Abstract
Mechanical behavior of four metallic alloys fabricated with layered, laser-heated methods of additive manufacturing (AM) was compared to that of similar alloys produced with conventional methods (wrought and machined). AM materials were produced by a leading commercial service provider, as opposed to incorporating material specimens produced by unique or specially-adapted equipment. The elastic moduli were measured in flexure, stress–strain characteristics were measured in tensile deformation, and fatigue strengths were measured in fully reversed bending. The effects of fabrication orientation, surface polishing, and hot isostatic pressing upon mechanical behavior were studied. The fatigue strengths exhibited by SLM AlSi10Mg and DMLS Ti6Al4V in the as-fabricated condition proved to be significantly inferior to that of conventional material. These lower fatigue strengths are a consequence of multiple fatigue cracks initiating at surface defects, internal voids and microcracks, and growing simultaneously during cyclic loading. Measured fatigue strengths of DMLS 316L and 17-4PH approached those of corresponding wrought materials when subjected to principal stresses aligned with the build planes. When cyclic stresses were applied across the build planes of the DMLS stainless steels, fatigue fractures often developed prematurely by separation of material. Post-processing the DMLS Ti6Al4V and SS316L with hot isostatic pressure elevated the fatigue strength significantly. Measurements of surface roughness with an optical profilometer, examinations of the material microstructures, and fractography contribute to an understanding of the mechanical behavior of the additive materials.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Laser additive manufacturing of metallic components: materials, processes and mechanisms
Gu, D. D., Meiners, W., Wissenbach, K., & Poprawe, R. (2012) · International Materials Reviews · doi:10.1179/1743280411y.0000000014 · Cited by 3,197
A study of the microstructural evolution during selective laser melting of Ti–6Al–4V
Thijs, L., Verhaeghe, F., Craeghs, T., Humbeeck, J. V., & Kruth, J.-P. (2010) · Acta Materialia · doi:10.1016/j.actamat.2010.02.004 · Cited by 2,929
Vrancken, B., Thijs, L., Kruth, J.-P., & Van Humbeeck, J. (2012) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2012.07.022 · Cited by 1,896
Leuders, S., Thöne, M., Riemer, A., Niendorf, T., Tröster, T., Richard, H. A., & Maier, H. J. (2013) · International Journal of Fatigue · doi:10.1016/j.ijfatigue.2012.11.011 · Cited by 1,475
Consolidation phenomena in laser and powder-bed based layered manufacturing
Kruth, J.-P., Levy, G., Klocke, F., & Childs, T. H. C. (2007) · CIRP Annals · doi:10.1016/j.cirp.2007.10.004 · Cited by 1,444
Binding mechanisms in selective laser sintering and selective laser melting
Kruth, J., Mercelis, P., Van Vaerenbergh, J., Froyen, L., & Rombouts, M. (2005) · Rapid Prototyping Journal · doi:10.1108/13552540510573365 · Cited by 1,383
Reducing porosity in AlSi10Mg parts processed by selective laser melting
Aboulkhair, N. T., Everitt, N. M., Ashcroft, I., & Tuck, C. (2014) · Additive Manufacturing · doi:10.1016/j.addma.2014.08.001 · Cited by 1,281
Brandl, E., Heckenberger, U., Holzinger, V., & Buchbinder, D. (2012) · Materials & Design · doi:10.1016/j.matdes.2011.07.067 · Cited by 1,151
Fatigue performance evaluation of selective laser melted Ti–6Al–4V
Edwards, P., & Ramulu, M. (2014) · Materials Science and Engineering: A · doi:10.1016/j.msea.2014.01.041 · Cited by 874
Mechanical Properties of AlSi10Mg Produced by Selective Laser Melting
Kempen, K., Thijs, L., Van Humbeeck, J., & Kruth, J.-P. (2012) · Physics Procedia · doi:10.1016/j.phpro.2012.10.059 · Cited by 849
Qiu, C., Adkins, N. J. E., & Attallah, M. M. (2013) · Materials Science and Engineering: A · doi:10.1016/j.msea.2013.04.099 · Cited by 821
On the fatigue crack growth behavior in 316L stainless steel manufactured by selective laser melting
