Oxidation After Breakdown of the Chromium-Rich Scale on Stainless Steels at High Temperature: Internal Oxidation
Open accessThe DOI matches its Crossref record; 42 of the 43 references it cites were found in a registry or an index.
Abstract
Breakaway oxidation of alloy 304L at 600 °C was studied in four environments (O2 + H2O + KCl, O2 + H2O + SO2 + KCl, H2 + H2O + Ar, O2 + K2CO3) for up to 168 h. The resulting scales were investigated by FIB/SEM, SEM/EDX, STEM/EELS, STEM/EDS and oxidation was elucidated by thermodynamic calculations (Thermo-Calc). The initial thin protective scale broke down in all cases. After breakaway, the scale consisted of two layers, i.e. an inward growing spinel/reaction zone and an outward growing iron-rich layer. The general features and microstructure of the scales after breakaway were similar in all environments and were explained in terms of: (1) Different diffusivities of Cr3+ and Fe2+ in the spinel oxide. (2) The appearance of a miscibility gap in the FeCr and FeCrNi spinel oxides. (3) The equilibrium composition of the spinel (at low pO2 Ni is not present in the spinel).
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Figures




![Fig. 5 a BSE image of a BIB cross-section through the oxide scale and into the alloy on the 304L (18Cr10Ni) samples exposed for 168 h at 600 ° C in 5%O2 ? 40%H2O ? KCl. A magnified image of the marked region close to the right hand side of the micrograph is shown in ( b ) and the SEM/EDX elemental maps from the central marked region is shown in ( d ). b BSE image of the marked area in ( a ). The inward growing oxide scale can be divided into darker areas (fully oxidized regions) and brighter areas , i.e. mixed oxide and metal (reaction zone). A TEM sample was taken from a similar region as indicated in the marked region. c HAADF image of a region similar to the marked region in ( b ). The inward growing oxide scale can be divided into a region of mixed oxide and metal, i.e. a reaction zone, and darker fully oxidized regions. At the alloy grain boundary a Fe-Cr oxide could be found. CBED patterns from the oxides are inseted in the image. The oxide at the grain boundary was indexed as a spinel structure (M3O4) with the zone axis [001] (i). The small oxide precipitates were also indexed as a spinel structure (M3O4) with the zone axis [001] (ii). d SEM/EDX elemental maps from the marked area in ( a ) of the sample exposed for 168 h in 5%O2 ? 40%H2O ? KCl](https://figures.cochat.ai/paper-figures/d8b0540923b6450d99bf1325b6e8a4b4/oxidation-after-breakdown-of-the-chromium-rich-scale-on-stainless-steels-at-high-figure-5.png)






Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
The cited source says what the claim attributes to it.
In the citing paper
“Previous studies performed on FeCr [25,37] and FeCrNi [37,26,27] alloys showed that the reaction zone was composed of Cr-rich oxide precipitates and Cr-depleted metal.”
From Beyond breakaway corrosion – Influence of chromium, nickel and aluminum on corrosion of iron-based alloys at 600 °C (2020) · cites this paper as [37]
The cited source says what the claim attributes to it.
In the citing paper
“Previous research, focused on the initiation/breakaway event, indicate a similar microstructure obtained after the onset of breakaway of Fe-based alloys, seemingly independent of suggested breakaway-reaction [8,20,22,29,31].”
From The influence of Nickel on the corrosion protection of FeCrNi alloys after breakaway corrosion at 600 °C (2024) · cites this paper as [29]
The cited source says what the claim attributes to it.
In the citing paper
“The microstructure suggest that the internal oxidation was of reaction zone-type (RZ) on the majority of the samples, meaning a region with mixed spinel type oxide and metal [37].”
From Beyond breakaway corrosion – Influence of chromium, nickel and aluminum on corrosion of iron-based alloys at 600 °C (2020) · cites this paper as [37]
The cited source says what the claim attributes to it.
In the citing paper
“Jonsson et al. [37] showed that several different corrosion environments gave similar oxide microstructure after breakaway at 600 • C.”
From Beyond breakaway corrosion – Influence of chromium, nickel and aluminum on corrosion of iron-based alloys at 600 °C (2020) · cites this paper as [37]
The cited source says what the claim attributes to it.
In the citing paper
“Jonsson et al. [37] showed that the environment had limited influence on the microstructure formed after breakaway oxidation.”
