The DOI matches its Crossref record; 410 of the 414 references it cites were found in a registry or an index.
Degradation mechanisms of proton exchange membrane fuel cell under typical automotive operating conditions
Abstract
Abstract The proton exchange membrane (PEM) fuel cell is an ideal automotive power source with great potential, owing to its high efficiency and zero emissions. However, the durability and life-span limit its large-scale application. Complex automotive operating conditions significantly accelerate fuel cell aging, and result in diverse degradation mechanisms that require comprehensive understanding. This review focuses on three harsh conditions of open-circuit/idling, dynamic load, and startup-shutdown. In-situ and ex-situ accelerated stress tests (ASTs) for the three conditions are summarized in terms of methodology, research objectives, and conditions of application. Reversible decay may arise during ASTs and lead to an over-estimation of the aging state, of which the causes and recovery procedures are emphasized. The degradation mechanisms are elaborated systematically according to parameter characteristics, microstructure, and aging reactions. First, increased gas permeation and a high cathode potential during open-circuit/idling combine to intensify generation of free radicals that cause membrane degradation. Pt degradation and migration are also accelerated, characterized by increased Pt particle growth and precipitation in the membrane. The debate regarding the effect of Pt precipitation on membrane degradation is resolved based on a literature review. Second, dynamic load brings about changes in the thermal/humidity state, altered reactant demand, and potential cycling, which lead to mechanical degradation, gas starvation, and Pt particle growth, respectively. To account for the accelerated particle growth, electrochemical Ostwald ripening and increased Pt dissolution are reviewed. Third, an air/hydrogen boundary appears in the anode under startup-shutdown condition and causes carbon corrosion in the local cathode via the reverse current mechanism. The cathode thereby suffers from severe and non-uniform structural damage and even structural collapse, accompanied by Pt agglomeration and detachment. Meanwhile, difficulties in mass transfer arise because of ionomer redistribution, decreased porosity, and carbon surface hydrophilization. In addition, cold start produces severe damage to component structures. This paper seeks to guide further investigation into improved fuel cell durability via mechanism analysis, condition optimization, control strategy development, structural design of the membrane electrode assembly, and component material development.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“at the anode, reactive oxygen species are likely to be generated under inappropriate operation (e.g., H 2 starvation, start-up/ shut-down and reversal), leading to aggressive material degradation (e.g., membrane and ionomer) [22].”
From Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly (2023) · cites this paper as [22]
Citations
Cites
1 retracted
Taherian, R. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.04.081 · Cited by 280
RetractedElectrochemical Methods: Fundamentals and Applications
Bard, A. J., & Faulkner, L. R. (1980) · Cited by 22,436
Electrocatalyst approaches and challenges for automotive fuel cells
Debe, M. K. (2012) · Nature · doi:10.1038/nature11115 · Cited by 5,885
Dicks, A. L., & Rand, D. A. J. (2018) · Wiley eBooks · doi:10.1002/9781118706992 · Cited by 4,241
Polymer Electrolyte Fuel Cell Model
Springer, T. E., Zawodzinski, T. A., & Gottesfeld, S. (1991) · Journal of The Electrochemical Society · doi:10.1149/1.2085971 · Cited by 3,528
Scientific Aspects of Polymer Electrolyte Fuel Cell Durability and Degradation
Borup, R. L., Meyers, J. P., Pivovar, B. S., Kim, Y. S., Mukundan, R., Garland, N., Myers, D. J., Wilson, M. S., Garzón, F. H., Wood, D. L., et al. (2007) · Chemical Reviews · doi:10.1021/cr050182l · Cited by 3,492
A review of PEM fuel cell durability: Degradation mechanisms and mitigation strategies
Wu, J., Yuan, X. Z., Martin, J. J., Wang, H., Zhang, J., Shen, J., Wu, S., & Merida, W. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.06.006 · Cited by 1,587
Sintering of Catalytic Nanoparticles: Particle Migration or Ostwald Ripening?
Hansen, T. W., Delariva, A. T., Challa, S. R., & Datye, A. K. (2013) · Accounts of Chemical Research · doi:10.1021/ar3002427 · Cited by 1,513
Instability of Pt∕C Electrocatalysts in Proton Exchange Membrane Fuel Cells
Ferreira, P. J., la O’, G. J., Shao‐Horn, Y., Morgan, D. D., Makharia, R. R., Kocha, S. S., & Gasteiger, H. A. (2005) · Journal of The Electrochemical Society · doi:10.1149/1.2050347 · Cited by 1,492
Water transport in polymer electrolyte membrane fuel cells
Jiao, K., & Li, X. (2011) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2010.06.002 · Cited by 1,086
Review: Durability and Degradation Issues of PEM Fuel Cell Components
de Bruijn, F. A., Dam, V. A. T., & Janssen, G. J. M. (2008) · Fuel Cells · doi:10.1002/fuce.200700053 · Cited by 998
A Reverse-Current Decay Mechanism for Fuel Cells
Reiser, C., Bregoli, L. J., Patterson, T. W., Yi, J. S., Yang, J., Perry, M. L., & Jarvi, T. D. (2005) · Electrochemical and Solid-State Letters · doi:10.1149/1.1896466 · Cited by 977
