.2024.08.423 · Cited by 10
In situ TiB-network-reinforced Al2O3/Ti6Al4V joints
Weiqi, Y., Xunuo, Y., Wei, D., Liutong, C., Lin, J., Ao, R., Xianfeng, M., & Lili, X. (2019) · Ceramics International · doi:10.1016/j.ceramint.2019.05.264 · Cited by 10
Zhang, S. S., Sun, W., Zhan, Z., Zhang, H. B., & Xiong, X. (2022) · ACS Omega · doi:10.1021/acsomega.1c05818 · Cited by 10
Shim, G. H., Kweon, B., Ji, M. K., Jun, T., & Ahn, H. S. (2022) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2022.103152 · Cited by 10
High Temperature Solid-Liquid Interactions in Metal-Ceramic Brazing: A Critical Review
Passerone, A., Valenza, F., & Muolo, M. L. (2017) · Materials science forum · doi:10.4028/www.scientific.net/msf.884.132 · Cited by 10
Microstructure and strength of high nitrogen steel joints brazed with Ni-Cr-B-Si filler
Zhu, W., Jiang, H., Zhang, H., Sun, S., & Liu, Y. (2018) · Materials Science and Technology · doi:10.1080/02670836.2017.1412040 · Cited by 10
The role of interlayers in the flash joining of Y2O3 transparent ceramic to titanium alloy
Zhang, K., Li, T., Wang, Z., Zhang, H., Liu, X., Huang, Z., & Liu, Y. (2024) · Ceramics International · doi:10.1016/j.ceramint.2024.02.373 · Cited by 9
Liu, D., Yin, Z., Guo, F., Li, X., & Yuan, J. (2023) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2023.07.041 · Cited by 9
Wang, Z., Li, C., Si, X., Zheng, M., Chen, L., Huang, Y., Qi, J., & Cao, J. (2021) · International Journal of Applied Ceramic Technology · doi:10.1111/ijac.13924 · Cited by 9
Zhang, B., Zhang, L., Sun, Z., Chang, Q., & Feng, J. (2022) · Corrosion Science · doi:10.1016/j.corsci.2022.110094 · Cited by 9
Corrosion of laser joined silicon carbide in gasification environment
Schaafhausen, S., Börner, F., Chand, T., Lippmann, W., Hurtado, A., & Müller, M. (2015) · Advances in Applied Ceramics Structural Functional and Bioceramics · doi:10.1179/1743676115y.0000000014 · Cited by 9
Siddiqui, M. S., & Jones, W. K. (2014) · International Journal of Materials Science and Engineering · doi:10.12720/ijmse.2.1.56-62 · Cited by 9
Surface Metallization of SiC Ceramic by Mo-Ni-Si Coatings for Improving Its Wettability by Molten Ag
Santuan, Z., Xiangzhao, Z., Guiwu, L., Valenza, F., MariaLuigia, M., Guanjun, Q., & Passerone, A. (2018) · 稀有金属材料与工程 · doi:10.1016/s1875-5372(18)30105-x · Cited by 9
The connection and repair of Ni-based superalloys by a simple heat-resistant adhesion technique
Wang, M., Dong, X. H., Li, Z., Lu, R., Liu, J., Guo, A., Wei, T., & Du, M. (2019) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2019.03.298 · Cited by 9
Xu, R., Chong, X., Zhou, Y., Jiang, Y., & Feng, J. (2019) · Materials Research Express · doi:10.1088/2053-1591/ab38f8 · Cited by 9
Кулик, В. И., Нилов, А. С., Bogachev, E. A., & Ларионов, Н. В. (2021) · Refractories and Industrial Ceramics · doi:10.1007/s11148-021-00586-5 · Cited by 9
Камынина, О. К., Вадченко, С. Г., Shkodich, N. F., & Ковалев, И. Д. (2021) · Metals · doi:10.3390/met12010038 · Cited by 9
From Processing to Performance: Innovations and Challenges in Ceramic-Based Materials
Sharma, S. K., Gajević, S., Sharma, L. K., Sharma, Y., Sharma, M., Milojević, S., Savić, S. R., & Stojаnović, B. (2026) · Crystals · doi:10.3390/cryst16020085 · Cited by 8
Dong, H., Wei, S., Li, Z., Song, X., He, W. X., & Feng, J. (2022) · Surfaces and Interfaces · doi:10.1016/j.surfin.2022.102491 · Cited by 8
Pressure-less sintering of molybdenum-reinforced ceramic cutting inserts with improved tool life
Ghosh, K., Goswami, S., Prajapati, P. K., Roy, P., & Mandal, N. (2024) · International Journal of Refractory Metals and Hard Materials · doi:10.1016/j.ijrmhm.2024.106619 · Cited by 8
Joining of SiC ceramics by iridium: The interfacial phenomena and joint strength
Golosov, M. A., Utkin, A. V., Lozanov, V. V., & Baklanova, N. I. (2024) · Ceramics International · doi:10.1016/j.ceramint.2024.10.061 · Cited by 8
Mechanism of Incongruent Reactions Between Zr-Cu Melts and Solid Tungsten Carbide
