Designable ultra-smooth ultra-thin solid-electrolyte interphases of three alkali metal anodes
Open accessThe DOI matches its Crossref record; 48 of the 48 references it cites were found in a registry or an index.
Abstract
Dendrite growth of alkali metal anodes limited their lifetime for charge/discharge cycling. Here, we report near-perfect anodes of lithium, sodium, and potassium metals achieved by electrochemical polishing, which removes microscopic defects and creates ultra-smooth ultra-thin solid-electrolyte interphase layers at metal surfaces for providing a homogeneous environment. Precise characterizations by AFM force probing with corroborative in-depth XPS profile analysis reveal that the ultra-smooth ultra-thin solid-electrolyte interphase can be designed to have alternating inorganic-rich and organic-rich/mixed multi-layered structure, which offers mechanical property of coupled rigidity and elasticity. The polished metal anodes exhibit significantly enhanced cycling stability, specifically the lithium anodes can cycle for over 200 times at a real current density of 2 mA cm–2 with 100% depth of discharge. Our work illustrates that an ultra-smooth ultra-thin solid-electrolyte interphase may be robust enough to suppress dendrite growth and thus serve as an initial layer for further improved protection of alkali metal anodes.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Li-O2 and Li-S batteries with high energy storage
Bruce, P. G., Freunberger, S. A., Hardwick, L. J., & Tarascon, J.-M. (2012) · Nature Materials · doi:10.1038/nmat3191 · Cited by 9,479
Reviving the lithium metal anode for high-energy batteries
Lin, D., Liu, Y., & Cui, Y. (2017) · Nature Nanotechnology · doi:10.1038/nnano.2017.16 · Cited by 6,763
Electrolytes and Interphases in Li-Ion Batteries and Beyond
Xu, K. (2014) · Chemical Reviews · doi:10.1021/cr500003w · Cited by 5,566
Lithium metal anodes for rechargeable batteries
Xu, W., Wang, J., Ding, F., Chen, X., Nasybulin, E., Zhang, Y., & Zhang, J.-G. (2014) · Energy Environ. Sci. · doi:10.1039/c3ee40795k · Cited by 4,704
A review of the features and analyses of the solid electrolyte interphase in Li-ion batteries
Verma, P., Maire, P., & Novák, P. (2010) · Electrochimica Acta · doi:10.1016/j.electacta.2010.05.072 · Cited by 2,903
A new class of Solvent-in-Salt electrolyte for high-energy rechargeable metallic lithium batteries
Suo, L., Hu, Y.-S., Li, H., Armand, M., & Chen, L. (2013) · Nature Communications · doi:10.1038/ncomms2513 · Cited by 2,314
Selective deposition and stable encapsulation of lithium through heterogeneous seeded growth
Yan, K., Lu, Z., Lee, H.-W., Xiong, F., Hsu, P.-C., Li, Y., Zhao, J., Chu, S., & Cui, Y. (2016) · Nature Energy · doi:10.1038/nenergy.2016.10 · Cited by 2,116
Self-citationDendrite-Free Lithium Deposition via Self-Healing Electrostatic Shield Mechanism
Ding, F., Xu, W., Graff, G. L., Zhang, J., Sushko, M. L., Chen, X., Shao, Y., Engelhard, M. H., Nie, Z., Xiao, J., et al. (2013) · Journal of the American Chemical Society · doi:10.1021/ja312241y · Cited by 2,107
