The DOI matches its Crossref record.
Capacity Fade Mechanisms and Side Reactions in Lithium‐Ion Batteries
Open accessAbstract
The capacity of a lithium‐ion battery decreases during cycling. This capacity loss or fade occurs due to several different mechanisms which are due to or are associated with unwanted side reactions that occur in these batteries. These reactions occur during overcharge or overdischarge and cause electrolyte decomposition, passive film formation, active material dissolution, and other phenomena. These capacity loss mechanisms are not included in the present lithium‐ion battery mathematical models available in the open literature. Consequently, these models cannot be used to predict cell performance during cycling and under abuse conditions. This article presents a review of the current literature on capacity fade mechanisms and attempts to describe the information needed and the directions that may be taken to include these mechanisms in advanced lithium‐ion battery models.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
The source backs part of the claim, not all of it — or backs it for a different population, condition or comparison.
In the citing paper
“During over-discharging, the anode potential increases abnormally which leads to the anodic dissolution of the copper (Cu) current collector and formation of Cu 2+ ions [37].Upon recharging, the reverse reaction can form copper dendrites, which may lead to internal short circuit [38].”
From Data-driven health estimation and lifetime prediction of lithium-ion batteries: A review (2019) · cites this paper as [38]
Experimental — accuracy not yet measured
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
The publisher hasn’t deposited this paper’s reference list.
Part of this paper’s reference list could not be split into single entries.
Research works printed but not linked: 101
- B. Scrosati, J. Electrochem. Soc., 139, 10 (1992).
- S. Megahed and B. Scrosati, Elect rochem. Soc. Inter- face, 4(4), 34 (1995).
- T. Nagaura, Prog. Batteries Battery Mater., 10, 218 (1991).
- K. G. McColl, J. Power Sources, 48, 29 (1994).
- D. Linden, Handbook of Batteries and Fuel Cells, 1st ed., McGraw-Hill Book Company, New York (1984).
- K. M. Abraham, Elect rochim. Acta, 38, 1233 (1993).
- K. Brandt, Solid State lonics, 69, 173 (1994).
- K. Sekai, H. Azuma, A. Omaru, S. Fujita, H. Imoto, T. Endo, K. Yamaura, and Y. Nishi, J. Power Sources, 43-44, 241 (1993).
- K. Ozawa, Solid State lonics, 69, 212 (1994).
- B. A. Johnson and R. E. White, J. Power Sources, 70/1, 48 (1998).
- S. Yoda, .1. Power Sources, 68, 3 (1997).
- B. C. Knutz, K. West, B. Z.-Christiansen, and S. Atlung, J. Power Sources, 43-44, 733 (1993).
- K. West, T. Jacobsen, and S. Atlung, J. Electrochem. Soc., 129, 1480 (1982).
- S. Atlung, K. West, and T. Jacobsen, J. Electrochem. Soc., 126, 1311 (1979).
- Atlung, B. Z,-Christiansen, K. West, and T. Jacob- sen, J. Electrochem. Soc., 131, 1200 (1984).
- Z. Mao and R. E. White, J. Power Sources, 43-44, 181 (1993).
- R. M. Spotnitz, D. Zuckerbrod, S. L. Johnson, J. T. Lundquist, and R. E. White, in Proceedings of the Symposium on Modeling of Batteries and Fuel Cells, R. E. White, M. W. Verbrugge, and J. F Stock- el, Editors, PV 91-10, p. 88, The Electrochemical Society, Proceedings Series, Pennington, NJ (1991).
- M. Doyle, T. F Fuller, and J. Newman, J. Electrochem. Soc., 140, 1527 (1993).
- T. F Fuller, M. Doyle, and J. Newman, J. Electrochem. Soc., 141, 1 (1994).
- M. Doyle, Ph.D Thesis, University of California, Berkeley, CA (1995).
- T. F Fuller, M. Doyle, and J. Newman, J. Electrochem. Soc., 141, 982 (1994).
- M. Doyle, J. Newman, A. S. Gozdz, C. N. Schmutz, and J. M. Tarascon, J. Electrochem. Soc., 143, 1890 (1996).
- M. Doyle, J. Newman, and J. Reimers, J. Power Sources, 52, 211 (1994).
- M. Doyle and J. Newman, J. Power Sources, 54, 46 (1995).
- Y. Chen and J. W. Evans, J. Electrochem Soc., 140, 1833 (1993).
- Y. Chen and J. W. Evans, J. Electrochem Soc., 141, 2947 (1994).
- Y. Chen and J. W. Evans, J. Electrochem Soc., 143, 2708 (1996).
- C. R. Pals and J. Newman, J. Electrochem Soc., 142, 3274 (1995).
- C. R. Pals and J. Newman, J. Electrochem Soc., 142, 3282 (1995).
- M. W. Verbrugge and B. J. Koch, J. Electrochem. Soc., 143, 24 (1996).
- M. W. Verbrugge and B. J. Koch, J. Elect rochem. Soc., 143, 600 (1996).
- S. R. Narayanan, S. Surampudi, A. I. Attia, and C. P. Bankston, J. Electrochem. Soc., 138, 8 (1991).
- R. Darling and J. Newman, J. Electrochem. Soc., 144, 4201 (1997).