From Beyond breakaway corrosion – Influence of chromium, nickel and aluminum on corrosion of iron-based alloys at 600 °C (2020) · cites this paper as [37]
2 more claims about this paper
Create a free account to see every claim other papers make about this one.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Thermo-Calc & DICTRA, computational tools for materials science
Andersson, J.-O., Helander, T., Höglund, L., Shi, P., & Sundman, B. (2002) · Calphad · doi:10.1016/s0364-5916(02)00037-8 · Cited by 4,322
Introduction to the High Temperature Oxidation of Metals
Birks, N., Meier, G. H., & Pettit, F. S. (2006) · doi:10.1017/cbo9781139163903 · Cited by 2,189
Electron Energy-Loss Spectroscopy in the Electron Microscope
Egerton, R. F. (2011) · Springer eBooks · doi:10.1007/978-1-4419-9583-4 · Cited by 1,850
(2006) · Electrochemistry and Corrosion Science · doi:10.1007/1-4020-7860-9_10 · Cited by 1,814
BIRKS, N., MEIER, G. H., & PETTIT, F. S. (1989) · Superalloys Supercomposites Superceramics · doi:10.1016/b978-0-12-690845-9.50020-8 · Cited by 1,513
High Temperature Oxidation and Corrosion of Metals
(2016) · Elsevier eBooks · doi:10.1016/c2014-0-00259-6 · Cited by 957
Introduction to Focused Ion Beams: Instrumentation, Theory, Techniques and Practice
(2005) · Springer eBooks · doi:10.1007/b101190 · Cited by 830
High Temperature Oxidation and Corrosion of Metals
(2008) · Corrosion Series · doi:10.1016/s1875-9491(08)00023-9 · Cited by 738
Asteman, H., Svensson, J.-E., Norell, M., & Johansson, L.-G. (2000) · Oxidation of Metals · doi:10.1023/a:1004642310974 · Cited by 325
Self-citationEnhanced oxidation of the 9%Cr steel P91 in water vapour containing environments
Ehlers, J., Young, D. J., Smaardijk, E. J., Tyagi, A. K., Penkalla, H. J., Singheiser, L., & Quadakkers, W. J. (2006) · Corrosion Science · doi:10.1016/j.corsci.2006.02.002 · Cited by 325
An assessment of the Fe-O system
Sundman, B. (1991) · Journal of Phase Equilibria · doi:10.1007/bf02645709 · Cited by 254
Asteman, H., Svensson, J.-E., & Johansson, L.-G. (2002) · Oxidation of Metals · doi:10.1023/a:1014877600235 · Cited by 218
Self-citationVan Orman, J. A., & Crispin, K. L. (2010) · Reviews in Mineralogy and Geochemistry · doi:10.2138/rmg.2010.72.17 · Cited by 210
Meier, G. H., Jung, K., Mu, N., Yanar, N. M., Pettit, F. S., Pirón Abellán, J., Olszewski, T., Nieto Hierro, L., Quadakkers, W. J., & Holcomb, G. R. (2010) · Oxidation of Metals · doi:10.1007/s11085-010-9215-5 · Cited by 204
Self-diffusion and impurity diffusion in oxides
Freer, R. (1980) · Journal of Materials Science · doi:10.1007/bf00552089 · Cited by 197
KCl Induced Corrosion of a 304-type Austenitic Stainless Steel at 600°C; The Role of Potassium
Pettersson, J., Asteman, H., Svensson, J. E., & Johansson, L. G. (2005) · Oxidation of Metals · doi:10.1007/s11085-005-5704-3 · Cited by 182
Self-citationEssuman, E., Meier, G. H., Żurek, J., Hänsel, M., Singheiser, L., & Quadakkers, W. J. (2007) · Scripta Materialia · doi:10.1016/j.scriptamat.2007.06.058 · Cited by 172
Point defects and cation tracer diffusion in (CrFe1 − )3 − O4 spinels
Töpfer, J., Aggarwal, S., & Dieckmann, R. (1995) · Solid State Ionics · doi:10.1016/0167-2738(95)00190-h · Cited by 169
Quantitative transmission X-ray microanalysis of ionic compounds
Van Cappellen, E., & Doukhan, J. C. (1994) · Ultramicroscopy · doi:10.1016/0304-3991(94)90047-7 · Cited by 166