Instability of Supported Platinum Nanoparticles in Low-Temperature Fuel Cells
Shao‐Horn, Y., Sheng, W., Chen, S., Ferreira, P. J., Holby, E. F., & Morgan, D. D. (2007) · Topics in Catalysis · doi:10.1007/s11244-007-9000-0 · Cited by 941
Sui, S., Wang, X., Zhou, X., Su, Y., Riffat, S., & Liu, C.-J. (2017) · Journal of Materials Chemistry A · doi:10.1039/c6ta08580f · Cited by 916
A review of the main parameters influencing long-term performance and durability of PEM fuel cells
Schmittinger, W., & Vahidi, A. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.01.070 · Cited by 820
A review on production, storage of hydrogen and its utilization as an energy resource
Dutta, S. (2014) · Journal of Industrial and Engineering Chemistry · doi:10.1016/j.jiec.2013.07.037 · Cited by 797
Advanced materials for improved PEMFC performance and life
Curtin, D. E., Lousenberg, R. D., Henry, T. J., Tangeman, P. C., & Tisack, M. E. (2004) · Journal of Power Sources · doi:10.1016/j.jpowsour.2004.01.023 · Cited by 786
Carbon support oxidation in PEM fuel cell cathodes
Maass, S., Finsterwalder, F., Frank, G. T., Hartmann, R., & Merten, C. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.08.053 · Cited by 743
Hydrogen: Trends, production and characterization of the main process worldwide
Veras, T. D. S., Mozer, T. S., dos Santos, D. D. C. R. M., & César, A. D. S. (2016) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2016.08.219 · Cited by 740
Electrocatalytic Corrosion of Carbon Support in PEMFC Cathodes
Roen, L. M., Paik, C. H., & Jarvi, T. D. (2003) · Electrochemical and Solid-State Letters · doi:10.1149/1.1630412 · Cited by 691
Kinetic Model of Platinum Dissolution in PEMFCs
Darling, R. M., & Meyers, J. P. (2003) · Journal of The Electrochemical Society · doi:10.1149/1.1613669 · Cited by 688
A review of platinum-based catalyst layer degradation in proton exchange membrane fuel cells
Zhang, S., Yuan, X., Hin, J. N. C., Wang, H., Friedrich, K. A., & Schulze, M. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.06.073 · Cited by 664
Characterization of Vulcan Electrochemically Oxidized under Simulated PEM Fuel Cell Conditions
Kangasniemi, K., Condit, D. A., & Jarvi, T. D. (2004) · Journal of The Electrochemical Society · doi:10.1149/1.1649756 · Cited by 624
Pei, P., & Chen, H. (2014) · Applied Energy · doi:10.1016/j.apenergy.2014.03.048 · Cited by 619
Self-citationGas crossover and membrane degradation in polymer electrolyte fuel cells
Inaba, M., Kinumoto, T., Kiriake, M., Umebayashi, R., Tasaka, A., & Ogumi, Z. (2006) · Electrochimica Acta · doi:10.1016/j.electacta.2006.03.008 · Cited by 614
A Critical Review of Modeling Transport Phenomena in Polymer-Electrolyte Fuel Cells
Weber, A. Z., Borup, R. L., Darling, R. M., Das, P. K., Dursch, T. J., Gu, W., Harvey, D., Kusoglu, A., Litster, S., Mench, M. M., et al. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0751412jes · Cited by 612
Kilic, M. S., Bazant, M. Z., & Ajdari, A. (2007) · Physical Review E · doi:10.1103/physreve.75.021503 · Cited by 600
Degradation Mechanisms of Pt/C Fuel Cell Catalysts under Simulated Start–Stop Conditions
Meier, J. C., Galeano, C., Katsounaros, I., Topalov, A. A., Kostka, A., Schüth, F., & Mayrhofer, K. J. J. (2012) · ACS Catalysis · doi:10.1021/cs300024h · Cited by 586
Design criteria for stable Pt/C fuel cell catalysts
Meier, J. C., Galeano, C., Katsounaros, I., Witte, J., Bongard, H. J., Topalov, A. A., Baldizzone, C., Mezzavilla, S., Schüth, F., & Mayrhofer, K. J. J. (2014) · Beilstein Journal of Nanotechnology · doi:10.3762/bjnano.5.5 · Cited by 559
Analysis of electrocatalyst degradation in PEMFC caused by cell reversal during fuel starvation
Taniguchi, A., Akita, T., Yasuda, K., & Miyazaki, Y. (2004) · Journal of Power Sources · doi:10.1016/j.jpowsour.2003.12.035 · Cited by 525
A review of accelerated stress tests of MEA durability in PEM fuel cells
ZHANG, S., YUAN, X., WANG, H., MERIDA, W., ZHU, H., SHEN, J., WU, S., & ZHANG, J. (2009) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2008.10.012 · Cited by 525
A quick evaluating method for automotive fuel cell lifetime
PEI, P., Chang, Q., & TANG, T. (2008) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2008.04.048 · Cited by 518
Self-citationPEM fuel cell cathode carbon corrosion due to the formation of air/fuel boundary at the anode
Tang, H., Qi, Z., Ramani, M., & Elter, J. F. (2005) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.10.059 · Cited by 490
Lifetime prediction and the economic lifetime of Proton Exchange Membrane fuel cells
Chen, H., Pei, P., & Song, M. (2015) · Applied Energy · doi:10.1016/j.apenergy.2014.12.062 · Cited by 477
Self-citationTowards a comprehensive understanding of platinum dissolution in acidic media
Topalov, A. A., Cherevko, S., Žeradjanin, A. R., Meier, J. C., Katsounaros, I., & Mayrhofer, K. J. J. (2013) · Chemical Science · doi:10.1039/c3sc52411f · Cited by 473
Zhao, J. F., & Li, X. (2019) · Energy Conversion and Management · doi:10.1016/j.enconman.2019.112022 · Cited by 449
Zatoń, M., Rozière, J., & Jones, D. J. (2017) · Sustainable Energy & Fuels · doi:10.1039/c7se00038c · Cited by 435
Castanheira, L., da Silva, W. O., Lima, F. H. B., Crisci, A., Dubau, L., & Maillard, F. M. (2015) · ACS Catalysis · doi:10.1021/cs501973j · Cited by 432
Dissolution of Platinum: Limits for the Deployment of Electrochemical Energy Conversion?
