Abstract

This comprehensive review explores the expansive design space of network architectures and their significant impact on the mechanical and viscoelastic properties of hydrogel systems. By examining the intricate relationships between molecular structure, network connectivity, and resulting bulk properties, we provide critical insights into rational design strategies for tailoring hydrogel mechanics for specific applications. Recent advances in sequence-defined crosslinkers, dynamic covalent chemistries, and biomimetic approaches have significantly expanded the toolbox for creating hydrogels with precisely controlled viscoelasticity, stiffness, and stress relaxation behavior—properties that are crucial for biomedical applications, particularly in tissue engineering and regenerative medicine.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.3390/gels11080588

Cites

163 of 163 references verified0 citation errors · 0 not checkable

Statistics

Figures

Figure 1 Schematic representation of crosslinker architectures highlighting the progression from linear (difunctional) to increasingly complex topologies such as branched, star-shaped, dendritic, and side-chain structures. The number of reactive sites (f) increases across this spectrum, leading to higher crosslinking density, network connectivity, stiffness, and elasticity, while simultaneously reducing chain flexibility, mesh size, swelling, permeability, and network homogeneity. This structural continuum underscores how crosslinker design serves as a versatile handle for tuning hydrogel mechanics and transport properties.
Figure 1 Schematic representation of crosslinker architectures highlighting the progression from linear (difunctional) to increasingly complex topologies such as branched, star-shaped, dendritic, and side-chain structures. The number of reactive sites (f) increases across this spectrum, leading to higher crosslinking density, network connectivity, stiffness, and elasticity, while simultaneously reducing chain flexibility, mesh size, swelling, permeability, and network homogeneity. This structural continuum underscores how crosslinker design serves as a versatile handle for tuning hydrogel mechanics and transport properties.CC BY · PubMed Central
Figure 2 Reversible bond exchange governing dynamic equilibrium in hydrogel networks.
Figure 2 Reversible bond exchange governing dynamic equilibrium in hydrogel networks.CC BY · PubMed Central
Figure 3 Tunable mechanical properties in recombinant ELP hydrogels through modular crosslinking design. (A) Schematic representation of strain-promoted azide-alkyne cycloaddition (SPAAC) used to crosslink azide-functionalized elastin-like proteins (ELPs) with BCN-bearing counterparts. (B) Rheological time sweep curves comparing gelation kinetics of SPAAC- and Staudin ger-crosslinked ELPs at two time scales ((i) and (ii), respectively). (C) Frequency sweep data showing the effect of crosslinking stoichiometry (BCN:ELP ratio). Reproduced with permission from Madl et al., Advanced Functional Materials; published by John Wiley & Sons, 2016 [96].
Figure 3 Tunable mechanical properties in recombinant ELP hydrogels through modular crosslinking design. (A) Schematic representation of strain-promoted azide-alkyne cycloaddition (SPAAC) used to crosslink azide-functionalized elastin-like proteins (ELPs) with BCN-bearing counterparts. (B) Rheological time sweep curves comparing gelation kinetics of SPAAC- and Staudin ger-crosslinked ELPs at two time scales ((i) and (ii), respectively). (C) Frequency sweep data showing the effect of crosslinking stoichiometry (BCN:ELP ratio). Reproduced with permission from Madl et al., Advanced Functional Materials; published by John Wiley & Sons, 2016 [96].CC BY · PubMed Central
Figure 4 Enzymatic crosslinking strategy and its impact on hydrogel mechanical properties. (A) (i) Functionalization of silk fibroin (SF) and gelatin (G) with tyramine (TA) to generate phenol-containing precursors (SF-TA, G-TA); (ii) subsequent enzymatic crosslinking via horseradish peroxidase (HRP) and H2O2 leads to covalently bonded hydrogels. (B) Time sweep rheology showing gelation kinetics of 3% hydrogels with 0.005% and 0.01% H2O2. (C) Gelation time points of 3% (w/v) silk-based hydrogels varying H2O2 concentrations, determined from rheological time sweep analysis. (D) G′ at equilibrium for the same formulations (n = 3, * p < 0.05, ** p < 0.01, and *** p < 0.001). (E) Mesh sizes for SF and G formulations calculated by rubber elasticity theory are shown as a function of functionalized biopolymer composition and H2O2 concentration. Reproduced with permission from Hasturk et al., Biomaterials; published by Elsevier, 2020 [97].
