Joining of engineering ceramics
The DOI matches its Crossref record; 324 of the 328 references it cites were found in a registry or an index.
Abstract
Engineering ceramics such as alumina, zirconia, silicon nitride and silicon carbide can now be manufactured reliably with reproducible properties. As such, they are of increasing interest to industry, particularly for use in demanding environments, where their thermomechanical performance is of critical importance, with applications ranging from fuel cells to cutting tools. One aspect common to virtually all applications of engineering ceramics is that eventually they must be joined with another material, most usually a metal. The joining of engineering ceramics to metals is not always easy. There are two main considerations. The first consideration is the basic difference in atomic bonding: the ionic or covalent bonding of the ceramic, compared to the metallic bond. The second consideration is the mismatch in the coefficient of thermal expansion. In general, ceramics have a lower coefficient of thermal expansion than metals and, if high tensile forces are produced in the ceramic, either as a consequence of operating conditions or from the joining procedure itself, failure can occur. The plethora of joining processes available will be reviewed in this article, placing them in context from both an academic and commercial perspective. Comment will be made on research reporting advances on known technology, as well as introducing ‘newer’ technologies developed over the last 10 years. Finally, reviews and commentary will be made on the potential applications of the various joining processes in the commercial environment.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Ceramic joining techniques are numerous and technically challenging, and often subject the entire sample to extreme conditions, such as high temperatures and/or vacuums [223].”
From Ultrafast Laser Additive Manufacturing: A Review (2023) · cites this paper as [223]
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Structural Inorganic Chemistry
(1971) · Nature · doi:10.1038/229453c0 · Cited by 5,766
The Superalloys: Fundamentals and Applications
Reed, R. C. (2008) · Cited by 3,725
The Superalloys: Fundamentals and Applications
Reed, R. C. (2006) · Cambridge University Press eBooks · doi:10.1017/cbo9780511541285 · Cited by 2,369
Transformation Toughening in Zirconia‐Containing Ceramics
Hannink, R. H. J., Kelly, P., & Muddle, B. C. (2000) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2000.tb01221.x · Cited by 2,268
Silicon Nitride and Related Materials
Riley, F. L. (2000) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2000.tb01182.x · Cited by 1,566
CRC Materials Science and Engineering Handbook
Shackelford, J. F., Han, Y.-H., Kim, S., & Kwon, S.-H. (2016) · CRC Press eBooks · doi:10.1201/b18971 · Cited by 1,274
Wettability at High Temperatures
(1999) · Pergamon materials series · doi:10.1016/s1470-1804(99)x8001-1 · Cited by 1,042
Current ceramic materials and systems with clinical recommendations: A systematic review
Conrad, H. J., Seong, W.-J., & Pesun, I. J. (2007) · The Journal of Prosthetic Dentistry · doi:10.1016/s0022-3913(07)60124-3 · Cited by 981
The application of the specular reflection of neutrons to the study of surfaces and interfaces
Penfold, J., & Thomas, R. K. (1990) · Journal of Physics Condensed Matter · doi:10.1088/0953-8984/2/6/001 · Cited by 742
Handbook of Ceramic Composites
Bansal, N. P. (2005) · Springer eBooks · doi:10.1007/b104068 · Cited by 654
Research works printed but not linked: 31
- M. F. Ashby: ‘Cambridge engineering selector v4’; 2007, Cambridge, Granta Design Limited.