Topalov, A. A., Katsounaros, I., Auinger, M., Cherevko, S., Meier, J. C., Klemm, S. O., & Mayrhofer, K. J. J. (2012) · Angewandte Chemie International Edition · doi:10.1002/anie.201207256 · Cited by 429
Zhang, T., Wang, P., Chen, H., & Pei, P. (2018) · Applied Energy · doi:10.1016/j.apenergy.2018.04.049 · Cited by 420
Self-citationNafion degradation in PEFCs from end plate iron contamination
Pozio, A., Silva, R. F., Francesco, M. D., & Giorgi, L. (2003) · Electrochimica Acta · doi:10.1016/s0013-4686(03)00026-4 · Cited by 418
Polymer Electrolyte Fuel Cell Durability
Büchi, F. N., Inaba, M., & Schmidt, T. J. (2009) · Springer eBooks · doi:10.1007/978-0-387-85536-3 · Cited by 407
Rodgers, M. P., Bonville, L. J., Kunz, H. R., Slattery, D. K., & Fenton, J. M. (2012) · Chemical Reviews · doi:10.1021/cr200424d · Cited by 398
Durability of platinum-based fuel cell electrocatalysts: Dissolution of bulk and nanoscale platinum
Cherevko, S., Kulyk, N., & Mayrhofer, K. J. J. (2016) · Nano Energy · doi:10.1016/j.nanoen.2016.03.005 · Cited by 386
Diagnostic tools in PEM fuel cell research: Part I Electrochemical techniques
Wu, J., Yuan, X., WANG, H., BLANCO, M., MARTIN, J., & Zhang, J. J. (2008) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2008.01.013 · Cited by 381
Yasuda, K., Taniguchi, A., Akita, T., Ioroi, T., & Siroma, Z. (2005) · Physical Chemistry Chemical Physics · doi:10.1039/b514342j · Cited by 376
Cold start of proton exchange membrane fuel cell
Luo, Y., & Jiao, K. (2017) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2017.10.003 · Cited by 363
Radical (HO • , H • and HOO • ) Formation and Ionomer Degradation in Polymer Electrolyte Fuel Cells
Gubler, L., Dockheer, S. M., & Koppenol, W. H. (2011) · Journal of The Electrochemical Society · doi:10.1149/1.3581040 · Cited by 359
Fuel cell catalyst degradation on the nanoscale
Mayrhofer, K. J. J., Meier, J. C., Ashton, S., Wiberg, G. K. H., Kraus, F., Hanzlik, M., & Arenz, M. (2008) · Electrochemistry Communications · doi:10.1016/j.elecom.2008.05.032 · Cited by 358
Theory and simulation of Ostwald ripening
Yao, J. H., Elder, K. R., Hong, G., & Grant, M. (1993) · Physical review. B, Condensed matter · doi:10.1103/physrevb.47.14110 · Cited by 358
A review of polymer electrolyte membrane fuel cell durability test protocols
Yuan, X., Li, H., Zhang, S., Martin, J. J., & Wang, H. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2011.07.082 · Cited by 357
Effect of Voltage on Platinum Dissolution
Wang, X. P., Kumar, R., & Myers, D. J. (2006) · Electrochemical and Solid-State Letters · doi:10.1149/1.2180536 · Cited by 349
Multi-phase models for water and thermal management of proton exchange membrane fuel cell: A review
Zhang, G., & Jiao, K. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.04.071 · Cited by 347
Chen, H., Zhao, X. Y., Zhang, T., & Pei, P. (2019) · Energy Conversion and Management · doi:10.1016/j.enconman.2018.12.049 · Cited by 346
Self-citationCarbon Corrosion in PEM Fuel Cells and the Development of Accelerated Stress Tests
Macauley, N., Papadias, D. D., Fairweather, J. D., Spernjak, D., Langlois, D. A., Ahluwalia, R., More, K. L., Mukundan, R., & Borup, R. L. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0061806jes · Cited by 346
Ohma, A., Shinohara, K., Iiyama, A., Yoshida, T., & Daimaru, A. (2011) · ECS Transactions · doi:10.1149/1.3635611 · Cited by 341
Degradations analysis and aging modeling for health assessment and prognostics of PEMFC
Jouin, M., Gouriveau, R., Hissel, D., Péra, M., & Noureddine Zerhouni, A. (2015) · Reliability Engineering & System Safety · doi:10.1016/j.ress.2015.12.003 · Cited by 340
Holby, E. F., Sheng, W., Shao‐Horn, Y., & Morgan, D. D. (2009) · Energy & Environmental Science · doi:10.1039/b821622n · Cited by 337
Park, J., Oh, H., Ha, T., Lee, Y., & Min, K. (2015) · Applied Energy · doi:10.1016/j.apenergy.2015.06.068 · Cited by 334
Extended Kalman Filter for prognostic of Proton Exchange Membrane Fuel Cell
Bressel, M., Hilairet, M., Hissel, D., & Bouamama, B. O. (2015) · Applied Energy · doi:10.1016/j.apenergy.2015.11.071 · Cited by 331
Degradation Study of MEA for PEMFCs under Low Humidity Conditions
Endoh, E., Terazono, S., Widjaja, H., & Takimoto, Y. (2004) · Electrochemical and Solid-State Letters · doi:10.1149/1.1739314 · Cited by 321
Yu, Y., Li, H., Wang, H., Yuan, X., Wang, G., & Pan, M. (2012) · Journal of Power Sources · doi:10.1016/j.jpowsour.2012.01.059 · Cited by 313
Electrochemical Ostwald Ripening of Colloidal Ag Particles on Conductive Substrates
Redmond, P. L., Hallock, A. J., & Brus, L. E. (2004) · Nano Letters · doi:10.1021/nl048204r · Cited by 308
Sustainable development of road transportation sector using hydrogen energy system
Salvi, B. L., & Subramanian, K. A. (2015) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2015.07.030 · Cited by 294
Hu, Z., Li, J., Xu, L., Song, Z., Fang, C., Ouyang, M., Dou, G. W., & Kou, G. (2016) · Energy Conversion and Management · doi:10.1016/j.enconman.2016.09.082 · Cited by 288
Kusoglu, A., Karlsson, A. M., Santare, M. H., Cleghorn, S., & Johnson, W. B. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.03.063 · Cited by 276
A review on prognostics and health monitoring of proton exchange membrane fuel cell
Sutharssan, T., Montalvão, D., Chen, Y., Wang, W.-C., Pisac, C., & Elemara, H. (2016) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2016.11.009 · Cited by 272
Barriers of scaling-up fuel cells: Cost, durability and reliability
Wang, J. (2014) · Energy · doi:10.1016/j.energy.2014.12.007 · Cited by 263
Effect of sub-freezing temperatures on a PEM fuel cell performance, startup and fuel cell components
Yan, Q., Toghiani, H., Lee, Y.-W., Liang, K., & Causey, H. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.02.075 · Cited by 263
Analysis of the control strategies for fuel saving in the hydrogen fuel cell vehicles