Figure 4 Enzymatic crosslinking strategy and its impact on hydrogel mechanical properties. (A) (i) Functionalization of silk fibroin (SF) and gelatin (G) with tyramine (TA) to generate phenol-containing precursors (SF-TA, G-TA); (ii) subsequent enzymatic crosslinking via horseradish peroxidase (HRP) and H2O2 leads to covalently bonded hydrogels. (B) Time sweep rheology showing gelation kinetics of 3% hydrogels with 0.005% and 0.01% H2O2. (C) Gelation time points of 3% (w/v) silk-based hydrogels varying H2O2 concentrations, determined from rheological time sweep analysis. (D) G′ at equilibrium for the same formulations (n = 3, * p < 0.05, ** p < 0.01, and *** p < 0.001). (E) Mesh sizes for SF and G formulations calculated by rubber elasticity theory are shown as a function of functionalized biopolymer composition and H2O2 concentration. Reproduced with permission from Hasturk et al., Biomaterials; published by Elsevier, 2020 [97].CC BY · PubMed Central
Figure 5 Effect of different PETRA concentrations (% w/w) on PEO hydrogels. (A) Representation of PEO radical generation using PETRA. (B) Swelling behavior over time. (C) Percentage elongation at break. (D) Young’s modulus. (E) Tensile strength (n = 3; * significant differences between all groups; ** significantly different from PETRA concentrations = 5% and 10% w/w; *** significantly different from PETRA concentration = 1% w/w; p < 0.05). Reproduced with permission from Wong et al., Pharmaceutics; published by MDPI, 2015 [93].
Figure 5 Effect of different PETRA concentrations (% w/w) on PEO hydrogels. (A) Representation of PEO radical generation using PETRA. (B) Swelling behavior over time. (C) Percentage elongation at break. (D) Young’s modulus. (E) Tensile strength (n = 3; * significant differences between all groups; ** significantly different from PETRA concentrations = 5% and 10% w/w; *** significantly different from PETRA concentration = 1% w/w; p < 0.05). Reproduced with permission from Wong et al., Pharmaceutics; published by MDPI, 2015 [93].CC BY · PubMed Central
Figure 6 (A) Preparation scheme of poly(NIPAM-co-AAc) hydrogels. (B) Mesh size variation in poly(NIPAM) hydrogels as a function of crosslinker concentration (Ccl), measured using three different methods: rheology (cubic and spherical models), dynamic swelling, and probe diffusion via PGSE NMR. Reproduced with permission from Wisniewska et al., Journal of Applied Polymer Science; published by John Wiley & Sons, 2018 [101].
Figure 6 (A) Preparation scheme of poly(NIPAM-co-AAc) hydrogels. (B) Mesh size variation in poly(NIPAM) hydrogels as a function of crosslinker concentration (Ccl), measured using three different methods: rheology (cubic and spherical models), dynamic swelling, and probe diffusion via PGSE NMR. Reproduced with permission from Wisniewska et al., Journal of Applied Polymer Science; published by John Wiley & Sons, 2018 [101].CC BY · PubMed Central
Figure 7 (A) Schematic representation of the different gel network design: (i) two tetra-PEG (4 × 4) network; (ii) tetra-functional (2 × 4) PEG network system with case A, representing a complete network, whereas case B represents an incomplete network. Blob size dependence on molecular weight between crosslinkers (Mc) for (B) case A and (C) case B. (D) Correlation blob size (ξc) in function of total polymer volume fraction (φ). Reproduced with permission from Tsuji et al., Gels; published by MDPI, 2018 [106].
Figure 7 (A) Schematic representation of the different gel network design: (i) two tetra-PEG (4 × 4) network; (ii) tetra-functional (2 × 4) PEG network system with case A, representing a complete network, whereas case B represents an incomplete network. Blob size dependence on molecular weight between crosslinkers (Mc) for (B) case A and (C) case B. (D) Correlation blob size (ξc) in function of total polymer volume fraction (φ). Reproduced with permission from Tsuji et al., Gels; published by MDPI, 2018 [106].CC BY · PubMed Central
