CoChat

Methacrylated Silk Fibroin Additive Manufacturing of Shape Memory Constructs with Possible Application in Bone Regeneration

Open access

The DOI matches its Crossref record; 51 of the 53 references it cites were found in a registry or an index.

Abstract

Methacrylated silk (Sil-MA) is a chemically modified silk fibroin specifically designed to be crosslinkable under UV light, which makes this material applicable in additive manufacturing techniques and allows the prototyping and development of patient-specific 2D or 3D constructs. In this study, we produced a thin grid structure based on crosslinked Sil-MA that can be withdrawn and ejected and that can recover its shape after rehydration. A complete chemical and physical characterization of Sil-MA was first conducted. Additionally, we tested Sil-MA biocompatibility according to the International Standard Organization protocols (ISO 10993) ensuring the possibility of using it in future trials. Sil-MA was also tested to verify its ability to support osteogenesis. Overall, Sil-MA was shown to be biocompatible and osteoconductive. Finally, two different additive manufacturing technologies, a Digital Light Processing (DLP) UV projector and a pneumatic extrusion technique, were used to develop a Sil-MA grid construct. A proof-of-concept of its shape-memory property was provided. Together, our data support the hypothesis that Sil-MA grid constructs can be injectable and applicable in bone regeneration applications.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.3390/gels8120833

