The DOI matches its Crossref record; 29 of the 30 references it cites were found in a registry or an index; none of the 8 sources its claims cite is checked for support yet.
Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths
Open accessAbstract
Four-armed poly(ε-caprolactone)-block-poly(d-lactide) (4-C-D) copolymers with different poly(d-lactide) (PDLA) block lengths (Mn,PDLAs) were synthesized by sequential ring-opening polymerization (ROP). The formation of stereocomplex (SC) crystallites in the 80/20 poly(l-lactide) (PLLA)/4-C-D blends were investigated with the change of Mn,PDLA from 0.5 to 1.5 kg/mol. It was found that the crystallization and alkaline degradation of the blends were profoundly affected by the formed SC crystallites. The PLLA/4-C-D0.5 blend had the lowest crystallization rate of the three blends, and it was difficult to see spherulites in this blend by polarized optical microscopy (POM) observation after isothermal crystallization at 140 °C for 4 h. Meanwhile, when Mn,PDLA was 1 kg/mol or 1.5 kg/mol, SC crystallites could be formed in the PLLA/4-C-D blend and acted as nucleators for the crystallization of PLLA homo-crystals. However, the overall crystallization rates of the two blends were still lower than that of the neat PLLA. In the PLLA/4-C-D1.5 blend, the Raman results showed that small isolated SC spherulites were trapped inside the big PLLA homo-spherulites during isothermal crystallization. The degradation rate of the PLLA/4-C-D blend decreased when Mn,PDLA increased from 0.5 to 1.5 kg/mol, and the degradation morphologies had a close relationship with the crystallization state of the blends. This work revealed the gradual formation of SC crystallites with the increase in Mn,PDLA in the PLLA/4-C-D blends and its significant effect on the crystallization and degradation behaviors of the blend films.
Overview
CoChat Summary
TL;DR
In 80/20 PLLA/4-C-D blends, stereocomplex (SC) crystallites form only when the PDLA block length reaches 1 kg/mol; they nucleate PLLA homo-crystallization but overall crystallization remains slower than neat PLLA. Increasing Mn,PDLA from 0.5 to 1.5 kg/mol slows alkaline degradation, and degradation morphology tracks the blend’s crystallization state.
Key findings
- SC crystallites were absent in PLLA/4-C-D0.5 but appeared when Mn,PDLA was 1 or 1.5 kg/mol; WAXD crystallinity of PLLA homo-crystals (Xhc) was 47.6% for neat PLLA, 22.2% for PLLA/4-C-D0.5, 28.8% for PLLA/4-C-D1 (with Xsc = 4.5%), and 15.0% for PLLA/4-C-D1.5 (with Xsc = 9.4%).
- PLLA/4-C-D0.5 showed no spherulites by POM after isothermal crystallization at 140 °C for 4 h and no exothermic peak within 100 min; PLLA/4-C-D1 had tp = 47.6 min and PLLA/4-C-D1.5 had tp = 72.3 min, both slower than neat PLLA. Spherulite growth rates were 5.5 μm/min for neat PLLA, 4.6 μm/min for PLLA/4-C-D1, and 3.4 μm/min for PLLA/4-C-D1.5.
- Raman showed small isolated spherulites in PLLA/4-C-D1.5 were SC crystallites trapped inside larger PLLA homo-spherulites.
- Alkaline degradation rate decreased as Mn,PDLA increased from 0.5 to 1.5 kg/mol; after 4 h, PLLA/4-C-D0.5 showed the largest spherulite morphologies, PLLA/4-C-D1 showed much smaller spherulites, and PLLA/4-C-D1.5 showed no clear spherulite structures.
Methods
- 4-C-D copolymers with fixed PCL block length (1 kg/mol) and different PDLA block lengths (Mn,PDLA = 0.5, 1, 1.5 kg/mol) were synthesized by sequential ring-opening polymerization using pentaerythritol as initiator; PLLA was synthesized using ethylene glycol.
- PLLA/4-C-D blends were prepared at a fixed 8/2 (w/w) ratio by solution casting from chloroform, followed by drying.
