Abstract

The structure of a catalyst layer (CL) significantly impacts the performance, durability, and cost of proton exchange membrane (PEM) fuel cells and is influenced by the catalyst ink and the CL formation process. This review focuses on the effect of the composition, formulation, and preparation of catalyst ink and the CL formation process on the CL structure.

Overview

CoChat Summary

TL;DR

This review synthesizes how the composition, formulation, and preparation of catalyst ink — and the subsequent coating and drying steps — govern the multiscale structure of conventional catalyst layers (CLs) in PEM fuel cells. It concludes that the ink–structure–performance relationship remains incompletely understood and that inconsistent literature conclusions stem from many simultaneously varying manufacturing variables.

Key findings

  • The CL is a three-dimensional network of Pt/C, ionomer, and pores with a multiscale structure: 2–5 nm Pt nanoparticles on 10–50 nm carbon black, ionomer films 3.5–20 nm thick, primary catalyst–ionomer agglomerates of a few hundred nm, and secondary agglomerates of a few µm, giving a bimodal pore distribution of 2–20 nm (primary) and >20 nm (secondary) pores; typical CL thickness is 5–10 µm.
  • Ink formulation controls ink microstructure and macroscopic properties: catalyst type (e.g., Pt/Ketjen ink is generally more viscous than Pt/Vulcan ink), ionomer type and I/C ratio, and solvent properties (dielectric constant, solubility parameter, viscosity, boiling point, surface tension). Ionomer adsorption follows a Langmuir-type plateau — absorbed ionomer rises from 0.25 to 0.50 I/C then stays nearly constant up to 1.00 I/C, while non-absorbed ionomer increases with I/C; the reported optimum Nafion content is 30 wt.% (I/C ≈ 0.7).
  • Ink preparation matters: premixing Pt/C, water, and ethanol before adding ionomer dispersion decreases agglomerate size and yields a more viscous, more homogeneous CL; insufficient dispersion leaves large agglomerates that raise proton, gas, and water transport resistance, while overly aggressive dispersion degrades Pt and ionomer.
  • CL formation process controls morphology: solid content requirements differ by technique (spray coating commonly <3 wt.%, e.g., ~0.6, ~1.8, or 2.5 wt.%; roll-to-roll commonly >5 wt.%, e.g., 5.76 wt.% or ~4.5–15 wt.%, up to 33.76 wt.% for screen printing); roll-to-roll can increase fabrication speed by over 500 times versus lab-scale spray coating; cracks arise from fast solvent evaporation, weak ionomer–catalyst interaction, or film defects.

Methods

  • Design: narrative review focused on conventional (ink-based) CLs, explicitly excluding structure-ordered CLs; the companion relationship between CL structure and cell performance/durability was covered in the authors' previous review.
  • Scope: (1) multiscale CL structure, (2) catalyst ink microstructure and macroscopic properties (rheology, surface tension, stability), (3) effects of catalyst, ionomer, I/C ratio, and solvent, (4) effects of mixing order and dispersion process, (5) CL formation (substrate, coating, drying), and (6) future directions.
  • Evidence base: synthesis of prior experimental and modeling literature, including characterization techniques such as DLS, SAS/SANS/SAXS, CV-SANS, ¹⁹F NMR, TEM/Cryo-TEM, SEM/Cryo-SEM, X-CT, and ELS (zeta potential), plus tabulated solvent and commercial ionomer dispersion properties.

Limitations

  • Stated by the paper: the relationship between ink formulation/preparation or CL formation and the multiscale CL structure (and ultimately performance and durability) is still unclear and sometimes inconsistent across studies; most ink characterization techniques require modifying the ink (dilution for DLS/ELS, consolidation for TEM/SEM) or only probe local structure; studies on high-solid-content ink, ink storage stability and reversibility of aged ink, and the drying process are limited; inconsistent conclusions arise when variables other than the one under study are not held constant.
  • Evident from the text: as a review, it reports no new primary data or meta-analysis; several quantitative values are cited from other works rather than generated here, and some passages (e.g., Table 3 entries and figure captions) are truncated or garbled in the provided text.

Model-written summary. Check it against the paper before relying on it.

Integrity signals

Registry

Crossref · 10.3390/app12083776

Cites

175 of 175 references verified0 citation errors · 0 not checkable

Statistics

Nothing to recompute.

