Environmentally Enhanced Fracture of Glass: A Historical Perspective
The DOI matches its Crossref record; 31 of the 31 references it cites were found in a registry or an index.
Abstract
In this paper, we review the phenomenon of delayed failure, a life‐limiting process for glasses that are subjected to tensile stresses. With the development of crack‐weakening theories (Ingles and Griffith) and the observation that surface damage enhances delayed failure, the scientific community recognized that delayed failure in glass is caused by the growth of cracks that are subjected to tensile stresses. Fracture mechanics techniques were used to quantify crack growth rates in terms of applied stress, temperature, and the chemical environments that cause subcritical crack growth. We review the theories that have been developed to rationalize subcritical crack growth data, including theories based on plastic deformation at the crack tip, chemical adsorption of the reacting species, and direct chemical reaction of the environment with the strained bonds at the crack tip. The latter theory seems to be most consistent with the finding that water reacts directly with the strained Si–O bond because of the ability of water to donate both electrons and protons to the strained bond. Other chemicals having this characteristic also cause subcritical crack growth. Finally, we review the quantum mechanical calculations that have been used to quantify the chemical reactions involved in subcritical crack growth.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Dewar, M. J. S., Zoebisch, E. G., Healy, E. F., & Stewart, J. J. P. (1985) · Journal of the American Chemical Society · doi:10.1021/ja00299a024 · Cited by 13,074
VI. The phenomena of rupture and flow in solids
Griffith, A. A. (1921) · Philosophical Transactions of the Royal Society of London. Series A, Containing Papers of a Mathematical or Physical Character · doi:10.1098/rsta.1921.0006 · Cited by 11,052
THE CONSTITUTION AND FUNDAMENTAL PROPERTIES OF SOLIDS AND LIQUIDS. PART I. SOLIDS.
Langmuir, I. (1916) · Journal of the American Chemical Society · doi:10.1021/ja02268a002 · Cited by 9,997
Yielding of steel sheets containing slits
Dugdale, D. S. (1960) · Journal of the Mechanics and Physics of Solids · doi:10.1016/0022-5096(60)90013-2 · Cited by 7,766
Lawn, B. (1993) · Cambridge University Press eBooks · doi:10.1017/cbo9780511623127 · Cited by 4,759
Influence of Water Vapor on Crack Propagation in Soda‐Lime Glass
WIEDERHORN, S. M. (1967) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1967.tb15145.x · Cited by 1,123
Self-citationStresses in a plate due to the presence of cracks and sharp corners
Inglis, C. E. (1913) · Medical Entomology and Zoology · Cited by 1,087
Stress Corrosion and Static Fatigue of Glass
Wiederhorn, S. M., & Bolz, L. H. (1970) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1970.tb15962.x · Cited by 1,024
Self-citationDirect Measurements of the Surface Energies of Crystals
Gilman, J. J. (1960) · Journal of Applied Physics · doi:10.1063/1.1735524 · Cited by 837
Handbook of Aqueous Solubility Data
Yalkowsky, S. H. (2003) · CRC Press eBooks · doi:10.1201/9780203490396 · Cited by 585
Fracture Surface Energy of Glass
WIEDERHORN, S. M. (1969) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1969.tb13350.x · Cited by 543
Self-citationA Molecular Mechanism for Stress Corrosion in Vitreous Silica
MICHALSKE, T. A., & FREIMAN, S. W. (1983) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1983.tb15715.x · Cited by 535
Self-citationA molecular interpretation of stress corrosion in silica
Michalske, T. A., & Freiman, S. W. (1982) · Nature · doi:10.1038/295511a0 · Cited by 470
Self-citationEffects of water and other dielectrics on crack growth
Wiederhorn, S. M., Freiman, S. W., Fuller, E. R., & Simmons, C. J. (1982) · Journal of Materials Science · doi:10.1007/bf00752191 · Cited by 292