Hameş, Y., Kaya, K., Baltacıoğlu, E., & Türksoy, A. (2018) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2017.12.150 · Cited by 260
Detection of Pt[sup z+] Ions and Pt Nanoparticles Inside the Membrane of a Used PEMFC
Guilminot, É., Corcella, A., Charlot, F., Maillard, F. M., & Chatenet, M. (2006) · Journal of The Electrochemical Society · doi:10.1149/1.2388863 · Cited by 250
PEM Fuel Cell Pt∕C Dissolution and Deposition in Nafion Electrolyte
Bi, W., Gray, G. E., & Fuller, T. F. (2007) · Electrochemical and Solid-State Letters · doi:10.1149/1.2712796 · Cited by 247
PEM fuel cell open circuit voltage (OCV) in the temperature range of 23°C to 120°C
Zhang, J., Tang, Y., Song, C., Zhang, J. J., & Wang, H. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.09.026 · Cited by 246
Ostwald ripening in a Pt/SiO2 model catalyst studied by in situ TEM
Simonsen, S. B., Chorkendorff, I., Dahl, S., Skoglundh, M., Sehested, J., & Helveg, S. (2011) · Journal of Catalysis · doi:10.1016/j.jcat.2011.04.011 · Cited by 243
Zhang, G., & Jiao, K. (2018) · Energy Conversion and Management · doi:10.1016/j.enconman.2018.09.031 · Cited by 242
Carbon nanotube architectures as catalyst supports for proton exchange membrane fuel cells
Zhang, W., Sherrell, P. C., Minett, A. I., Razal, J. M., & Chen, J. (2010) · Energy & Environmental Science · doi:10.1039/c0ee00139b · Cited by 236
Analysis of degradation in PEMFC caused by cell reversal during air starvation
Taniguchi, A., Akita, T., Yasuda, K., & MIYAZAKI, Y. (2008) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2008.02.049 · Cited by 233
Damage to the Cathode Catalyst of a PEM Fuel Cell Caused by Localized Fuel Starvation
Patterson, T. W., & Darling, R. M. (2006) · Electrochemical and Solid-State Letters · doi:10.1149/1.2167930 · Cited by 232
Effect of Agglomeration of Pt/C Catalyst on Hydrogen Peroxide Formation
Inaba, M., Yamada, H., Tokunaga, J., & Tasaka, A. (2004) · Electrochemical and Solid-State Letters · doi:10.1149/1.1814595 · Cited by 232
3D Imaging of Catalyst Support Corrosion in Polymer Electrolyte Fuel Cells
Schulenburg, H., Schwanitz, B., Linse, N., Scherer, G. G., Wokaun, A. J., Krbanjevic, J., Grothausmann, R., & Manke, I. (2011) · The Journal of Physical Chemistry C · doi:10.1021/jp203016u · Cited by 230
Effect of contaminants on polymer electrolyte membrane fuel cells
Zamel, N., & Li, X. (2010) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2010.06.003 · Cited by 226
Electrocatalysts for PEM Fuel Cells
Ioroi, T., Siroma, Z., Yamazaki, S., & Yasuda, K. (2018) · Advanced Energy Materials · doi:10.1002/aenm.201801284 · Cited by 226
Ghassemzadeh, L., Kreuer, K., Maier, J., & Müller, K. (2010) · The Journal of Physical Chemistry C · doi:10.1021/jp102533v · Cited by 224
A review of durability test protocols of the proton exchange membrane fuel cells for vehicle
Chen, H., Song, Z. Y., Zhao, X. Y., Zhang, T., Pei, P., & Liang, C. (2018) · Applied Energy · doi:10.1016/j.apenergy.2018.04.050 · Cited by 217
Self-citationMulti-phase simulation of proton exchange membrane fuel cell with 3D fine mesh flow field
Zhang, G., Xie, B., Bao, Z., Niu, Z., & Jiao, K. (2018) · International Journal of Energy Research · doi:10.1002/er.4215 · Cited by 214
Membrane and Active Layer Degradation upon PEMFC Steady-State Operation
Guilminot, É., Corcella, A., Chatenet, M., Maillard, F. M., Charlot, F., Berthomé, G., Iojoiu, C., Sanchez, J., Rossinot, E., & Claude, E. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2775218 · Cited by 211
Statistic analysis of operational influences on the cold start behaviour of PEM fuel cells
Oszcipok, M., Riemann, D., Kronenwett, U., Kreideweis, M., & Zedda, M. (2005) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.02.058 · Cited by 210
Qiu, D., Peng, L., Lai, X., Ni, M., & Lehnert, W. (2019) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2019.109289 · Cited by 208
In Situ Detection of Hydrogen Peroxide in PEM Fuel Cells
Liu, W., & Zuckerbrod, D. (2005) · Journal of The Electrochemical Society · doi:10.1149/1.1904988 · Cited by 206
Speder, J., Zana, A., Spanos, I., Kirkensgaard, J. J. K., Mortensen, K., Hanzlik, M., & Arenz, M. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.03.039 · Cited by 204
The Impact of Carbon Stability on PEM Fuel Cell Startup and Shutdown Voltage Degradation
Yu, P. T., Gu, W., Makharia, R. R., Wagner, F. T., & Gasteiger, H. A. (2006) · ECS Transactions · doi:10.1149/1.2356199 · Cited by 201
Surface oxidation of carbon supports due to potential cycling under PEM fuel cell conditions
Avasarala, B., Moore, R., & Haldar, P. (2010) · Electrochimica Acta · doi:10.1016/j.electacta.2010.03.056 · Cited by 196
Large-scale multi-phase simulation of proton exchange membrane fuel cell
Zhang, G., Xie, X., Xie, B., Du, Q., & Jiao, K. (2019) · International Journal of Heat and Mass Transfer · doi:10.1016/j.ijheatmasstransfer.2018.10.122 · Cited by 196
Characterizing the Structural Degradation in a PEMFC Cathode Catalyst Layer: Carbon Corrosion
Young, A. P., Stumper, J., & Gyenge, E. L. (2009) · Journal of The Electrochemical Society · doi:10.1149/1.3139963 · Cited by 194
Physical Theory of Platinum Nanoparticle Dissolution in Polymer Electrolyte Fuel Cells
Rinaldo, S. G., Stumper, J., & Eikerling, M. H. (2010) · The Journal of Physical Chemistry C · doi:10.1021/jp9101509 · Cited by 185
System integration, durability and reliability of fuel cells: Challenges and solutions
Wang, J. (2016) · Applied Energy · doi:10.1016/j.apenergy.2016.12.083 · Cited by 185
Effect of Relative Humidity on Oxygen Reduction Kinetics in a PEMFC
Neyerlin, K. C., Gasteiger, H. A., Mittelsteadt, C. K., Jorné, J., & Gu, W. (2005) · Journal of The Electrochemical Society · doi:10.1149/1.1897368 · Cited by 183
Cathode Loading Impact on Voltage Cycling Induced PEMFC Degradation: A Voltage Loss Analysis