Lin, D., Liu, Y., Liang, Z., Lee, H.-W., Sun, J., Wang, H., Yan, K., Xie, J., & Cui, Y. (2016) · Nature Nanotechnology · doi:10.1038/nnano.2016.32 · Cited by 1,798
Interconnected hollow carbon nanospheres for stable lithium metal anodes
Zheng, G., Lee, S. W., Liang, Z., Lee, H.-W., Yan, K., Yao, H., Wang, H., Li, W., Chu, S., & Cui, Y. (2014) · Nature Nanotechnology · doi:10.1038/nnano.2014.152 · Cited by 1,764
Cited by
Interfaces and Interphases in All-Solid-State Batteries with Inorganic Solid Electrolytes
Banerjee, A., Wang, X., Fang, C., Wu, E. A., & Meng, Y. S. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.0c00101 · Cited by 1,526
Dendrites in Zn‐Based Batteries
Yang, Q., Li, Q., Liu, Z., Wang, D., Guo, Y., Li, X., Tang, Y., Li, H., Dong, B., & Zhi, C. (2020) · Advanced Materials · doi:10.1002/adma.202001854 · Cited by 1,181
Artificial Interphases for Highly Stable Lithium Metal Anode
Xu, R., Cheng, X.-B., Yan, C., Zhang, X.-Q., Xiao, Y., Zhao, C.-Z., Huang, J.-Q., & Zhang, Q. (2019) · Matter · doi:10.1016/j.matt.2019.05.016 · Cited by 721
Self-citationLiu, W., Liu, P., & Mitlin, D. (2020) · Advanced Energy Materials · doi:10.1002/aenm.202002297 · Cited by 687
Solid electrolyte interphases in lithium metal batteries
Jagger, B., & Pasta, M. (2023) · Joule · doi:10.1016/j.joule.2023.08.007 · Cited by 592
Toward Critical Electrode/Electrolyte Interfaces in Rechargeable Batteries
Yan, C., Xu, R., Xiao, Y., Ding, J., Xu, L., Li, B., & Huang, J. (2020) · Advanced Functional Materials · doi:10.1002/adfm.201909887 · Cited by 510
Liu, D.-H., Bai, Z., Li, M., Yu, A., Luo, D., Liu, W., Yang, L., Lu, J., Amine, K., & Chen, Z. (2020) · Chemical Society Reviews · doi:10.1039/c9cs00636b · Cited by 483
Self-citationXiao, P., Yun, X., Chen, Y., Guo, X., Gao, P., Zhou, G., & Zheng, C. (2023) · Chemical Society Reviews · doi:10.1039/d3cs00151b · Cited by 443
Toward Green Battery Cells: Perspective on Materials and Technologies
Dühnen, S., Betz, J., Kolek, M., Schmuch, R., Winter, M., & Placke, T. (2020) · Small Methods · doi:10.1002/smtd.202000039 · Cited by 395
Surface-enhanced Raman spectroscopy: a half-century historical perspective
Yi, J., You, E.-M., Hu, R., Wu, D.-Y., Liu, G.-K., Yang, Z.-L., Zhang, H., Gu, Y., Wang, Y.-H., Wang, X., et al. (2025) · Chemical Society Reviews · doi:10.1039/d4cs00883a · Cited by 382
Self-citationA robust all-organic protective layer towards ultrahigh-rate and large-capacity Li metal anodes
Li, S., Huang, J., Cui, Y., Liu, S., Chen, Z., Huang, W., Li, C., Liu, R., Fu, R., & Wu, D. (2022) · Nature Nanotechnology · doi:10.1038/s41565-022-01107-2 · Cited by 380
Self-citationElectrolytes and Interphases in Potassium Ion Batteries
Zhou, M., Bai, P., Ji, X., Yang, J., Wang, C., & Xu, Y. (2021) · Advanced Materials · doi:10.1002/adma.202003741 · Cited by 379
Zou, P., Sui, Y., Zhan, H., Wang, C., Xin, H. L., Cheng, H.-M., Kang, F., & Yang, C. (2021) · Chemical Reviews · doi:10.1021/acs.chemrev.0c01100 · Cited by 368