Riemer, A., Leuders, S., Thöne, M., Richard, H. A., Tröster, T., & Niendorf, T. (2014) · Engineering Fracture Mechanics · doi:10.1016/j.engfracmech.2014.03.008 · Cited by 669
High Power Selective Laser Melting (HP SLM) of Aluminum Parts
Buchbinder, D., Schleifenbaum, H., Heidrich, S., Meiners, W., & Bültmann, J. (2011) · Physics Procedia · doi:10.1016/j.phpro.2011.03.035 · Cited by 666
Direct selective laser sintering of metals
Agarwala, M., Bourell, D., Beaman, J., Marcus, H., & Barlow, J. (1995) · Rapid Prototyping Journal · doi:10.1108/13552549510078113 · Cited by 571
Ductility of a Ti‐6Al‐4V alloy produced by selective laser melting of prealloyed powders
Facchini, L., Magalini, E., Robotti, P., Molinari, A., Höges, S., & Wissenbach, K. (2010) · Rapid Prototyping Journal · doi:10.1108/13552541011083371 · Cited by 512
Fatigue performance of additive manufactured metallic parts
Spierings, A. B., Starr, T. L., & Wegener, K. (2013) · Rapid Prototyping Journal · doi:10.1108/13552541311302932 · Cited by 426
Microstructures and Properties of 17-4 PH Stainless Steel Fabricated by Selective Laser Melting
Murr, L. E., Martinez, E., Hernandez, J., Collins, S., Amato, K. N., Gaytan, S. M., & Shindo, P. W. (2012) · Journal of Materials Research and Technology · doi:10.1016/s2238-7854(12)70029-7 · Cited by 425
Rafi, H. K., Starr, T. L., & Stucker, B. E. (2013) · The International Journal of Advanced Manufacturing Technology · doi:10.1007/s00170-013-5106-7 · Cited by 335
Chan, K. S., Koike, M., Mason, R. L., & Okabe, T. (2013) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-012-1470-4 · Cited by 320
Liu, Q. C., Elambasseril, J., Sun, S. J., Leary, M., Brandt, M., & Sharp, P. K. (2014) · Advanced Materials Research · doi:10.4028/www.scientific.net/amr.891-892.1519 · Cited by 201
Microstructure of additive layer manufactured Ti–6Al–4V after exceptional post heat treatments
Brandl, E., & Greitemeier, D. (2012) · Materials Letters · doi:10.1016/j.matlet.2012.04.116 · Cited by 121
On the Determination of Fatigue Properties of Ti6Al4V Produced by Selective Laser Melting
Hooreweder, B. V., Boonen, R., Moens, D., Kruth, J., & Sas, P. (2012) · AIAA/ASME/ASCE/AHS/ASC Structures, Structural Dynamics, and Materials Conference (SDM) · doi:10.2514/6.2012-1733 · Cited by 51
Rekedal, K. D., & Liu, D. (2015) · CRC Press eBooks · doi:10.1201/9781003537762-33 · Cited by 46
Cited by
Additive manufacturing of metallic components – Process, structure and properties
DebRoy, T., Wei, H. L., Zuback, J. S., Mukherjee, T., Elmer, J. W., Milewski, J. O., Beese, A. M., Wilson-Heid, A., De, A., & Zhang, W. (2018) · Progress in Materials Science · doi:10.1016/j.pmatsci.2017.10.001 · Cited by 8,805
Additively manufactured hierarchical stainless steels with high strength and ductility
Wang, Y. M., Voisin, T., McKeown, J. T., Ye, J., Calta, N. P., Li, Z., Zeng, Z., Zhang, Y., Chen, W., Roehling, T. T., et al. (2018) · Nature Materials · doi:10.1038/nmat5021 · Cited by 2,613
Additive manufacturing of Ti6Al4V alloy: A review
Liu, S., & Shin, Y. C. (2019) · Materials & Design · doi:10.1016/j.matdes.2018.107552 · Cited by 2,472
Aboulkhair, N. T., Simonelli, M., Parry, L., Ashcroft, I., Tuck, C., & Hague, R. (2019) · Progress in Materials Science · doi:10.1016/j.pmatsci.2019.100578 · Cited by 1,552
SLM lattice structures: Properties, performance, applications and challenges
Maconachie, T., Leary, M., Lozanovski, B., Zhang, X., Qian, M., Faruque, O., & Brandt, M. (2019) · Materials & Design · doi:10.1016/j.matdes.2019.108137 · Cited by 1,497
Metadata
- Authors
- Mower, T. M., & Long, M. J.
- Venue
- Materials Science and Engineering: A
- Publisher
- Elsevier BV
- Published
- 2016-01
- Volume
- 651
- Pages
- 198-213
- ISSN
- 0921-5093 (ISSN-L)
- OpenAlex
- W2200477759
- Cited by
- 1,001
- References
- 23
- FWCI
- 52.96
- Type
- journal article
- Language
- en
- Open access
- hybrid
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.