Halvarsson, M., Tang, J. E., Asteman, H., Svensson, J.-E., & Johansson, L.-G. (2006) · Corrosion Science · doi:10.1016/j.corsci.2005.08.012 · Cited by 146
Self-citationTemperature dependence of oxide scale formation on high-Cr ferritic steels in Ar–H2–H2O
Young, D. J., Zurek, J., Singheiser, L., & Quadakkers, W. J. (2011) · Corrosion Science · doi:10.1016/j.corsci.2011.02.031 · Cited by 124
Othman, N. K., Othman, N. K., Zhang, J., & Young, D. J. (2009) · Corrosion Science · doi:10.1016/j.corsci.2009.08.032 · Cited by 123
Hultquist, G., Tveten, B., & Hörnlund, E. (2000) · Oxidation of Metals · doi:10.1023/a:1004610626903 · Cited by 113
Pujilaksono, B., Jonsson, T., Heidari, H., Halvarsson, M., Svensson, J.-E., & Johansson, L.-G. (2011) · Oxidation of Metals · doi:10.1007/s11085-010-9229-z · Cited by 109
Self-citationModeling of iron diffusion in the iron oxides magnetite and hematite with variable stoichiometry
Hallström, S., Höglund, L., & Ågren, J. (2011) · Acta Materialia · doi:10.1016/j.actamat.2010.08.032 · Cited by 101
Water Vapour Effects on Fe–Cr Alloy Oxidation
Othman, N. K., Zhang, J., & Young, D. J. (2009) · Oxidation of Metals · doi:10.1007/s11085-009-9183-9 · Cited by 98
Oxidation of iron at 400–600°C in dry and wet O2
Pujilaksono, B., Jonsson, T., Halvarsson, M., Svensson, J., & Johansson, L. (2010) · Corrosion Science · doi:10.1016/j.corsci.2010.01.002 · Cited by 97
Self-citationHigh temperature corrosion of superheater steels by KCl and K2CO3 under dry and wet conditions
Lehmusto, J., Yrjas, P., Skrifvars, B.-J., & Hupa, M. M. (2012) · Fuel Processing Technology · doi:10.1016/j.fuproc.2012.05.020 · Cited by 79
Jonsson, T., Froitzheim, J., Pettersson, J., Svensson, J.-E., Johansson, L.-G., & Halvarsson, M. (2009) · Oxidation of Metals · doi:10.1007/s11085-009-9156-z · Cited by 76
Self-citationMu, N., Jung, K., Yanar, N. M., Meier, G. H., Pettit, F. S., & Holcomb, G. R. (2012) · Oxidation of Metals · doi:10.1007/s11085-012-9302-x · Cited by 74
Oxidation of Fe–10Cr in O2 and in O2+H2O environment at 600°C: A microstructural investigation
Jonsson, T., Pujilaksono, B., Heidari, H., Liu, F., Svensson, J.-E., Halvarsson, M., & Johansson, L.-G. (2013) · Corrosion Science · doi:10.1016/j.corsci.2013.06.016 · Cited by 64
Self-citationAn ESEM in situ investigation of the influence of H2O on iron oxidation at 500°C
Jonsson, T., Pujilaksono, B., Hallström, S., Ågren, J., Svensson, J., Johansson, L.-G., & Halvarsson, M. (2009) · Corrosion Science · doi:10.1016/j.corsci.2009.05.016 · Cited by 55
Self-citationMicrostructural Investigation of Protective and Non-Protective Oxides on 11% Chromium Steel
Liu, F., Tang, J. E., Jonsson, T., Canovic, S., Segerdahl, K., Svensson, J., & Halvarsson, M. (2006) · Oxidation of Metals · doi:10.1007/s11085-006-9035-9 · Cited by 52
Self-citationMicrostructure Evolution During Steam Oxidation of a Nb Stabilized Austenitic Stainless Steel
Hansson, A. N., Pantleon, K., Grumsen, F. B., & Somers, M. A. J. (2009) · Oxidation of Metals · doi:10.1007/s11085-009-9182-x · Cited by 47
Karlsson, S., Jonsson, T., Hall, J., Svensson, J.-E., & Liske, J. (2014) · Energy & Fuels · doi:10.1021/ef402127h · Cited by 41
Self-citationThe Effect of Traces of SO2 on Iron Oxidation: A Microstructural Study
Jonsson, T., Järdnäs, A., Svensson, J. E., Johansson, L.-G., & Halvarsson, M. (2007) · Oxidation of Metals · doi:10.1007/s11085-007-9051-4 · Cited by 36
Self-citationJonsson, T., Folkeson, N., Halvarsson, M., Svensson, J., & Johansson, L. G. (2014) · Oxidation of Metals · doi:10.1007/s11085-013-9468-x · Cited by 33