- G. Nagarajan, J. W. VanZee, and R. M. Spotnitz, J. Electrochem. Soc., 145, 771 (1998).
- F. Darling and J. Newman, J. Electrochem. Soc., 145, 990 (1998).
- M. Armand, Solid State lonics, 9&10, 745 (1983).
- J. M. Tarascon and D. Guyomard, Electrochim. Acta, 38, 1221 (1993).
- D. Guyomard and J. M. Tarascon, Solid State lonics, 69, 222 (1994).
- R. Pollard and J. Newman, J. Electrochem Soc., 128, 491 (1981).
- A. B. Yu, R. P. Zou, and N. Standish, md. Eng. Chem. Res., 35, 3730 (1996).
- D. Guyomard and J. M. Tarascon, J. Electrochem. Soc., 139, 4 (1992).
- R. Fong, U. von Sacken, and J. R. Dahn, J. Elec- trochem. Soc., 137, 2009 (1990).
- D. Fauteux and R. Kosbang, J. Appl. Electrochem., 22, 1 (1992).
- T. Zheng, Y. Liu, E, W. Fuller, S. Tseng, U. von Sack- en, and J. R. Dahn, J. Electrochem. Soc., 142, 2581 (1995).
- W. Xing and J. R. Dahn, J. Electrochem. Soc., 144, 1195 (1997).
- J. R. Dahn, T. Zheng, Y. Liu, and J. S. Xue, Science, 270, 590 (1995).
- J. M. Tarascon and D. Guyomard, J. Electrochem. Soc., 138, 2865 (1991).
- J. M. Tarascon and D. Guyomard, J. Power Sources, 43-44, 689 (1993).
- D. Peramunage, K. M. Abraham, and E. B. Willstaedt, in 13th Proceedings of the Annual Battery Confer- ence on Applications and Advances, Long Beach, CA, p. 107, Jan 13-16, 1998.
- E. Peled, Abstract 72, p. 114, The Electrochemical Society Meeting Abstracts, Vol. 94-2, Miami Beach, FL, Oct 9-14, 1994.
- F. Peled, in Lithium Batteries, J. P Gabano, Editor, Academic Press New York (1983).
- J. F. Dahn, E, W. Fuller, M. Obravae, and U. von Sacken, Solid State lonics, 69, 265 (1994).
- A. S. Gozdz and R. K. Jaworski, Abstract 43, p. 52, The Electrochemical Society Meeting Abstracts, Vol. 96-1, Los Angeles, CA, May 5-10, 1996.
- Y. Em-Eli, B. Markovsky, D. Aurbach, Y. Carmeli, H. Yamin, and S. Luski, Electrochim. Acta, 39, 2559 (1994).
- R. J. Staniewicz, in 13th Proceedings of The Interna- tional Seminar on Primary and Secondary Battery Technology and Applications, Boca Raton, FL, March 4-7, 1996.
- F. A. Cotton and G. Wilkinson, Advanced Inorganic Chemistry, 3rd ed. John Wiley & Sons, Inc., New York (1993).
- G. A. Nazri, A. Rougier, and K. F Kia, Mater. Res. Soc. Symp. Proc., 453, 635 (1997).
- M. Hasegawa, B. Yasuhiko, M. Toshihide, and T. Yoshinori, U.S. Pat. 5,631,105 (1997).
- Y. Junichi, 0. Kazuhiro, and N. Yoshiaki, U.S. Pat. 5,626,635 (1997).
- C. Delmas, Solid State lonics, 53-56, 370 (1992).
- W Li and J. C. Currie, J. Electrochem. Soc., 144, 2773 (1997).
- M. M. Thackeray, M. F Mansuetto, D. W. Dees, and D. R. Vissers, Mater. Res. Bull., 31, 133 (1996).
- Y. Gao and J. F. Dahn, Solid State Ionics, 84, 33 (1996).
- J. M. Tarascon and D. Guyomard, Solid State Ionics, 69, 293 (1994).
- A. Campbell, C. Bowes, and R. S. McMillan, J. Electroanal. Chem., 284, 195 (1990).
- K. Kanamura, S. Toriyama, S. Shiraishi, and Z. Take- hara, J. Elect rochem. Soc., 142, 1383 (1995).
- A. M. Christie and C. A. Vincent, J. Appl. Electro- chem., 26, 255 (1996),
- J. Electrochem. Soc., Vol. 145, No. 10, October 1998 Electrochemical Society, Inc.
- F Ossola, G. Pistoia, F. Seeber, and P. Ugo, Electro- chim. Acta, 33, 47 (1988).
- P Novak, P. A. Christensen, T. Iwasita, and W. Viel- stich, J. Elect roanal. Chem., 263, 37 (1989).
- F. Cattaneo and J. Ruch, J. Power Sources, 43-44, 341 (1993).
- G. Eggert, and J. Heitbaum, Electrochim. Acta, 31, 1443 (1986).
- K. Kanamura, H. Takezawa, S. Shiraishi, and Z. Takehara, J. Elect rochem. Soc., 144, 1900 (1997).
- K. Kanamura, S. Toriyama, S. Shiraishi, and Z. Take- hara, J. Electrochem. Soc., 143, 2548 (1996).
- Oishi, T. Abe, T. Nagaura, and M. Watanabe, U.S. Pat. 4,943,497 (1990).