Wang, D., & Wang, Y. (2020) · Metallurgical and Materials Transactions B · doi:10.1007/s11663-020-01846-4 · Cited by 8
Theoretical Investigations on Interfacial Behavior of Ag–Cu–Ti/Si3N4 Wetting System
Gui, X., Zhang, M., Zhang, X., Guo, Q., Hussain, S., Qiao, G., & Liu, G. (2021) · Journal of Nanoelectronics and Optoelectronics · doi:10.1166/jno.2021.3111 · Cited by 8
In-situ scanning transmission electron microscopy study of Al-amorphous SiO2 layer-SiC interface
Adabifiroozjaei, E., Rastkerdar, E., NEMOTO, Y., Nakayama, Y., Nishimiya, Y., Fronzi, M., Yao, Y., Nguyen, M. T., Molina‐Luna, L., & Suzuki, T. (2023) · Journal of Materials Science · doi:10.1007/s10853-023-08186-z · Cited by 8
Oscillatory pressure-assisted plastic joining of zirconia ceramics with excellent flexural strength
Fan, J., Ren, K., Xia, J., Zhao, K., Liu, J., Zhao, X., Zhang, B., & Liu, D. (2024) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2024.116668 · Cited by 8
Joining technologies for a temperature-stable integration of a LTCC-based pressure sensor
Schilm, J., Goldberg, A., Partsch, U., Dürfeld, W., Arndt, D., Pönicke, A., & Michaelis, A. (2016) · Journal of sensors and sensor systems · doi:10.5194/jsss-5-73-2016 · Cited by 8
Tillmann, W., Anar, N. B., Wojarski, L., & Lassner, J. J. (2020) · Metallography Microstructure and Analysis · doi:10.1007/s13632-020-00663-0 · Cited by 8
Bending strength of ceramic compounds bonded with silicate-based glass solder
Saß, J., Jakobi, A., Mitrovic, A., Ganz, C., Wilken, J., Burmeister, U., Lang, H., Bader, R., & Vogel, D. (2021) · Materials Testing · doi:10.1515/mt-2020-0098 · Cited by 8
Yan, J., Ma, L., & Wang, J. (2023) · Mechanics of Materials · doi:10.1016/j.mechmat.2023.104660 · Cited by 8
Yang, Z., Zhang, L. X., Ren, W., Xue, Q., He, P., & Feng, J. C. (2012) · Materials Science and Engineering A · doi:10.1016/j.msea.2012.10.042 · Cited by 8
Heo, H., Kim, G., Park, Y.-C., Jung, K., & Kang, C.-Y. (2018) · Metals · doi:10.3390/met8100752 · Cited by 8
Lan, L. Y., Ren, Z., Yu, J., Li, C., & Zhong, Y. (2016) · Journal of Adhesion Science and Technology · doi:10.1080/01694243.2016.1146393 · Cited by 8
Ren, M., You, X., Luo, H., Chen, X., Liao, C., Yang, J., Zhang, X., & Dong, S. (2025) · Ceramics International · doi:10.1016/j.ceramint.2025.04.135 · Cited by 7
Laser welding-brazing of alumina to 304 stainless steel with an Ag-based filler material
Zhang, Y., Chen, Y., Zhou, J., Sun, D., & Li, H. (2020) · Metallurgical Research & Technology · doi:10.1051/metal/2020086 · Cited by 7
Wang, Q., Wang, Q., Wei, Y., Chen, J., Cui, T., Yan, H., Duan, J., Li, K., & Ding, J. (2024) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2024.116925 · Cited by 7
Ali, M., Knowles, K. M., Mallinson, P. M., & Fernie, J. A. (2017) · The Philosophical Magazine A Journal of Theoretical Experimental and Applied Physics · doi:10.1080/14786435.2017.1400702 · Cited by 7
Self-citationJoining of Al2O3 ceramics via preceramic polymer and inorganic additives
Wang, X., Wang, J., & Wang, H. (2013) · Materials Science and Engineering A · doi:10.1016/j.msea.2013.03.060 · Cited by 7
Additive plasma metallization of spatial ceramic injection molded components
Braun, T., Franke, J. E., Greiner, S., & Drummer, D. (2016) · International Congress Molded Interconnect Devices (MID) · doi:10.1109/icmid.2016.7738930 · Cited by 7
Chiker, N., Haddad, A., Hadji, Y., Benamar, M. E. A., Azzaz, M., Yahi, M., Sahraoui, T., Hadji, M., & Barsoum, M. W. (2017) · Ceramics International · doi:10.1016/j.ceramint.2017.11.102 · Cited by 7
Metadata
- Authors
- Fernie, J. A., Drew, R. A. L., & Knowles, K. M.
- Venue
- International Materials Reviews
- Publisher
- SAGE Publications
- Published
- 2009-09
- Volume
- 54
- Issue
- 5
- Pages
- 283-331
- ISSN
- 0950-6608 (ISSN-L)
- 1743-2804
- OpenAlex
- W1985755219
- Cited by
- 282
- References
- 328
- FWCI
- 10.33
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.