Harzer, G. S., Schwämmlein, J. N., Damjanović, A. M., Ghosh, S., & Gasteiger, H. A. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0161806jes · Cited by 182
In Situ and Operando Characterization of Proton Exchange Membrane Fuel Cells
Meyer, Q. P.-G., Zeng, Y., & Zhao, C. (2019) · Advanced Materials · doi:10.1002/adma.201901900 · Cited by 182
Effect of Hydrogen and Oxygen Partial Pressure on Pt Precipitation within the Membrane of PEMFCs
Zhang, J., Litteer, B. A., Gu, W., Liu, H., & Gasteiger, H. A. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2764240 · Cited by 180
Yan, X. C., Hou, M., Sun, L., LIANG, D., SHEN, Q., Xu, H., Ming, P., & Yi, B. (2007) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2007.06.024 · Cited by 180
A review on water fault diagnosis of PEMFC associated with the pressure drop
Pei, P., Li, Y., Xu, H., & Wu, Z. (2016) · Applied Energy · doi:10.1016/j.apenergy.2016.04.064 · Cited by 179
Self-citationRecent Advances in Catalyst Accelerated Stress Tests for Polymer Electrolyte Membrane Fuel Cells
Stariha, S. A., Macauley, N., Sneed, B. T., Langlois, D. A., More, K. L., Mukundan, R., & Borup, R. L. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0881807jes · Cited by 179
Reversible and irreversible degradation in fuel cells during Open Circuit Voltage durability testing
Kundu, S., Fowler, M. W., Simon, L. C., & Abouatallah, R. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.04.009 · Cited by 175
Kim, S., & Mench, M. M. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.08.111 · Cited by 175
Durst, J., Lamibrac, A., Charlot, F., Dillet, J., Castanheira, L., Maranzana, G., Dubau, L., Maillard, F. M., Chatenet, M., & Lottin, O. (2013) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2013.03.021 · Cited by 173
Danilczuk, M., Coms, F. D., & Schlick, S. (2009) · The Journal of Physical Chemistry B · doi:10.1021/jp901597f · Cited by 172
The effect of humidity and oxygen partial pressure on degradation of Pt/C catalyst in PEM fuel cell
Bi, W., Sun, Q., Deng, Y., & Fuller, T. F. (2008) · Electrochimica Acta · doi:10.1016/j.electacta.2008.10.008 · Cited by 167
Liang, D. S., Shen, Q., Hou, M., Shao, Z., & Yi, B. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.06.059 · Cited by 161
Modeling of PEM fuel cell Pt/C catalyst degradation
Bi, W., & Fuller, T. F. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.12.007 · Cited by 160
Kim, J., Lee, J., & Tak, Y. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.03.039 · Cited by 156
The effect of platinum on carbon corrosion behavior in polymer electrolyte fuel cells
Linse, N., Gubler, L., Scherer, G. G., & Wokaun, A. J. (2011) · Electrochimica Acta · doi:10.1016/j.electacta.2011.06.093 · Cited by 155
Kim, S., Ahn, B. K., & Mench, M. M. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.12.114 · Cited by 154
Zhou, D., Al‐Durra, A., Zhang, K., Ravey, A., & Gao, F. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.06.098 · Cited by 154
Degradation prediction of PEM fuel cell using a moving window based hybrid prognostic approach
Zhou, D., Gao, F., Breaz, E., Ravey, A., & Miraoui, A. (2017) · Energy · doi:10.1016/j.energy.2017.07.096 · Cited by 154
Wu, B., Zhao, M., Shi, W., Liu, W., Liu, J., Xing, D., Yao, Y., Hou, Z., Ming, P., Gu, J., et al. (2014) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2014.02.142 · Cited by 153
Ghassemzadeh, L., Peckham, T. J., Weissbach, T., Luo, X., & Holdcroft, S. (2013) · Journal of the American Chemical Society · doi:10.1021/ja408032p · Cited by 153
Proton Exchange Membrane Fuel Cell Reversal: A Review
Qin, C., Wang, J., Yang, D., Li, B., & Zhang, C. (2016) · Catalysts · doi:10.3390/catal6120197 · Cited by 152
Zhang, G., Yuan, H. S., Wang, Y., & Jiao, K. (2019) · Applied Energy · doi:10.1016/j.apenergy.2019.113865 · Cited by 152
Mukundan, R., Baker, A. M., Kusoglu, A., Beattie, P. D., Knights, S., Weber, A. Z., & Borup, R. L. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0101806jes · Cited by 149
Wilberforce, T., Ijaodola, O., Ogungbemi, E., Khatib, F. N., Leslie, T., El-Hassan, Z., Thomposon, J., & Olabi, A. G. (2019) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2019.109286 · Cited by 147
Javed, K., Gouriveau, R., Noureddine Zerhouni, A., & Hissel, D. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.05.092 · Cited by 143
Akita, T., Taniguchi, A., Maekawa, J., Siroma, Z., Tanaka, K., Kohyama, M., & Yasuda, K. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.10.111 · Cited by 142
Proton exchange membrane fuel cell ageing forecasting algorithm based on Echo State Network
Morando, S., Jemeï, S., Hissel, D., Gouriveau, R., & Noureddine Zerhouni, A. (2016) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2016.05.286 · Cited by 140
Electrochemical Ostwald ripening of Pt and Ag catalysts supported on carbon
Parthasarathy, P., & Virkar, A. V. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.01.115 · Cited by 139
Load profile based empirical model for the lifetime prediction of an automotive PEM fuel cell
Zhang, X., Yang, D., Luo, M., & Dong, Z. (2017) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2017.02.146 · Cited by 139
Particle-size effect of Pt cathode catalysts on durability in fuel cells
Yano, H., Watanabe, M., Iiyama, A., & Uchida, H. (2016) · Nano Energy · doi:10.1016/j.nanoen.2016.02.016 · Cited by 135
Effect of operating conditions on carbon corrosion in polymer electrolyte membrane fuel cells
Lim, K. H., Oh, H., Jang, S.-E., Ko, Y., Kim, H.-J., & Kim, H. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.04.006 · Cited by 134
Oxygen starvation analysis during air feeding faults in PEMFC
Gérard, M., Poirot-Crouvezier, J.-P., Hissel, D., & Péra, M. (2010) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2010.08.028 · Cited by 134
Is H[sub 2]O[sub 2] Involved in the Membrane Degradation Mechanism in PEMFC?