- M. N. Golovin, D. P. Wilkinson, J. T. Dudley, D. Holonko, and S. Woo, J. Electrochem. Soc., 139, 5 (1992).
- T. J. Richardson and P. N. Ross, Jr., J. Electrochem. Soc., 143, 3992 (1996).
- K. M. Abraham, D. M. Pasquariello, and E. B. Will- staedt, in Proceedings of the 33rd Power Sources Symposium, Cherry Hill, NJ, June 13-16, p. 38, The Electrochemical Society, Inc. (1988).
- W. K. Behl and D. T. Chin, J. Electrochem. Soc., 135, 18 (1988).
- W. K. Behl and D. T. Chin, J. Electrochem. Soc., 135, 21 (1988).
- K. J. Hanson and C. W Tobias, J. Electroche;n. Soc., 134, 2204 (1987).
- K. J. Hanson, M. J. Matlosz, C. W Tobias, andJ. New- man, J. Electrochem. Soc., 134, 2210 (1987).
- K. Ozawa, Solid State Ionics, 69, 212 (1994).
- F. C. Laman, M. A. Gee, and J. Denovan, J. Elec- trochem. Soc., 140, L51 (1993).
- J. P Lundquist, C. B. Lundsager, N. I. Palmer, and H. J. Troffkin, U.S. Pat. 4,650,730 (1987).
- J. T. Lundquist, C. B. Lundsager, N. I. Palmer, and H. J. Troffkin, U.S. Pat. 4,731,304 (1988).
- H. T. Taskier, S. M. Mullins, F. A. Langford, and R. J. Fleming, U.S. Pat. 4,973,532 (1990).
- H. Spotnitz and M. Ferebree, Abstract 132, p. 179, The Electrochemical Society Meeting Abstracts, Vol. 96- 2, San Antonio, TX, Oct 6-11, 1996.
- U. von Sacken, Paper presented at POWER '97, 5th International Conference on Power Requirements for Mobile Computing and Wireless Communica- tions, Santa Clara, CA, Oct 12-15, 1997.
- D. Guyomard and J. M. Tarascon, J. Power Sources, 54, 92 (1995).
- D. Aurbach, Y. Em-Eli, 0. Chusid, Y. Carmeli, M. Babai, and H. Yamin, J. Electrochem. Soc., 141, 603 (1994).
- A. N. Dey and B. P. Sullivan, J. Electrochem. Soc., 117, 222 (1970).
- Chusid, Y. Em-Eli, and D. Aurbach, J. Power Sources, 43-44, 47 (1993).
- Y. Matsumura, S. Wang, and J. Mondori, J. Elec- trochem. Soc., 142, 2914 (1995).
- Z. X. Shu, R. S. McMillan, and J. J. Murray, J. Elec- trochem. Soc., 140, 922 (1993).
- A. C. Chu, J. V. Josefowicz, and G. C. Farrington, J. Electrochem. Soc., 144, 4161 (1997).
- D. Aurbach, M. L. Daroux, P. W. Faguy, and E. Yeager, J. Electrochem. Soc., 134, 1611 (1987).
- V. Em-Eli, S. R. Thomas, and V. R. Koch, J. Elec- trochem. Soc, 144, 1159 (1997). 100. V. Em-Eli, S. F McDevitt, D. Aurbach, B. Markovsky, and A. Schechter, J. Electrochem. Soc., 144, L180 (1997), 101.
- K. Yokoyama, A. Hiwara, S. Fujita, and A. Omaru, U.S. Pat. 5,633,099 (1997). 102. Z. X. Shu, F. S. McMHlan and J. J. Murray, U.S. Pat. 5,571,635 (1996). 103. Z. X. Shu, R. S. McMillan, J. J. Murray, and I. J. Davidson, J. Electrochem. Soc., 142, L161 (1995): 104.