Figure 8 Rheological characterizations of SCX, LX, and SX hydrogels. (A) Schematic representation of side-chain crosslinker (SCX) (i), linear crosslinker (LX) (ii), and star crosslinker (SX) (iii) architectures. (B) The stress relaxation half-time and elastic modulus of hydrazone hydrogels with SCX, LX, and SX. (C) Stress relaxation half-time of LX (i) and SX (ii) hydrogels with varying linear polyethylene glycol-dialdehyde (PEG-2ALD) and four-arm polyethylene glycol-aldehyde (PEG-4ALD) cross-linker concentration of different MWs. (D) Loss tangent (i), and stress relaxation half-times (ii) of SCX hydrogels with varying total cross-linker concentration, maintaining an alginate–hydrazone (AG-HYD) to alginate–aldehyde (AG-ALD) ratio of 1:1. n = 3, 4, 2, and 4 replicates for 1, 2, 3, and 4 wt.%, respectively. Data are presented as mean ± SD. One-way ANOVA with Tukey’s post hoc test. * p ≤ 0.05, ** p ≤ 0.01. (E) Loss tangent (i), and stress relaxation half-time (ii) of hydrogels with varying AG-HYD to AG-ALD ratios, all at a total cross-linker concentration of 2 wt.%. n = 1, 1, 4, 1, and one replicate for 3:1, 2:1, 1:1, 1:2, and 1:3 ratios, respectively. Data are presented as mean ± SD. One-way ANOVA with Tukey’s post hoc test. * p ≤ 0.05, ** p ≤ 0.01. (F) Elastic modulus (i) and stress relaxation half-time (ii) of LX versus SX hydrogels. Data are presented as mean ± SD. Multiple unpaired Welch’s t-test with Holm-Šídák multiple comparison. * p ≤ 0.05, ** p ≤ 0.01, *** p ≤ 0.001, **** p ≤ 0.0001. Reproduced with permission from Lin et al., Advanced Healthcare Materials; published by John Wiley & Sons, 2024 [27].
Figure 8 Rheological characterizations of SCX, LX, and SX hydrogels. (A) Schematic representation of side-chain crosslinker (SCX) (i), linear crosslinker (LX) (ii), and star crosslinker (SX) (iii) architectures. (B) The stress relaxation half-time and elastic modulus of hydrazone hydrogels with SCX, LX, and SX. (C) Stress relaxation half-time of LX (i) and SX (ii) hydrogels with varying linear polyethylene glycol-dialdehyde (PEG-2ALD) and four-arm polyethylene glycol-aldehyde (PEG-4ALD) cross-linker concentration of different MWs. (D) Loss tangent (i), and stress relaxation half-times (ii) of SCX hydrogels with varying total cross-linker concentration, maintaining an alginate–hydrazone (AG-HYD) to alginate–aldehyde (AG-ALD) ratio of 1:1. n = 3, 4, 2, and 4 replicates for 1, 2, 3, and 4 wt.%, respectively. Data are presented as mean ± SD. One-way ANOVA with Tukey’s post hoc test. * p ≤ 0.05, ** p ≤ 0.01. (E) Loss tangent (i), and stress relaxation half-time (ii) of hydrogels with varying AG-HYD to AG-ALD ratios, all at a total cross-linker concentration of 2 wt.%. n = 1, 1, 4, 1, and one replicate for 3:1, 2:1, 1:1, 1:2, and 1:3 ratios, respectively. Data are presented as mean ± SD. One-way ANOVA with Tukey’s post hoc test. * p ≤ 0.05, ** p ≤ 0.01. (F) Elastic modulus (i) and stress relaxation half-time (ii) of LX versus SX hydrogels. Data are presented as mean ± SD. Multiple unpaired Welch’s t-test with Holm-Šídák multiple comparison. * p ≤ 0.05, ** p ≤ 0.01, *** p ≤ 0.001, **** p ≤ 0.0001. Reproduced with permission from Lin et al., Advanced Healthcare Materials; published by John Wiley & Sons, 2024 [27].CC BY · PubMed Central
Figure 9 Graphical representation (A) of different physically assembled SDC hydrogel networks. (B) Rheological analysis of 4-SDC (i), 8-SDC (ii), and 16-SDC (iii) hydrogels using dynamic amplitude sweep at 5.0 wt % (γ = 0.1% for 240 s (white), then γ = 40% for 240 s (red), then γ = 0.1% for 240 s, then γ = 40% for 240 s, then γ = 0.1% for 240 s, all at ω = 1 rad/s). Reproduced with permission from Cosgrave et al., Biomacromolecules; published by American Chemical Society, 2024 [26].
Figure 9 Graphical representation (A) of different physically assembled SDC hydrogel networks. (B) Rheological analysis of 4-SDC (i), 8-SDC (ii), and 16-SDC (iii) hydrogels using dynamic amplitude sweep at 5.0 wt % (γ = 0.1% for 240 s (white), then γ = 40% for 240 s (red), then γ = 0.1% for 240 s, then γ = 40% for 240 s, then γ = 0.1% for 240 s, all at ω = 1 rad/s). Reproduced with permission from Cosgrave et al., Biomacromolecules; published by American Chemical Society, 2024 [26].CC BY · PubMed Central
