CoChat

Biofilm and Diatom Succession on Polyethylene (PE) and Biodegradable Plastic Bags in Two Marine Habitats: Early Signs of Degradation in the Pelagic and Benthic Zone?

Open access

The DOI matches its Crossref record; 37 of the 38 references it cites were found in a registry or an index.

Abstract

The production of biodegradable plastic is increasing. Given the augmented littering of these products an increasing input into the sea is expected. Previous laboratory experiments have shown that degradation of plastic starts within days to weeks. Little is known about the early composition and activity of biofilms found on biodegradable and conventional plastic debris and its correlation to degradation in the marine environment. In this study we investigated the early formation of biofilms on plastic shopper bags and its consequences for the degradation of plastic. Samples of polyethylene and biodegradable plastic were tested in the Mediterranean Sea for 15 and 33 days. The samples were distributed equally to a shallow benthic (sedimentary seafloor at 6 m water depth) and a pelagic habitat (3 m water depth) to compare the impact of these different environments on fouling and degradation. The amount of biofilm increased on both plastic types and in both habitats. The diatom abundance and diversity differed significantly between the habitats and the plastic types. Diatoms were more abundant on samples from the pelagic zone. We anticipate that specific surface properties of the polymer types induced different biofilm communities on both plastic types. Additionally, different environmental conditions between the benthic and pelagic experimental site such as light intensity and shear forces may have influenced unequal colonisation between these habitats. The oxygen production rate was negative for all samples, indicating that the initial biofilm on marine plastic litter consumes oxygen, regardless of the plastic type or if exposed in the pelagic or the benthic zone. Mechanical tests did not reveal degradation within one month of exposure. However, scanning electron microscopy (SEM) analysis displayed potential signs of degradation on the plastic surface, which differed between both plastic types. This study indicates that the early biofilm formation and composition are affected by the plastic type and habitat. Further, it reveals that already within two weeks biodegradable plastic shows signs of degradation in the benthic and pelagic habitat.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1371/journal.pone.0137201

