Low-pressure decomposition of chrysotile as a function of time and temperature
The DOI matches its Crossref record.
Abstract
Chrysotile from Thetford, Quebec, was heated at constant temperature in quench furnaces from 200 to 1000 °C for 4 to 720 h, and the products were analyzed by XRD and optical microscopy. XRD patterns for chrysotile from Thedford, Jeffrey Quebec, and New Idria, California, heated for up to 8 h at constant temperatures from 400 to 800 °C in hydrothermal diamond-anvil cells, were obtained at 300 s intervals by using synchrotron radiation. The studies show that differences in the decomposition temperatures of chrysotile reported in the literature can be explained by differences in the temperatures, time at temperature, particle size, and partial pressure of water. Chrysotile heated for 30 days is destroyed between 475 and 500 °C, whereas chrysotile heated to 800 °C survives for only minutes. A prograde heating experiment, consistent with the literature, shows chrysotile destruction beginning at 600 °C and completed at 750 °C, demonstrating that such experiments should not be used to establish temperatures of thermal stability. Forsterite forms readily at 600 °C when water is retained transiently in the decomposition products, but does not form after 4 h of heating samples of small fiber size and high surface area from which water is readily lost. When water is retained in the sample chamber during heating to 800 °C over 4 h, a rapid destruction of chrysotile and formation of forsterite was observed, followed by the appearance and later destruction of the intermediate reaction products talc, a tridymite-like phase, and anthophyllite; enstatite appearance coincides with the destruction of the tridymite-like phase and talc. In quench experiments, a 10+ Å phase is observed between 500 and 600 °C, and talc is observed between 587 and 800 °C. The optical properties of the run products between 600 and 900 °C are highly variable, with a range in the index of refraction perpendicular to length of up to 0.06 and a minimum index of refraction 0.03 below the starting material in fibers in the 650 °C run product; the variability reflects the inhomogeneity in products and reactants in this temperature range. In quench experiments, the intensity of the XRD patterns of chrysotile decreased on heating between 200 and 400 °C, and increased at 450 °C, demonstrating recrystallization of chrysotile. A gradual heating experiment showed a similar pattern with the lowest intensities at 250 °C and maximum intensities at 550 °C. The two types of chrysotile reported in the literature may reflect simply the presence of chrysotile of different particle sizes. Chrysotile may also possess a spectrum of stabilities due to variable strain energies of curvature. The presence of a tridymite-like phase supports the formation of a Si-rich dehydroxylate II. The absence of forsterite and chrysotile in brake-wear debris reflects the high temperature and disaggregated fiber bundles resulting from friction.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cited by
The dehydroxylation of serpentine group minerals
Gualtieri, A. F., Giacobbe, C., & Viti, C. (2012) · American Mineralogist · doi:10.2138/am.2012.3952 · Cited by 89
“According to Capitani and Mellini (2004), antigorite may derive a greater thermal stability from a more effective interlayer interaction due to the inversion of the tetrahedral sheet.”
BackgroundInfluentialLarachi, F., Daldoul, I., & Beaudoin, G. (2010) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2010.03.007 · Cited by 86
Rim, G., Marchese, A. K., Stallworth, P., Greenbaum, S. G., & Park, A.-H. A. (2020) · Chemical Engineering Journal · doi:10.1016/j.cej.2020.125204 · Cited by 72
Pasquier, L.-C., Mercier, G., Blais, J.-F., Cecchi, E., & Kentish, S. (2014) · Applied Geochemistry · doi:10.1016/j.apgeochem.2014.08.008 · Cited by 66
Obmiński, A. (2022) · Science of The Total Environment · doi:10.1016/j.scitotenv.2022.157275 · Cited by 30
Airborne Asbestos Concentrations Associated with Heavy Equipment Brake Removal
(2009) · The Annals of Occupational Hygiene · doi:10.1093/annhyg/mep056 · Cited by 20
Metadata
- Authors
- Candela, P. A., Crummett, C. D., Earnest, D. J., Frank, M. R., & Wylie, A. G.
- Venue
- American Mineralogist
- Publisher
- Mineralogical Society of America
- Published
- 2007-10-01
- Volume
- 92
- Issue
- 10
- Pages
- 1704-1713
- ISSN
- 0003-004X (ISSN-L)
- OpenAlex
- W2045301607
- Cited by
- 47
- References
- 0
- FWCI
- 1.28
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.