- D. Aurbach, B. Markovsky, A Shechter, and V. Em- Eli, J. Electrochem. Soc., 143, 3809 (1996). 105. D. Aurbach, B. Markovsky, A. Shechter, and V. Em- Eli, J. Electrochem. Soc., 143, 3809 (1997). 106. D. Aurbach, V. Em-Eli, B. Markovsky, A. Zaban, A. Schechter, S. Luski, V. Carmeli, and H. Yamin, in Rechargeable Lithium and Lithium-Ion Batteries S. Megahed, B. M. Barnett, and L. Xie, Editors, PV 94-28, p. 26, The Electrochemical Society Proceed- ings Series, Pennington, NJ (1994). 107. F. Imhof and P. Novak, Abstract 125, p. 139, The Elec- trochemical Society Meeting Abstracts. Vol. 97-2, Paris, France, Aug 31-Sept 5, 1997. 108. M. Jean, A. Chausse, and F. Messina, Abstract 146, p. 169, The Electrochemical Society Meeting Ab- stracts, Vol. 97-2, Paris, France, Aug 3l-Sept 5, 1997. 109. B. Simon, J. P Boeuve, and M. Broussely, J. Power Sources, 43-44, 65 (1993). 110. G. Pistoia, D. Zane, and V. Zhang, J. Electrochem. Soc., 142, 2551 (1995). 111. G. Pistoia, A. Antonini, R. Rosati and D. Zane, Elec- trochim. Acta, 41, 2683 (1996). 112. F. Peled, D. Golodnitsky, G. Ardel, C. Menachem, D. Bar Tow, and V. Eshkenazy, Moter. Res. Soc. Symp. Proc., 393, 209 (1995). 113. F. Peled, J. Power Sources, 9, 253 (1983). 114. F. Peled, D. Golodnitsky, C. Ardel, and V Eshkenazy, Electrochim. Acta, 40, 2197 (1995). 115. A. Meitav and F. Peled, J. Electrochem. Soc., 128, 825 (1981). 116. F. Peled and H. Straze, J. Electrochem. Soc., 124, 1030 (1977). 117. U. von Sacken, F. Nodwell, A. Sundher, and J. R. Dahn, Solid State lonics, 69, 284 (1994). 118. M. Garreau, J. Thevenin, and B. Milandou, in Lithium Batteries, A. N. Dey, Editor, PV 84-1, p. 28, The Flectrochemical Society Proceedings Series, Pen- nington, NJ (1984). 119. J. W. Braithwaite, A. Gonzales, S. L. Lucero, D. F. Peebles, J. A. Ohlhausen, W. R. Ciesalk, and C. Nagasubramanian, Sandia National Laboratories Report, SAND97-0507 (1997). 120. J. Braithwaite, C. Nagasubramanian, S. Lucero, and W Cieslak, Abstract 64, p. 85, The Flectrochemical Society Meeting Abstracts, Vol. 96-2, San Antonio, TX, Oct 6-11, 1996. 121. C. Pistoia, A. Antonini, F. Rosati, and C. Bellitto, Abstract 213, p. 257, The Flectrochemical Society Meeting Abstracts, Vol. 97-2, Paris, France, Aug 31- Sept 5, 1997. 122. V. Chen, L. Song, T. M. Devine, and J. W. Evans, Two papers presented at Advanced Non-Aqueous Bat- tery Technology Research and Development Work- shop, p. 49, Oct 15-17, 1997. 123. IUPAC Chemical Data Series-No.22, Stability Con- stants of Metal-Ion Complexes, Part B, Organic Lig- ands, Compiled by Douglas D. Perrin, Pergamon Press, New York (1979). 124. G. G. Amatucci, Unpublished results. 125. M. M. Thackeray, J. Electrochem. Soc., 142, 2558 (1995). 126. M. M. Thackeray, J. Electrochem. Soc., 144, L100 (1997). 127. J. M. Tarascon, W. R. McKinnon, F Coowar, P N. Bowmer, G. Amatucci, and D. Guyomard, J. Elec- trochem. Soc., 141, 1421 (1994). 128. R. J. Gummow, A. de Kock, and M. M. Thackeray, Solid State lonics, 69, 59 (1994). 129. S. J. Wen, T. J. Richardson, L. Ma, K. A. Striebel, P. N. Ross, Jr., and E. J. Cairns, J. Elect rochem. Soc., 143, L136 (1996). 130. Y. Xia, V. Zhou, and M. Yoshio, J. Electrochem. Soc., 144, 2593 (1997). 131. A. Blyr, C. Sigala, G. Amatucci, D. Guyomard, V. Chabre, and J-M. Tarascon, J. Electrochem. Soc., 145, 194 (1998). 132.
- Levenspiel, Chemical Reaction Engineering, 2nd ed., Wiley Eastern Limited, New York (1972).
Cited by
Sorted by citations
Items 401–500 of 1,000
Lee, S.-B., & Pyun, S.-I. (2002) · Carbon · doi:10.1016/s0008-6223(02)00144-6 · Cited by 52
Simulation of capacity loss in carbon electrode for lithium-ion cells during storage
Ramasamy, R. P., Lee, J., & Popov, B. N. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.12.086 · Cited by 74
Post-Mortem Analysis of Calendar-Aged 16 Ah NMC/Graphite Pouch Cells for EV Application
Iturrondobeitia, A., Aguesse, F., Géniès, S., Waldmann, T., Kasper, M., Ghanbari, N., Wohlfahrt‐Mehrens, M., & Bekaert, É. (2017) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.7b05416 · Cited by 73
Olson, J. Z., López, C. M., & Dickinson, E. J. F. (2023) · Chemistry of Materials · doi:10.1021/acs.chemmater.2c01976 · Cited by 73
Lee, C. R., Jang, H. Y., Leem, H. J., Lee, M. A., Kim, W., Kim, J., Song, J. H., Yu, J., Mun, J., Back, S., et al. (2023) · Advanced Energy Materials · doi:10.1002/aenm.202302906 · Cited by 74
Permanent gas analysis using gas chromatography with vacuum ultraviolet detection
Bai, L., Smuts, J. P., Walsh, P. J., et al. (2015) · Journal of Chromatography A · doi:10.1016/j.chroma.2015.02.007 · Cited by 73
“The determination of hazardous decomposition products from thermal runaway reaction of lithium-ion and lithium-metal bateries is another important gas analysis application [7].”