Cites

37 of 37 references verified0 citation errors · 0 not checkable

Statistics

Figures

Fig 1 Photo of representatives for each diatom group based on morphological features. No example is shown for group G13 (i.e. unknown diatoms) in this figure. Image source for G2: [33] modified, and for G11: [34] modified.
Fig 1 Photo of representatives for each diatom group based on morphological features. No example is shown for group G13 (i.e. unknown diatoms) in this figure. Image source for G2: [33] modified, and for G11: [34] modified.CC BY · PubMed Central
Fig 2 Biofilm development over time. The relative amount of biofilm found on PE (white) and biodegradable plastic (grey) after 15 and after 33 days of the experiment. Time 0 represents the polymer without biofilm. The error bars indicate the standard error. (A) Results of benthic samples (6 m water depth). (B) Results of pelagic samples (3 m water depth).
Fig 2 Biofilm development over time. The relative amount of biofilm found on PE (white) and biodegradable plastic (grey) after 15 and after 33 days of the experiment. Time 0 represents the polymer without biofilm. The error bars indicate the standard error. (A) Results of benthic samples (6 m water depth). (B) Results of pelagic samples (3 m water depth).CC BY · PubMed Central
Fig 3 Diatom abundance per treatment. The number of diatoms found per square centimetre on PE (white) and biodegradable plastic (grey) is displayed after 15 and 33 days of the experiments. The error bars indicate the standard error. (A) Results of benthic samples (6 m water depth). (B) Results of pelagic samples (3 m water depth).
Fig 3 Diatom abundance per treatment. The number of diatoms found per square centimetre on PE (white) and biodegradable plastic (grey) is displayed after 15 and 33 days of the experiments. The error bars indicate the standard error. (A) Results of benthic samples (6 m water depth). (B) Results of pelagic samples (3 m water depth).CC BY · PubMed Central
Fig 4 Detrended correspondence analysis (DCA) for the diatom community on PE and biodegradable plastic in the benthic (A) and in the pelagic zone (B). Diatoms were categorised by morphology. Each data point represents a plastic sample, the distance between the data points shows the similarity of the diatom composition found on the sample. The smaller the distance, the more similar the composition was between the samples. Different symbols were used to group the samples by plastic type and sampling time. Around the centroid of all data points for these groups an ellipse indicating the 95% confidence interval of their standard error was drawn. If these ellipses do not overlap the groups are assumed to be significantly different (P ≤ 0.05).
Fig 4 Detrended correspondence analysis (DCA) for the diatom community on PE and biodegradable plastic in the benthic (A) and in the pelagic zone (B). Diatoms were categorised by morphology. Each data point represents a plastic sample, the distance between the data points shows the similarity of the diatom composition found on the sample. The smaller the distance, the more similar the composition was between the samples. Different symbols were used to group the samples by plastic type and sampling time. Around the centroid of all data points for these groups an ellipse indicating the 95% confidence interval of their standard error was drawn. If these ellipses do not overlap the groups are assumed to be significantly different (P ≤ 0.05).CC BY · PubMed Central
Fig 5 Oxygen production rate. Amount of oxygen (µmol) produced per day per square centimetre of plastic surface (white for PE, grey for biodegradable plastic) after 15 days and after 33 days of the experiment. Time 0 represents the polymer without biofilm. The error bars indicate the standard error. (A) Results of benthic samples (6 m water depth). (B) Results of pelagic samples (3 m water depth).
Fig 5 Oxygen production rate. Amount of oxygen (µmol) produced per day per square centimetre of plastic surface (white for PE, grey for biodegradable plastic) after 15 days and after 33 days of the experiment. Time 0 represents the polymer without biofilm. The error bars indicate the standard error. (A) Results of benthic samples (6 m water depth). (B) Results of pelagic samples (3 m water depth).CC BY · PubMed Central
Fig 6 SEM pictures of the plastic surface of PE samples following removal of the biofilm. Each sample is displayed in two magnifications. (A) and (B) show untreated PE; (C) and (D) PE after 15 days; (E) and (F) PE after 33 days. Arrows in (F) mark fissures close to remains of the biofilm.
Fig 6 SEM pictures of the plastic surface of PE samples following removal of the biofilm. Each sample is displayed in two magnifications. (A) and (B) show untreated PE; (C) and (D) PE after 15 days; (E) and (F) PE after 33 days. Arrows in (F) mark fissures close to remains of the biofilm.CC BY · PubMed Central
Fig 7 SEM pictures of the plastic surface of biodegradable plastic samples following removal of the biofilm. Each sample is displayed in two magnifications. (A) and (B) show untreated samples of biodegradable plastic; (C) and (D) of biodegradable plastic after 15 days; (E) and (F) of biodegradable plastic after 33 days. Arrows in (B) mark apparent starch particles and in (D) and (F) remaining holes.
Fig 7 SEM pictures of the plastic surface of biodegradable plastic samples following removal of the biofilm. Each sample is displayed in two magnifications. (A) and (B) show untreated samples of biodegradable plastic; (C) and (D) of biodegradable plastic after 15 days; (E) and (F) of biodegradable plastic after 33 days. Arrows in (B) mark apparent starch particles and in (D) and (F) remaining holes.CC BY · PubMed Central

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Research works printed but not linked: 1

  1. 1994, Marine Debris: Solid Waste Management Action Plan for the Wider Caribbean, Intergov Oceanogr Comm Tech Ser, 42, 1

Cited by

See all 216

Metadata

Authors
Eich, A., Mildenberger, T., Laforsch, C., & Weber, M.
Affiliations
  • University of Bremen (DE)
  • University of Bayreuth (DE)
Corresponding author
Weber, Miriam
Venue
PLOS ONE
Published
2015-09-22
Volume
10
Issue
9
Pages
e0137201
ISSN
1932-6203 (ISSN-L)
OpenAlex
W1844587767
Cited by
216
References
38
Citations by year
2026: 12 · 2025: 21 · 2024: 22 · 2023: 32 · 2022: 40 · 2021: 20 · 2020: 25 · 2019: 18 · 2018: 10 · 2017: 15 · 2016: 1
FWCI
5.40
Type
journal article
Language
en
Open access
Locations
  • PLoS ONE (publishedVersion, cc-by)
  • Europe PMC (PubMed Central) (publishedVersion, cc-by)
  • PubMed Central (publishedVersion, cc-by)
  • PubMed (publishedVersion)
  • DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion, cc-by-sa)
  • Figshare (submittedVersion, cc-by)
Topics
  • Physical Sciences › Environmental Science › Pollution › Microplastics and Plastic Pollution
  • Physical Sciences › Engineering › Ocean Engineering › Marine Biology and Environmental Chemistry
  • Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
Keywords
biodegradable plastics, polyethylene, plastic degradation, biofilm formation, diatoms, marine plastic debris, pelagic zone, benthic zone, fouling, oxygen consumption, polymer surface properties, Mediterranean Sea
MeSH terms
Light, Mediterranean Sea, Microscopy, Electron, Scanning, Oxygen, Tensile Strength, Diatoms, Ecosystem, Biofilms, Polyethylene, Biodegradable Plastics

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.