- Fernie J. A., 1999, Ind Ceram, 19, 172
- Imai H., 2006, JSME Int. J. Ser. A, 49, 450
- Lindner P., 2004, Solid State Technol, 47, 55
- Ito M., 1991, US Patent 5073085
- Duvall D. S., 1974, Weld, 1, 203
- 10.1016/j.ijrmhm.2004.01.003 · doi:10.1016/j.ijrmhm.2004.01.003
- Fernie J. A., 1999, Mater. World, 7, 686
- Loehman R. E., 1989, Am. Ceram. Soc. Bull, 68, 891
- Eustathopoulos N., 1998, Acta Mater, 46, 2319
- Sobczak N., 2005, Curr. Opin. Solid State Mater. Set, 9, 241 — 253
- Derby B., 2004, Interf Set, 12, 29
- Ormston D. R., 2001, ‘The particulate reinforcement of active broze alloys for joining silicon carbide’, Cambridge
- Knowles K. M., 2002, Ceram. Trans, 138, 103
- Nolte H. J., 1954, US Patent 2667432
- Kim J. Y., 2005, J. Electrochem. Soc, 152, J52—J58
- Paulasto M., 1997, Ceram. Trans, 77, 91
- Peteves S. D., 1998, Acta. Mater, 46, 2407
- Reichel U., 1999, Z. Metallkd, 90, 699
- Gasse A., 1997, World Patent WO 9747568
- Chaumat G., 2001, European Patent EP 806402
- Gasse A., 2008, US Patent 7318547
- Pask J. A., 1971, Proc. Porcelain Enamel Inst. Tech. Forum, 33, 1
- Pask J. A., 1987, Am. Ceram. Soc. Bull, 66, 1587
- Ghosh S., 2008, J. Electrochem. Soc, 155, B473—B478
- Kobsiriphat W., 2008, J. Fuel Cell Set Technot, 011002
- Henager C. H., J. Nucl. Mater, 2007, 367
- Appendino P., 1563, J. Nucl. Mater, 2004, 329
- Barabash V., J. Nucl. Mater, 2000, 283
- Ferraris M., 1546, J. Nucl. Mater, 1998, 258
- Suryanarayana C., 2001, Adv. Mater. Processes, 159, 29
Cited by
Items 201–300 of 302
Tian, W., Kita, H., Kondo, N., Hyuga, H., & Nagaoka, T. (2010) · Journal of the Ceramic Society of Japan · doi:10.2109/jcersj2.118.799 · Cited by 7
Strengthened and toughened SiHfBCN-based high-temperature resistant adhesive with SiC NWs
Luan, X., Xiyue, Z. H. U., Dong, X., Li, M., & Cheng, L. (2024) · Chinese Journal of Aeronautics · doi:10.1016/j.cja.2024.05.013 · Cited by 6
Yan, J., Zhu, J., & Ma, L. (2022) · International Journal of Solids and Structures · doi:10.1016/j.ijsolstr.2022.111567 · Cited by 6
Tao, L., Haitao, X., Xianming, M., Guo, W., Zhang, S., & Wu, H. (2023) · International Journal of Applied Ceramic Technology · doi:10.1111/ijac.14607 · Cited by 6
Existence of advanced ceramic materials in human life
Srivastava, S. K., Gupta, G. K., Joshi, T. C., Pandey, A. K., Muchhala, D., Shrivastava, V., Singh, P. K., Mondal, D. P., Kumar, R., & Ranjan, S. (2022) · Elsevier eBooks · doi:10.1016/b978-0-323-89952-9.00013-0 · Cited by 6
Yang, Y., Bhowmik, A., Tan, J. L., Du, Z., & Zhou, W. (2022) · Metals · doi:10.3390/met12050887 · Cited by 6
Кулик, В. И., Нилов, А. С., & Bogachev, E. A. (2022) · Refractories and Industrial Ceramics · doi:10.1007/s11148-022-00684-y · Cited by 6
Joining of alumina to Tetragonal Zirconia Polycrystal (TZP) using a Bi2O3-Y2O3 filler
Nejabat, M., Hadian, A. M., & Zamani, C. (2024) · Ceramics International · doi:10.1016/j.ceramint.2024.07.391 · Cited by 5
Microstructure and mechanical strength of Ti3AlC2 joints bonded using oxides as interlayer
Tan, Y., Li, S., Chen, C., Han, X., Xue, J., Liu, T., Zhou, X., Peng, S., & Zhang, H. (2019) · Ceramics International · doi:10.1016/j.ceramint.2019.05.282 · Cited by 5
Si3N4 ceramics joined with Si3N4-Li2O-Y2O3 by spark plasma sintering