BackgroundQuantification of bottlenecks to fast charging of lithium-ion-insertion cells for electric vehicles
Chandrasekaran, R. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.07.106 · Cited by 72
Shapira, A., Tiurin, O., Solomatin, N., et al. (2018) · ACS Applied Energy Materials · doi:10.1021/acsaem.8b01048 · Cited by 72
Applications of carbon nanotubes in high performance lithium ion batteries
Wu, Y., Wang, J., Jiang, K., et al. (2013) · Frontiers of Physics · doi:10.1007/s11467-013-0308-x · Cited by 72
Dong, Y., Md, K., Chui, Y., et al. (2015) · Electrochimica Acta · doi:10.1016/j.electacta.2015.07.144 · Cited by 72
Liu, Y., Liu, Q., Li, Z.-F., Ren, Y., Xie, J., He, H., & Xu, F. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.090404jes · Cited by 72
Liu, C., Gao, Y., & Liu, L. (2020) · International Journal of Energy Research · doi:10.1002/er.5924 · Cited by 71
“In the review literature on lithium combustion, the author stated that ignition and combustion would occur when the lithiumparticle size is smaller than 22 μm.(15) The small size increases the reaction area for lithium atoms and reactants, so this reaction is vigorous.”
BackgroundInfluentialLi, J., Wang, L., Zhang, Q., et al. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.08.011 · Cited by 71
Correlating capacity fade with film resistance loss in fast charging of lithium-ion battery
Gargh, P. P., Sarkar, A., Lui, Y. H., Shen, S., Hu, C. K., Hu, S., Nlebedim, C. I., & Shrotriya, P. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2020.229360 · Cited by 69
Nagpure, S. C., Bhushan, B., & Babu, S. S. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.001311jes · Cited by 70
Dokko, K., Horikoshi, S., Itoh, T., et al. (2000) · Journal of Power Sources · doi:10.1016/s0378-7753(00)00456-0 · Cited by 70
The Cell Cooling Coefficient: A Standard to Define Heat Rejection from Lithium-Ion Batteries
Hales, A., Diaz, L. B., Marzook, M. W., Zhao, Y., Patel, Y., & Offer, G. J. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.0191912jes · Cited by 70
Rapid impedance measurement using chirp signals for electrochemical system analysis
Bullecks, B., Suresh, R., & Rengaswamy, R. (2017) · Computers & Chemical Engineering · doi:10.1016/j.compchemeng.2017.05.018 · Cited by 69
Day, R. P., Xia, J., Petibon, R., et al. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0181514jes · Cited by 69
Optimization of hybrid off-grid system consisting of renewables and Li-ion batteries
Jung, W., Jeong, J., Kim, J., & Chang, D. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2020.227754 · Cited by 68
Shao, J., Li, J., Yuan, W.-Z., Dai, C., Wang, Z., Zhao, M. S., & PECHT, M. G. (2023) · Journal of Energy Storage · doi:10.1016/j.est.2023.106788 · Cited by 68
Scanning probe microscopy based characterization of battery materials, interfaces, and processes
Kempaiah, R., Vasudevamurthy, G., & Subramanian, A. (2019) · Nano Energy · doi:10.1016/j.nanoen.2019.103925 · Cited by 68
Chu, Z., Plett, G. L., Trimboli, M. S., et al. (2019) · Journal of Energy Storage · doi:10.1016/j.est.2019.100828 · Cited by 68
Robert, R., & Novák, P. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0721509jes · Cited by 67
Three-dimensional conductive network formed by carbon nanotubes in aqueous processed NMC electrode
Du, Z., Li, J., Wood, M., Mao, C., Daniel, C., & Wood, D. L. (2018) · Electrochimica Acta · doi:10.1016/j.electacta.2018.03.063 · Cited by 67
Waterproof lithium metal anode enabled by cross-linking encapsulation
Xiao, Y., Xu, R. X., Yan, C., Liang, Y., Ding, J., & Huang, J. (2020) · 中国科学通报:英文版 · doi:10.1016/j.scib.2020.02.022 · Cited by 67
“Moreover, the presence of water also favorably promotes the reactions between Li and other gas constituents [12,13].”
BackgroundLee, Y. K. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2020.229270 · Cited by 66
Lithium-ion batteries under pulsed current operation to stabilize future grids
Qin, Y., Chen, X., Tomaszewska, A., Chen, H., Wei, Y., Zhu, H., Li, Y., Cui, Z., Huang, J., Du, J., et al. (2021) · Cell Reports Physical Science · doi:10.1016/j.xcrp.2021.100708 · Cited by 64
Mai, W., Yang, M. S., & Soghrati, S. (2018) · Electrochimica Acta · doi:10.1016/j.electacta.2018.10.072 · Cited by 67
Zeng, G., Bai, Z., Huang, P., & Wang, Q. (2020) · International Journal of Energy Research · doi:10.1002/er.5125 · Cited by 68
“The potential Van(x) and Vca(y) are obtained through the relationship with the SOC of the electrode, as shown in Equations (18) and (19).”