Self-citationWiederhorn, S. M., Johnson, H. H., Diness, A. M., & Heuer, A. H. (1974) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1974.tb10917.x · Cited by 261
Self-citationThe Fatigue of Glass Under Stress
OROWAN, E. (1944) · Nature · doi:10.1038/154341a0 · Cited by 260
LAWN, B. R. (1983) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1983.tb09980.x · Cited by 199
The structure of abraded glass surfaces
Preston, F. W. (1922) · Transactions of the Optical Society · doi:10.1088/1475-4878/23/3/301 · Cited by 144
Stress-dependent molecular pathways of silica–water reaction
Zhu, T., Li, J., Lin, X., & Sidney Yip, A. (2005) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2005.02.002 · Cited by 130
Suratwala, T. I., Steele, R. A., Wilke, G. D., Campbell, J. H., & Takeuchi, K. (2000) · Journal of Non-Crystalline Solids · doi:10.1016/s0022-3093(99)00680-8 · Cited by 126
He, M. Y., Turner, M. R., & Evans, A. G. (1995) · Acta Metallurgica et Materialia · doi:10.1016/0956-7151(95)00036-u · Cited by 122
Fatigue limit and crack arrest in alkali-containing silicate glasses
Gehrke, E., Ullner, C., & Hähnert, M. (1991) · Journal of Materials Science · doi:10.1007/bf02403942 · Cited by 82
The Mechanical Properties of Glass
PRESTON, F. W. (1942) · Journal of Applied Physics · doi:10.1063/1.1714811 · Cited by 75
Subcritical Crack Growth in a Phosphate Laser Glass
Crichton, S. N., Tomozawa, M., Hayden, J. S., Suratwala, T. I., & Campbell, J. H. (1999) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1999.tb02208.x · Cited by 69
Specimen for fracture mechanics studies on glass
Janssen, C. (1977) · Revue de Physique Appliquée · doi:10.1051/rphysap:01977001205080300 · Cited by 62
Dynamic condensation of water at crack tips in fused silica glass
Ciccotti, M., George, M., Ranieri, V., Wondraczek, L., & Marlière, C. (2007) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2007.06.090 · Cited by 44
Wondraczek, L., Dittmar, A., Oelgardt, C., Célarié, F., Ciccotti, M., & Marlière, C. (2005) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2005.00765.x · Cited by 39
Crack‐Tip Structure in Soda–Lime–Silicate Glass
Guin, J., Wiederhorn, S. M., & Fett, T. (2005) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2005.00108.x · Cited by 39
Self-citationAnomalous temperature dependence of sub-critical crack growth in silica glass
Suratwala, T. I., & Steele, R. A. (2003) · Journal of Non-Crystalline Solids · doi:10.1016/s0022-3093(02)01799-4 · Cited by 37
Crack Growth in Silica Glass Under Dynamic Loading
Hibino, Y., Sakaguchi, S., & Tajima, Y. (1984) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1984.tb19150.x · Cited by 26
Subcritical crack growth in silica aerogel
Despetis, F., Etienne, P., & Calas-Etienne, S. (2004) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2004.07.017 · Cited by 11
Cited by
Performance of Dental Ceramics: Challenges for Improvements
Rekow, E. D., Silva, N. R. F. A., Coelho, P. G., Zhang, Y., Guess, P., & Thompson, V. P. (2011) · Journal of Dental Research · doi:10.1177/0022034510391795 · Cited by 453
Laubach, S. E., Lander, R. H., Criscenti, L. J., Anovitz, L. M., Urai, J. L., Pollyea, R. M., Hooker, J. N., Narr, W., Evans, M. A., Kerisit, S. N., et al. (2019) · Reviews of Geophysics · doi:10.1029/2019rg000671 · Cited by 349
“Several reviews and key papers cover the history and development of our understanding of subcritical crack growth in glass (Ciccotti, 2009; Freiman et al., 2009; Pallares et al., 2015; Wiederhorn, Fett, et al., 2011; Wiederhorn, Guin, et al., 2011; Wiederhorn, Fett, Guin, et al., 2013, Wiederhorn, Fett, Rizzi, et al.,…”
Background
Metadata
- Authors
- Freiman, S. W., Wiederhorn, S. M., & Mecholsky, Jr.
- Venue
- Journal of the American Ceramic Society
- Publisher
- Wiley
- Published
- 2009-06-26
- Volume
- 92
- Issue
- 7
- Pages
- 1371-1382
- ISSN
- 0002-7820 (ISSN-L)
- 1551-2916
- OpenAlex
- W2121735512
- Cited by
- 164
- References
- 31
- FWCI
- 13.22
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.