The DOI matches its Crossref record; 1 of the 1 references it cites were found in a registry or an index.
Highly Oriented Monolayer Graphene Grown on a Cu/Ni(111) Alloy Foil
Abstract
Fast-growth of single crystal monolayer graphene by CVD using methane and hydrogen has been achieved on “homemade” single crystal Cu/Ni(111) alloy foils over large area. Full coverage was achieved in 5 min or less for a particular range of composition (1.3 at.% to 8.6 at.% Ni), as compared to 60 min for a pure Cu(111) foil under identical growth conditions. These are the bulk atomic percentages of Ni, as a superstructure at the surface of these foils with stoichiometry Cu 6 Ni 1 (for 1.3 to 7.8 bulk at.% Ni in the Cu/Ni(111) foil) was discovered by low energy electron diffraction (LEED). Complete large area monolayer graphene films are either single crystal or close to single crystal, and include folded regions that are essentially parallel and that were likely wrinkles that “fell over” to bind to the surface; these folds are separated by large, wrinkle-free regions. The folds occur due to the buildup of interfacial compressive stress (and its release) during cooling of the foils from 1075 °C to room temperature. The fold heights measured by atomic force microscopy (AFM) and scanning tunneling microscopy (STM) prove them to all be 3 layers thick, and scanning electron microscopy (SEM) imaging shows them to be around 10 to 300 nm wide and separated by roughly 20 μm. These folds are always essentially perpendicular to the steps in this Cu/Ni(111) substrate. Joining of well-aligned graphene islands (in growths that were terminated prior to full film coverage) was investigated with high magnification SEM and aberration-corrected high-resolution transmission electron microscopy (TEM) as well as AFM, STM, and optical microscopy. These methods show that many of the “join regions” have folds, and these arise from interfacial adhesion mechanics (they are due to the buildup of compressive stress during cool-down, but these folds are different than for the continuous graphene films—they occur due to “weak links” in terms of the interface mechanics). Such Cu/Ni(111) alloy foils are promising substrates for the large-scale synthesis of single-crystal graphene film.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Fine Structure Constant Defines Visual Transparency of Graphene
Nair, R. R., Blake, P., Grigorenko, A. N., Novoselov, K. S., Booth, T. J., Stauber, T., Peres, N. M. R., & Geim, A. K. (2008) · Science · doi:10.1126/science.1156965 · Cited by 9,084
Cited by
Graphene and two-dimensional materials for silicon technology
Akinwande, D., Huyghebaert, C., Wang, C.-H., Serna, M. I., Goossens, S., Li, L.-J., Wong, H.-S. P., & Koppens, F. H. L. (2019) · Nature · doi:10.1038/s41586-019-1573-9 · Cited by 1,713
Production and processing of graphene and related materials
Backes, C., Abdelkader, A. M., Alonso, C., Andrieux-Ledier, A., Arenal, R., Azpeitia, J., Balakrishnan, N., Banszerus, L., Barjon, J., Bartali, R., et al. (2020) · 2D Materials · doi:10.1088/2053-1583/ab1e0a · Cited by 501
Single-crystal, large-area, fold-free monolayer graphene
Wang, M., Huang, M., Luo, D., Li, Y., Choe, M., Seong, W. K., Kim, M., Jin, S., Wang, M., Chatterjee, S., et al. (2021) · Nature · doi:10.1038/s41586-021-03753-3 · Cited by 401
Self-citationKumar, R., Sahoo, S., Joanni, E., Singh, R. K., Yadav, R. M., Verma, R. K., Singh, D. P., Tan, W. K., Pérez del Pino, A., Moshkalev, S. A., et al. (2019) · Nano Research · doi:10.1007/s12274-019-2467-8 · Cited by 383
The Road for 2D Semiconductors in the Silicon Age
Wang, S., Liu, X., & Zhou, P. (2022) · Advanced Materials · doi:10.1002/adma.202106886 · Cited by 277
Self-citation
Metadata
- Authors
- Huang, M., Biswal, M., Park, H. J., Jin, S., Qu, D., Hong, S., Zhu, Z., Qiu, L., Luo, D., Liu, X., Yang, Z., Liu, Z., Huang, Y., Lim, H., Yoo, W. J., Ding, F., Wang, Y., Lee, Z., & Ruoff, R. S.
- Venue
- ACS Nano
- Publisher
- American Chemical Society (ACS)
- Published
- 2018-05-23
- Volume
- 12
- Issue
- 6
- Pages
- 6117-6127
- ISSN
- 1936-0851 (ISSN-L)
- 1936-086X
- OpenAlex
- W2804032756
- Cited by
- 170
- References
- 1
- FWCI
- 8.40
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.