BackgroundPareek, T., Dwivedi, S., Ahmad, S. A., Badole, M., & Kumar, S. (2020) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2020.153991 · Cited by 65
Gong, Z., Liu, H., Guo, X.-J., et al. (2004) · Journal of Power Sources · doi:10.1016/j.jpowsour.2004.05.022 · Cited by 66
Martinet, S., Durand, R., Ozil, P., Leblanc, P. P., & Blanchard, P. (1999) · Journal of Power Sources · doi:10.1016/s0378-7753(99)00272-4 · Cited by 66
Repurposing Used Electric Car Batteries: A Review of Options
DeRousseau, M., Gully, B. H., Taylor, C., Apelian, D., & Wang, Y. (2017) · JOM · doi:10.1007/s11837-017-2368-9 · Cited by 66
Ullah, A., Majid, A., & Rani, N. (2017) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2017.09.007 · Cited by 67
Nilsson, V., Younesi, R., Brandell, D., Edström, K., & Johansson, P. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.03.019 · Cited by 69
Patrissi, C. J., & Martin, C. R. (2001) · Journal of The Electrochemical Society · doi:10.1149/1.1407831 · Cited by 66
Thermal Behavior Modeling of Lithium-Ion Batteries: A Comprehensive Review
Madani, S. S., Ziebert, C., & Marzband, M. (2023) · Symmetry · doi:10.3390/sym15081597 · Cited by 65
“Arora P et al. [59] conducted a study focusing on the capacity loss or fade observed in lithium-ion batteries during cycling.”
Feinauer, J., Brereton, T. J., Spettl, A., Weber, M., Manke, I., & Schmidt, V. (2015) · Computational Materials Science · doi:10.1016/j.commatsci.2015.06.025 · Cited by 64
“For example, lithium plating can occur at low temperatures; see [2, 3, 4, 5].”
BackgroundImproved Voltage and Cycling for Li+ Intercalation in High‐Capacity Disordered Oxyfluoride Cathodes
Ren, S., Chen, R., Maawad, E., Dolotko, O., Guda, A. A., Шаповалов, В. В., Wang, D., Hahn, H., & Fichtner, M. (2015) · Advanced Science · doi:10.1002/advs.201500128 · Cited by 69
Zampardi, G., Mantia, F. L., & Schuhmann, W. (2015) · RSC Advances · doi:10.1039/c5ra02940f · Cited by 42
Degradation of lithium-ion batteries and how to fight it: A review
Kanevskii, L. S., & Dubasova, V. S. (2005) · Russian Journal of Electrochemistry · doi:10.1007/s11175-005-0042-y · Cited by 68
Gu, W., Sun, Z., Wei, X., & Dai, H. (2014) · Electrochimica Acta · doi:10.1016/j.electacta.2014.03.186 · Cited by 65
Optimal charging profiles for mechanically constrained lithium-ion batteries
Suthar, B., Ramadesigan, V., De, S., Braatz, R. D., & Subramanian, V. R. (2013) · Physical Chemistry Chemical Physics · doi:10.1039/c3cp52806e · Cited by 66
13C Solid State NMR Suggests Unusual Breakdown Products in SEI Formation on Lithium Ion Electrodes
Leifer, N., Smart, M., Prakash, G., González, L., Sanchez, L. M., Smith, K., Bhalla, P., Grey, C., & Greenbaum, S. (2011) · Journal of The Electrochemical Society · doi:10.1149/1.3559551 · Cited by 59
Klett, M., Svens, P. I., Tengstedt, C., Seyeux, A., Światowska, J., Lindbergh, G., & Lindström, R. W. (2014) · The Journal of Physical Chemistry C · doi:10.1021/jp509665e · Cited by 63
Investigation of the Reasons for Capacity Fading in Li-Ion Battery Cells
Ziv, B., Borgel, V., Aurbach, D., et al. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0731410jes · Cited by 64
Probing the Thermal Implications in Mechanical Degradation of Lithium-Ion Battery Electrodes
An, K., Barai, P., Smith, K. A., & Mukherjee, P. P. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.069406jes · Cited by 64
Ghannoum, A., Norris, R. C., Iyer, K., et al. (2016) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.6b03638 · Cited by 64
Intan, N. N., & Pfaendtner, J. (2021) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.0c18414 · Cited by 63
Muñoz‐Márquez, M. Á., Zarrabeitia, M., Passerini, S., et al. (2022) · Advanced Materials Interfaces · doi:10.1002/admi.202101773 · Cited by 63
Solubilization of SEI lithium salts in alkylcarbonate solvents
Jones, J., Anouti, M., Caillon-Caravanier, M., Willmann, P., Sizaret, P.-Y., & Lemordant, D. (2011) · Fluid Phase Equilibria · doi:10.1016/j.fluid.2011.03.007 · Cited by 65
Aklalouch, M., Rojas, R. M., Rojo, J. M., et al. (2009) · Electrochimica Acta · doi:10.1016/j.electacta.2009.08.012 · Cited by 63
Zhou, A., Dai, X., Lu, Y., et al. (2016) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.6b11630 · Cited by 63
On Leakage Current Measured at High Cell Voltages in Lithium-Ion Batteries
Vadivel, N. R., Ha, S., He, M., et al. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.1341702jes · Cited by 63
Lamprecht, X., Speck, F. D., Marzak, P., Cherevko, S., & Bandarenka, A. S. (2022) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.1c21219 · Cited by 63
Jie, Y., Liu, X., Lei, Z., Wang, S., Chen, Y., Huang, F., Cao, R., Zhang, G., & Jiao, S. (2019) · Angewandte Chemie · doi:10.1002/ange.201914250 · Cited by 61
