The DOI matches its Crossref record; 175 of the 175 references it cites were found in a registry or an index; 71 of the 306 sources its claims cite were checked for support.
Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells
Open accessAbstract
The structure of a catalyst layer (CL) significantly impacts the performance, durability, and cost of proton exchange membrane (PEM) fuel cells and is influenced by the catalyst ink and the CL formation process. This review focuses on the effect of the composition, formulation, and preparation of catalyst ink and the CL formation process on the CL structure.
Overview
CoChat Summary
TL;DR
This review synthesizes how the composition, formulation, and preparation of catalyst ink — and the subsequent coating and drying steps — govern the multiscale structure of conventional catalyst layers (CLs) in PEM fuel cells. It concludes that the ink–structure–performance relationship remains incompletely understood and that inconsistent literature conclusions stem from many simultaneously varying manufacturing variables.
Key findings
- The CL is a three-dimensional network of Pt/C, ionomer, and pores with a multiscale structure: 2–5 nm Pt nanoparticles on 10–50 nm carbon black, ionomer films 3.5–20 nm thick, primary catalyst–ionomer agglomerates of a few hundred nm, and secondary agglomerates of a few µm, giving a bimodal pore distribution of 2–20 nm (primary) and >20 nm (secondary) pores; typical CL thickness is 5–10 µm.
- Ink formulation controls ink microstructure and macroscopic properties: catalyst type (e.g., Pt/Ketjen ink is generally more viscous than Pt/Vulcan ink), ionomer type and I/C ratio, and solvent properties (dielectric constant, solubility parameter, viscosity, boiling point, surface tension). Ionomer adsorption follows a Langmuir-type plateau — absorbed ionomer rises from 0.25 to 0.50 I/C then stays nearly constant up to 1.00 I/C, while non-absorbed ionomer increases with I/C; the reported optimum Nafion content is 30 wt.% (I/C ≈ 0.7).
- Ink preparation matters: premixing Pt/C, water, and ethanol before adding ionomer dispersion decreases agglomerate size and yields a more viscous, more homogeneous CL; insufficient dispersion leaves large agglomerates that raise proton, gas, and water transport resistance, while overly aggressive dispersion degrades Pt and ionomer.
- CL formation process controls morphology: solid content requirements differ by technique (spray coating commonly <3 wt.%, e.g., ~0.6, ~1.8, or 2.5 wt.%; roll-to-roll commonly >5 wt.%, e.g., 5.76 wt.% or ~4.5–15 wt.%, up to 33.76 wt.% for screen printing); roll-to-roll can increase fabrication speed by over 500 times versus lab-scale spray coating; cracks arise from fast solvent evaporation, weak ionomer–catalyst interaction, or film defects.
Methods
- Design: narrative review focused on conventional (ink-based) CLs, explicitly excluding structure-ordered CLs; the companion relationship between CL structure and cell performance/durability was covered in the authors' previous review.
- Scope: (1) multiscale CL structure, (2) catalyst ink microstructure and macroscopic properties (rheology, surface tension, stability), (3) effects of catalyst, ionomer, I/C ratio, and solvent, (4) effects of mixing order and dispersion process, (5) CL formation (substrate, coating, drying), and (6) future directions.
- Evidence base: synthesis of prior experimental and modeling literature, including characterization techniques such as DLS, SAS/SANS/SAXS, CV-SANS, ¹⁹F NMR, TEM/Cryo-TEM, SEM/Cryo-SEM, X-CT, and ELS (zeta potential), plus tabulated solvent and commercial ionomer dispersion properties.
Limitations
- Stated by the paper: the relationship between ink formulation/preparation or CL formation and the multiscale CL structure (and ultimately performance and durability) is still unclear and sometimes inconsistent across studies; most ink characterization techniques require modifying the ink (dilution for DLS/ELS, consolidation for TEM/SEM) or only probe local structure; studies on high-solid-content ink, ink storage stability and reversibility of aged ink, and the drying process are limited; inconsistent conclusions arise when variables other than the one under study are not held constant.
- Evident from the text: as a review, it reports no new primary data or meta-analysis; several quantitative values are cited from other works rather than generated here, and some passages (e.g., Table 3 entries and figure captions) are truncated or garbled in the provided text.
Model-written summary. Check it against the paper before relying on it.