Figure 10 Schematic representation of two polymer network architectures: (A) crosslinking of linear polymers and (B) end-linking of star-shaped polymers. (C–E) Chemical structures of: (C) hydrazine and aldehyde functionalized HA, (D) hydrazine and aldehyde functionalized PEG, and (E) catalyst used to accelerate hydrazone exchange. Reproduced with permission from Lou et al., Advanced Materials; published by John Wiley & Sons, 2021 [62].
Figure 10 Schematic representation of two polymer network architectures: (A) crosslinking of linear polymers and (B) end-linking of star-shaped polymers. (C–E) Chemical structures of: (C) hydrazine and aldehyde functionalized HA, (D) hydrazine and aldehyde functionalized PEG, and (E) catalyst used to accelerate hydrazone exchange. Reproduced with permission from Lou et al., Advanced Materials; published by John Wiley & Sons, 2021 [62].CC BY · PubMed Central
Figure 11 Comparison of the mechanical properties of branched hydrogels at different triene compositions. (A) Master curves at 25 °C from oscillatory shear and creep experiments; (B) comparison of the high-frequency moduli; (C) comparison of the entanglement moduli, determined from the converted low-frequency plateau. Reproduced with permission from Tang et al., Frontiers in Chemistry; published by Frontiers, 2014 [112].
Figure 11 Comparison of the mechanical properties of branched hydrogels at different triene compositions. (A) Master curves at 25 °C from oscillatory shear and creep experiments; (B) comparison of the high-frequency moduli; (C) comparison of the entanglement moduli, determined from the converted low-frequency plateau. Reproduced with permission from Tang et al., Frontiers in Chemistry; published by Frontiers, 2014 [112].CC BY · PubMed Central
Figure 12 (A) Schematic of a hydrogel made from force-responsive crosslinkers and LBMs, including TIP-1:Kir, GB1, HP67, and SH3 domains. Mechanical performance of Gel-3 mediated by reversibly unfolding SH3 domains. (B) Stress–strain curve for Gel-3 under uniaxial tension. (C) Representative loading–unloading cycles for Gel-3 at increasing strain levels. (D) Theoretical modeling of Gel-3 stress–strain behavior under cyclic loading. (E) Fraction of unfolded SH3 domains increases with applied strain. Reproduced with permission from Wu et al., Nature Communications; published by Nature, 2018 [116].
Figure 12 (A) Schematic of a hydrogel made from force-responsive crosslinkers and LBMs, including TIP-1:Kir, GB1, HP67, and SH3 domains. Mechanical performance of Gel-3 mediated by reversibly unfolding SH3 domains. (B) Stress–strain curve for Gel-3 under uniaxial tension. (C) Representative loading–unloading cycles for Gel-3 at increasing strain levels. (D) Theoretical modeling of Gel-3 stress–strain behavior under cyclic loading. (E) Fraction of unfolded SH3 domains increases with applied strain. Reproduced with permission from Wu et al., Nature Communications; published by Nature, 2018 [116].CC BY · PubMed Central
Figure 13 (A) Schematic of the dynamic imine-crosslinked hydrogel: (i) reversible imine bond formation and (ii) network illustration of biomimetic responses under mechanical strain. Rheological evaluation of CC/DP8k hydrogels under increasing deformation: (B) G′ and G″ during cyclic strain sweeps. (C) G′/G0 ratios at γ = 1%. (D) G′ and G″ under alternating cycles of low and extreme strain. Reproduced with permission from Liu et al., ACS Applied Materials and Interfaces; published by American Chemical Society, 2022 [118].
Figure 13 (A) Schematic of the dynamic imine-crosslinked hydrogel: (i) reversible imine bond formation and (ii) network illustration of biomimetic responses under mechanical strain. Rheological evaluation of CC/DP8k hydrogels under increasing deformation: (B) G′ and G″ during cyclic strain sweeps. (C) G′/G0 ratios at γ = 1%. (D) G′ and G″ under alternating cycles of low and extreme strain. Reproduced with permission from Liu et al., ACS Applied Materials and Interfaces; published by American Chemical Society, 2022 [118].CC BY · PubMed Central
Figure 14 Theoretical and experimental validation of a double-network hydrogel system combining covalent and ionic crosslinking. (A) Schematic representation of network architectures: (i) single-network versus double-network hydrogel; (ii) classification of double-network hydrogels based on their crosslinking types, including chemically and physically crosslinked configurations. Reproduced with permission from Yin et al., Advances in Colloid and Interface Science; published by Elsevier, 2023 [121]. (iii) SF-PG double-network hydrogel. (B) Compressive modulus of SF–PG hydrogels made with 60 or 120 min MD silk fibroin (n = 5, *** p < 0.001). (C) Stress–strain curves for 120 min MD SF–PG hydrogels over seven days. (D) Quantified compressive modulus over seven days of cyclic treatment (n = 5, *** p < 0.001). Reproduced with permission from Hasturk et al., Polymer; published by Elsevier, 2023 [122].