- Characterization included 1H NMR, GPC, WAXD, DSC, POM, Raman spectroscopy, alkaline degradation in 1 M NaOH at 37 °C, SEM, and one-way ANOVA on weight loss from triplicate degradation samples.
Limitations
- The paper does not explicitly state limitations.
- Evident from the text: the study is restricted to three PDLA block lengths around 0.5–1.5 kg/mol, a fixed PCL block length of 1 kg/mol, and a single 80/20 PLLA/4-C-D blend ratio, so broader compositional or block-length generalization is not established.
- Evident from the text: degradation was tested only in 1 M NaOH at 37 °C, not under physiological or other hydrolytic conditions, and mechanical properties motivated in the introduction were not reported.
Model-written summary. Check it against the paper before relying on it.
Integrity signals
Registry
Cites
Statistics
Figures






Verification
Claims the paper makes
0 Valid · 0 Not valid · 8 Not checked · 66 Own results and interpretations
A result the paper reports from its own data — it cites no other source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“Then it increased to 28.8% as SC crystallites (Xsc = 4.5%) were formed in the PLLA/4-C-D1 blend”
§ Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths > 3. Results and Discussion > 3.3. Crystal Structure of the PLLA/4-C-D Blends
plainstates a causeSingle case- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
A result the paper states — it cites no source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“no spherulite could be seen in the PLLA/4-C-D0.5 blend even after isothermal crystallization for 4 h”
- Also stated in: § Abstract · hedged
“it was difficult to see spherulites in this blend by polarized optical microscopy (POM) observation after isothermal crystallization at 140 °C for 4 h.”
§ Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths > 3. Results and Discussion > 3.4. Spherulite Morphologies and Growth Rates
plainSingle case- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Also stated in: § Abstract · hedged
A result the paper reports from its own data — it cites no other source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“It was found that the crystallization rates of all the blend samples were slower than that of the neat PLLA during isothermal crystallization at 140 °C”
- Also stated in: § Abstract · plain
“However, the overall crystallization rates of the two blends were still lower than that of the neat PLLA.”
§ Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths > 3. Results and Discussion > 3.5. Isothermal Crystallization
plain- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Also stated in: § Abstract · plain
A result the paper reports from its own data — it cites no other source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“No SC crystallites were formed when Mn,PDLA was 0.5 kg/mol”
§ Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths > 3. Results and Discussion > 3.3. Crystal Structure of the PLLA/4-C-D Blends
plainSingle case- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
A result the paper reports from its own data — it cites no other source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“and it decreased a lot to 22.2% when the 4-C-D0.5 copolymer was introduced into PLLA.”
§ Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths > 3. Results and Discussion > 3.3. Crystal Structure of the PLLA/4-C-D Blends
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
49 more claims
Create a free account to see all 74 claims and every source verdict.
- It may state two separate claims as one. 18
- Probably not a substantial claim. 2
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
Each contradiction between two passages listed here was confirmed by an independent check.
Rated minor: it would not touch a result — a value no result rests on, a p-value that stays on the same side of the significance level, or a conflict that is clerical, resolved elsewhere in the paper, or outside its own findings.
In the paper
§ Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths > 3. Results and Discussion > 3.3. Crystal Structure of the PLLA/4-C-D Blends
“(1)Xsc = IhcItotal×100%”
§ Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths > 3. Results and Discussion > 3.3. Crystal Structure of the PLLA/4-C-D Blends
“Meanwhile, Xhc and Xsc represent the crystallinities of PLLA homo-crystals and SC crystals, respectively.”
Rated minor: it would not touch a result — a value no result rests on, a p-value that stays on the same side of the significance level, or a conflict that is clerical, resolved elsewhere in the paper, or outside its own findings.
In the paper
§ Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths > 3. Results and Discussion > 3.3. Crystal Structure of the PLLA/4-C-D Blends
“The three peaks of the SC crystallites are present in the PLLA/4-C-D1, PLLA/4-C-D1.5, and PLLA/4-C-D2 blends.”
§ Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths > 4. Conclusions
“A series of 4-C-D with different Mn,PDLAs (0.5, 1, 1.5 kg/mol) was successfully prepared by ring-opening polymerization.”
Citations
Cites
The return of a forgotten polymer—Polycaprolactone in the 21st century
Woodruff, M. A., & Hutmacher, D. W. (2010) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2010.04.002 · Cited by 4,033 · cited 1×
“Poly(ε-caprolactone) (PCL) is also a famous degradable polymer with excellent biocompatibility, biodegradability, and it is very flexible at room temperature because of a very low glass transition temperature (Tg) of about −60 ◦C [9,10].”
BackgroundPoly(lactic acid) modifications
Rasal, R. M., Janorkar, A. V., & Hirt, D. E. (2010) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2009.12.003 · Cited by 2,204 · cited 1×
“Among them, polylactic acid (PLA) has been widely used in packaging and biomedical fields [4].”
BackgroundPoly(lactic acid) crystallization
Saeidlou, S., Huneault, M. A., Li, H., & Park, C. B. (2012) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2012.07.005 · Cited by 1,606 · cited 1×
“Commercial PLA is usually an l-rich mixture as the majority of bacteria used in fermentation processes predominantly produce l-lactic acid [5].”
BackgroundStereocomplex formation between enantiomeric poly(lactides)
Ikada, Y., Jamshidi, K., Tsuji, H., & Hyon, S. H. (1987) · Macromolecules · doi:10.1021/ma00170a034 · Cited by 1,409
Stereocomplex Formation between Enantiomeric Poly(lactide)s
박은하, & 진인주 (2010) · 한국고분자학회 학술대회 연구논문 초록집 · Cited by 1,084
Polylactic acid (PLA) controlled delivery carriers for biomedical applications
Tyler, B., Gullotti, D., Mangraviti, A., Utsuki, T., & Brem, H. (2016) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2016.06.018 · Cited by 1,050
Amass, W., Amass, A., & Tighe, B. (1998) · Polymer International · doi:10.1002/(sici)1097-0126(1998100)47:2<89::aid-pi86>3.0.co;2-f · Cited by 1,001
Poly(lactic acid) stereocomplexes: A decade of progress
Tsuji, H. (2016) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2016.04.017 · Cited by 535
Phase Structure, Compatibility, and Toughness of PLA/PCL Blends: A Review
Fortelny, I., Ujcic, A., Fambri, L., & Slouf, M. (2019) · Frontiers in Materials · doi:10.3389/fmats.2019.00206 · Cited by 238
Sun, Y., Yang, L., Lu, X., & He, C. (2015) · Journal of Materials Chemistry A · doi:10.1039/c4ta05991c · Cited by 178 · cited 1×
“In these modifiers, the soft middle segments could be a PCL copolymer and introduce elastic properties into the material [17].”
BackgroundCastillo, R. V., Müller, A. J., Raquez, J.-M., & Dubois, P. (2010) · Macromolecules · doi:10.1021/ma100201g · Cited by 175
de Jong, S. J., van Dijk-Wolthuis, W. N. E., Kettenes-van den Bosch, J. J., Schuyl, P. J. W., & Hennink, W. E. (1998) · Macromolecules · doi:10.1021/ma980553i · Cited by 172
Highly Biodegradable and Tough Polylactic Acid–Cellulose Nanocrystal Composite
Muiruri, J. K., Liu, S., Teo, W. S., Kong, J., & He, C. (2017) · ACS Sustainable Chemistry & Engineering · doi:10.1021/acssuschemeng.6b03123 · Cited by 169 · cited 1×
“In recent years, copolymers or composites with soft middle blocks and outer PDLA blocks have been a hotspot of scientific interest as PLLA modifiers [7,15,16].”
BackgroundBlending Effects on Polymorphic Crystallization of Poly( l -lactide)
Pan, P., Liang, Z., Zhu, B., Dong, T., & Inoue, Y. (2009) · Macromolecules · doi:10.1021/ma8024943 · Cited by 163 · cited 1×
“It is well known that the glass transition temperature (Tg) of a polymer material determines its crystallization behavior [21].”
