Highly Oriented Monolayer Graphene Grown on a Cu/Ni(111) Alloy Foil

Huang, Ming, Biswal, Mandakini, Park, Hyo Ju, Jin, Sunghwan, Qu, Deshun, Hong, Seokmo, Zhu, Zhili, Qiu, Lu, Luo, Da, Liu, Xiaochi, Yang, Zheng, Liu, Zhongliu, Huang, Yuan, Lim, Hyunseob, Yoo, Won Jong, Ding, Feng, Wang, Yeliang, Lee, Zonghoon, Ruoff, Rodney S. · 2018 · ACS Nano

Abstract

Fast-growth of single crystal monolayer graphene by CVD using methane and hydrogen has been achieved on “homemade” single crystal Cu/Ni(111) alloy foils over large area. Full coverage was achieved in 5 min or less for a particular range of composition (1.3 at.% to 8.6 at.% Ni), as compared to 60 min for a pure Cu(111) foil under identical growth conditions. These are the bulk atomic percentages of Ni, as a superstructure at the surface of these foils with stoichiometry Cu 6 Ni 1 (for 1.3 to 7.8 bulk at.% Ni in the Cu/Ni(111) foil) was discovered by low energy electron diffraction (LEED). Complete large area monolayer graphene films are either single crystal or close to single crystal, and include folded regions that are essentially parallel and that were likely wrinkles that “fell over” to bind to the surface; these folds are separated by large, wrinkle-free regions. The folds occur due to the buildup of interfacial compressive stress (and its release) during cooling of the foils from 1075 °C to room temperature. The fold heights measured by atomic force microscopy (AFM) and scanning tunneling microscopy (STM) prove them to all be 3 layers thick, and scanning electron microscopy (SEM) imaging shows them to be around 10 to 300 nm wide and separated by roughly 20 μm. These folds are always essentially perpendicular to the steps in this Cu/Ni(111) substrate. Joining of well-aligned graphene islands (in growths that were terminated prior to full film coverage) was investigated with high magnification SEM and aberration-corrected high-resolution transmission electron microscopy (TEM) as well as AFM, STM, and optical microscopy. These methods show that many of the “join regions” have folds, and these arise from interfacial adhesion mechanics (they are due to the buildup of compressive stress during cool-down, but these folds are different than for the continuous graphene films—they occur due to “weak links” in terms of the interface mechanics). Such Cu/Ni(111) alloy foils are promising substrates for the large-scale synthesis of single-crystal graphene film.

Overview

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1021/acsnano.8b02444

Cites

1 of 1 references verified0 citation errors · 0 not checkable

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 1 references

Cited by

Metadata

Authors
Huang, M., Biswal, M., Park, H. J., Jin, S., Qu, D., Hong, S., Zhu, Z., Qiu, L., Luo, D., Liu, X., Yang, Z., Liu, Z., Huang, Y., Lim, H., Yoo, W. J., Ding, F., Wang, Y., Lee, Z., & Ruoff, R. S.
Venue
ACS Nano
Published
2018-05-23
Volume
12
Issue
6
Pages
6117-6127
ISSN
  • 1936-0851 (ISSN-L)
  • 1936-086X
OpenAlex
W2804032756
Cited by
170
References
1
FWCI
8.40
Type
journal article
Language
en
Open access
closed

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.