Figures

Figure 1 Material-structure-properties relation of the CL (T: temperature, RH: relative humidity, Figure 1. Material-structure-properties relation of the CL (T: temperature, RH: relative humidity, P: pressure, ECSA: electrochemical active surface area).
Figure 1 Material-structure-properties relation of the CL (T: temperature, RH: relative humidity, Figure 1. Material-structure-properties relation of the CL (T: temperature, RH: relative humidity, P: pressure, ECSA: electrochemical active surface area).From the PDF
Figure 2 Illustration of ionomer-coated catalyst agglomerate [21,45]. Figure 2. Illustration of ionomer-coated catalyst agglomerate [21,45].
Figure 2 Illustration of ionomer-coated catalyst agglomerate [21,45]. Figure 2. Illustration of ionomer-coated catalyst agglomerate [21,45].From the PDF
Image 3
From the PDF
Figure 4 The effect of the formulation and preparation processes of catalyst ink on its microstructure and macroscopic properties and further on the fabricated CLs. Figure 4. The effect of the formulation and preparation processes of catalyst ink on its microstructure and macroscopic properties and further on the fabricated CLs.
Figure 4 The effect of the formulation and preparation processes of catalyst ink on its microstructure and macroscopic properties and further on the fabricated CLs. Figure 4. The effect of the formulation and preparation processes of catalyst ink on its microstructure and macroscopic properties and further on the fabricated CLs.From the PDF
Figure 5 Viscosity of Nafion ionomer dispersions ( a ), Pt/HSC dispersions ( b ), Pt/HSC and ionomer dispersions with a fixed 3 wt.% carbon ( c ) in 1-propanol and aqueous solvent mixture (3:1 mass ratio) at different concentrations or I/C ratios (Reprinted with permission from ref. [53]. Copyright (2018) American Chemical Society). Figure 5. Viscosity of Nafion ionomer dispersions ( a ), Pt/HSC dispersions ( b ), Pt/HSC and ionomer dispersions with a fixed 3 wt.% carbon ( c ) in 1-propanol and aqueous solvent mixture (3:1 mass ratio) at different concentrations or I/C ratios (Reprinted with permission from ref. [53]. Copyright (2018) American Chemical Society).
Figure 5 Viscosity of Nafion ionomer dispersions ( a ), Pt/HSC dispersions ( b ), Pt/HSC and ionomer dispersions with a fixed 3 wt.% carbon ( c ) in 1-propanol and aqueous solvent mixture (3:1 mass ratio) at different concentrations or I/C ratios (Reprinted with permission from ref. [53]. Copyright (2018) American Chemical Society). Figure 5. Viscosity of Nafion ionomer dispersions ( a ), Pt/HSC dispersions ( b ), Pt/HSC and ionomer dispersions with a fixed 3 wt.% carbon ( c ) in 1-propanol and aqueous solvent mixture (3:1 mass ratio) at different concentrations or I/C ratios (Reprinted with permission from ref. [53]. Copyright (2018) American Chemical Society).From the PDF
Figure 6 Schematics of the distribution of ionomer on carbon and Pt nanoparticles in the conventional case ( left ), the selective distribution of ionomer on only carbon surface through masking Pt nanoparticles ( right ), as well as the oxygen/proton transport in both cases. (Reprinted from Ref. [103] with permission from the Royal Society of Chemistry). Figure 6. Schematics of the distribution of ionomer on carbon and Pt nanoparticles in the conventional case ( left ), the selective distribution of ionomer on only carbon surface through masking Pt nanoparticles ( right ), as well as the oxygen/proton transport in both cases. (Reprinted from Ref. [103] with permission from the Royal Society of Chemistry).
Figure 6 Schematics of the distribution of ionomer on carbon and Pt nanoparticles in the conventional case ( left ), the selective distribution of ionomer on only carbon surface through masking Pt nanoparticles ( right ), as well as the oxygen/proton transport in both cases. (Reprinted from Ref. [103] with permission from the Royal Society of Chemistry). Figure 6. Schematics of the distribution of ionomer on carbon and Pt nanoparticles in the conventional case ( left ), the selective distribution of ionomer on only carbon surface through masking Pt nanoparticles ( right ), as well as the oxygen/proton transport in both cases. (Reprinted from Ref. [103] with permission from the Royal Society of Chemistry).From the PDF
Figure 7 The chemical structures of 3M PFIA ionomer, Nafion ionomer, 3M PFSA ionomer, and Aquivion ionomer [108,112]. Figure 7. The chemical structures of 3M PFIA ionomer, Nafion ionomer, 3M PFSA ionomer, and Aquivion ionomer [108,112].