Zhu, L.-L., Tan, X., Chen, J., Chen, X.-H., Dong, C.-H., Liu, H., Jian, Y., Zhang, G.-X., & Lin, H. (2024) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2024.116800 · Cited by 5
Brazing of ZTA ceramic with titanium for biomedical application
Fedotov, I., Ivannikov, A. A., Terekhova, S., Dzhumaev, P. S., Kozlov, I. V., Svetogorov, R. D., Klyushin, I., & Sevryukov, O. N. (2024) · The International Journal of Advanced Manufacturing Technology · doi:10.1007/s00170-024-14417-7 · Cited by 5
Joining Methods for Hard Ceramics
Osendi, M. I., & Miranzo, P. (2014) · Elsevier eBooks · doi:10.1016/b978-0-08-096527-7.00026-x · Cited by 5
Reactive-Element-Free, Silver-Based Brazes for SOFC Applications
Zhou, Q., Bieler, T. R., & Nicholas, J. D. (2017) · ECS Transactions · doi:10.1149/07801.1759ecst · Cited by 5
Halbig, M. C., & Singh, M. (2015) · Wiley eBooks · doi:10.1002/9781119100430.ch18 · Cited by 5
Phase relationship of the Ag–Zr–Cr system at 1000 and 750°C
Shi, C., Pan, Y., Yang, B., Liu, Y., Liu, S., Du, Y., & Liang, J. (2018) · International Journal of Materials Research (formerly Zeitschrift fuer Metallkunde) · doi:10.3139/146.111659 · Cited by 5
Coddington, B., Asthana, R., Halbig, M. C., & Singh, M. (2010) · Ceramic engineering and science proceedings · doi:10.1002/9780470944066.ch14 · Cited by 5
Ji, H., Chen, H., & Li, M. (2014) · International Conference on Electronic Packaging Technology (ICEPT) · doi:10.1109/icept.2014.6922880 · Cited by 5
Laser Welding of Alumina Ceramic Substrates with Two Fixed Beams
Sedore, B. W. C. (2013) · QSpace (Queen's University Library) · Cited by 5
REACTION LAYERS IN DIFFUSION BONDED OF SIALON TO FERRITIC STEEL
Firmanto, H. (2011) · UTPedia (Universiti Teknologi Petronas) · Cited by 5
Xu, K., Sun, Y., Yu, C., Lu, X., Liu, J., Liu, K., Huang, N., Zhang, Z., Zhu, H., Li, D., et al. (2025) · Ceramics International · doi:10.1016/j.ceramint.2025.09.359 · Cited by 4
Microstructure and Mechanical Properties of SiC Joint Brazed by Al-Ti Alloys as Filler Metal
Puhao, X. U., Zhang, X., Liu, G., Zhang, M., Gui, X., & Qiao, G. (2022) · Journal of Inorganic Materials · doi:10.15541/jim20210652 · Cited by 4
Characterization of the interfaces formed at the silicon nitride superalloy joints
Tunçkan, O., Turan, D., Dogan, A., & Turan, S. (2016) · Journal of the Australian Ceramic Society · doi:10.1007/s41779-016-0012-8 · Cited by 4
Tomographic microscopy of functionally graded polymer-derived SiCN ceramics with tunable gradients
Hagelüken, L., Makowska, M. G., Marone, F., & Brügger, J. (2024) · Materialia · doi:10.1016/j.mtla.2024.102025 · Cited by 4
Tian, W.-B., Kita, H., Hyuga, H., Kondo, N., & Sekine, K. (2012) · Materials Science and Engineering A · doi:10.1016/j.msea.2012.01.088 · Cited by 4
Formation of Interfacial Reaction Layers in Al2O3/SS 430 Brazed Joints Using Cu-7Al-3.5Zr Alloys
Heo, H., Joung, H., Jung, K., & Kang, C.-Y. (2018) · Metals · doi:10.3390/met8120990 · Cited by 4
Effect of annealing on grain growth and Y segregation behavior in tetragonal ZrO 2 thin film
Nakade, H., Tochigi, E., Feng, B., Ishikawa, R., Ohta, H., Shibata, N., & Ikuhara, Y. (2021) · Journal of the American Ceramic Society · doi:10.1111/jace.18217 · Cited by 4
Ultrarapid Transient-Liquid-Phase Bonding of Advanced Ceramics
