A highly flexible and sensitive piezoresistive sensor based on MXene with greatly changed interlayer distances

Open access

Abstract

Since the successful synthesis of the first MXenes, application developments of this new family of two-dimensional materials on energy storage, electromagnetic interference shielding, transparent conductive electrodes and field-effect transistors, and other applications have been widely reported. However, no one has found or used the basic characteristics of greatly changed interlayer distances of MXene under an external pressure for a real application. Here we report a highly flexible and sensitive piezoresistive sensor based on this essential characteristics. An in situ transmission electron microscopy study directly illustrates the characteristics of greatly changed interlayer distances under an external pressure, supplying the basic working mechanism for the piezoresistive sensor. The resultant device also shows high sensitivity (Gauge Factor ~ 180.1), fast response (<30 ms) and extraordinarily reversible compressibility. The MXene-based piezoresistive sensor can detect human being’s subtle bending-release activities and other weak pressure.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1038/s41467-017-01136-9

Cites

39 of 39 references verified0 citation errors · 0 not checkable

Statistics

Figures

Fig. 1 Working micromechanism of MXene-material for piezoresistive sensor. a The distances between two neighboring interlayers of the MXenes in the sensor decrease under an external pressure. The wider distance (D w) between two interlayers is easier to be compressed, while the narrower distance (D n) between two lattices has a smaller compress ratio. b The equivalent circuit diagram of MXene-based piezoresistive sensor, where the total resistance falls due to the distance decrease
Fig. 1 Working micromechanism of MXene-material for piezoresistive sensor. a The distances between two neighboring interlayers of the MXenes in the sensor decrease under an external pressure. The wider distance (D w) between two interlayers is easier to be compressed, while the narrower distance (D n) between two lattices has a smaller compress ratio. b The equivalent circuit diagram of MXene-based piezoresistive sensor, where the total resistance falls due to the distance decreaseCC BY · PubMed Central
Fig. 2 The MXene’s typical microstructure and the in situ dynamic process under an external pressure. a Cross-sectional TEM image of the MXene and its two insets shows the lamellar structure. b The MXene’s plan view HRTEM image and its corresponding diffraction pattern in the inset, showing well the hexagonal characteristics. c In an in situ force instrument, a nanoindenter supported by a tapered needle point is locally applied on the FIB processed MXene sample. d–f The wider distance in the MXene suffers a rapidly decrease under the external force, from ~12 nm, via ~3 nm to ~0 nm at 7, 9 and 10 s in sequence. g–i The narrower distance (4 spacings) labeled by a red line ranges from 5.23 nm, via 4.98 nm then to 4.81 nm at 7, 9 and 10 s in sequence. j–l The analysis on g–i using the digital micrograph software. Measured from the original state in g, the strain values were 4.78 and 8.03% at the states h, i, respectively. Scale bar for a, b is 4 nm, c is 200 nm, d–f is 40 nm and g–i is 20 nm
Fig. 2 The MXene’s typical microstructure and the in situ dynamic process under an external pressure. a Cross-sectional TEM image of the MXene and its two insets shows the lamellar structure. b The MXene’s plan view HRTEM image and its corresponding diffraction pattern in the inset, showing well the hexagonal characteristics. c In an in situ force instrument, a nanoindenter supported by a tapered needle point is locally applied on the FIB processed MXene sample. d–f The wider distance in the MXene suffers a rapidly decrease under the external force, from ~12 nm, via ~3 nm to ~0 nm at 7, 9 and 10 s in sequence. g–i The narrower distance (4 spacings) labeled by a red line ranges from 5.23 nm, via 4.98 nm then to 4.81 nm at 7, 9 and 10 s in sequence. j–l The analysis on g–i using the digital micrograph software. Measured from the original state in g, the strain values were 4.78 and 8.03% at the states h, i, respectively. Scale bar for a, b is 4 nm, c is 200 nm, d–f is 40 nm and g–i is 20 nmCC BY · PubMed Central
Fig. 3 The response of the MXene-based sensor to pressures. a The I–T curves under the pressures below 13 kPa. The current monotonically increases with the pressure. b The linear relation of the I–V curves suggests the ohmic contacts between MXene and interdigital electrodes. c The ∆R/R off first undergoes a sharp increase as function of pressure below 5 kPa, then a small increase above 5 kPa. Here, the SD for the data is in the range of 1.44–8.21%, which is shown by the error bars and calculated by analyzing five sets of data under each pressure. d The ∆R/R off vs strain. The highest GF, 180.1 was obtained. Here, the SD for the data is in the range of 0.26–1.78%, which is shown by the error bars and calculated by analyzing four sets of data under each strain value. e I–T relation under various bending angles. f An amplifying I–T curve part exhibiting a fast responsive time <30 ms. g Both the output current and external pressure on time kept well in step with the loading and unloading. h The resistivity change ratio ∆R/R off keeps a good stability
Fig. 3 The response of the MXene-based sensor to pressures. a The I–T curves under the pressures below 13 kPa. The current monotonically increases with the pressure. b The linear relation of the I–V curves suggests the ohmic contacts between MXene and interdigital electrodes. c The ∆R/R off first undergoes a sharp increase as function of pressure below 5 kPa, then a small increase above 5 kPa. Here, the SD for the data is in the range of 1.44–8.21%, which is shown by the error bars and calculated by analyzing five sets of data under each pressure. d The ∆R/R off vs strain. The highest GF, 180.1 was obtained. Here, the SD for the data is in the range of 0.26–1.78%, which is shown by the error bars and calculated by analyzing four sets of data under each strain value. e I–T relation under various bending angles. f An amplifying I–T curve part exhibiting a fast responsive time <30 ms. g Both the output current and external pressure on time kept well in step with the loading and unloading. h The resistivity change ratio ∆R/R off keeps a good stabilityCC BY · PubMed Central
Fig. 4 The MXene-based sensor was used to explore the full-range human activities. The current change of the sensor, corresponding to minimal strain change of eye blinking a cheek bulging b and throat swallowing c were precisely recorded. d–f The current change for the bending-release movement of the elbow d, fingers e and ankle f were also recorded. g The I–T curve of knee bending-release. h The sensor was connected in series to a micro circuit implanted with a Bluetooth, which transformed the current signal to a mobile phone. i The knee motion from the micro circuit implanted with a Bluetooth is quite similar to that from the Agilent equipment both in amplitude and shape, but in a faster frequency than that in g
Fig. 4 The MXene-based sensor was used to explore the full-range human activities. The current change of the sensor, corresponding to minimal strain change of eye blinking a cheek bulging b and throat swallowing c were precisely recorded. d–f The current change for the bending-release movement of the elbow d, fingers e and ankle f were also recorded. g The I–T curve of knee bending-release. h The sensor was connected in series to a micro circuit implanted with a Bluetooth, which transformed the current signal to a mobile phone. i The knee motion from the micro circuit implanted with a Bluetooth is quite similar to that from the Agilent equipment both in amplitude and shape, but in a faster frequency than that in gCC BY · PubMed Central
Fig. 5 The as-fabricated 4 × 4 MXene-based sensor arrays. a 4 × 4 MXene-based sensor pixel arrays to detect pressure distribution (scale bar is 5 mm). b A watch was placed on the sensor arrays. c The corresponding output at each pixel was recorded and measured. The color contrast in c mapping local pressure distribution agreed with the watch position in b
Fig. 5 The as-fabricated 4 × 4 MXene-based sensor arrays. a 4 × 4 MXene-based sensor pixel arrays to detect pressure distribution (scale bar is 5 mm). b A watch was placed on the sensor arrays. c The corresponding output at each pixel was recorded and measured. The color contrast in c mapping local pressure distribution agreed with the watch position in bCC BY · PubMed Central