Integrity signals
Registry
Cites
Statistics
Figures

![Figure 2 Illustration of ionomer-coated catalyst agglomerate [21,45]. Figure 2. Illustration of ionomer-coated catalyst agglomerate [21,45].](/paper-figures/db0c1df119f047a2821d28c7fd83fc86/effect-of-catalyst-ink-and-formation-process-on-the-multiscale-structure-of-figure-2.png)


![Figure 5 Viscosity of Nafion ionomer dispersions ( a ), Pt/HSC dispersions ( b ), Pt/HSC and ionomer dispersions with a fixed 3 wt.% carbon ( c ) in 1-propanol and aqueous solvent mixture (3:1 mass ratio) at different concentrations or I/C ratios (Reprinted with permission from ref. [53]. Copyright (2018) American Chemical Society). Figure 5. Viscosity of Nafion ionomer dispersions ( a ), Pt/HSC dispersions ( b ), Pt/HSC and ionomer dispersions with a fixed 3 wt.% carbon ( c ) in 1-propanol and aqueous solvent mixture (3:1 mass ratio) at different concentrations or I/C ratios (Reprinted with permission from ref. [53]. Copyright (2018) American Chemical Society).](/paper-figures/c8224a962e504bf795c9bc2d448bf161/effect-of-catalyst-ink-and-formation-process-on-the-multiscale-structure-of-figure-5.png)
![Figure 6 Schematics of the distribution of ionomer on carbon and Pt nanoparticles in the conventional case ( left ), the selective distribution of ionomer on only carbon surface through masking Pt nanoparticles ( right ), as well as the oxygen/proton transport in both cases. (Reprinted from Ref. [103] with permission from the Royal Society of Chemistry). Figure 6. Schematics of the distribution of ionomer on carbon and Pt nanoparticles in the conventional case ( left ), the selective distribution of ionomer on only carbon surface through masking Pt nanoparticles ( right ), as well as the oxygen/proton transport in both cases. (Reprinted from Ref. [103] with permission from the Royal Society of Chemistry).](/paper-figures/d4d0b60cc2c14103b97670c443ce43fc/effect-of-catalyst-ink-and-formation-process-on-the-multiscale-structure-of-figure-6.png)
![Figure 7 The chemical structures of 3M PFIA ionomer, Nafion ionomer, 3M PFSA ionomer, and Aquivion ionomer [108,112]. Figure 7. The chemical structures of 3M PFIA ionomer, Nafion ionomer, 3M PFSA ionomer, and Aquivion ionomer [108,112].](/paper-figures/59c7b792fcf44f4cb0dc2ecaf3cff4ae/effect-of-catalyst-ink-and-formation-process-on-the-multiscale-structure-of-figure-7.png)
![Figure 8 ( a ) The physical properties of solvent and their effects on the microstructure and macroscopic properties of catalyst ink, or evaporation rate; ( b ) the size and morphologies of Nafion ionomer in different solvents (Adapted with permission from [128], Copyright (2012) American Chemical Society; Reprinted from [26], Copyright (2013), with permission from Elsevier). Figure 8. ( a ) The physical properties of solvent and their effects on the microstructure and macroscopic properties of catalyst ink, or evaporation rate; ( b ) the size and morphologies of Nafion ionomer in different solvents (Adapted with permission from [128], Copyright (2012) American Chemical Society; Reprinted from [26], Copyright (2013), with permission from Elsevier).](/paper-figures/afb87606d70e45d89b9023b9441d0401/effect-of-catalyst-ink-and-formation-process-on-the-multiscale-structure-of-figure-8.png)
![Figure 9 The structures of Pt/C-Nafion ionomer and CL with insufficient ( a , d ), appropriate ( b , e ), and excessive ( c , f ) dispersion. (( a -c ) Modified with permission from [156], Copyright (2019), American Chemical Society; ( d -e ) Reprinted with permission from [24], Copyright (2019), American Chemical Society; ( f ) Reprinted from [159], Copyright (2014), with permission from Elsevier). Figure 9. The structures of Pt/C-Nafion ionomer and CL with insufficient ( a , d ), appropriate ( b , e ), and excessive ( c , f ) dispersion. (( a -c ) Modified with permission from [156], Copyright (2019), American Chemical Society; ( d -e ) Reprinted with permission from [24], Copyright (2019), American Chemical Society; ( f ) Reprinted from [159], Copyright (2014), with permission from Elsevier).](/paper-figures/6afd56e4348a4fb59baff8cb4eef7fd8/effect-of-catalyst-ink-and-formation-process-on-the-multiscale-structure-of-figure-9.png)