Hong, S. M., Bartlow, C. C., Reynolds, T. B., Saito, N., & Glaeser, A. M. (2010) · Advances in science and technology · doi:10.4028/www.scientific.net/ast.64.88 · Cited by 4
Fabrication of Reliable Joints of Alumina Ceramics by Microwave-Assisted Reactive Brazing Technique
Shukla, M., Ghosh, S., Dandapat, N., Mandal, A. K., & Balla, V. K. (2016) · MATERIALS TRANSACTIONS · doi:10.2320/matertrans.m2015350 · Cited by 4
Advances and Challenges in Ultra‐High Temperature Materials for Aerospace Applications—A Review
Lewise, K. A. S., Brindha, S., & Hindu, M. (2026) · International Journal of Applied Ceramic Technology · doi:10.1111/ijac.70222 · Cited by 3
Min, P., Tong, X.-Y., Yuan, Y., Li, H., Cheng, Y., Liu, H., Song, P., & Wang, H. (2025) · Ceramics International · doi:10.1016/j.ceramint.2025.05.262 · Cited by 3
Wang, Q., Tao, J., Shan, H., Cui, T., Ding, J., & Wang, J. N. (2024) · Polymers · doi:10.3390/polym16040557 · Cited by 3
Laser Joining of Tight Ceramic‐Glass Composites for Use in Ceramic Heat Pipes
Börner, F., Lippmann, W., & Hurtado, A. (2014) · Chemie Ingenieur Technik · doi:10.1002/cite.201400016 · Cited by 3
DC‐driven ultrafast transient liquid phase bonding of 3YSZ and GH3128 superalloy using Ni interlayer
Li, L., & Shen, P. (2022) · Journal of the American Ceramic Society · doi:10.1111/jace.18570 · Cited by 3
Joining of aluminum and ceramic substrates by interposing molten aluminum–silicon alloy
Kita, K., & Hotta, M. (2022) · International Journal of Applied Ceramic Technology · doi:10.1111/ijac.14198 · Cited by 3
Herzog, S., Kaletsch, A., & Broeckmann, C. (2023) · Membranes · doi:10.3390/membranes13050504 · Cited by 3
de Portu, G., Glaeser, A. M., Reynolds, T. B., Takahashi, Y., Boffelli, M., & Pezzotti, G. (2014) · Journal of Materials Science · doi:10.1007/s10853-014-8803-1 · Cited by 3
Joining of SiC by Tape-Cast SiC-Al2O3-Y2O3 Interlayer
Tian, W. B., Kita, H., Hyuga, H., & Kondo, N. (2011) · Key engineering materials · doi:10.4028/www.scientific.net/kem.484.26 · Cited by 3
Raisson, R., Guillemet‐Fritsch, S., Dufour, P., Boisard, A., Duchesne, C., & Vidal, P.-É. (2025) · Ceramics International · doi:10.1016/j.ceramint.2025.07.132 · Cited by 2
Juri, A. Z., Basak, A. K., Omar, A., Basir, A., Al-Hammadi, R. A., & Sulong, A. B. (2026) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-026-13459-0 · Cited by 2
Enhancement mechanism of shear properties for SiO2 ceramics by laser welding with Al2O3/SiO2 powder
Zuo, Q., Yin, X., Chen, C., Zhang, Y., Kuang, M., & Mei, S. (2024) · Ceramics International · doi:10.1016/j.ceramint.2024.04.397 · Cited by 2
Research of the DBC joining interface
Krasniy, I., Berkin, A., Minskiy, G., Denisova, A. A., & Kumacheva, S. (2016) · International Forum on Strategic Technology · doi:10.1109/ifost.2016.7884079 · Cited by 2
Joining of Cf/SiBCN Composite with a Ni-Cr-Pd(Si,B) Filler Alloy
Li, W.-W., Chen, B., Xiong, H., Cheng, Y., & Zou, W. (2019) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-019-04420-5 · Cited by 2
Thuniki, N. R., Gangavarapu, K. P., Brijendra, V. G., Budda, K., & Prasad, V. V. B. (2023) · International Journal of Applied Ceramic Technology · doi:10.1111/ijac.14614 · Cited by 2
Xing, L., Ao, R., & Yang, W. (2020) · Journal of Luminescence · doi:10.1016/j.jlumin.2020.117773 · Cited by 2