Figure 14 Theoretical and experimental validation of a double-network hydrogel system combining covalent and ionic crosslinking. (A) Schematic representation of network architectures: (i) single-network versus double-network hydrogel; (ii) classification of double-network hydrogels based on their crosslinking types, including chemically and physically crosslinked configurations. Reproduced with permission from Yin et al., Advances in Colloid and Interface Science; published by Elsevier, 2023 [121]. (iii) SF-PG double-network hydrogel. (B) Compressive modulus of SF–PG hydrogels made with 60 or 120 min MD silk fibroin (n = 5, *** p < 0.001). (C) Stress–strain curves for 120 min MD SF–PG hydrogels over seven days. (D) Quantified compressive modulus over seven days of cyclic treatment (n = 5, *** p < 0.001). Reproduced with permission from Hasturk et al., Polymer; published by Elsevier, 2023 [122].CC BY · PubMed Central
Figure 15 Structural design and mechanical reinforcement in PEG–alginate double-network (DN) hydrogels. (A(i–iii)) Chemical structures and network schematics for PEGDA, PEGDMA, and PEG4AC, along with representative architectures of SN and DN hydrogels formed with linear PEG (top) or four-arm PEG (bottom). Mechanical characterization comparing linear and four-arm PEG-based SN and DN systems: (B) compressive modulus, (C) compressive strength, and (D) toughness. Strain-rate sensitivity analysis for four-arm PEG-based hydrogels: (E) compressive modulus and (F) toughness at 0.01 mm/s and 0.1 mm/s (The label “n.s.” indicates that the statistical tests did not reveal a significant difference and “*” represents a significant difference with p < 0.05). Reproduced with permission from Huang et al., Acta Biomaterialia; published by Elsevier, 2022 [123].
Figure 15 Structural design and mechanical reinforcement in PEG–alginate double-network (DN) hydrogels. (A(i–iii)) Chemical structures and network schematics for PEGDA, PEGDMA, and PEG4AC, along with representative architectures of SN and DN hydrogels formed with linear PEG (top) or four-arm PEG (bottom). Mechanical characterization comparing linear and four-arm PEG-based SN and DN systems: (B) compressive modulus, (C) compressive strength, and (D) toughness. Strain-rate sensitivity analysis for four-arm PEG-based hydrogels: (E) compressive modulus and (F) toughness at 0.01 mm/s and 0.1 mm/s (The label “n.s.” indicates that the statistical tests did not reveal a significant difference and “*” represents a significant difference with p < 0.05). Reproduced with permission from Huang et al., Acta Biomaterialia; published by Elsevier, 2022 [123].CC BY · PubMed Central
Figure 16 (A) Chemical specification for each peptoid crosslinker. (B) Peptoid-crosslinkers structures used as an architecture design to modulate bulk hydrogel mechanics. (C) Storage moduli via oscillatory rheometry for different hydrogel formulations. (D(i,ii)). Proliferation quantified for different hydrogel formulations (* denotes p < 0.05, ** p < 0.01, *** p < 0.001, **** p < 0.0001. All statistics were calculated by one-way ANOVA with post-hoc Tukey HSD test. & indicates p < 0.01 and # indicates p < 0.0001 between that condition with and without IFN-γ). Reproduced with permission from Morton et al., Acta Biomaterialia; published by Elsevier, 2023 [38].
Figure 16 (A) Chemical specification for each peptoid crosslinker. (B) Peptoid-crosslinkers structures used as an architecture design to modulate bulk hydrogel mechanics. (C) Storage moduli via oscillatory rheometry for different hydrogel formulations. (D(i,ii)). Proliferation quantified for different hydrogel formulations (* denotes p < 0.05, ** p < 0.01, *** p < 0.001, **** p < 0.0001. All statistics were calculated by one-way ANOVA with post-hoc Tukey HSD test. & indicates p < 0.01 and # indicates p < 0.0001 between that condition with and without IFN-γ). Reproduced with permission from Morton et al., Acta Biomaterialia; published by Elsevier, 2023 [38].CC BY · PubMed Central

