Epitaxial Induced Plating Current‐Collector Lasting Lifespan of Anode‐Free Lithium Metal Battery
Abstract
Anode‐free designs can obtain the ultimate energy density of lithium metal batteries. However, without a continuous Li supply from the anode side, it is much more challenging to achieve high capacity retention with a competitive energy density. Here, the lifespan of an anode‐free Li metal battery is prolonged by applying an epitaxial induced plating current‐collector (E‐Cu). The functional layer on E‐Cu initiates Li storage by an alloying approach, forming an epitaxial induce layer, which exhibits speedy surface diffusion for of Li‐ions, resulting in the block like epitaxial growth of Li. Moreover, this alloying process also promotes the formation of a LiF‐rich solid electrolyte interphase (SEI), which is very useful for uniform Li plating. Due to the benefits of epitaxial Li plating and LiF‐rich SEI, the initial coulombic efficiency of the E‐Cu/Li asymmetric cell increases from 93.24 to 98.24%, and the capacity retention of anode‐free NCM811/E‐Cu pouch cell increases from 66 to 84% with a remarkable energy density of 420 Wh kg−1 in the condition of limited electrolyte addition (E/C ratio of 2 g Ah−1). This strategy is promising in the development of high energy batteries in extending their lifespans.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Reviving the lithium metal anode for high-energy batteries
Lin, D., Liu, Y., & Cui, Y. (2017) · Nature Nanotechnology · doi:10.1038/nnano.2017.16 · Cited by 6,763
Fluoroethylene Carbonate Additives to Render Uniform Li Deposits in Lithium Metal Batteries
Zhang, X., Cheng, X., Chen, X., Yan, C., & Zhang, Q. (2017) · Advanced Functional Materials · doi:10.1002/adfm.201605989 · Cited by 1,699
Advanced Model for Solid Electrolyte Interphase Electrodes in Liquid and Polymer Electrolytes
Peled, E., Golodnitsky, D., & Ardel, G. (1997) · Journal of The Electrochemical Society · doi:10.1149/1.1837858 · Cited by 1,205
High-Efficiency Lithium-Metal Anode Enabled by Liquefied Gas Electrolytes
Yang, Y., Davies, D. M., Yin, Y., Borodin, O., Lee, J. Z., Fang, C., Olguin, M., Zhang, Y., Sablina, E. S., Wang, X., et al. (2019) · Joule · doi:10.1016/j.joule.2019.06.008 · Cited by 268
Cited by
Strategies toward the development of high-energy-density lithium batteries
Niu, H., Zhang, N., Lu, Y., Zhang, Z., Li, M., Liu, J., Zhang, N., Song, W., Zhao, Y., & Miao, Z. (2024) · Journal of Energy Storage · doi:10.1016/j.est.2024.111666 · Cited by 327
Surface engineering toward stable lithium metal anodes
Lu, G., Nai, J., Luan, D., Tao, X., & Lou, X. W. (. (2023) · Science Advances · doi:10.1126/sciadv.adf1550 · Cited by 289
Anode‐Free Solid‐State Lithium Batteries: A Review
Huang, W., Zhao, C., Wu, P., Yuan, H., Feng, W., Liu, Z., Lu, Y., Sun, S., Fu, Z., Hu, J., et al. (2022) · Advanced Energy Materials · doi:10.1002/aenm.202201044 · Cited by 278
Metadata
- Authors
- Lin, L., Suo, L., Hu, Y., Li, H., Huang, X., & Chen, L.
- Venue
- Advanced Energy Materials
- Publisher
- Wiley
- Published
- 2021-01-14
- Volume
- 11
- Issue
- 9
- ISSN
- 1614-6832 (ISSN-L)
- 1614-6840
- OpenAlex
- W3119071070
- Cited by
- 237
- References
- 4
- FWCI
- 11.31
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Epitaxial Induced Plating Current‐Collector Lasting Lifespan of Anode‐Free Lithium Metal Battery. https://app.cochat.ai/papers/10.1002/aenm.202003709
- The paper
- Lin, L., Suo, L., Hu, Y., Li, H., Huang, X., & Chen, L. (2021). Epitaxial Induced Plating Current‐Collector Lasting Lifespan of Anode‐Free Lithium Metal Battery. Advanced Energy Materials. https://doi.org/10.1002/aenm.202003709
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.