Yan, J. W., Zhang, J., Su, Y., et al. (2009) · Electrochimica Acta · doi:10.1016/j.electacta.2009.10.068 · Cited by 62
Barnes, T., Kamiński, J. W., Borodin, O. A., et al. (2015) · The Journal of Physical Chemistry C · doi:10.1021/jp510882g · Cited by 62
Wagner, R., Streipert, B., Kraft, V., et al. (2016) · Advanced Materials Interfaces · doi:10.1002/admi.201600096 · Cited by 62
Yasuhara, S., Yasui, S., Teranishi, T., Chajima, K., Yoshikawa, Y., Majima, Y., Taniyama, T., & Itoh, M. (2019) · Nano Letters · doi:10.1021/acs.nanolett.8b04690 · Cited by 63
Wang, J., Li, D., Zeng, W., Chen, X., Zhang, Y., Zhang, S., Li, Z., Li, C., & Mu, S. (2025) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2024.11.016 · Cited by 62
Wang, Y., Jin, Y., Zhao, C., et al. (2018) · Journal of Colloid and Interface Science · doi:10.1016/j.jcis.2018.08.011 · Cited by 61
Hao, F., & Fang, D. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.05.098 · Cited by 61
Campestrini, C., Kosch, S., & Jossen, A. (2017) · Journal of Energy Storage · doi:10.1016/j.est.2017.04.011 · Cited by 61
Empirical Li-ion aging model derived from single particle model
Rechkemmer, S. K., Zang, X., Zhang, W.-M., & Sawodny, O. (2019) · Journal of Energy Storage · doi:10.1016/j.est.2019.01.005 · Cited by 60
Battery state of health monitoring by estimation of the number of cyclable Li-ions
Zhou, X., Stein, J. L., & Ersal, T. (2017) · Control Engineering Practice · doi:10.1016/j.conengprac.2017.05.009 · Cited by 60
Atomic layer deposited Li4Ti5O12 on nitrogen-doped carbon nanotubes
Meng, X., Liu, J., Li, X., et al. (2013) · RSC Advances · doi:10.1039/c3ra00033h · Cited by 60
Direct measurement of lithium transport in graphite electrodes using neutrons
Owejan, J. P., Gagliardo, J. J., Harris, S. J., et al. (2012) · Electrochimica Acta · doi:10.1016/j.electacta.2012.01.047 · Cited by 60
Degradation mechanism of LiCoO2/mesocarbon microbeads battery based on accelerated aging tests
Guan, T., Zuo, P., Sun, S., Du, C., Zhang, L., Cui, Y., Yang, L., Gao, Y., Yin, G., & Wang, F. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.06.113 · Cited by 60
Diffusion Induced Damage and Impedance Response in Lithium-Ion Battery Electrodes
Chen, C., Barai, P., & Mukherjee, P. P. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0651414jes · Cited by 60
Effect of Relaxation Periods over Cycling Performance of a Li-Ion Battery
Rashid, M. M., & Gupta, A. K. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0201502jes · Cited by 60
Simulation-Supported Analysis of Calendering Impacts on the Performance of Lithium-Ion-Batteries
Lenze, G., Röder, F., Bockholt, H., et al. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.1141706jes · Cited by 60
Jang, S. H., Lee, K., Mun, J., Han, Y., & Yim, T. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.11.008 · Cited by 58
Feasibility of Chemically Modified Cellulose Nanofiber Membranes as Lithium-Ion Battery Separators
Kim, H., Mattinen, U., Guccini, V., et al. (2020) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.0c08820 · Cited by 59
Oukahou, S., Elomrani, A., Maymoun, M., et al. (2021) · Computational Materials Science · doi:10.1016/j.commatsci.2021.111006 · Cited by 59
Optimal Control of Film Growth in Lithium-Ion Battery Packs via Relay Switches
Moura, S. J., Forman, J. C., Bashash, S., et al. (2010) · IEEE Transactions on Industrial Electronics · doi:10.1109/tie.2010.2087294 · Cited by 59
Comparison between cyclic voltammetry and differential charge plots from galvanostatic cycling
Palagonia, M. S., Erinmwingbovo, C., Brogioli, D., et al. (2019) · Journal of Electroanalytical Chemistry · doi:10.1016/j.jelechem.2019.05.052 · Cited by 58
Lithium-ion battery physics and statistics-based state of health model
Crawford, A., Choi, D., Balducci, P., Subramanian, V. R., & Viswanathan, V. (2021) · Journal of Power Sources · doi:10.1016/j.jpowsour.2021.230032 · Cited by 57
Studies on the degradation of Li-ion batteries by the use of microreference electrodes
Zhou, J., & Notten, P. H. L. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.11.032 · Cited by 58
Mistry, A. N., Smith, K. A., & Mukherjee, P. P. (2018) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b08993 · Cited by 57
Atomic Layer Deposition for Electrochemical Energy: from Design to Industrialization
Zhao, Z., Huang, G., Kong, Y., Cui, J., Solovev, A. A., Li, X., & Mei, Y. (2022) · Electrochemical Energy Reviews · doi:10.1007/s41918-022-00146-6 · Cited by 56
Cu[sub 2]Sb Thin-Film Electrodes Prepared by Pulsed Laser Deposition for Lithium Batteries
Song, S., Reade, R. P., Cairns, E. J., Vaughey, J. T., Thackeray, M. M., & Striebel, K. A. (2004) · Journal of The Electrochemical Society · doi:10.1149/1.1758719 · Cited by 57