BackgroundIñiguez-Franco, F., Auras, R., Burgess, G., Holmes, D., Fang, X., Rubino, M., & Soto-Valdez, H. (2016) · Polymer · doi:10.1016/j.polymer.2016.07.018 · Cited by 159 · cited 1×
“It is well known that the degradation of PCL and PLA are carried out through the cleavage of ester bonds [26], and the degradation behavior of degradable polymers has a close relationship with the crystalline state [27].”
BackgroundFerri, J. M., Fenollar, O., Jorda‐Vilaplana, A., García‐Sanoguera, D., & Balart, R. (2016) · Polymer International · doi:10.1002/pi.5079 · Cited by 141 · cited 1×
“However, it was found that the poor interfacial compatibility between PLLA and PCL limits the enhancement of the mechanical properties [12,13].”
BackgroundResearch progress in the heat resistance, toughening and filling modification of PLA
Yang, Y., Zhang, L., Xiong, Z., Tang, Z., Zhang, R., & Zhu, J. (2016) · Science China Chemistry · doi:10.1007/s11426-016-0222-7 · Cited by 137 · cited 1×
“As a result, various methods have been used for the modification of PLLA [8].”
MethodXu, H., Teng, C., & Yu, M. (2006) · Polymer · doi:10.1016/j.polymer.2006.03.090 · Cited by 113
Remarkable melting behavior of PLA stereocomplex in linear PLLA/PDLA blends
Shao, J., Xiang, S., Bian, X., Sun, J., Li, G., & Chen, X. (2015) · Industrial & Engineering Chemistry Research · doi:10.1021/ie504484b · Cited by 113 · cited 1×
“3◦, which correspond to the (103), (010), (200)/(110), (203), and (210) planes of the α-form crystals of PLLA [22], could be observed in all the samples.”
BackgroundLi, Z., Muiruri, J. K., Thitsartarn, W., Zhang, X., Tan, B. H., & He, C. (2018) · Composites Science and Technology · doi:10.1016/j.compscitech.2018.02.026 · Cited by 105 · cited 2×
“However, the lower ability of crystallization, poor thermal stability and brittleness of PLLA limit its further application [6,7].”
BackgroundTsuji, H., Yamada, T., Suzuki, M., & Itsuno, S. (2003) · Polymer International · doi:10.1002/pi.1093 · Cited by 101
A mini review on the functional biomaterials based on poly (lactic acid) stereocomplex
Jing, Y., Quan, C., Liu, B., Jiang, Q., & Zhang, C. (2016) · Polymer Reviews · doi:10.1080/15583724.2015.1111380 · Cited by 92
Role of PEG Segment in Stereocomplex Crystallization for PLLA/PDLA-b-PEG-b-PDLA Blends
Song, Y., Wang, D., Jiang, N., & Gan, Z. (2015) · ACS Sustainable Chemistry & Engineering · doi:10.1021/acssuschemeng.5b00214 · Cited by 59 · cited 1×
“8◦ correspond to the (110), (300)/(030), and (220) planes of the SC crystals, respectively [23].”
BackgroundHu, J. S., Wang, J., Wang, M., Ozaki, Y., Sato, H., & Zhang, J. (2019) · Polymer · doi:10.1016/j.polymer.2019.03.049 · Cited by 50 · cited 1×
“A similar fitting process was used as reported in [25].”
MethodSelf-citationPreparation of Porous Polylactide Microspheres and Their Application in Tissue Engineering
Shi, X., Sun, P., & Gan, Z. (2018) · Chinese Journal of Polymer Science · doi:10.1007/s10118-018-2079-x · Cited by 28
Four-armed PCL-b-PDLA diblock copolymer: 1. Synthesis, crystallization and degradation
Ning, Z., Jiang, N., & Gan, Z. (2014) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2014.05.016 · Cited by 16 · cited 1×
“It is well known that the degradation of PCL and PLA are carried out through the cleavage of ester bonds [26], and the degradation behavior of degradable polymers has a close relationship with the crystalline state [27].”