Figure 7 The chemical structures of 3M PFIA ionomer, Nafion ionomer, 3M PFSA ionomer, and Aquivion ionomer [108,112]. Figure 7. The chemical structures of 3M PFIA ionomer, Nafion ionomer, 3M PFSA ionomer, and Aquivion ionomer [108,112].From the PDF
Figure 8 ( a ) The physical properties of solvent and their effects on the microstructure and macroscopic properties of catalyst ink, or evaporation rate; ( b ) the size and morphologies of Nafion ionomer in different solvents (Adapted with permission from [128], Copyright (2012) American Chemical Society; Reprinted from [26], Copyright (2013), with permission from Elsevier). Figure 8. ( a ) The physical properties of solvent and their effects on the microstructure and macroscopic properties of catalyst ink, or evaporation rate; ( b ) the size and morphologies of Nafion ionomer in different solvents (Adapted with permission from [128], Copyright (2012) American Chemical Society; Reprinted from [26], Copyright (2013), with permission from Elsevier).
Figure 8 ( a ) The physical properties of solvent and their effects on the microstructure and macroscopic properties of catalyst ink, or evaporation rate; ( b ) the size and morphologies of Nafion ionomer in different solvents (Adapted with permission from [128], Copyright (2012) American Chemical Society; Reprinted from [26], Copyright (2013), with permission from Elsevier). Figure 8. ( a ) The physical properties of solvent and their effects on the microstructure and macroscopic properties of catalyst ink, or evaporation rate; ( b ) the size and morphologies of Nafion ionomer in different solvents (Adapted with permission from [128], Copyright (2012) American Chemical Society; Reprinted from [26], Copyright (2013), with permission from Elsevier).From the PDF
Figure 9 The structures of Pt/C-Nafion ionomer and CL with insufficient ( a , d ), appropriate ( b , e ), and excessive ( c , f ) dispersion. (( a -c ) Modified with permission from [156], Copyright (2019), American Chemical Society; ( d -e ) Reprinted with permission from [24], Copyright (2019), American Chemical Society; ( f ) Reprinted from [159], Copyright (2014), with permission from Elsevier). Figure 9. The structures of Pt/C-Nafion ionomer and CL with insufficient ( a , d ), appropriate ( b , e ), and excessive ( c , f ) dispersion. (( a -c ) Modified with permission from [156], Copyright (2019), American Chemical Society; ( d -e ) Reprinted with permission from [24], Copyright (2019), American Chemical Society; ( f ) Reprinted from [159], Copyright (2014), with permission from Elsevier).
Figure 9 The structures of Pt/C-Nafion ionomer and CL with insufficient ( a , d ), appropriate ( b , e ), and excessive ( c , f ) dispersion. (( a -c ) Modified with permission from [156], Copyright (2019), American Chemical Society; ( d -e ) Reprinted with permission from [24], Copyright (2019), American Chemical Society; ( f ) Reprinted from [159], Copyright (2014), with permission from Elsevier). Figure 9. The structures of Pt/C-Nafion ionomer and CL with insufficient ( a , d ), appropriate ( b , e ), and excessive ( c , f ) dispersion. (( a -c ) Modified with permission from [156], Copyright (2019), American Chemical Society; ( d -e ) Reprinted with permission from [24], Copyright (2019), American Chemical Society; ( f ) Reprinted from [159], Copyright (2014), with permission from Elsevier).From the PDF
Figure 10 Three ways of fabricating catalyst coated membranes. Figure 10. Three ways of fabricating catalyst coated membranes.
Figure 10 Three ways of fabricating catalyst coated membranes. Figure 10. Three ways of fabricating catalyst coated membranes.From the PDF
Figure 11 Stylus profilometry traces of Nafion membrane ( a1 ), CL deposited on membrane (the surface facing the GDL) ( a2 ), GDL (the surface of MPL facing CL) ( b1 ), and CL of GDE (the surface facing the membrane) ( b2 ) (Reprinted from [75] with permission of John Wiley & Sons); ( c , d ) SEM images of cross-section view of the MEA. Cathode: a good CL/membrane interface due to the ionomer overlayer deposited on GDE; Anode: the observed gaps at the interface of MPL and CL which was deposited on the membrane, due to the high MPL surface roughness (root mean square surface roughness: 15.85 µm) (Reprinted with permission from [166]. Copyright (2019) American Chemical Society). The CCM-based MEAs, GDE-based MEAs, and DTM-based MEAs generally have Figure 11. Stylus profilometry traces of Nafion membrane ( a1 ), CL deposited on membrane (the surface facing the GDL) ( a2 ), GDL (the surface of MPL facing CL) ( b1 ), and CL of GDE (the surface facing the membrane) ( b2 ) (Reprinted from [75] with permission of John Wiley & Sons); ( c , d ) SEM images of cross-section view of the MEA. Cathode: a good CL/membrane interface due to the ionomer overlayer deposited on GDE; Anode: the observed gaps at the interface of MPL and CL which was deposited on the membrane, due to the high MPL surface roughness (root mean square surface roughness: 15.85 µ m) (Reprinted with permission from [166]. Copyright (2019) American Chemical Society).