Mittal, V. O., Kunz, H. R., & Fenton, J. M. (2006) · Electrochemical and Solid-State Letters · doi:10.1149/1.2192696 · Cited by 133
Mechanism of Catalyst Degradation in Proton Exchange Membrane Fuel Cells
Virkar, A. V., & Zhou, Y. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2722563 · Cited by 133
Dissolution Mechanism of Platinum in Sulfuric Acid Solution
Sugawara, Y., Okayasu, T., Yadav, A. P., Nishikata, A., & Tsuru, T. (2012) · Journal of The Electrochemical Society · doi:10.1149/2.017212jes · Cited by 133
Proton exchange membrane fuel cell degradation under close to open-circuit conditions
Wu, J., Yuan, X., Martin, J. J., Wang, H., Yang, D., Qiao, J., & Ma, J. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.08.095 · Cited by 131
Jovanovič, P., Pavlišič, A., Šelih, V. S., Šala, M., Hodnik, N., Bele, M., Hočevar, S. B., & Gaberšček, M. (2013) · ChemCatChem · doi:10.1002/cctc.201300936 · Cited by 131
Wong, K. H., & Kjeang, E. (2015) · ChemSusChem · doi:10.1002/cssc.201402957 · Cited by 131
Study on the processes of start-up and shutdown in proton exchange membrane fuel cells
Shen, Q., Hou, M., Liang, D. S., Zhou, Z., Li, X., Shao, Z., & Yi, B. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.12.075 · Cited by 129
Pei, P., Ren, P., Li, Y., Wu, Z., Chen, D., Huang, S., & Jia, X. (2018) · Applied Energy · doi:10.1016/j.apenergy.2018.11.005 · Cited by 128
Self-citationDegradation mechanism of electrocatalyst during long-term operation of PEMFC
Chung, C. G., Kim, L. C., Sung, Y. W., Lee, J., & Chung, J. S. (2009) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2009.08.094 · Cited by 127
Decomposition mechanism of perfluorosulfonic acid electrolyte in polymer electrolyte fuel cells
Aoki, M., Uchida, H., & Watanabe, M. (2006) · Electrochemistry Communications · doi:10.1016/j.elecom.2006.07.017 · Cited by 127
Yuan, X., Zhang, S., Wang, H., Wu, J., Sun, J. C., Hiesgen, R., Friedrich, K. A., Schulze, M., & Haug, A. (2010) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.06.023 · Cited by 127
The Impact of Cycle Profile on PEMFC Durability
Uchimura, M., & Kocha, S. S. (2007) · ECS Transactions · doi:10.1149/1.2781035 · Cited by 126
Electrocatalyst Durability under Simulated Automotive Drive Cycles
Uchimura, M., Sugawara, S., Suzuki, Y., Zhang, J., & Kocha, S. S. (2008) · ECS Transactions · doi:10.1149/1.2981858 · Cited by 125
Nanomaterials Chemistry: Recent Developments and New Directions
Rao, C. N. R., Müller, A., & Cheetham, A. K. (2007) · Nano Today · doi:10.1016/s1748-0132(07)70117-2 · Cited by 125
Membrane Degradation Behavior during Open-Circuit Voltage Hold Test
Ohma, A., Suga, S., Yamamoto, S., & Shinohara, K. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2741129 · Cited by 125
Pérez-Alonso, F. J., Elkjær, C. F., Shim, S. S., Abrams, B. L., Stephens, I. E. L., & Chorkendorff, I. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2011.03.064 · Cited by 122
3D Analysis of Fuel Cell Electrocatalyst Degradation on Alternate Carbon Supports
Sneed, B. T., Cullen, D. A., Reeves, K. S., Dyck, O., Langlois, D. A., Mukundan, R., Borup, R. L., & More, K. L. (2017) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.7b09716 · Cited by 122
Gazdzicki, P., Mitzel, J., Sánchez, D. G., Schulze, M., & Friedrich, K. A. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.07.049 · Cited by 122
Zhang, S., Yuan, X., Hin, J. N. C., Wang, H., Wu, J., Friedrich, K. A., & Schulze, M. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.08.070 · Cited by 121
Analysis of PEMFC freeze degradation at −20°C after gas purging
Hou, J., Yu, H., Zhang, S., Sun, S., Wang, H., Yi, B., & Ming, P. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.07.010 · Cited by 120
Zihrul, P., Hartung, I., Kirsch, S., Hübner, G., Hasché, F., & Gasteiger, H. A. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.0561606jes · Cited by 118
Futter, G. A., Latz, A., & Jahnke, T. (2019) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.10.085 · Cited by 118
Wang, G., Huang, F., Yu, Y., Wen, S., & Tu, Z. (2018) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2018.01.020 · Cited by 117
Accelerated durability testing via reactants relative humidity cycling on PEM fuel cells
Panha, K., Fowler, M. W., Yuan, X., & Wang, H. (2011) · Applied Energy · doi:10.1016/j.apenergy.2011.05.011 · Cited by 117
Alink, R., Gerteisen, D., & Oszcipok, M. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.03.074 · Cited by 117
Systems Strategies to Mitigate Carbon Corrosion in Fuel Cells
Perry, M. L., Patterson, T. W., & Reiser, C. (2006) · ECS Transactions · doi:10.1149/1.2356198 · Cited by 116
Membrane degradation mechanism during open-circuit voltage hold test
Ohma, A., Yamamoto, S., & Shinohara, K. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.03.078 · Cited by 116
Shao, Y., Wang, J., Kou, R., Engelhard, M., Li, B., Wang, Y., & Lin, Y. (2008) · Electrochimica Acta · doi:10.1016/j.electacta.2008.12.001 · Cited by 115
Papadias, D. D., Ahluwalia, R., Thomson, J. K., Meyer, H. M., Brady, M. P., Wang, H., Turner, J. A. A., Mukundan, R., & Borup, R. L. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.02.053 · Cited by 115
Ishigami, Y., Takada, K., Yano, H., Inukai, J., Uchida, M., Nagumo, Y., Hyakutake, T., Nishide, H., & Watanabe, M. (2010) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.11.092 · Cited by 113
Petrone, R., Hissel, D., Péra, M., Chamagne, D., & Gouriveau, R. (2015) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2015.07.026 · Cited by 113
