Apatite formation on the surface of ceravital‐type glass‐ceramic in the body
The DOI matches its Crossref record; 13 of the 13 references it cites were found in a registry or an index.
Abstract
Previous studies on surface structural changes in vitro as well as in vivo of bioactive A‐W‐type glass‐ceramics and Bioglass‐type glasses showed that the essential condition for glasses and glassceramics to bond to living bone is formation of a bonelike apatite layer on their surfaces in the body. Gross et al., however, had explained the bone‐bonding mechanism of Ceravital‐type apatitecontaining glass‐ceramic without mentioning formation of the surface apatite layer. In the present study, apatite formation on the surface of one of Ceravitaltype glass‐ceramics was investigated in vitro as well as in vivo. An apatitecontaining glass‐ceramic of the composition Na 2 O 5, CaO 33, SiO 2 46, Ca(PO 3)2 16 wt%, which was named KGS by Gross et al., was soaked in an acellular simulated body fluid which had ion concentrations almost equal to those of the human blood plasma. The same kind of glassceramic was implanted into a rabbit tibia. Thin‐film x‐ray diffraction, Fourier transform infrared reflection spectroscopy, and scanning electron microscopic observation of the surfaces of the specimens soaked in the simulated body fluid showed that Ceravital‐type glass‐ceramic also forms a layer of carbonate‐containing hydroxyapatite of small crystallites and/or a defective structure on its surface in the fluid. Electron probe x‐ray microanalysis of the interface between the glassceramic and the surrounding bone showed that a thin layer rich in Ca and P is present at the interface. These findings indicated that Ceravital‐type glassceramics also form the bonelike apatite layer on its surface in the body and bond to living bone through the apatite layer.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Raman spectroscopy showed that both spherulitic and nonspherulitic dolomitic crystals are surrounded by OM and apatite (Fig. 7 C and D), both of which are linked to biological processes (41).”
From Massive formation of early diagenetic dolomite in the Ediacaran ocean: Constraints on the "dolomite problem" (2020) · cites this paper as [41]
Citations
Cites
Solutions able to reproduce in vivo surface‐structure changes in bioactive glass‐ceramic A‐W3
Kokubo, T., Kushitani, H., Sakka, S., Kitsugi, T., & Yamamuro, T. (1990) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820240607 · Cited by 3,836
Self-citationCa, P‐rich layer formed on high‐strength bioactive glass‐ceramic A‐W
Kokubo, T., Ito, S., Huang, Z. T., Hayashi, T., Sakka, S., Kitsugi, T., & Yamamuro, T. (1990) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820240306 · Cited by 859
Self-citationChemical anatomy, physiology and pathology of extracellular fluid
Gamble, J. L. (1954) · University Microfilms International eBooks · Cited by 579
A new glass‐ceramic for bone replacement: Evaluation of its bonding to bone tissue
Nakamura, T., Yamamuro, T., Higashi, S., Kokubo, T., & Itoo, S. (1985) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820190608 · Cited by 441
Self-citationFundamental aspects of biocompatibility
Williams, D. F. (1981) · CRC Press eBooks · Cited by 301
The interface of various glasses and glass ceramics with a bony implantation bed
Gross, U., & Strunz, V. (1985) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820190308 · Cited by 223
Bone bonding behavior of three kinds of apatite containing glass ceramics
Kitsugi, T., Yamamuro, T., Nakamura, T., Higashi, S., Kakutani, Y., Hyakuna, K., Ito, S., Kokubo, T., Takagi, M., & Shibuya, T. (1986) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820200906 · Cited by 178
Self-citationKitsugi, T., Nakamura, T., Yamamura, T., Kokubu, T., Shibuya, T., & Takagi, M. (1987) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820211008 · Cited by 157
The ultrastructure of the interface between a glass ceramic and bone
Gross, U., Brandes, J., Strunz, V., Bab, I., & Sela, J. (1981) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820150302 · Cited by 128
Bone bonding behavior of MgOCaOSiO2P2O5CaF2 glass (mother glass of A · W‐glass‐ceramics)
Kitsugi, T., Yamamuro, T., Nakamura, T., & Kokubo, T. (1989) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820230607 · Cited by 111
Self-citationBonding behavior between two bioactive ceramics in vivo
Kitsugi, T., Yamamuro, T., Nakamura, T., Kokubo, T., Takagi, M., Shibuya, T., Takeuchi, H., & Ono, M. (1987) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820210905 · Cited by 83
Self-citationBonding between Bioactive Glasses, Glass-Ceramics or Ceramics in a Simulated Body Fluid
KOKUBO, T., HAYASHI, T., Sakka, S., Kitsugi, T., & Yamamuro, T. (1987) · Journal of the Ceramic Association Japan · doi:10.2109/jcersj1950.95.1104_785 · Cited by 79
Self-citationThe bonding of glass ceramics to bone
Kitsugi, T., Yamamuro, T., Nakamura, T., & Kokubo, T. (1989) · International Orthopaedics · doi:10.1007/bf00268048 · Cited by 56
Self-citation
Research works printed but not linked: 4
- Kokubo T., 1987, Ceramics in Clinical Application, 175
- Kokubo T., 1990, Bioceramics, 113
- Nakamura T., 1983, Treatise on Biomedical Materials, 109
- Hench L. L., 1982, Biocompatibility of Orthopaedic Implants, 129
Cited by
How useful is SBF in predicting in vivo bone bioactivity?