Solid Electrolyte Interphases on Sodium Metal Anodes
Bao, C., Wang, B., Liu, P., Wu, H., Zhou, Y., Wang, D., Liu, H., & Dou, S. (2020) · Advanced Functional Materials · doi:10.1002/adfm.202004891 · Cited by 354
MXene‐Based Dendrite‐Free Potassium Metal Batteries
Tang, X., Zhou, D., Li, P., Guo, X., Sun, B., Liu, H., Yan, K., Gogotsi, Y., & Wang, G. (2020) · Advanced Materials · doi:10.1002/adma.201906739 · Cited by 346
Solid electrolyte interphase (SEI) in potassium ion batteries
Wang, H., Zhai, D., & Kang, F. (2020) · Energy & Environmental Science · doi:10.1039/d0ee01638a · Cited by 314
Surface engineering toward stable lithium metal anodes
Lu, G., Nai, J., Luan, D., Tao, X., & Lou, X. W. (. (2023) · Science Advances · doi:10.1126/sciadv.adf1550 · Cited by 289
Exploring and Understanding the Roles of Li2Sn and the Strategies to beyond Present Li-S Batteries
Lei, J., Liu, T., Chen, J., Zheng, M., Zhang, Q., Mao, B., & Dong, Q. (2020) · Chem · doi:10.1016/j.chempr.2020.06.032 · Cited by 268
Self-citationGuo, S., Liang, S., Zhang, B., Fang, G., Ma, D., & Zhou, J. (2019) · ACS Nano · doi:10.1021/acsnano.9b07042 · Cited by 264
Huang, J., Guo, X., Du, X., Lin, X., Huang, J.-Q., Tan, H., Zhu, Y., & Zhang, B. (2019) · Energy & Environmental Science · doi:10.1039/c8ee03632b · Cited by 253
Tang, S., Zhang, Y., Zhang, X., Li, J., Wang, X., Yan, J., Wu, D., Zheng, M., Dong, Q., & Mao, B. (2019) · Advanced Materials · doi:10.1002/adma.201807495 · Cited by 229
Self-citationGuo, F., Wu, C., Chen, H., Zhong, F., Ai, X., Yang, H., & Qian, J. (2020) · Energy Storage Materials · doi:10.1016/j.ensm.2019.06.010 · Cited by 208
Ye, S., Wang, L., Liu, F., Shi, P., Wang, H., Wu, X., & Yu, Y. (2020) · Advanced Energy Materials · doi:10.1002/aenm.202002647 · Cited by 183
Zhao, Y., Amirmaleki, M., Sun, Q., Zhao, C., Codirenzi, A., Goncharova, L. V., Wang, C., Adair, K., Li, X., Yang, X., et al. (2019) · Matter · doi:10.1016/j.matt.2019.06.020 · Cited by 169
“The unstable SEI layer with non-uniform Li flux distribution can promote the dendrite growth, whereby the collapse of the SEI film can lead to the non-homogeneous local current buildup and non-homogeneous nucleation.(18,19) In this case, significant efforts have been attempted to create artificial SEI layers to stabil…”
BackgroundEliminating Tip Dendrite Growth by Lorentz Force for Stable Lithium Metal Anodes
Wang, A., Deng, Q., Deng, L., Guan, X., & Luo, J. (2019) · Advanced Functional Materials · doi:10.1002/adfm.201902630 · Cited by 159
Metadata
- Authors
- Gu, Y., Wang, W.-W., Li, Y.-J., Wu, Q.-H., Tang, S., Yan, J.-W., Zheng, M.-S., Wu, D.-Y., Fan, C.-H., Hu, W.-Q., Chen, Z.-B., Fang, Y., Zhang, Q.-H., Dong, Q.-F., & Mao, B.-W.
- Venue
- Nature Communications
- Published
- 2018-04-09
- Volume
- 9
- Issue
- 1
- Pages
- 1339-1339
- ISSN
- 2041-1723 (ISSN-L)
- OpenAlex
- W2797224235
- Cited by
- 355
- References
- 48
- FWCI
- 15.43
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.