Purge strategy optimization of proton exchange membrane fuel cell with anode recirculation
Wang, B., Deng, H., & Jiao, K. (2018) · Applied Energy · doi:10.1016/j.apenergy.2018.04.058 · Cited by 113
Zhong, D., Lin, R., Jiang, Z., Zhu, Y., Liu, D., Cai, X. L., & Chen, L. (2020) · Applied Energy · doi:10.1016/j.apenergy.2020.114626 · Cited by 113
Shen, G., Liu, J., Wu, H. B., Xu, P., Liu, F., Tongsh, C., Jiao, K., Li, J., Liu, M., Cai, M., et al. (2020) · Nature Communications · doi:10.1038/s41467-020-14822-y · Cited by 113
Effect of freeze-thaw cycles on the properties and performance of membrane-electrode assemblies
Guo, Q., & Qi, Z. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.02.093 · Cited by 112
Péron, J., Nédellec, Y., Jones, D. J., & Rozière, J. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.06.098 · Cited by 112
Platinum Dissolution and Redeposition from Pt/C Fuel Cell Electrocatalyst at Potential Cycling
Pavlišič, A., Jovanovič, P., Šelih, V. S., Šala, M., Hodnik, N., & Gaberšček, M. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0191806jes · Cited by 112
Ghassemzadeh, L., & Holdcroft, S. (2013) · Journal of the American Chemical Society · doi:10.1021/ja4037466 · Cited by 111
Huo, S., Cooper, N. J., Smith, T. L., Park, J. W., & Jiao, K. (2017) · Applied Energy · doi:10.1016/j.apenergy.2017.06.028 · Cited by 110
Improved methods to measure hydrogen crossover current in proton exchange membrane fuel cell
Pei, P., Wu, Z., Li, Y., Jia, X., Chen, D., & Huang, S. (2018) · Applied Energy · doi:10.1016/j.apenergy.2018.02.002 · Cited by 110
Self-citationWhite, R. T., Wu, A., Najm, M., Orfino, F. P., Dutta, M., & Kjeang, E. (2017) · Journal of Power Sources · doi:10.1016/j.jpowsour.2017.03.058 · Cited by 109
Takei, C., Kakinuma, K., Kawashima, K., Tashiro, K., Watanabe, M., & Uchida, M. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.05.117 · Cited by 109
Surface Platinum Electrooxidation in the Presence of Oxygen
Kongkanand, A., & Ziegelbauer, J. M. (2012) · The Journal of Physical Chemistry C · doi:10.1021/jp211490a · Cited by 108
Investigation of Platinum Oxidation in PEM Fuel Cells at Various Relative Humidities
Xu, H., Kunz, R., & Fenton, J. M. (2006) · Electrochemical and Solid-State Letters · doi:10.1149/1.2372230 · Cited by 107
30,000 h operation of a 70 kW stationary PEM fuel cell system using hydrogen from a chlorine factory
Verhage, A. J. L., Coolegem, J. F., Mulder, M. J. J., Yildirim, M. H., & de Bruijn, F. A. (2013) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2013.01.152 · Cited by 107
Effects of MEA fabrication method on durability of polymer electrolyte membrane fuel cells
Prasanna, M. D., Cho, E. A., Lim, T.-H., & Oh, I.-H. (2008) · Electrochimica Acta · doi:10.1016/j.electacta.2008.02.068 · Cited by 107
Alavijeh, A. S., Khorasany, R. M. H., Nunn, Z. R., Habisch, A., Lauritzen, M. V., Rogers, E., Wang, G. G., & Kjeang, E. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0471514jes · Cited by 107
Dynamics of electrochemical Pt dissolution at atomic and molecular levels
Lopes, P. P., Tripković, D. V., Martins, P. F. B. D., Strmcnik, D. S., Ticianelli, E. A., Stamenković, V. R., & Marković, N. M. (2017) · Journal of Electroanalytical Chemistry · doi:10.1016/j.jelechem.2017.09.047 · Cited by 107
Ren, P., Pei, P., Li, Y., Wu, Z., Chen, D., Huang, S., & Jia, X. (2019) · Applied Energy · doi:10.1016/j.apenergy.2019.01.235 · Cited by 107
Self-citationOxygen-Enhanced Dissolution of Platinum in Acidic Electrochemical Environments
Matsumoto, M., Miyazaki, T., & Imai, H. (2011) · The Journal of Physical Chemistry C · doi:10.1021/jp201959h · Cited by 105
Modeling the Effect of Chemical Membrane Degradation on PEMFC Performance
Singh, R., Sui, P. C., Wong, K. H., Kjeang, E., Knights, S., & Djilali, N. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0351806jes · Cited by 105
Ionomer Degradation in Polymer Electrolyte Membrane Fuel Cells
Young, A. P., Stumper, J., Knights, S., & Gyenge, E. L. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3281899 · Cited by 104
Behaviors of proton exchange membrane fuel cells under oxidant starvation
Dou, M., Hou, M., Liang, D., Shen, Q., Zhang, H., Lu, W., Shao, Z., & Yi, B. (2010) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.11.005 · Cited by 102
Kneer, A., Janković, J., Susac, D., Putz, A. M. V., Wagner, N., Sabharwal, M., & Secanell, M. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0271806jes · Cited by 102
Understanding the voltage reversal behavior of automotive fuel cells
Mandal, P., Hong, B. K., Oh, J., & Litster, S. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.06.083 · Cited by 102
Xie, T., & Hayden, C. A. (2007) · Polymer · doi:10.1016/j.polymer.2007.07.043 · Cited by 101
Local resolved investigation of PEMFC performance degradation mechanism during dynamic driving cycle
Jing, S., Lin, R., Xia, S., Liu, D., & Zhang, Q. Y. (2016) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2016.01.048 · Cited by 101
On-line mass spectrometry study of carbon corrosion in polymer electrolyte membrane fuel cells
Oh, H., Oh, J.-G., Haam, S., Kundu, A., Roh, B., Hwang, I.-C., & Kim, H. (2008) · Electrochemistry Communications · doi:10.1016/j.elecom.2008.05.006 · Cited by 100
Sharma, R., & Andersen, S. M. (2018) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2018.08.045 · Cited by 100
Kim, L. C., Chung, C. G., Sung, Y. W., & Chung, J. S. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.05.062 · Cited by 100
Numerical analysis of operating conditions effects on PEMFC with anode recirculation