Figure 11 Stylus profilometry traces of Nafion membrane ( a1 ), CL deposited on membrane (the surface facing the GDL) ( a2 ), GDL (the surface of MPL facing CL) ( b1 ), and CL of GDE (the surface facing the membrane) ( b2 ) (Reprinted from [75] with permission of John Wiley & Sons); ( c , d ) SEM images of cross-section view of the MEA. Cathode: a good CL/membrane interface due to the ionomer overlayer deposited on GDE; Anode: the observed gaps at the interface of MPL and CL which was deposited on the membrane, due to the high MPL surface roughness (root mean square surface roughness: 15.85 µm) (Reprinted with permission from [166]. Copyright (2019) American Chemical Society). The CCM-based MEAs, GDE-based MEAs, and DTM-based MEAs generally have Figure 11. Stylus profilometry traces of Nafion membrane ( a1 ), CL deposited on membrane (the surface facing the GDL) ( a2 ), GDL (the surface of MPL facing CL) ( b1 ), and CL of GDE (the surface facing the membrane) ( b2 ) (Reprinted from [75] with permission of John Wiley & Sons); ( c , d ) SEM images of cross-section view of the MEA. Cathode: a good CL/membrane interface due to the ionomer overlayer deposited on GDE; Anode: the observed gaps at the interface of MPL and CL which was deposited on the membrane, due to the high MPL surface roughness (root mean square surface roughness: 15.85 µ m) (Reprinted with permission from [166]. Copyright (2019) American Chemical Society).From the PDF
Figure 12 ( a ) Schematic of the roll-to-roll manufacturing process coupled with slot-die coating, (Reprinted from [165], Copyright (2020), with permission from Elsevier), ( b ) illustration of slot-die coating (Adapted from [39], Copyright (2019), with permission from Elsevier), ( c ) illustration of gravure coating (Adapted from [38]). Figure 12. ( a ) Schematic of the roll-to-roll manufacturing process coupled with slot-die coating, (Reprinted from [165], Copyright (2020), with permission from Elsevier), ( b ) illustration of slot-die coating (Adapted from [39], Copyright (2019), with permission from Elsevier), ( c ) illustration of gravure coating (Adapted from [38]).
Figure 12 ( a ) Schematic of the roll-to-roll manufacturing process coupled with slot-die coating, (Reprinted from [165], Copyright (2020), with permission from Elsevier), ( b ) illustration of slot-die coating (Adapted from [39], Copyright (2019), with permission from Elsevier), ( c ) illustration of gravure coating (Adapted from [38]). Figure 12. ( a ) Schematic of the roll-to-roll manufacturing process coupled with slot-die coating, (Reprinted from [165], Copyright (2020), with permission from Elsevier), ( b ) illustration of slot-die coating (Adapted from [39], Copyright (2019), with permission from Elsevier), ( c ) illustration of gravure coating (Adapted from [38]).From the PDF
Figure 13 Weight change of the ink film at different drying conditions (20 or 40 °C, dry-0% R humid-80% RH) and the schematics of the structure change from the ink film to the dried CL (R printed from [56], Copyright (2016), with permission from Elsevier). Figure 13. Weight change of the ink film at different drying conditions (20 or 40 ◦ C, dry-0% RH, humid-80% RH) and the schematics of the structure change from the ink film to the dried CL (Reprinted from [56], Copyright (2016), with permission from Elsevier).
Figure 13 Weight change of the ink film at different drying conditions (20 or 40 °C, dry-0% R humid-80% RH) and the schematics of the structure change from the ink film to the dried CL (R printed from [56], Copyright (2016), with permission from Elsevier). Figure 13. Weight change of the ink film at different drying conditions (20 or 40 ◦ C, dry-0% RH, humid-80% RH) and the schematics of the structure change from the ink film to the dried CL (Reprinted from [56], Copyright (2016), with permission from Elsevier).From the PDF