![Figure 11 Stylus profilometry traces of Nafion membrane ( a1 ), CL deposited on membrane (the surface facing the GDL) ( a2 ), GDL (the surface of MPL facing CL) ( b1 ), and CL of GDE (the surface facing the membrane) ( b2 ) (Reprinted from [75] with permission of John Wiley & Sons); ( c , d ) SEM images of cross-section view of the MEA. Cathode: a good CL/membrane interface due to the ionomer overlayer deposited on GDE; Anode: the observed gaps at the interface of MPL and CL which was deposited on the membrane, due to the high MPL surface roughness (root mean square surface roughness: 15.85 µm) (Reprinted with permission from [166]. Copyright (2019) American Chemical Society). The CCM-based MEAs, GDE-based MEAs, and DTM-based MEAs generally have Figure 11. Stylus profilometry traces of Nafion membrane ( a1 ), CL deposited on membrane (the surface facing the GDL) ( a2 ), GDL (the surface of MPL facing CL) ( b1 ), and CL of GDE (the surface facing the membrane) ( b2 ) (Reprinted from [75] with permission of John Wiley & Sons); ( c , d ) SEM images of cross-section view of the MEA. Cathode: a good CL/membrane interface due to the ionomer overlayer deposited on GDE; Anode: the observed gaps at the interface of MPL and CL which was deposited on the membrane, due to the high MPL surface roughness (root mean square surface roughness: 15.85 µ m) (Reprinted with permission from [166]. Copyright (2019) American Chemical Society).](/paper-figures/ddc2cb855a164348b938a49c1097adb3/effect-of-catalyst-ink-and-formation-process-on-the-multiscale-structure-of-figure-11.png)
![Figure 12 ( a ) Schematic of the roll-to-roll manufacturing process coupled with slot-die coating, (Reprinted from [165], Copyright (2020), with permission from Elsevier), ( b ) illustration of slot-die coating (Adapted from [39], Copyright (2019), with permission from Elsevier), ( c ) illustration of gravure coating (Adapted from [38]). Figure 12. ( a ) Schematic of the roll-to-roll manufacturing process coupled with slot-die coating, (Reprinted from [165], Copyright (2020), with permission from Elsevier), ( b ) illustration of slot-die coating (Adapted from [39], Copyright (2019), with permission from Elsevier), ( c ) illustration of gravure coating (Adapted from [38]).](/paper-figures/2ec7807590cc4eebbdf1aef0c98880fa/effect-of-catalyst-ink-and-formation-process-on-the-multiscale-structure-of-figure-12.png)
![Figure 13 Weight change of the ink film at different drying conditions (20 or 40 °C, dry-0% R humid-80% RH) and the schematics of the structure change from the ink film to the dried CL (R printed from [56], Copyright (2016), with permission from Elsevier). Figure 13. Weight change of the ink film at different drying conditions (20 or 40 ◦ C, dry-0% RH, humid-80% RH) and the schematics of the structure change from the ink film to the dried CL (Reprinted from [56], Copyright (2016), with permission from Elsevier).](/paper-figures/0f08e3663fbf4033af01d3475c5a0809/effect-of-catalyst-ink-and-formation-process-on-the-multiscale-structure-of-figure-13.png)
Verification
Claims the paper makes
61 Valid · 20 Not valid · 137 Not checked · 126 Own results and interpretations
At least one cited source doesn’t support this claim or points to a different paper, and none confirmed it — see the verdicts below.
In the paper
“The equilibrium constant of ionomer adsorption on catalyst decreases with increasing the amount of the surface oxygen-containing groups [96].”
§ Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells > 4.1. Catalyst and Catalyst Content in the Ink
What the sources say
- Disputedcites [96] Andersen, 2014, Adsorption Behavior of Perfluorinated Sulfonic Acid Ionomer on Highly Graphitized Carbon Nanofibers and Their Thermal Stabilities, J. Phys. Chem. C sourceExperimental — accuracy not yet measured
The Discussion (p. 8) reports that the equilibrium constant first falls as oxygen-containing groups increase, but rises to about 21 for the more highly oxidized CNFF3 sample. The Conclusions (p. 10) likewise describe an initial decrease followed by an increase, contrary to the claimed continuous decrease. (LLM, conf=0.90)
Checked by a reasoning model — may be wrong.