Kokubo, T., & Takadama, H. (2006) · Biomaterials · doi:10.1016/j.biomaterials.2006.01.017 · Cited by 9,576
Self-citationNovel bioactive materials with different mechanical properties
Kokubo, T., Kim, H.-M., & Kawashita, M. (2003) · Biomaterials · doi:10.1016/s0142-9612(03)00044-9 · Cited by 1,914
Self-citationNavarro, M., Michiardi, A., Castaño, O., & Planell, J. A. (2008) · Journal of The Royal Society Interface · doi:10.1098/rsif.2008.0151 · Cited by 1,513
Bioactive glass ceramics: properties and applications
Kokubo, T. (1991) · Biomaterials · doi:10.1016/0142-9612(91)90194-f · Cited by 1,202
Self-citationPreparation and assessment of revised simulated body fluids
Oyane, A., Kim, H., Furuya, T., Kokubo, T., Miyazaki, T., & Nakamura, T. (2003) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.10482 · Cited by 1,117
Self-citation
Metadata
- Authors
- Ohtsuki, C., Kushitani, H., Kokubo, T., Kotani, S., & Yamamuro, T.
- Affiliations
- Kyoto University Institute for Chemical Research (JP)
- Kyoto University (JP)
- Corresponding author
- Ohtsuki, C.
- ORCID
- Ohtsuki, C.
- Venue
- Journal of Biomedical Materials Research
- Publisher
- Wiley
- Published
- 1991-11
- Volume
- 25
- Issue
- 11
- Pages
- 1363-1370
- ISSN
- 0021-9304 (ISSN-L)
- 1097-4636
- OpenAlex
- W1979146632
- Cited by
- 259
- References
- 13
- Citations by year
- 2026: 1 · 2025: 1 · 2024: 3 · 2023: 6 · 2022: 10 · 2021: 6 · 2020: 7 · 2019: 8 · 2018: 5 · 2017: 7 · 2016: 14 · 2015: 10 · 2014: 5 · 2013: 17 · 2012: 12
- FWCI
- 5.14
- Type
- journal article
- Language
- en
- Open access
- closed
- Locations
- Journal of Biomedical Materials Research (publishedVersion)
- PubMed (publishedVersion)
- Topics
- Physical Sciences › Engineering › Biomedical Engineering › Bone Tissue Engineering Materials
- Physical Sciences › Engineering › Mechanical Engineering › Surface Treatment and Coatings
- Health Sciences › Dentistry › General Dentistry › Dental materials and restorations
- Keywords
- apatite formation, hydroxyapatite layer, bioactive glass-ceramics, bone bonding, simulated body fluid, rabbit tibia implantation, calcium phosphate, bone-implant interface, surface structural changes
- MeSH terms
- Animals, Apatites, Body Fluids, Bone Development, Ceramics, Humans, Microscopy, Electron, Scanning, Rabbits, Spectrophotometry, Infrared, Surface Properties, X-Ray Diffraction, Prostheses and Implants
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.