Verification

Claims the paper makes

61 Valid · 20 Not valid · 137 Not checked · 126 Own results and interpretations

174 more claims · 32 with their cited sources checked

Create a free account to see all 344 claims and to verify the 4 references still open.

See all claims — free account
  • Probably not a substantial claim. 57
  • It may state two separate claims as one. 128
  • The quote only partly states this claim. 1

Create a free account to see these claims.

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

Each contradiction between two passages listed here was confirmed by an independent check.

2 of 2

Citations

Cites

Research works printed but not linked: 3

  1. Bird, B.R., Armstrong, R.C., and Hassager, O. (1987). Dynamics of Polymeric Liquids, Volume 1: Fluid Mechanics, Wiley-Interscience. [2nd ed.].
  2. (2022, March 21). Ion Exchange Materials. Available online: https://www.fuelcellearth.com/wp-content/uploads/converted_files/pdf/D520-D521-D1021-D2020-D2021-Product-Bulletin-Chemours.pdf.
  3. Rumble, J.R. (2017). CRC Handbook of Chemistry and Physics, CRC Press Taylor & Francis Group.

Metadata

Authors
Liu, H., Ney, L., Zamel, N., & Li, X.
Affiliations
  • University of Waterloo (CA)
  • Fraunhofer Institute for Solar Energy Systems (DE)
Corresponding author
  • Zamel, Nada
  • Li, Xianguo
Venue
Applied Sciences
Publisher
MDPI AG
Published
2022-04-08
Volume
12
Issue
8
Pages
3776
ISSN
2076-3417 (ISSN-L)
OpenAlex
W4224267685
Cited by
85
References
171
Citations by year
2026: 21 · 2025: 26 · 2024: 26 · 2023: 11 · 2022: 1
FWCI
4.38
Type
journal article
Language
en
Open access
Locations
  • Applied Sciences (publishedVersion, cc-by)
  • DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion)
  • Fraunhofer-Publica (Fraunhofer-Gesellschaft) (submittedVersion, cc-by)
  • Fraunhofer-Publica (Fraunhofer-Gesellschaft)
Funders
  • Canadian Urban Transit Research and Innovation Consortium (160028)
  • the Ministry of the Environment, Climate, Protection and the Energy Sector Baden-Württemberg (L75 20113)
  • German National Innovation Program Hydrogen and Fuel Cell Technology and The Federal Ministry of Transport and Digital Infrastructur (03B11018A)
Topics
  • Physical Sciences › Engineering › Electrical and Electronic Engineering › Fuel Cells and Related Materials
  • Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › Electrocatalysts for Energy Conversion
  • Physical Sciences › Materials Science › Materials Chemistry › Advancements in Solid Oxide Fuel Cells
Keywords
catalyst layer, proton exchange membrane fuel cells, catalyst ink, multiscale structure, ionomers, catalyst dispersion, coating application, drying, membrane electrode assembly, ink aging, catalyst microstructure

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

The claim verdicts this report counts are experimental: their accuracy is not yet measured.

A language model drew the claims from the paper on 2026-09-28, under version 3 of the claim definition (prompt extract-v3).

A second model labelled each claim on 2026-09-28 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).

Cited sources are checked with a language model’s help (gpt-6-sol).

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.