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Disputed
At least one cited source doesn’t support this claim or points to a different paper, and none confirmed it — see the verdicts below.
In the paper
“The penetration degree depends on the deposition method due to the difference in the viscosity of the used ink or the drying rates for various coating techniques [38].”
§ Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells > •
What the sources say
- Disputedcites [38] Mauger, 2018, Gravure coating for roll-to-roll manufacturing of proton-exchange-membrane fuel cell catalyst layers, J. Electrochem. Soc. sourceExperimental — accuracy not yet measured
The Results and Discussion section reports no significant catalyst penetration into the microporous layer with either gravure or spray coating. Although the paper describes differences in ink concentration, viscosity, and drying between the methods, it says the observed penetration difference relative to another study is likely due to the substrate’s microporous layer, not the coating method. (LLM, conf=0.90)
Checked by a reasoning model — may be wrong.
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Disputed
The cited sources support only part of this claim — read each source’s verdict below.
In the paper
“al. found that the decrease in the primary and secondary agglomerates size resulting from dilution approaches 20%, through studying the ink with and without dilution by using a recent DLS apparatus [34].”
§ Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells > 3.1. Microstructure of Catalyst Ink
What the sources say
- Partly supportedcites [34] Shukla, 2017, Experimental and theoretical analysis of ink dispersion stability for polymer electrolyte fuel cell applications, J. Electrochem. Soc. sourceExperimental — accuracy not yet measured
The ink-dilution discussion and Table V report that average carbon-ink particle diameter fell from 284.5 to 233.1 nm—less than 20%—as the ink was diluted. The Sample preparation section confirms that DLS was used to compare diluted and undiluted ink. The paper does not report separate size decreases for primary and secondary agglomerates. Exact page numbers are unavailable in our copy. (LLM, conf=0.87)
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Partly supported
The cited sources support only part of this claim — read each source’s verdict below.
In the paper
“During the solvent evaporation process, the movement, aggregation, or self-assembly of the agglomerates in the ink film occur, determining the final structure of the CL [40,41].”
§ Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells > 1. Introduction
What the sources say
- Partly supportedcites [40] Zhao, 2019, The effect of ink dilution and evaporation on the microstructures of catalyst layers in polymer electrolyte membrane fuel cells, Int. J. Energy Res. sourceExperimental — accuracy not yet measured
The Introduction (page unavailable) says solvent evaporation determines initial catalyst-layer microstructures and affects catalyst-particle movement. Section 3.2 (page unavailable) describes particles moving and accumulating as droplets dry, but does not establish self-assembly or aggregation of agglomerates in an ink film. (LLM, conf=0.84)
- Partly supportedcites [41] Mauger, 2021, Development of high-performance roll-to-roll-coated gas-diffusion-electrode-based fuel cells, J. Power Sources sourceExperimental — accuracy not yet measured
The Introduction (pp. 4–5) explains that evaporation and diffusion affect particle distribution as an ink film dries, and the Results and Discussion (p. 14) report likely ionomer migration during drying. This supports movement shaping the final catalyst-layer structure, but the cited passages do not establish that agglomerates aggregate or self-assemble during evaporation. (LLM, conf=0.84)
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Partly supported
The sources with a verdict support this claim; the rest weren’t checked yet, have no full text we could read, or their verdicts aren’t rated yet.
In the paper
“Therefore, the secondary catalyst-ionomer agglomerates usually exhibit a bimodal pore size distribution, including 2-20 nm-sized pores within primary agglomerates and larger over 20 nm-sized pores between primary agglomerates in the secondary agglomerates-the former is often referred to as the primary pores, and the latter the secondary pores [47,48].”
§ Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells > 2. Multiscale Structure of CL in PEM Fuel Cell
What the sources say
- Not checked — no full text of the sourcecites [47] Ohma, 2011, Analysis of proton exchange membrane fuel cell catalyst layers for reduction of platinum loading at Nissan, Electrochim. Acta source
- Supportedcites [48] Soboleva, 2010, On the Micro-, Meso-, and Macroporous Structures of Polymer Electrolyte Membrane Fuel Cell Catalyst Layers, ACS Appl. Mater. Interfaces source
The Carbon Powders section describes 2–20 nm pores within carbon-particle agglomerates and pores larger than 20 nm between agglomerates. The introductory section describes this as a bimodal pore-size distribution and calls the two groups primary and secondary pores. (LLM, conf=0.91)
plain- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
174 more claims · 32 with their cited sources checked
Create a free account to see all 344 claims and to verify the 4 references still open.
- Probably not a substantial claim. 57
- It may state two separate claims as one. 128
- The quote only partly states this claim. 1
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
Each contradiction between two passages listed here was confirmed by an independent check.
Rated minor: it would not touch a result — a value no result rests on, a p-value that stays on the same side of the significance level, or a conflict that is clerical, resolved elsewhere in the paper, or outside its own findings.
In the paper
§ Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells > 8. Concluding Remarks
“| Formamide | HCONH 2 | 111 | 3.34 | 210 | 57.03 | 16.6 | 17.2 | 26.2 | 19.0 |”
§ Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells > 4.3. Solvent
“δ = δ total = δ D 2 + δ P 2 + δ H 2 (3”
Rated minor: it would not touch a result — a value no result rests on, a p-value that stays on the same side of the significance level, or a conflict that is clerical, resolved elsewhere in the paper, or outside its own findings.
In the paper
“1 MPa 1/2 is equal to 2.0455 (cal/cm 3 ) 1/2 [129].”
§ Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells > 4.3. Solvent
Reported 2.0455 · recomputed 0.488878
Citations
Cites
Electrocatalyst approaches and challenges for automotive fuel cells
Debe, M. K. (2012) · Nature · doi:10.1038/nature11115 · Cited by 5,885 · cited 1×
“, internal combustion engines or other kinds of fuel cells, PEM fuel cells also have the advantages of high energy efficiency and low operation temperature [3,4].”
BackgroundHansen Solubility Parameters: A User's Handbook, Second Edition
Hansen, C. M. (2007) · CRC Press eBooks · doi:10.1201/9781420006834 · Cited by 3,156
New Insights into Perfluorinated Sulfonic-Acid Ionomers
Kusoglu, A., & Weber, A. Z. (2017) · Chemical Reviews · doi:10.1021/acs.chemrev.6b00159 · Cited by 2,432
Biaxially strained PtPb/Pt core/shell nanoplate boosts oxygen reduction catalysis
Bu, L., Zhang, N., Guo, S., Zhang, X., Li, J., Yao, J., Wu, T., Lu, G., Ma, J.-Y., Su, D., et al. (2016) · Science · doi:10.1126/science.aah6133 · Cited by 1,642
Ultrafine jagged platinum nanowires enable ultrahigh mass activity for the oxygen reduction reaction
Li, M., Zhao, Z., Cheng, T., Fortunelli, A., Chen, C.-Y., Yu, R., Zhang, Q., Gu, L., Merinov, B. V., Lin, Z., et al. (2016) · Science · doi:10.1126/science.aaf9050 · Cited by 1,605
Engineering bunched Pt-Ni alloy nanocages for efficient oxygen reduction in practical fuel cells
Tian, X., Zhao, X., Su, Y.-Q., Wang, L., Wang, H., Dang, D., Chi, B., Liu, H., Hensen, E. J. M., Lou, X. W. (., et al. (2019) · Science · doi:10.1126/science.aaw7493 · Cited by 1,527
Self-citationKonsistenzmessungen von Gummi-Benzollösungen
Herschel, W. H., & Bulkley, R. (1926) · Kolloid-Zeitschrift · doi:10.1007/bf01432034 · Cited by 1,499
New roads and challenges for fuel cells in heavy-duty transportation
Cullen, D. A., Neyerlin, K. C., Ahluwalia, R. K., Mukundan, R., More, K. L., Borup, R. L., Weber, A. Z., Myers, D. J., & Kusoglu, A. (2021) · Nature Energy · doi:10.1038/s41560-021-00775-z · Cited by 1,277
Wang, Y.-J., Zhao, N., Fang, B., Li, H., Bi, X. T., & Wang, H. (2015) · Chemical Reviews · doi:10.1021/cr500519c · Cited by 1,267 · cited 1×
“platinum (Pt)-based catalysts is necessary to promote the electrode reactions to supply the required performance and durability for practical application [5].”