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 163 references

Cited by

See all 97

Metadata

Authors
Roca-Arroyo, A. F., Gutierrez-Rivera, J. A., Morton, L. D., & Castilla-Casadiego, D. A.
Affiliations
  • University of Miami (US)
  • Tufts University (US)
  • Department of Biomedical Engineering, University of Miami, Coral Gables, FL 33146, USA
Corresponding author
Morton, Logan D.
Venue
Gels
Publisher
MDPI AG
Published
2025-07-30
Volume
11
Issue
8
Pages
588
ISSN
2310-2861 (ISSN-L)
OpenAlex
W4412750500
Cited by
88
References
163
Citations by year
2026: 76 · 2025: 12
FWCI
5.66
Type
journal article
Language
en
Open access
Locations
  • Gels (publishedVersion, cc-by)
  • Europe PMC (PubMed Central) (publishedVersion, cc-by)
  • PubMed Central (publishedVersion, cc-by)
  • PubMed (publishedVersion)
  • DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion, cc-by-sa)
Funders
National Institute of General Medical Sciences of the National Institutes of Health (R00GM151459)
Topics
  • Physical Sciences › Materials Science › Biomaterials › Hydrogels: synthesis, properties, applications
  • Physical Sciences › Engineering › Mechanical Engineering › Advanced Materials and Mechanics
  • Physical Sciences › Materials Science › Biomaterials › Silk-based biomaterials and applications
Keywords
hydrogels, network architecture, dynamic covalent chemistry, viscoelasticity, mechanical properties, stress relaxation, stiffness, network connectivity, biomimetic hydrogels, tissue engineering, regenerative medicine

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Hydrogel Network Architecture Design Space: Impact on Mechanical and Viscoelastic Properties. https://app.cochat.ai/papers/10.3390/gels11080588
The paper
Roca-Arroyo, A. F., Gutierrez-Rivera, J. A., Morton, L. D., & Castilla-Casadiego, D. A. (2025). Hydrogel Network Architecture Design Space: Impact on Mechanical and Viscoelastic Properties. Gels. https://doi.org/10.3390/gels11080588

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.