A Moisture‐ and Oxygen‐Impermeable Separator for Aprotic Li‐O2 Batteries
The DOI matches its Crossref record.
Abstract
Despite the unparalleled theoretical gravimetric energy, Li‐O 2 batteries are still under a research stage because of their insufficient cycle lives. While the reversibility in air‐cathodes has been lately improved significantly by the deepened understanding on the electrode–electrolyte reaction and the integration of diverse catalysts, the stability of the Li metal interface has received relatively much less attention. The destabilization of the Li metal interface by crossover of water and oxygen from the air‐cathode side can indeed cause as fatal degradation for the cycle life as the irreversibility of the air‐cathodes. Here, it is reported that cheap poreless polyurethane separator can effectively suppress this crossover while allowing Li ions to diffuse through selectively. The polyurethane separator also protects Li metal anodes from redox mediators used for enhancing the reversibility of the air‐cathode reaction. Based on the Li metal protection, a persistent capacity of 600 mAh g−1 is preserved for more than 200 cycles. The current approach can be readily applicable to many other rechargeable batteries that suffer from similar interfacial degradation by side products from the other electrode.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Because of the poreless structure, the Gurley time (the time required for 100 cm 3 of air to pass through a separator under air pressure of 0.862 kgf cm -2 ) was out of the detection range in an air permeability test (Fig. 31b(iii)), suggesting that the PU membrane is air-impermeable.The PU membrane also has excellent electrolyte wettability and Li ion conductivity (Fig. 31b(iv)), and therefore”
From Current Challenges and Routes Forward for Nonaqueous Lithium–Air Batteries (2020) · cites this paper as [289]
In the citing paper
“While the PU separator successfully prevents the crossover of H 2 O and O 2 , Li dendrite still grows, possibly due to the low mechanical strength.”
From Current Challenges and Routes Forward for Nonaqueous Lithium–Air Batteries (2020) · cites this paper as [289]
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
No references could be resolved yet.
Research works printed but not linked: 70
- 10.1038/nmat3191 · DOI · Paper page
- 10.1002/aenm.201000010 · DOI · Paper page
- 10.1002/adfm.201200688 · DOI · Paper page
- 10.1021/jz300243r · DOI · Paper page
- 10.1021/ja310258x · DOI · Paper page
- 10.1021/nl4021649 · DOI · Paper page
- 10.1002/anie.201102357 · DOI · Paper page
- 10.1021/ja2021747 · DOI · Paper page
- 10.1149/1.3168564 · DOI · Paper page
- 10.1002/cssc.201200810 · DOI · Paper page
- 10.1016/j.jpowsour.2012.10.011 · DOI
- 10.1149/2.005204esl · DOI · Paper page
- 10.1021/ja311518s · DOI · Paper page
- 10.1038/nchem.1499 · DOI · Paper page
- 10.1002/anie.201400711 · DOI · Paper page
- 10.1002/anie.201307976 · DOI · Paper page
- 10.1038/srep04225 · DOI
- 10.1038/ncomms3383 · DOI · Paper page
- 10.1126/science.1223985 · DOI · Paper page
- 10.1038/nmat3737 · DOI · Paper page
- 10.1021/am504463b · doi:10.1021/am504463b
- 10.1039/c2cc32844e · DOI · Paper page
- 10.1002/cssc.201200801 · DOI
- 10.1002/aenm.201400867 · DOI · Paper page
- 10.1021/ja2111543 · DOI · Paper page
- 10.1038/ncomms3255 · DOI · Paper page
- 10.1002/cssc.201402567 · doi:10.1002/cssc.201402567
- 10.1016/j.elecom.2013.12.022 · DOI
- 10.1149/2.087405jes · DOI
- 10.1002/anie.201408008 · DOI
- 10.1021/nl303087j · doi:10.1021/nl303087j
- 10.1002/adma.201501490 · DOI · Paper page
- 10.1021/cm501578v · DOI
- Massey L. K., 2003, Permeability Properties of Plastics and Elastomers: A Guide to Packaging and Barrier Materials
- 10.1007/s10856-012-4595-5 · doi:10.1007/s10856-012-4595-5
- 10.1016/j.memsci.2006.01.047 · DOI
- 10.1016/j.polymer.2006.08.062 · doi:10.1016/j.polymer.2006.08.062
- 10.1002/app.1976 · doi:10.1002/app.1976
- 10.1002/app.1963.070070207 · DOI · Paper page
- 10.1002/(SICI)1097-4628(19980725)69:4<775::AID-APP16>3.0.CO;2-O · doi:10.1002/(sici)1097-4628(19980725)69:4<775::aid-app16>3.0.co;2-o