BackgroundBoosting Fuel Cell Performance with Accessible Carbon Mesopores
Yarlagadda, V., Carpenter, M. K., Moylan, T. E., Kukreja, R. S., Koestner, R., Gu, W., Thompson, L., & Kongkanand, A. (2018) · ACS Energy Letters · doi:10.1021/acsenergylett.8b00186 · Cited by 686
Research works printed but not linked: 3
- Bird, B.R., Armstrong, R.C., and Hassager, O. (1987). Dynamics of Polymeric Liquids, Volume 1: Fluid Mechanics, Wiley-Interscience. [2nd ed.].
- (2022, March 21). Ion Exchange Materials. Available online: https://www.fuelcellearth.com/wp-content/uploads/converted_files/pdf/D520-D521-D1021-D2020-D2021-Product-Bulletin-Chemours.pdf.
- Rumble, J.R. (2017). CRC Handbook of Chemistry and Physics, CRC Press Taylor & Francis Group.
Cited by
(2023) · doi:10.1038/s41929-023-00949-w · Cited by 195
Bierling, M., McLaughlin, D., Mayerhöfer, B., & Thiele, S. (2023) · Advanced Energy Materials · doi:10.1002/aenm.202203636 · Cited by 59
Murugaiah, D. K., & Shahgaldi, S. (2024) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2024.04.036 · Cited by 57
Liu, P., Yang, D., Li, B., Zhang, C., & Ming, P. (2023) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2023.02.022 · Cited by 49
Liu, G., McLaughlin, D., Thiele, S., & Pham, C. V. (2022) · Chemical Engineering Journal · doi:10.1016/j.cej.2023.141757 · Cited by 45
Metadata
- Authors
- Liu, H., Ney, L., Zamel, N., & Li, X.
- Affiliations
- University of Waterloo (CA)
- Fraunhofer Institute for Solar Energy Systems (DE)
- Corresponding author
- Zamel, Nada
- Li, Xianguo
- Venue
- Applied Sciences
- Publisher
- MDPI AG
- Published
- 2022-04-08
- Volume
- 12
- Issue
- 8
- Pages
- 3776
- ISSN
- 2076-3417 (ISSN-L)
- OpenAlex
- W4224267685
- Cited by
- 85
- References
- 171
- Citations by year
- 2026: 21 · 2025: 26 · 2024: 26 · 2023: 11 · 2022: 1
- FWCI
- 4.38
- Type
- journal article
- Language
- en
- Open access
- gold
- doi.org
- Licence
- Locations
- Applied Sciences (publishedVersion, cc-by)
- DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion)
- Fraunhofer-Publica (Fraunhofer-Gesellschaft) (submittedVersion, cc-by)
- Fraunhofer-Publica (Fraunhofer-Gesellschaft)
- Funders
- Canadian Urban Transit Research and Innovation Consortium (160028)
- the Ministry of the Environment, Climate, Protection and the Energy Sector Baden-Württemberg (L75 20113)
- German National Innovation Program Hydrogen and Fuel Cell Technology and The Federal Ministry of Transport and Digital Infrastructur (03B11018A)
- Topics
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Fuel Cells and Related Materials
- Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › Electrocatalysts for Energy Conversion
- Physical Sciences › Materials Science › Materials Chemistry › Advancements in Solid Oxide Fuel Cells
- Keywords
- catalyst layer, proton exchange membrane fuel cells, catalyst ink, multiscale structure, ionomers, catalyst dispersion, coating application, drying, membrane electrode assembly, ink aging, catalyst microstructure
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
The claim verdicts this report counts are experimental: their accuracy is not yet measured.
A language model drew the claims from the paper on 2026-09-28, under version 3 of the claim definition (prompt extract-v3).
A second model labelled each claim on 2026-09-28 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).
Cited sources are checked with a language model’s help (gpt-6-sol).
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells. https://app.cochat.ai/papers/10.3390/app12083776
- The paper
- Liu, H., Ney, L., Zamel, N., & Li, X. (2022). Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells. Applied Sciences. https://doi.org/10.3390/app12083776
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.