Wang, B., Wu, K., Xi, F., Xuan, J., Xie, X. L., Wang, X., & Jiao, K. (2019) · Energy · doi:10.1016/j.energy.2019.02.115 · Cited by 100
Robin, C., Gérard, M., Quinaud, M., d'Arbigny, J. B., & Bultel, Y. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.07.018 · Cited by 98
Spernjak, D., Fairweather, J. D., Mukundan, R., Rockward, T., & Borup, R. L. (2012) · Journal of Power Sources · doi:10.1016/j.jpowsour.2012.04.086 · Cited by 96
Degradation forecast for PEMFC cathode-catalysts under cyclic loads
Moein‐Jahromi, M., Kermani, M. J., & Movahed, S. (2017) · Journal of Power Sources · doi:10.1016/j.jpowsour.2017.05.102 · Cited by 96
Meyer, Q. P.-G., Zeng, Y., & Zhao, C. (2019) · Journal of Power Sources · doi:10.1016/j.jpowsour.2019.226922 · Cited by 96
Investigation of the effect of micro-porous layer on PEM fuel cell cold start operation
Xie, X. L., Wang, R., Jiao, K., Zhang, G., Zhou, J., & Du, Q. (2017) · Renewable Energy · doi:10.1016/j.renene.2017.10.039 · Cited by 96
Wang, C., Wang, S., Peng, L., Zhang, J., Shao, Z., Huang, J., Sun, C., Ouyang, M., & He, X. (2016) · Energies · doi:10.3390/en9080603 · Cited by 95
Alavijeh, A. S., Goulet, M., Khorasany, R. M. H., Ghataurah, J., Lim, C. K., Lauritzen, M. V., Kjeang, E., Wang, G. G., & Rajapakse, R. K. N. D. (2014) · Fuel Cells · doi:10.1002/fuce.201400040 · Cited by 95
Dillet, J., Spernjak, D., Lamibrac, A., Maranzana, G., Mukundan, R., Fairweather, J. D., Didierjean, S., Borup, R. L., & Lottin, O. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.10.141 · Cited by 93
Proton exchange membrane fuel cell degradation and testing: review
El-Kharouf, A., Chandan, A., Hattenberger, M., & Pollet, B. G. (2012) · Journal of the Energy Institute · doi:10.1179/1743967112z.00000000036 · Cited by 92
Qu, S., Li, X., Hou, M., Shao, Z., & Yi, B. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.06.080 · Cited by 91
Flagged first, then by citations
4 of the 414 references couldn’t be matched to a known paper.
Research works printed but not linked: 4
- WolfVielstich, ArnoldLamm, Gasteiger H.Handbook of fuel cells: fundamentals, technology, and applications: Wiley; 2009.
- Yuan, 2012, Degradation of a PEM fuel cell stack with Nafion® membranes of different thicknesses, Part II: Ex situ diagnosis. Journal of Power Sources., 205, 324
- Hild, 2010, Cathode humidification of a PEM fuel cell through exhaust gas recirculation into a positive displacement compressor, Google Patents
- Weber, 2014, A critical review of modeling transport phenomena in polymer-electrolyte fuel cells, Journal of The Electrochemical Society, 161, F1254, 10.1149/2.0751412jes · DOI
Cited by
Sorted by citations
Nafion degradation mechanisms in proton exchange membrane fuel cell (PEMFC) system: A review
Okonkwo, P. C., Belgacem, I. B., Emori, W., & Uzoma, P. C. (2021) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2021.06.032 · Cited by 332
A review on lifetime prediction of proton exchange membrane fuel cells system
Hua, Z., Zheng, Z., Pahon, E., Péra, M., & Gao, F. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2022.231256 · Cited by 294
Zhang, G., Qu, Z., Tao, W., Wang, X., Wu, L., Wu, S., Xie, X. L., Tongsh, C., Huo, W., Bao, Z., et al. (2022) · Chemical Reviews · doi:10.1021/acs.chemrev.2c00539 · Cited by 274
Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly
Mo, S., Du, L., Huang, Z., Chen, J., Zhou, Y., Wu, P., Meng, L., Wang, N., Xing, L., Zhao, M., et al. (2023) · Electrochemical Energy Reviews · doi:10.1007/s41918-023-00190-w · Cited by 277
“This does not signify that the anode catalyst is not important—at the anode, reactive oxygen species are likely to be generated under inappropriate operation (e.g., H 2 starvation, start-up/ shut-down and reversal), leading to aggressive material degradation (e.g., membrane and ionomer) [22].”
Rashidi, S., Karimi, N., Sunden, B. A., Kim, K. C., Olabi, A. G., & Mahian, O. (2021) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2021.100966 · Cited by 271
Metadata
- Authors
- Ren, P., Pei, P., Li, Y., Wu, Z., Chen, D., & Huang, S.
- Affiliations
- Tsinghua University (CN)
- Corresponding author
- Pei, Pucheng
- Venue
- Progress in Energy and Combustion Science
- Publisher
- Elsevier BV
- Published
- 2020-09
- Volume
- 80
- Pages
- 100859
- ISSN
- 0360-1285 (ISSN-L)
- OpenAlex
- W3033731711
- Semantic Scholar
- 5ff232ae7c1e6f9caa643b36c9457c5f54e0cb63
- Cited by
- 737
- References
- 414
- Citations by year
- 2026: 141 · 2025: 162 · 2024: 161 · 2023: 104 · 2022: 85 · 2021: 76 · 2020: 8
- FWCI
- 23.42
- Type
- journal article
- Language
- en
- Update notices
- erratum (2020-11-01)
- Open access
- closed
- Locations
- Progress in Energy and Combustion Science (publishedVersion)
- Funders
- National Natural Science Foundation of China (21676158, 21376138, 21975143)
- National Basic Research Program of China (2016YFB0101305, 2016YFB0101208, 2017YFB0102705)
- Topics
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Fuel Cells and Related Materials
- Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › Electrocatalysts for Energy Conversion
- Physical Sciences › Engineering › Automotive Engineering › Electric and Hybrid Vehicle Technologies
- Keywords
- proton exchange membrane fuel cells, fuel cell durability, accelerated stress testing, dynamic loading, gas permeation, free radicals, membrane degradation, gas starvation, mechanical degradation, Ostwald ripening, platinum dissolution, carbon corrosion, cold start, membrane electrode assembly
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review