Cites

51 of 51 references verified0 citation errors · 0 not checkable

Statistics

Figures

Figure 1 (A) FTIR-ATR spectra of regenerated silk fibroin (rSF) and methacrylated silk fibroin (Sil-MA); as reference, the spectrum of glycidyl methacrylate (GMA) was reported. Several modifications (indicated by yellow areas) of the Sil-MA spectra compared to the rSF spectra could be attributed to the presence of functional groups. (B) Calibration curve done using β alanine and the TNBS assay and used to determine the percentage of functional groups in Sil-MA. (C,D) NMR spectra of (C) rSF and (D) Sil-MA; the peaks present in Sil-MA but not in rSF are numbered and highlighted in red; they confirm the functionalization, except for peak 3, which is the lysine contribution.
Figure 1 (A) FTIR-ATR spectra of regenerated silk fibroin (rSF) and methacrylated silk fibroin (Sil-MA); as reference, the spectrum of glycidyl methacrylate (GMA) was reported. Several modifications (indicated by yellow areas) of the Sil-MA spectra compared to the rSF spectra could be attributed to the presence of functional groups. (B) Calibration curve done using β alanine and the TNBS assay and used to determine the percentage of functional groups in Sil-MA. (C,D) NMR spectra of (C) rSF and (D) Sil-MA; the peaks present in Sil-MA but not in rSF are numbered and highlighted in red; they confirm the functionalization, except for peak 3, which is the lysine contribution.CC BY · PubMed Central
Figure 2 (A) Storage (G′) and loss (G″) moduli reported in the function of the oscillation strain (in log scale); all the curve results were linear up to 1%. (B) Tan δ in the functioning of the oscillation strain; the trend for the 5 s crosslinked material was different from the other due to the incomplete crosslinking. (C) G′ and G″ in the functioning of the angular frequency at a constant strain of 1%. (D) Tan δ in the functioning of the angular frequency with a constant strain of 1%. (E) Swelling ratio during 72 h with different exposure times (5 s and 30 s); as expected, the less exposed samples tend to sell faster, reaching a higher amount of incorporated water.
Figure 2 (A) Storage (G′) and loss (G″) moduli reported in the function of the oscillation strain (in log scale); all the curve results were linear up to 1%. (B) Tan δ in the functioning of the oscillation strain; the trend for the 5 s crosslinked material was different from the other due to the incomplete crosslinking. (C) G′ and G″ in the functioning of the angular frequency at a constant strain of 1%. (D) Tan δ in the functioning of the angular frequency with a constant strain of 1%. (E) Swelling ratio during 72 h with different exposure times (5 s and 30 s); as expected, the less exposed samples tend to sell faster, reaching a higher amount of incorporated water.CC BY · PubMed Central
Figure 3 (A) Graph of LDH assay; (B) graph of Alamar Blue assay; (C) graph of Pico Green assay; (E) Representative confocal images on days 1, 3, and 6; (D) graph representing Alizarin Red staining quantification; representative images of Alizarin Red staining. Groups were considered statistically different with a p < 0.05. The confidence levels were assigned as follows: p ≤ 0.05 (*), p ≤ 0.01 (**), p ≤ 0.001 (***), p ≤ 0.0001 (****).
Figure 3 (A) Graph of LDH assay; (B) graph of Alamar Blue assay; (C) graph of Pico Green assay; (E) Representative confocal images on days 1, 3, and 6; (D) graph representing Alizarin Red staining quantification; representative images of Alizarin Red staining. Groups were considered statistically different with a p < 0.05. The confidence levels were assigned as follows: p ≤ 0.05 (*), p ≤ 0.01 (**), p ≤ 0.001 (***), p ≤ 0.0001 (****).CC BY · PubMed Central
Figure 4 (A–C) A series of different grids were printed by the DLP projector; t indicates the length of the lines while h the side of the squared pore. By decreasing both t and h, the pores became rounded instead of squared. This could be also due to the imperfect control of the focus in our system. (D) Structures with more than one layer (e.g., multilayered steering wheels) were also difficult to print due to the manual adjustment. (E) A single-layer structure (e.g., BIOtech logo) was well-defined. The BIOtech logo has been printed, adding red food coloring to enhance the contrast.
Figure 4 (A–C) A series of different grids were printed by the DLP projector; t indicates the length of the lines while h the side of the squared pore. By decreasing both t and h, the pores became rounded instead of squared. This could be also due to the imperfect control of the focus in our system. (D) Structures with more than one layer (e.g., multilayered steering wheels) were also difficult to print due to the manual adjustment. (E) A single-layer structure (e.g., BIOtech logo) was well-defined. The BIOtech logo has been printed, adding red food coloring to enhance the contrast.CC BY · PubMed Central
Figure 5 (A) Box plot of the line thickness of the first three structures of Figure 2. The lines indicate the nominal quotation. (B) Box plot of the percentage difference between the measured and the nominal thickness. The difference should be 0. All of the measures were higher than the nominal value, and more packed structures with a smaller line thickness had a higher percentage difference.
Figure 5 (A) Box plot of the line thickness of the first three structures of Figure 2. The lines indicate the nominal quotation. (B) Box plot of the percentage difference between the measured and the nominal thickness. The difference should be 0. All of the measures were higher than the nominal value, and more packed structures with a smaller line thickness had a higher percentage difference.CC BY · PubMed Central
Figure 6 (A) Crosslinking of the 3D extrusion-printed Sil-MA structure by UV-irradiation and obtained structure embedded in poloxamer. (B) Brightfield microscopy, composed by several micrographies and (C) a singular micrography, wherein the quantification of the filament dimension has been performed. (D) Withdrawal, ejection, and shape recovery of a Sil-MA 10-layer structure.
Figure 6 (A) Crosslinking of the 3D extrusion-printed Sil-MA structure by UV-irradiation and obtained structure embedded in poloxamer. (B) Brightfield microscopy, composed by several micrographies and (C) a singular micrography, wherein the quantification of the filament dimension has been performed. (D) Withdrawal, ejection, and shape recovery of a Sil-MA 10-layer structure.CC BY · PubMed Central
Figure 7 (A) Scheme of Sil-MA production starting from Bombyx Mori silk cocoons and (B) supposed chemical reaction for the formation of the Sil-MA; a primary amide in the lysine group became a di-β-hydroxyamide, through the nucleophilic substitution of nitrogen on one carbon atom of the epoxy ring of GMA and the consequent ring opening. (C) Scheme of the Sil-MA constructs formation through the digital light processing (DPL) projector. (D) Scheme of the printing through the use of a pneumatic strand dispenser (PSD) inside a poloxamer support bath, of the crosslinking with LAP and of the removal of the poloxamer by decreasing the temperature below the gel-to-sol transition. (E) Scheme of the crosslinking reaction. (1) Formation of radicals under UV light because of the photoinitiator, LAP. (2) Formation of radicals on the protein chain because of the effect of the radicals formed by the photoinitiator (here indicated with R) and the opening of the carbon double bond. (3) Formation of a cross-linking between two chains because of the opening of the carbon double bond.
Figure 7 (A) Scheme of Sil-MA production starting from Bombyx Mori silk cocoons and (B) supposed chemical reaction for the formation of the Sil-MA; a primary amide in the lysine group became a di-β-hydroxyamide, through the nucleophilic substitution of nitrogen on one carbon atom of the epoxy ring of GMA and the consequent ring opening. (C) Scheme of the Sil-MA constructs formation through the digital light processing (DPL) projector. (D) Scheme of the printing through the use of a pneumatic strand dispenser (PSD) inside a poloxamer support bath, of the crosslinking with LAP and of the removal of the poloxamer by decreasing the temperature below the gel-to-sol transition. (E) Scheme of the crosslinking reaction. (1) Formation of radicals under UV light because of the photoinitiator, LAP. (2) Formation of radicals on the protein chain because of the effect of the radicals formed by the photoinitiator (here indicated with R) and the opening of the carbon double bond. (3) Formation of a cross-linking between two chains because of the opening of the carbon double bond.CC BY · PubMed Central

