Trends in fireside corrosion damage to superheaters in air and oxy-firing of coal/biomass
Open accessThe DOI matches its Crossref record; 4 of the 4 references it cites were found in a registry or an index.
Abstract
This paper compares the laboratory-based fireside corrosion tests on superheater/reheater materials in simulated air-firing combustion conditions with oxy-firing combustion conditions (with hot gas recycling before flue gas de-sulphurisation). The gaseous combustion environment was calculated based on a specific co-firing ratio of CCP with Daw Mill coal. The fireside corrosion tests were carried out using the “deposit recoat” test method to simulate the damage anticipated in specific environments. A synthetic deposit (Na2SO4:K2SO4:Fe2O3 = 1.5:1.5:1 mol.) which has commonly been used in fireside corrosion screening trials and is a mix that forms alkali-iron tri-sulphate (identified in many investigations as a cause of fireside corrosion) was used in these tests. The air-fired tests were carried out at temperatures of 600, 650 and 700 °C and oxy-fired tests were carried out at temperatures of 600, 650, 700 and 750 °C to represent the superheater/reheater metal temperatures anticipated in future power plants with and without synthetic deposits, with four candidate materials: T92, HR3C and 347HFG steels; nickel-based alloy 625 (alloy 625 was only tested with screening deposits). The progress of the samples during their exposures was measured using mass change methods. After the exposures, the samples were examined by SEM/EDX to characterise the damage. To quantify the metal damage, pre-exposure micrometre measurements were compared to the post-exposure image analyser measurements on sample cross-sections. The trends in corrosion damage in both air and oxy-firing conditions showed a “bell-shaped” curve, with the highest metal damage levels (peak) observed at 650 °C for air-firing and 700 °C for oxy-firing tests. However, at 600 and 650 °C similar damage levels were observed in both environments. The shift in peak corrosion damage in oxy-firing condition is believed to be the presence of higher levels of SOx, which stabilised the alkali-iron tri-sulphate compounds. Generally, in both air and oxy-firing conditions the mean metal damage was reduced with increasing the amount of Cr in the alloys. However, at the highest temperatures in both air-firing (700 °C) and oxy-firing conditions (750 °C) the metal damage of nickel based superalloy 625 was higher than HR3C.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Deposition of potassium salts on heat transfer surfaces in straw-fired boilers: a pilot-scale study
Nielsen, H. P., Baxter, L. L., Sclippab, G., Morey, C., Frandsen, F. J., & Dam-Johansen, K. (2000) · Fuel · doi:10.1016/s0016-2361(99)00090-3 · Cited by 202 · cited 1×
“Herbaceous biomass has higher levels of elements such as K and Cl but much less S compared to most coals [8,9,11,12].”
BackgroundReducing superheater corrosion in wood‐fired boilers
Henderson, P., Szakálos, P., Pettersson, R., Andersson, C., & Högberg, J. (2006) · Materials and Corrosion · doi:10.1002/maco.200503899 · Cited by 87
Fireside Corrosion of Superheater Materials in Coal/Biomass Co-fired Advanced Power Plants
Hussain, T., Syed, A. U., & Simms, N. J. (2013) · Oxidation of Metals · doi:10.1007/s11085-013-9394-y · Cited by 38
Self-citationEnvironmental degradation of boiler components
Simms, N. J. (2011) · Power Plant Life Management and Performance Improvement · doi:10.1533/9780857093806.2.145 · Cited by 25
Self-citation
Cited by
Fireside corrosion on T24 steel pipes and HVOF NiCr coatings exposed to different salt mixtures
Abu-warda, N., López, A. J., Pedraza, F., & Utrilla, M. V. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108747 · Cited by 32
“5 corrosion to represent the composition of alkali-iron tri-sulfate [21].”
BackgroundImpacts of Applied Stresses on High Temperature Corrosion Behavior of HR3C in Molten Salt
Fu, J., Li, N., Zhou, Q., & Guo, P. (2015) · Oxidation of Metals · doi:10.1007/s11085-014-9522-3 · Cited by 31
Fireside Corrosion of Heat Exchanger Materials for Advanced Solid Fuel Fired Power Plants
Mori, S., Pidcock, A., Sumner, J., Simms, N., & Oakey, J. (2022) · Oxidation of Metals · doi:10.1007/s11085-021-10094-z · Cited by 11
Self-citationFireside corrosion and deposition on heat exchangers in biomass combustion systems
Mori, S., Sanusi, T., Simms, N., & Sumner, J. (2023) · Materials at High Temperatures · doi:10.1080/09603409.2022.2138007 · Cited by 8
Self-citationJinyang, H., Jintao, L., Zhen, Y., Yongli, Z., Yingying, D., & Yong, Y. (2018) · 2018 International Conference on Power System Technology (POWERCON) · doi:10.1109/powercon.2018.8601684 · Cited by 6
Metadata
- Authors
- Hussain, T., Syed, A. U., & Simms, N. J.
- Venue
- Fuel
- Publisher
- Elsevier BV
- Published
- 2013-11
- Volume
- 113
- Pages
- 787-797
- ISSN
- 0016-2361 (ISSN-L)
- OpenAlex
- W2031538267
- Cited by
- 64
- References
- 4
- FWCI
- 8.57
- Type
- journal article
- Language
- en
- Open access
- hybrid
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Trends in fireside corrosion damage to superheaters in air and oxy-firing of coal/biomass. https://app.cochat.ai/papers/10.1016/j.fuel.2013.04.005
- The paper
- Hussain, T., Syed, A. U., & Simms, N. J. (2013). Trends in fireside corrosion damage to superheaters in air and oxy-firing of coal/biomass. Fuel. https://doi.org/10.1016/j.fuel.2013.04.005
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.