Toughening Ceramic Joints through Strategic Fracture Path Control
Feng, J. X., Herrmann, M., & Hurtado, A. (2024) · Advanced Materials Technologies · doi:10.1002/admt.202400535 · Cited by 2
Joining of Refractory and Dissimilar Materials
Mukasyan, A. S. (2017) · Elsevier eBooks · doi:10.1016/b978-0-12-804173-4.00084-3 · Cited by 2
Fernie, J. A., & Knowles, K. M. (2021) · Elsevier eBooks · doi:10.1016/b978-0-12-818542-1.00061-8 · Cited by 2
Self-citationJoining of Advanced Ceramics and Metals
Xia, J. (2026) · IntechOpen eBooks · doi:10.5772/intechopen.1012386 · Cited by 1
Autothermal reforming of methane for syngas production in a novel ceramic microchannel reactor
Blakeley, B. (2015) · Digital Collections of Colorado (Colorado State University) · Cited by 1
TRIBOLOGICAL PROPERTIES OF AL2O3-ZrO2 COMPOSITE COATING BY LUBRICATION
Al-Samarai, R. A., & Haftirman, H. (2021) · SINERGI · doi:10.22441/sinergi.2021.3.014 · Cited by 1
Diffusion bonding of Ti‐coated C f ‐SiC f /SiBCN composites to Nb using Ag–Pd interlayer
Lin, J., Zhang, X., Wang, W., Yu, D., Jia, D., Lin, T., Lin, P., & He, P. (2021) · International Journal of Applied Ceramic Technology · doi:10.1111/ijac.13902 · Cited by 1
Effect of Surface-Treated Filler on the Wettability of Composite Solder: Short Review
Saufee, W. H. M., Leong, W. K., Mohammad, A. A., & Nazeri, M. F. M. (2023) · Springer proceedings in physics · doi:10.1007/978-981-19-9267-4_86 · Cited by 1
Research on Ceramic/Steel Connection Using a Single Interlayer Method
Yu, D., Zhang, Y., Zhou, J., Sun, D., & Li, H. (2023) · International Journal of Materials Science and Applications · doi:10.11648/j.ijmsa.20231203.12 · Cited by 1
Yao, X., Tian, S., Fang, Y., Jiao, H., Wang, J., Wang, B., Zhou, J. F., & Xue, F. (2023) · Materials Research Express · doi:10.1088/2053-1591/acfae8 · Cited by 1
Microstructure and bonding mechanism of MgAl2O4/MgAl2O4 joints brazed using B2O3-ZnO-SiO2 glass
Guo, W., Fan, P., Xin, J., & Li, X. (2025) · Ceramics International · doi:10.1016/j.ceramint.2025.02.283 · Cited by 1
Wu, Y., Gu, X., Jia, M., Shen, Q., & Chen, F. (2025) · Ceramics International · doi:10.1016/j.ceramint.2025.07.100 · Cited by 1
Zhou, L., Yang, B., Li, C., Cui, H., Si, X., Qi, J., & Cao, J. (2025) · Materials Science and Engineering A · doi:10.1016/j.msea.2025.149652 · Cited by 1
Flash joining of alumina ceramics by spark plasma sintering with Ni and Ti interlayers
Timm, V., Blugan, G., Stosz, M., Fulanović, L., Minnert, C., Schwiedrizik, J., & Ramlow, H. (2026) · Ceramics International · doi:10.1016/j.ceramint.2026.02.370 · Cited by 1
Wang, X., Zhang, T., Dong, H., Wang, J., Qi, B., Ma, R., Du, A. Y., Fan, Y., Zhao, X., & Cao, X. (2026) · Ceramics International · doi:10.1016/j.ceramint.2026.07.012 · Cited by 1
The Joining of Oxide Ceramics with Quartz Fiber by Interlayer
Zhao, Y. N., Zhang, W., Hou, G. Q., & Liu, L. H. (2011) · Advanced materials research · doi:10.4028/www.scientific.net/amr.337.392 · Cited by 1
Vacuum brazing of diamond to tungsten carbide
Yin, Z. (2016) · Digital Commons - Montana Tech (Montana Tech of the University of Montana) · Cited by 1
Wang, N., Wang, D., Yang, Z. W., & Wang, Y. (2018) · Materials science forum · doi:10.4028/www.scientific.net/msf.913.542 · Cited by 1
