Abstract
The electrical conductivity, sigma, of donor‐doped and undoped strontium titanate (SrTiO 3 ) ceramics and, in some cases, single crystals, Sr1‐xLaxTiO 3 (0 ≤ to x ≤ 0.1), was investigated in the temperature range of 1000°‐1400°C under oxygen partial pressures, PO 2 , of 10 ‐20 ‐1 bar. In conjunction with Hall data and thermopower data from related papers, a set of constants for a defect‐chemical model was determined, precisely describing point‐defect concentrations and transport properties of these materials. In contrast to former works, temperature‐dependent transport parameters and their non‐negligible influence on the determination of the constants was considered, as well as the equilibrium restoration phenomena of the cation sublattice, which can be studied only at such high temperatures. It was shown that defects in the cation sublattice completely govern the electrical behavior of donor‐doped and undoped SrTiO 3 . In the latter case, frozen‐in strontium vacancies act as intrinsic acceptors, determining the sigma(PO 2 ) curves at lower temperatures. This intrinsic acceptor concentration also can be calculated with this model. The very good agreement between calculation and measurement is shown in many examples.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Relations between the Concentrations of Imperfections in Crystalline Solids
Kröger, F. A., & Vink, H. J. (1956) · Solid State Physics · doi:10.1016/s0081-1947(08)60135-6 · Cited by 2,125
The compound Sr3Ti2O7and its structure
Ruddlesden, S. N., & Popper, P. (1958) · Acta Crystallographica · doi:10.1107/s0365110x58000128 · Cited by 1,373
GOODENOUGH, J. (1971) · Progress in Solid State Chemistry · doi:10.1016/0079-6786(71)90018-5 · Cited by 1,239
dc Electrical Degradation of Perovskite‐Type Titanates: I, Ceramics
Waser, R., Baiatu, T., & Härdtl, K. (1990) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1990.tb09809.x · Cited by 680
Chan, N. ‐., Sharma, R. K., & Smyth, D. M. (1981) · Journal of The Electrochemical Society · doi:10.1149/1.2127727 · Cited by 463
dc Electrical Degradation of Perovskite‐Type Titanates: III, A Model of the Mechanism
Baiatu, T., Waser, R., & Härdtl, K. (1990) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1990.tb09811.x · Cited by 446
Bulk Conductivity and Defect Chemistry of Acceptor‐Doped Strontium Titanate in the Quenched State
Waser, R. (1991) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1991.tb07812.x · Cited by 433
Electronic Energy Bands in Strontium Titanate
Kahn, A. H., & Leyendecker, A. J. (1964) · Physical Review · doi:10.1103/physrev.135.a1321 · Cited by 406
dc Electrical Degradation of Perovskite‐Type Titanates: II, Single Crystals
Waser, R., Baiatu, T., & Härdtl, K. (1990) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1990.tb09810.x · Cited by 342
Sensors — a comprehensive survey
Sharma, A. K. (1993) · Biosensors and Bioelectronics · doi:10.1016/0956-5663(93)85019-k · Cited by 153
Cited by
Interaction of nanostructured metal overlayers with oxide surfaces
Fu, Q., & Wagner, T. (2007) · Surface Science Reports · doi:10.1016/j.surfrep.2007.07.001 · Cited by 794
Strain-controlled oxygen vacancy formation and ordering in CaMnO3
Aschauer, U., Pfenninger, R., Selbach, S. M., Grande, T., & Spaldin, N. A. (2013) · Physical Review B · doi:10.1103/physrevb.88.054111 · Cited by 422
Oxygen vacancies: The (in)visible friend of oxide electronics
Gunkel, F., Christensen, D. V., Chen, Y. Z., & Pryds, N. (2020) · Applied Physics Letters · doi:10.1063/1.5143309 · Cited by 406
Point Defects in Oxides: Tailoring Materials Through Defect Engineering
Tuller, H. L., & Bishop, S. R. (2011) · Annual Review of Materials Research · doi:10.1146/annurev-matsci-062910-100442 · Cited by 389
Setter, N., & Waser, R. (2000) · Acta Materialia · doi:10.1016/s1359-6454(99)00293-1 · Cited by 379
Merkle, R., & Maier, J. (2008) · Angewandte Chemie International Edition · doi:10.1002/anie.200700987 · Cited by 374
Origin of the Ultra‐nonlinear Switching Kinetics in Oxide‐Based Resistive Switches
Menzel, S., Waters, M., Marchewka, A., Böttger, U., Dittmann, R., & Waser, R. (2011) · Advanced Functional Materials · doi:10.1002/adfm.201101117 · Cited by 348
First-principles study on structures and energetics of intrinsic vacancies inSrTiO3
Tanaka, T., Matsunaga, K., Ikuhara, Y., & Yamamoto, T. (2003) · Physical Review B · doi:10.1103/physrevb.68.205213 · Cited by 221
High temperature oxygen sensors based on doped SrTiO3
Menesklou, W., Schreiner, H.-J., Härdtl, K. H., & Ivers-Tiffée, E. (1999) · Sensors and Actuators B: Chemical · doi:10.1016/s0925-4005(99)00218-x · Cited by 221
De Souza, R. A., Metlenko, V., Park, D., & Weirich, T. E. (2012) · Physical Review B · doi:10.1103/physrevb.85.174109 · Cited by 216
Ion conduction and redistribution at grain boundaries in oxide systems
Gregori, G., Merkle, R., & Maier, J. (2017) · Progress in Materials Science · doi:10.1016/j.pmatsci.2017.04.009 · Cited by 211
Nanoionic memristive phenomena in metal oxides: the valence change mechanism
Dittmann, R., Menzel, S., & Waser, R. (2021) · Advances in Physics · doi:10.1080/00018732.2022.2084006 · Cited by 194
Carrasco, J., Illas, F., Lopez, N., Kotomin, E. A., Zhukovskii, Y. F., Evarestov, R. A., Mastrikov, Y. A., Piskunov, S., & Maier, J. (2006) · Physical Review B · doi:10.1103/physrevb.73.064106 · Cited by 167
Surface point defects on bulk oxides: atomically-resolved scanning probe microscopy
Setvín, M., Wagner, M., Schmid, M., Parkinson, G. S., & Diebold, U. (2017) · Chemical Society Reviews · doi:10.1039/c7cs00076f · Cited by 134
Metadata
- Authors
- Moos, R., & Hardtl, K. H.
- Venue
- Journal of the American Ceramic Society
- Publisher
- Wiley
- Published
- 1997-10
- Volume
- 80
- Issue
- 10
- Pages
- 2549-2562
- ISSN
- 0002-7820 (ISSN-L)
- 1551-2916
- OpenAlex
- W2000539362
- Cited by
- 540
- References
- 13
- FWCI
- 7.19
- Type
- journal article
- Language
- en
- Open access
- bronze
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.