Self-citationEffect of water vapour on the oxidation of Fe–13Cr–5Ni martensitic alloy at 973K
Liu, L., Yang, Z.-G., Zhang, C., Ueda, M., Kawamura, K., & Maruyama, T. (2012) · Corrosion Science · doi:10.1016/j.corsci.2012.04.008 · Cited by 28
The Influence of H2O on Iron Oxidation at 600°C: A Microstructural Study
Jonsson, T., Pujilaksono, B., Fuchs, A., Svensson, J. E., Johansson, L. G., & Halvarsson, M. (2008) · Materials Science Forum · doi:10.4028/www.scientific.net/msf.595-598.1005 · Cited by 17
Self-citationJonsson, T., Liu, F., Canovic, S., Asteman, H., Svensson, J.-E., Johansson, L.-G., & Halvarsson, M. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2768909 · Cited by 16
Self-citationEssuman, E., Meier, G. H., Zurek, J., Hänsel, M., Singheiser, L., & Quadakkers, W. J. (2008) · Materials Science Forum · doi:10.4028/www.scientific.net/msf.595-598.699 · Cited by 13
Galerie, A., Pint, B. A., & Monceau, D. (2013) · Oxidation of Metals · doi:10.1007/s11085-013-9462-3 · Cited by 9
Research works printed but not linked: 2
- H. Asteman, J.-E. Svensson, M. Norell and L.-G. Johansson, Oxidition of Metals 54, 11 (2000). · DOI · Paper page
- B. Pujilaksono, T. Jonsson, H. Heidari, M. Halvarsson, J. E. Svensson and L. G. Johansson, Oxidation of Metals 75, 183 (2011). · DOI · Paper page
Cited by
Col, A., Parry, V., & Pascal, C. (2017) · Corrosion Science · doi:10.1016/j.corsci.2016.10.029 · Cited by 144
Bai, M., Reddy, L., & Hussain, T. (2018) · Corrosion Science · doi:10.1016/j.corsci.2018.02.047 · Cited by 81
Eklund, J., Jönsson, B., Persdotter, A., Liske, J., Svensson, J.-E., & Jonsson, T. (2018) · Corrosion Science · doi:10.1016/j.corsci.2018.09.004 · Cited by 55
Self-citationOxidation behaviors and mechanical properties of L12-strengthened high-entropy alloys at 700 ℃
Liu, S., Kai, W., Hou, J., Zhao, Y., Li, Q., Yang, C.-H., Yang, T., & Kai, J. (2022) · Corrosion Science · doi:10.1016/j.corsci.2022.110499 · Cited by 47
Persdotter, A., Eklund, J., Liske, J., & Jonsson, T. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108961 · Cited by 44
Self-citation
Metadata
- Authors
- Jonsson, T., Karlsson, S., Hooshyar, H., Sattari, M., Liske, J., Svensson, J.-E., & Johansson, L.-G.
- Affiliations
- Chalmers University of Technology (SE)
- Corresponding author
- Jonsson, T.
- Venue
- Oxidation of Metals
- Published
- 2016-01-20
- Volume
- 85
- Issue
- 5-6
- Pages
- 509-536
- ISSN
- 0030-770X (ISSN-L)
- 1573-4889
- OpenAlex
- W2287046081
- Cited by
- 103
- References
- 43
- Citations by year
- 2026: 16 · 2025: 10 · 2024: 9 · 2023: 7 · 2022: 7 · 2021: 11 · 2020: 12 · 2019: 9 · 2018: 12 · 2017: 6 · 2016: 4
- FWCI
- 12.62
- Type
- journal article
- Language
- en
- Open access
- hybrid
- doi.org
- Locations
- Oxidation of Metals (publishedVersion, cc-by)
- Chalmers Research (Chalmers University of Technology) (submittedVersion)
- Funders
- Chalmers Tekniska Högskola
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Materials Science › Metals and Alloys › Hydrogen embrittlement and corrosion behaviors in metals
- Physical Sciences › Materials Science › Materials Chemistry › Advancements in Solid Oxide Fuel Cells
- Keywords
- breakaway oxidation, internal oxidation, high-temperature oxidation, spinel oxides, miscibility gap, scale microstructure, thermodynamic calculation
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.