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 39 references

Cited by

See all 821

Metadata

Authors
Ma, Y., Liu, N., Li, L., Hu, X., Zou, Z., Wang, J., Luo, S., & Gao, Y.
Affiliations
  • Wuhan National Laboratory for Optoelectronics (CN)
  • Guangxi University (CN)
  • Wuhan University (CN)
  • Hubei University of Automotive Technology (CN)
Corresponding author
Gao, Yihua
Venue
Nature Communications
Published
2017-10-31
Volume
8
Issue
1
Pages
1207-1207
ISSN
2041-1723 (ISSN-L)
OpenAlex
W2765934971
Cited by
788
References
39
Citations by year
2026: 56 · 2025: 80 · 2024: 109 · 2023: 92 · 2022: 131 · 2021: 129 · 2020: 86 · 2019: 71 · 2018: 33
FWCI
21.92
Type
journal article
Language
en
Open access
Licence
Locations
  • Nature Communications (publishedVersion, cc-by)
  • Europe PMC (PubMed Central) (publishedVersion, cc-by)
  • PubMed Central (publishedVersion, cc-by)
  • PubMed (publishedVersion)
  • RePEc: Research Papers in Economics (submittedVersion)
  • DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion)
  • DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion, cc-by-sa)
Funders
  • Drexel University
  • Wuhan University
Topics
  • Physical Sciences › Materials Science › Materials Chemistry › MXene and MAX Phase Materials
  • Physical Sciences › Engineering › Biomedical Engineering › Advanced Sensor and Energy Harvesting Materials
  • Physical Sciences › Engineering › Electrical and Electronic Engineering › Gas Sensing Nanomaterials and Sensors
Keywords
MXene, piezoresistive sensors, interlayer spacing, external pressure, two-dimensional materials, gauge factor, flexible sensors, human motion detection, in situ transmission electron microscopy

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: A highly flexible and sensitive piezoresistive sensor based on MXene with greatly changed interlayer distances. https://app.cochat.ai/papers/10.1038/s41467-017-01136-9
The paper
Ma, Y., Liu, N., Li, L., Hu, X., Zou, Z., Wang, J., Luo, S., & Gao, Y. (2017). A highly flexible and sensitive piezoresistive sensor based on MXene with greatly changed interlayer distances. Nature Communications. https://doi.org/10.1038/s41467-017-01136-9

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.