Microstructural investigation of the KCl-induced corrosion of the austenitic alloy Sanicro 28 (35Fe27Cr31Ni) at 600°C
The DOI matches its Crossref record; 10 of the 10 references it cites were found in a registry or an index.
Abstract
High-temperature corrosion of stainless steel is important, particularly in bio-fuelled boiler applications. The flue gas is rich in water vapour and alkali salts, which accelerate the corrosion of the boiler material. The focus of this paper is on the breakdown of the protective oxide scale formed on Sanicro 28, which is a highly alloyed austenitic stainless steel (35Fe27Cr31Ni), in the presence of KCl(s). Laboratory exposures were carried out at 600°C in 5% O2+40% H2O for 1, 24 and 168 hours. The samples were coated with 0.10 mg/cm2 KCl prior to exposure and uncoated samples were exposed for reference. The aim was to link the observed mass gains and microstructure to oxidation mechanisms. The oxidized samples were analyzed by XRD, SEM/EDX, FIB and TEM/EDX. The exposures results in a very complex corrosion chemistry, including, e.g. the formation of potassium chromate and the rapid transport of iron species on the surface resulting in accumulation of oxide on the former KCl particles. However, the consumption of chromium and the presence of chloride on the surface does not result in the breakdown of the protective oxide. The ability of the alloy to withstand this harsh environment is tentatively attributed to the high Cr/Fe ratio.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Grabke, H. J., Reese, E., & Spiegel, M. (1995) · Corrosion Science · doi:10.1016/0010-938x(95)00011-8 · Cited by 537
Asteman, H., Svensson, J.-E., Norell, M., & Johansson, L.-G. (2000) · Oxidation of Metals · doi:10.1023/a:1004642310974 · Cited by 325
Self-citationAsteman, H., Svensson, J.-E., Johansson, L.-G., & Norell, M. (1999) · Oxidation of Metals · doi:10.1023/a:1018875024306 · Cited by 304
Self-citationDeposition and high temperature corrosion in a 10 MW straw fired boiler
Michelsen, H. P., Frandsen, F., Dam-Johansen, K., & Larsen, O. H. (1998) · Fuel Processing Technology · doi:10.1016/s0378-3820(97)00062-3 · Cited by 258
KCl Induced Corrosion of a 304-type Austenitic Stainless Steel at 600°C; The Role of Potassium
Pettersson, J., Asteman, H., Svensson, J. E., & Johansson, L. G. (2005) · Oxidation of Metals · doi:10.1007/s11085-005-5704-3 · Cited by 182 · cited 1×
“The breakdown of the protective scale was then attributed primarily to the formation of K2CrO4, depleting the protective oxide in chromium [12,13].”
BackgroundSelf-citationHalvarsson, M., Tang, J. E., Asteman, H., Svensson, J.-E., & Johansson, L.-G. (2006) · Corrosion Science · doi:10.1016/j.corsci.2005.08.012 · Cited by 146 · cited 1×
“Silicon is enriched at the oxideymetal interface, as is often reported [17,18].”
BackgroundSelf-citationAccelerated oxidation rate of chromium induced by sodium chloride
Shinata, Y. (1987) · Oxidation of Metals · doi:10.1007/bf00659274 · Cited by 129
Pettersson, C., Pettersson, J., Asteman, H., Svensson, J.-E., & Johansson, L.-G. (2006) · Corrosion Science · doi:10.1016/j.corsci.2005.05.018 · Cited by 112
Self-citationInitial Stages of the HCl-Induced High-Temperature Corrosion of Alloy 310
Folkeson, N., Johansson, L.-G., & Svensson, J.-E. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2754174 · Cited by 66 · cited 1×
“It was recently reported that thermodynamically metastable FeCl2 forms at the oxideyair interface when stainless steel is exposed to HCl-containing air at 500 C [27]:”
BackgroundSelf-citationPettersson, C., Johansson, L.-G., & Svensson, J.-E. (2008) · Oxidation of Metals · doi:10.1007/s11085-008-9118-x · Cited by 40
Self-citation
Cited by
Pettersson, J., Folkeson, N., Johansson, L.-G., & Svensson, J.-E. (2011) · Oxidation of Metals · doi:10.1007/s11085-011-9240-z · Cited by 117
Self-citationFolkeson, N., Jonsson, T., Halvarsson, M., Johansson, L. ‐., & Svensson, J. ‐. (2011) · Materials and Corrosion · doi:10.1002/maco.201005942 · Cited by 93
Self-citationKarlsson, S., Åmand, L.-E., & Liske, J. (2015) · Fuel · doi:10.1016/j.fuel.2014.09.007 · Cited by 79
“Similar to laboratory exposure with KCl and NaCl on 304L [7,9,17], the oxide scale is divided into two parts: an outer Fe-rich oxide and an inner oxide rich in Fe, Cr and Ni rich oxide (see Fig.”
Phother-Simon, J., Hanif, I., Liske, J., & Jonsson, T. (2021) · Corrosion Science · doi:10.1016/j.corsci.2021.109315 · Cited by 37
Self-citationThe Effects of KCl, NaCl and K2CO3 on the High-Temperature Oxidation Onset of Sanicro 28 Steel
Sui, J., Lehmusto, J., Bergelin, M., & Hupa, M. (2016) · Oxidation of Metals · doi:10.1007/s11085-016-9613-4 · Cited by 19
Metadata
- Authors
- Proff, C., Jonsson, T., Pettersson, C., Svensson, J.-E., Johansson, L.-G., & Halvarsson, M.
- Venue
- Materials at High Temperatures
- Publisher
- Informa UK Limited
- Published
- 2009-01
- Volume
- 26
- Issue
- 2
- Pages
- 113-125
- ISSN
- 0960-3409 (ISSN-L)
- 1878-6413
- OpenAlex
- W2028361663
- Cited by
- 19
- References
- 10
- FWCI
- 2.58
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Microstructural investigation of the KCl-induced corrosion of the austenitic alloy Sanicro 28 (35Fe27Cr31Ni) at 600°C. https://app.cochat.ai/papers/10.1179/096034009x464339
- The paper
- Proff, C., Jonsson, T., Pettersson, C., Svensson, J.-E., Johansson, L.-G., & Halvarsson, M. (2009). Microstructural investigation of the KCl-induced corrosion of the austenitic alloy Sanicro 28 (35Fe27Cr31Ni) at 600°C. Materials at High Temperatures. https://doi.org/10.1179/096034009x464339
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.