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 51 references

Cited by

See all 31

Metadata

Authors
Bucciarelli, A., Petretta, M., Grigolo, B., Gambari, L., Bossi, A. M., Grassi, F., & Maniglio, D.
Affiliations
  • Istituto Ortopedico Rizzoli (IT)
  • University of Verona (IT)
  • University of Trento (IT)
Corresponding author
  • Bucciarelli, Alessio
  • Maniglio, Devid
Venue
Gels
Publisher
MDPI AG
Published
2022-12-16
Volume
8
Issue
12
Pages
833
ISSN
2310-2861 (ISSN-L)
OpenAlex
W4312129977
Cited by
31
References
53
Citations by year
2026: 10 · 2025: 9 · 2024: 7 · 2023: 5
FWCI
1.23
Type
journal article
Language
en
Open access
Locations
  • Gels (publishedVersion, cc-by)
  • Preprints.org (acceptedVersion, cc-by)
  • PubMed Central (publishedVersion, cc-by)
  • PubMed (publishedVersion)
  • Institutional Research Information System (Università degli Studi di Trento) (submittedVersion, cc-by)
  • DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion, cc-by-sa)
Funders
Istituto Ortopedico Rizzoli di Bologna
Topics
  • Physical Sciences › Materials Science › Biomaterials › Silk-based biomaterials and applications
  • Physical Sciences › Engineering › Biomedical Engineering › Bone Tissue Engineering Materials
  • Physical Sciences › Engineering › Industrial and Manufacturing Engineering › Additive Manufacturing and 3D Printing Technologies
Keywords
shape memory polymers, UV crosslinking, additive manufacturing, digital light processing, pneumatic extrusion, injectable scaffolds, bone regeneration, bone formation, biocompatibility, osteoconduction

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Methacrylated Silk Fibroin Additive Manufacturing of Shape Memory Constructs with Possible Application in Bone Regeneration. https://app.cochat.ai/papers/10.3390/gels8120833
The paper
Bucciarelli, A., Petretta, M., Grigolo, B., Gambari, L., Bossi, A. M., Grassi, F., & Maniglio, D. (2022). Methacrylated Silk Fibroin Additive Manufacturing of Shape Memory Constructs with Possible Application in Bone Regeneration. Gels. https://doi.org/10.3390/gels8120833

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.