Lasergestützte Herstellung keramischer Wärmerohre zur Energierückgewinnung aus Vergasungsprozessen
Börner, F., Lippmann, W., & Hurtado, A. (2018) · Springer eBooks · doi:10.1007/978-3-662-46251-5_27 · Cited by 1
Development and construction of AISI H11/ZrO2 joints for injection molding tools
Tillmann, W., Anar, N. B., Manka, M., Wojarski, L., & Lehmert, B. (2019) · Welding in the World · doi:10.1007/s40194-019-00800-6 · Cited by 1
In situ sol‐gel surface modification of alumina for a better wettability by brazing filler metals
Tillmann, W., & Ferreira, M. (2020) · Materialwissenschaft und Werkstofftechnik · doi:10.1002/mawe.201700067 · Cited by 1
Alumina joints brazed by screen-printed B4C–SiO2 in air
Zhu, L., Dai, M.-M., Xu, X., Zhang, G.-X., Jian, Y., Zhao, C., & Lin, H. (2022) · Ceramics International · doi:10.1016/j.ceramint.2022.01.196 · Cited by 1
Zhang, Q., Zheng, K., Wang, J., & Ke, Z. (2024) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2024.04.035 · Cited by 1
Review paper on joining of alumina to metal through brazing
Mohammad, G. (2025) · International Journal of Research Publication and Reviews · doi:10.55248/gengpi.6.0225.1011 · Cited by 1
Drozda, F. O. (2013) · LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas) · Cited by 1
Transient-Liquid-Phase Bonding of Ceramics
Saito, N., Hong, S. M., Nakashima, K., & Glaeser, A. M. (2011) · 高温学会誌 · doi:10.7791/jhts.37.10 · Cited by 1
Estudio interfacial de uniones disimiles Al2O3/Ti
Custodio, N. B. G. (2012) · LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas) · Cited by 1
Joining of Ceramics and Ceramic Matrix Composites (CMC) for Aerospace and Energy Applications
Gianchandani, P. K. (2018) · PORTO@Iris · Cited by 1
Zhang, H., Jiang, X., Li, Q., Wu, C., Sun, K., Lan, Z., & Yu, Z. (2024) · Journal of Advanced Ceramics · doi:10.26599/jac.2025.9221197
Design, manufacturing, and characterization of advanced ceramics
Shakib, M. A. (2025) · Iowa Research Online (The University of Iowa) · doi:10.25820/etd.007835
Plasmabasierte Kupfermetallisierung von leistungselektronischen Bauelementen
Hensel, A. (2025) · OPUS FAU (Kooperativer Bibliotheksverbund Berlin-Brandenburg (KOBV), on behalf of the Universitätsbibliothek Erlangen-Nürnberg) · doi:10.25593/978-3-96147-869-9
Sintering Technologies in Materials Design and Processing
Vizureanu, P., & Bălțatu, M. S. (2026) · IntechOpen eBooks · doi:10.5772/intechopen.1012152
Localized Heating Joining for Ceramic Matrix Composites
Ferraris, M., & Pandey, K. (2026) · Springer eBooks · doi:10.1007/978-981-97-1929-7_65-1
(2025) · Springer eBooks · doi:10.1007/978-981-97-2998-2_192
Thamm, L., Blugan, G., Minnert, C., Schwiedrzik, J. J., Manukyan, K. V., Eriksson, M., Johnsson, M., & Ramlow, H. (2026) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2026.118836
Ibrahim, N. N. M., Hussain, P., & Awang, M. B. (2015) · AIP conference proceedings · doi:10.1063/1.4919173
Diffusion Bonding of Rigid Alumina Pieces using Porous Alumina Interlayers
Miyazaki, H., Hotta, M., Kita, H., & lzutsu, Y. (2012) · Ceramic engineering and science proceedings · doi:10.1002/9781118217528.ch10
The Interlayer Designation for ZTM Ceramics and Fibre Joining
Zhao, Y. N., Liu, J. C., Wang, C. F., & Zhang, W. (2011) · Advanced materials research · doi:10.4028/www.scientific.net/amr.291-294.878