BackgroundSelf-citationSong, Z., Huang, X., Lu, X., Lv, Q., Xu, N., Pang, S., Pan, L., & Li, T. (2018) · Journal of Applied Polymer Science · doi:10.1002/app.46536 · Cited by 14 · cited 1×
“However, it was found that the poor interfacial compatibility between PLLA and PCL limits the enhancement of the mechanical properties [12,13].”
BackgroundNing, Z., Liu, J., Jiang, N., & Gan, Z. (2017) · Polymer International · doi:10.1002/pi.5352 · Cited by 11 · cited 2×
“In recent years, copolymers or composites with soft middle blocks and outer PDLA blocks have been a hotspot of scientific interest as PLLA modifiers [7,15,16].”
BackgroundResultSelf-citationSchmidt (2001) · doi:10.1002/1099-0488(20010201)39:3<300::aid-polb1002>3.0.co;2-m
Cited by
Yousfi, R. E., Brahmi, M., Dalli, M., Achalhi, N., Azougagh, O., Tahani, A., Touzani, R., & Idrissi, A. E. (2023) · Polymers · doi:10.3390/polym15081835 · Cited by 68
Rahaman, M. H., Haque, M. A., Rahman, M. A., et al. (2022) · Reactions · doi:10.3390/reactions3010016 · Cited by 15
“The crystallinity of PLLA was re- ported to 47.6% by Dai et al. (2020) [53].”
BackgroundInfluentialChalid, M., Gustiraharjo, G., Pangesty, A. I., Adyandra, A., Whulanza, Y., & Supriadi, S. (2023) · JOURNAL OF RENEWABLE MATERIALS · doi:10.32604/jrm.2023.026788 · Cited by 13
da Silva, T. S., Horvath-Pereira, B. D. O., da Silva-Júnior, L. N., Fireman, J. V. B. T., Mattar, M., Félix, M., Buchaim, R. L., Carreira, A. C. O., Miglino, M. A., & Soares, M. M. (2023) · Polymers · doi:10.3390/polym15214213 · Cited by 9
“This conclusion is supported by the fact that all identified peaks belonged to pure materials [65,66].”
BackgroundAzapagic, A., Agarwal, J. P., Gale, B. K., Shea, J., Wojtalewicz, S., & Sant, H. J. (2024) · Biomedical Microdevices · doi:10.1007/s10544-024-00717-y · Cited by 9
“2023), while PLLA degrades slightly faster (Dai et al .”
Metadata
- Authors
- Dai, S., Wang, M., Zhuang, Z., & Ning, Z.
- Affiliations
- State Key Laboratory of Organic-Inorganic Composite Materials (CN)
- Corresponding author
- Ning, Zhenbo
- Venue
- Polymers
- Publisher
- MDPI AG
- Published
- 2020-09-25
- Volume
- 12
- Issue
- 10
- Pages
- 2195
- ISSN
- 2073-4360 (ISSN-L)
- PMC
- PMC7599906
- OpenAlex
- W3088416922
- Semantic Scholar
- e3506f97722121fdec1bf217c32a762726b12b06
- Cited by
- 8
- References
- 30
- Citations by year
- 2025: 1 · 2024: 1 · 2023: 5 · 2022: 1
- FWCI
- 0.39
- Type
- journal article
- Language
- en
- Open access
- gold
- doi.org
- Licence
- Locations
- Polymers (publishedVersion, cc-by)
- PubMed Central (publishedVersion, cc-by)
- PubMed (publishedVersion)
- DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion, cc-by-sa)
- Funders
- National Natural Science Foundation of China (51603005,51973010)
- Topics
- Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
- Physical Sciences › Materials Science › Polymers and Plastics › Polymer crystallization and properties
- Physical Sciences › Engineering › Biomedical Engineering › Bone Tissue Engineering Materials
- Keywords
- poly(L-lactic acid), stereocomplex crystallites, polymer blends, crystallization, alkaline degradation, block length, nucleation, spherulites, isothermal crystallization, ring-opening polymerization, biodegradable polymers
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
A language model drew the claims from the paper on 2026-10-10, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).
A second model labelled each claim on 2026-10-10 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.