Lithium-Ion Battery Life Model with Electrode Cracking and Early-Life Break-in Processes
Smith, K. A., Gasper, P. J., Colclasure, A. M., Shimonishi, Y., & Yoshida, S. (2021) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac2ebd · Cited by 57
“For the graphite anode, mechanisms include solid-electrolyte interface (SEI) growth(9,10) and acceleration of SEI growth due to graphite microcracking(11) and transition metal dissolution/migration to the anode.(12,13) Thick SEI can reduce electrode porosity, clogging pores and blocking Li diffusion in the electrolyte…”
BackgroundLiu, J., Wen, P., Yang, M., Jin, K., Liu, P., Sun, J., & Wang, Q. (2022) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2022.130756 · Cited by 57
Wang, Y., Cao, Z., Wahyudi, W., Ma, Z., Liang, Y., Cavallo, L., Li, Q., & Ming, J. (2023) · Advanced Energy Materials · doi:10.1002/aenm.202301354 · Cited by 40
Capacity fading in lithium/sulfur batteries: A linear four-state model
Risse, S., Angioletti‐Uberti, S., Dzubiella, J., & Ballauff, M. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.05.076 · Cited by 57
Kim, Y., Dudney, N. J., Chi, M., Martha, S. K., Nanda, J., Veith, G. M., & Liang, C. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.017305jes · Cited by 55
Keil, J., Paul, N., Baran, V. V., Keil, P., Gilles, R., & Jossen, A. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.1271915jes · Cited by 57
Poly(acrylonitrile) encapsulated graphite as anode materials for lithium ion batteries
Guo, K. (2002) · Journal of Power Sources · doi:10.1016/s0378-7753(02)00347-6 · Cited by 55
Martha, S. K., Dudney, N. J., Kiggans, J., et al. (2012) · Journal of The Electrochemical Society · doi:10.1149/2.041210jes · Cited by 55
Phase Field Modeling of Solid Electrolyte Interface Formation in Lithium Ion Batteries
Deng, J., Wagner, G. J., & Muller, R. P. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.052303jes · Cited by 55
The Effect of Pre-Analysis Washing on the Surface Film of Graphite Electrodes
Somerville, L., Bareño, J., Jennings, P., et al. (2016) · Electrochimica Acta · doi:10.1016/j.electacta.2016.04.133 · Cited by 55
“This film, a solid electrolyte interphase (SEI) [5] layer, passivates the electrode surface to further reaction with the components of the electrolyte [6].”
BackgroundIn Situ TEM Investigation of ZnO Nanowires during Sodiation and Lithiation Cycling
Asayesh‐Ardakani, H., Yao, W., Yuan, Y., et al. (2017) · Small Methods · doi:10.1002/smtd.201700202 · Cited by 55
Multi-dimensional modeling of large-scale lithium-ion batteries
Jung, S., & Kang, D. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.09.103 · Cited by 54
Cherkashinin, G., Ensling, D., & Jaegermann, W. (2013) · Journal of Materials Chemistry A · doi:10.1039/c3ta14509c · Cited by 54
Li, Y., Sun, Y., Xu, G., et al. (2014) · Journal of Materials Chemistry A · doi:10.1039/c4ta01562b · Cited by 54
Quinlan, F. T., Sano, K., Willey, T. M., et al. (2001) · Chemistry of Materials · doi:10.1021/cm010335v · Cited by 54
Oxygen Vacancy Diffusion and Condensation in Lithium‐Ion Battery Cathode Materials
Lee, S., Jin, W., Kim, S. H., et al. (2019) · Angewandte Chemie · doi:10.1002/ange.201904469 · Cited by 53
Cyberphysical Security of Grid Battery Energy Storage Systems
Trevizan, R. D., Obert, J., Angelis, V. D., Nguyen, T. A., Rao, V. S., & Chalamala, B. R. (2022) · IEEE Access · doi:10.1109/access.2022.3178987 · Cited by 59
Metadata
- Authors
- Arora, P., White, R. E., & Doyle, M.
- Affiliations
- DuPont (United States) (US)
- ORCID
- White, Ralph E.
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 1998-10-01
- Volume
- 145
- Issue
- 10
- Pages
- 3647-3667
- ISSN
- 0013-4651 (ISSN-L)
- 1945-7111
- OpenAlex
- W2014862314
- Cited by
- 1,408
- References
- 0
- Citations by year
- 2026: 43 · 2025: 69 · 2024: 59 · 2023: 75 · 2022: 74 · 2021: 70 · 2020: 89 · 2019: 96 · 2018: 86 · 2017: 117 · 2016: 87 · 2015: 96 · 2014: 92 · 2013: 63 · 2012: 39
- FWCI
- 47.70
- Type
- journal article
- Language
- en
- Open access
- bronze
- doi.org
- Licence
- Locations
- Journal of The Electrochemical Society (publishedVersion)
- Scholar Commons (University of South Carolina) (submittedVersion)
- Topics
- Physical Sciences › Engineering › Automotive Engineering › Battery Modeling and Management
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advancements in Battery Materials
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advanced Battery Materials and Technologies
- Keywords
- lithium-ion batteries, capacity fade, capacity loss mechanisms, side reactions, overcharging, overdischarge, electrolyte decomposition, passive film formation, active material dissolution, cycling performance
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review