Effect of temperature on the mechanical behavior of B4C joints bonded by Al infiltrated TiC tape
Tian, W., Sun, Z., Zhang, P., & Zhang, Y. M. (2018) · Journal of the Australian Ceramic Society · doi:10.1007/s41779-018-0191-6
Gestrich, T., Kaiser, A., Meinl, J., Schilm, J., Linseis, F., Seibt, S., & Göllner, M. (2016) · Keramische Zeitschrift · doi:10.1007/bf03400266
Fabrication and Characterization of Shape Memory Alloy (SMA) - Max Phase Bilayers and Composites
Kothalkar, A. (2015) · OakTrust (Texas A&M University Libraries)
Effect of Lubrication on the Wear Resistance of Plasma Sprayed Composite Coatings (Al2O3+ZrO2∙5CaO)
Abhinav, A., Ribeirio, R., Bodra, N., Goala, B., Raghav, R. J., Vardhan, A., & Ali, M. M. A. M. (2020) · Tribology in Industry · doi:10.24874/ti.2020.42.01.05
Soldering methods for obtaining permanent joints of ceramic composites with metals (review article)
Кулик, В. И., Нилов, А. С., Bogachev, E. A., & Ларионов, Н. В. (2021) · NOVYE OGNEUPORY (NEW REFRACTORIES) · doi:10.17073/1683-4518-2021-4-42-52
Technologies for Applying Current-Heat-Conducting Copper Coatings on Corundum Substrates
Плетнев, П. М., Nepochatov, Y. K., & Denisova, A. (2022) · Lecture notes in networks and systems · doi:10.1007/978-3-030-96383-5_33
Zhao, Y., Fan, R., Gao, Y., Li, Y., Wang, R., & Zhang, Y. (2022) · Journal of Physics Conference Series · doi:10.1088/1742-6596/2285/1/012030
Ranjan, P., & Ghildiyal, S. (2024) · Journal of Micromanufacturing · doi:10.1177/25165984241237379
Zhao, Z., Qi, Q., Liu, X., Huang, Z., & Liu, Y. (2025) · Advanced Engineering Materials · doi:10.1002/adem.202402449
Córdova, S. B. A. (2018) · LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas)
Producción y caracterización de ensambles híbridos alúmina/acero AISI 410S por el método brazing
López, A. C. (2015) · LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas)
Júnior, M. N. D. S. (2022) · Portuguese National Funding Agency for Science, Research and Technology (RCAAP Project by FCT) · doi:10.34626/eja9-5594
Selective Laser Melting (SLM) as preferred process for multimaterial components production
de Oliveira, G. V. M. G. (2017) · Portuguese National Funding Agency for Science, Research and Technology (RCAAP Project by FCT)
Wells, A., Schneiderman, B., Zhao, Y., Magdum, R., Lipke, D. W., & Yu, Z. (2026) · SSRN Electronic Journal · doi:10.2139/ssrn.6452114
Capillary migration of molten Si through C and SiC fabrics to join SiC using Si–C reaction bonding
Jin, G.-E., Park, S., Joo, S., Song, J. S., Eom, J., Cheong, H. N., & Yoon, D. (2026) · Journal of the Korean Ceramic Society · doi:10.1007/s43207-026-00607-4
Brazing mechanisms of the Ti2AlC ceramics using nickel-based filler alloy
Lu, C. (2018) · theses.fr (ABES) · doi:10.70675/2d527419z5957z466czbec9z56260d8bc007
Joining metals to oxide ceramics
Yang, Z., & Sabolsky, E. M. (2026) · Ceramics International · doi:10.1016/j.ceramint.2026.09.026
Metadata
- Authors
- Fernie, J. A., Drew, R. A. L., & Knowles, K. M.
- Venue
- International Materials Reviews
- Publisher
- SAGE Publications
- Published
- 2009-09
- Volume
- 54
- Issue
- 5
- Pages
- 283-331
- ISSN
- 0950-6608 (ISSN-L)
- 1743-2804
- OpenAlex
- W1985755219
- Cited by
- 282
- References
- 328
- FWCI
- 10.33
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.