Abstract
In this study, porous components of a proton exchange membrane (PEM) fuel cell, i.e., single-layer gas diffusion layer (GDL, carbon paper), double-layer GDL (microporous layer (MPL) deposited carbon papers), and catalyzed electrodes, are subjected to 60 repetitive freeze-thaw cycles between −40 °C and 30 °C under water-submerged conditions; and their morphological and microstructural characteristics are investigated at each 15 cycles and compared with those of virgin materials. The results indicate that consecutive cycling of temperature causes different degradation patterns in different components. The single-layer GDL shows a unique degradation mechanism, in which macro-scale pores volumetrically expand, and relatively small-scale hollows and cracks form on the polymeric binder and carbon fiber interfaces, respectively. For the double-layer GDL, large-scale surface cracks form on the MPL surface after 15 cycles, and the morphology and microstructure degradation gains momentum with the formation of these cracks, and upon completion of 30 cycles, large-scale carbon/hydrophobic agent flakes start to detach from the surface. For the catalyzed electrodes, due to their inherently cracked surface, the catalyst layers (CLs) degrade first through expansion of the cracks in the in- and through-plane directions, and then through swelling and agglomeration of the ionomer; and combination of these two patterns triggers detachment of large CL flakes from the surface, negatively affecting the microstructure.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Omrani, R., & Shabani, B. (2017) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2017.09.132 · Cited by 245
Shahgaldi, S., Ozden, A., Li, X., & Hamdullahpur, F. (2018) · Energy Conversion and Management · doi:10.1016/j.enconman.2018.06.078 · Cited by 121
Self-citation
Cited by
Ren, P., Pei, P., Li, Y., Wu, Z., Chen, D., & Huang, S. (2020) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2020.100859 · Cited by 737
Zhao, J., & Li, X. (2019) · Energy Conversion and Management · doi:10.1016/j.enconman.2019.112022 · Cited by 430
Self-citationChen, Q., Zhang, G., Zhang, X., Sun, C., Jiao, K., & Wang, Y. (2021) · Applied Energy · doi:10.1016/j.apenergy.2021.116496 · Cited by 298
Zhang, G., Qu, Z., Tao, W.-Q., Wang, X., Wu, L., Wu, S., Xie, X., Tongsh, C., Huo, W., Bao, Z., et al. (2023) · Chemical Reviews · doi:10.1021/acs.chemrev.2c00539 · Cited by 274
Fouzaï, I., Gentil, S., Bassetto, V. C., Silva, W. O., Maher, R., & Girault, H. H. (2021) · Journal of Materials Chemistry A · doi:10.1039/d0ta07470e · Cited by 102
Metadata
- Authors
- Ozden, A., Shahgaldi, S., Zhao, J., Li, X., & Hamdullahpur, F.
- Venue
- International Journal of Hydrogen Energy
- Publisher
- Elsevier BV
- Published
- 2020-01
- Volume
- 45
- Issue
- 5
- Pages
- 3618-3631
- ISSN
- 0360-3199 (ISSN-L)
- OpenAlex
- W2901722584
- Cited by
- 83
- References
- 2
- FWCI
- 2.35
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Degradations in porous components of a proton exchange membrane fuel cell under freeze-thaw cycles: Morphology and microstructure effects. https://app.cochat.ai/papers/10.1016/j.ijhydene.2018.10.209
- The paper
- Ozden, A., Shahgaldi, S., Zhao, J., Li, X., & Hamdullahpur, F. (2020). Degradations in porous components of a proton exchange membrane fuel cell under freeze-thaw cycles: Morphology and microstructure effects. International Journal of Hydrogen Energy. https://doi.org/10.1016/j.ijhydene.2018.10.209
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.