- 10.1016/S0142-9612(98)00250-6 · DOI
- 10.1016/S0079-6700(00)00036-8 · DOI · Paper page
- 10.1021/nl403860k · DOI · Paper page
- 10.1533/9781845690694.74 · doi:10.1533/9781845690694.74
- 10.1016/S0378-7753(98)00193-1 · DOI · Paper page
- 10.1023/A:1024458513004 · doi:10.1023/a:1024458513004
- 10.1590/S1516-14392010000200015 · DOI
- 10.1002/cnma.201500055 · DOI
- 10.1149/1.1379740 · DOI
- 10.1021/jp311114u · DOI · Paper page
- 10.1021/jz300430s · DOI
- 10.1039/c2cc37042e · doi:10.1039/c2cc37042e
- 10.1021/jz201070t · DOI · Paper page
- 10.1002/adma.201204018 · DOI · Paper page
- 10.1039/c3ta11792h · doi:10.1039/c3ta11792h
- 10.1002/aenm.201401030 · DOI
- 10.1016/j.jpowsour.2013.06.097 · DOI
- 10.1016/S0167-2738(02)00080-2 · DOI · Paper page
- 10.1002/adfm.201400935 · DOI · Paper page
- 10.1038/ncomms2855 · DOI · Paper page
- 10.1021/cm5040003 · DOI · Paper page
- 10.1016/j.jallcom.2013.12.208 · doi:10.1016/j.jallcom.2013.12.208
- 10.1038/ncomms2907 · DOI · Paper page
- 10.1021/acs.nanolett.5b02116 · DOI · Paper page
- 10.1134/1.1537411 · doi:10.1134/1.1537411
- 10.4028/www.scientific.net/MSF.480-481.405 · doi:10.4028/www.scientific.net/msf.480-481.405
- 10.1039/C4TA07085B · DOI
- Tietze S., 2013, Adsorption and revaporisation studies of thin iodine oxide and CsI aerosol deposits from containment surface materials in LWRs: NKS‐285
- 10.1149/1.2100852 · doi:10.1149/1.2100852
- Lyday P. A., 2000, Iodine and Iodine Compounds in Ullmann's Encyclopedia of Industrial Chemistry
Cited by
Toward Safe Lithium Metal Anode in Rechargeable Batteries: A Review
Cheng, X.-B., Zhang, R., Zhao, C.-Z., & Zhang, Q. (2017) · Chemical Reviews · doi:10.1021/acs.chemrev.7b00115 · Cited by 6,197
Lithium–Oxygen Batteries and Related Systems: Potential, Status, and Future
Kwak, W.-J., Rosy, Sharon, D., Xia, C., Kim, H., Johnson, L. R., Bruce, P. G., Nazar, L. F., Sun, Y.-K., Frimer, A. A., et al. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.9b00609 · Cited by 1,009
Self-citationTowards practical lithium-metal anodes
Zhang, X., Yang, Y., & Zhou, Z. (2020) · Chemical Society Reviews · doi:10.1039/c9cs00838a · Cited by 726
Beyond lithium ion batteries: Higher energy density battery systems based on lithium metal anodes
Shen, X., Liu, H., Cheng, X.-B., Yan, C., & Huang, J.-Q. (2018) · Energy Storage Materials · doi:10.1016/j.ensm.2017.12.002 · Cited by 653
Current Challenges and Routes Forward for Nonaqueous Lithium–Air Batteries
Liu, T., Vivek, J. P., Zhao, E. W., Lei, J., Garcia-Araez, N., & Grey, C. P. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.9b00545 · Cited by 618
Metadata
- Authors
- Kim, B. G., Kim, J., Min, J., Lee, Y., Choi, J. H., Jang, M. C., Freunberger, S. A., & Choi, J. W.
- Affiliations
- Graduate School of Energy, Environment, Water, and Sustainability (EEWS) Korea Advanced Institute of Science and Technology (KAIST) 291 Daehakro Yuseong‐gu Daejeon 305‐701 Republic of Korea
- Department of Biomedical Engineering Georgia Institute of Technology 313 Ferst Drive Atlanta GA 30332 USA
- Future Technology Research Center Corporate R&D LG Chem Research Park 188 Munji‐ro Yuseong‐gu Daejeon 305‐738 Republic of Korea
- Institute for Chemistry and Technology of Materials Graz University of Technology Stremayrgasse 9 8010 Graz Austria
- Venue
- Advanced Functional Materials
- Publisher
- Wiley
- Published
- 2016-02-03
- Volume
- 26
- Issue
- 11
- Pages
- 1747-1756
- ISSN
- 1616-301X
- 1616-3028
- Cited by
- 152
- References
- 0
- Language
- en
- Funders
- National Research Foundation of Korea
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: A Moisture‐ and Oxygen‐Impermeable Separator for Aprotic Li‐O2 Batteries. https://app.cochat.ai/papers/10.1002/adfm.201504437
- The paper
- Kim, B. G., Kim, J., Min, J., Lee, Y., Choi, J. H., Jang, M. C., Freunberger, S. A., & Choi, J. W. (2016). A Moisture‐ and Oxygen‐Impermeable Separator for Aprotic Li‐O2 Batteries. Advanced Functional Materials. https://doi.org/10.1002/adfm.201504437
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.