CoChat

Melt Structure and its Transformation by Sequential Crystallization of the Two Blocks within Poly( L ‐lactide)‐ block ‐Poly( ε ‐caprolactone) Double Crystalline Diblock Copolymers

Open access
Hamley, I. W., Parras, P., Castelletto, V., Castillo, R. V., Müller, A. J., Pollet, E., Dubois, P., Martin, C. M. · 2006 · Macromolecular Chemistry and Physics

The DOI matches its Crossref record; 29 of the 29 references it cites were found in a registry or an index; 2 of the 40 sources its claims cite were checked for support.

Abstract

Abstract Summary: Sequential crystallization of poly( L ‐lactide) (PLLA) followed by poly( ε ‐caprolactone) (PCL) in double crystalline PLLA‐ b ‐PCL diblock copolymers is studied by differential scanning calorimetry (DSC), polarized optical microscopy (POM), wide‐angle X‐ray scattering (WAXS) and small‐angle X‐ray scattering (SAXS). Three samples with different compositions are studied. The sample with the shortest PLLA block (32 wt.‐% PLLA) crystallizes from a homogeneous melt, the other two (with 44 and 60% PLLA) from microphase separated structures. The microphase structure of the melt is changed as PLLA crystallizes at 122 °C (a temperature at which the PCL block is molten) forming spherulites regardless of composition, even with 32% PLLA. SAXS indicates that a lamellar structure with a different periodicity than that obtained in the melt forms (for melt segregated samples). Where PCL is the majority block, PCL crystallization at 42 °C following PLLA crystallization leads to rearrangement of the lamellar structure, as observed by SAXS, possibly due to local melting at the interphases between domains. POM results showed that PCL crystallizes within previously formed PLLA spherulites. WAXS data indicate that the PLLA unit cell is modified by crystallization of PCL, at least for the two majority PCL samples. The PCL minority sample did not crystallize at 42 °C (well below the PCL homopolymer crystallization temperature), pointing to the influence of pre‐crystallization of PLLA on PCL crystallization, although it did crystallize at lower temperature. Crystallization kinetics were examined by DSC and WAXS, with good agreement in general. The crystallization rate of PLLA decreased with increase in PCL content in the copolymers. The crystallization rate of PCL decreased with increasing PLLA content. The Avrami exponents were in general depressed for both components in the block copolymers compared to the parent homopolymers. Polarized optical micrographs during isothermal crystallization of (a) homo‐PLLA, (b) homo‐PCL, (c) and (d) block copolymer after 30 min at 122 °C and after 15 min at 42 °C. magnified image Polarized optical micrographs during isothermal crystallization of (a) homo‐PLLA, (b) homo‐PCL, (c) and (d) block copolymer after 30 min at 122 °C and after 15 min at 42 °C.

Overview

CoChat Summary

TL;DR

Sequential crystallization of PLLA then PCL in three PLLA-b-PCL diblock copolymers was studied by DSC, POM, WAXS, and SAXS. PLLA crystallizes first at 122 °C forming spherulites even with only 32 wt.-% PLLA, and subsequent PCL crystallization at 42 °C rearranges the lamellar and unit-cell structure while slowing crystallization kinetics relative to homopolymers.

Key findings

  • The shortest-PLLA sample L32⁷C68¹⁵ (32 wt.-% PLLA) crystallizes from a homogeneous/disordered melt, whereas L44¹¹C56¹⁴ and L60¹²C40⁹ crystallize from microphase-separated lamellar melts formed on supercooling. PLLA crystallizes at 122 °C, where PCL is molten, forming spherulites regardless of composition, even at 32% PLLA.
  • SAXS shows that PLLA crystallization transforms the melt microdomain structure; for L44¹¹C56¹⁴ a lamellar structure with different periodicity than the melt forms. PCL crystallization at 42 °C in PCL-majority samples rearranges the lamellar structure, possibly via local melting at interphases, and POM shows PCL crystallizes within previously formed PLLA spherulites. WAXS indicates the PLLA unit cell is modified by PCL crystallization, at least for the two majority-PCL samples.
  • The PCL-minority sample L60¹²C40⁹ did not crystallize at 42 °C within the experiment, well below the PCL homopolymer crystallization temperature, but did crystallize at lower temperature (30 °C).
  • Crystallization kinetics by DSC/WAXS: PLLA rate decreased with increasing PCL content; PCL rate decreased with increasing PLLA content. Avrami exponents were generally depressed versus homopolymers: PLLA homopolymer n = 2.85, t₅₀ = 4.75 min at 122 °C; L60 n = 2.56, t₅₀ = 6.88 min; L44 n = 2.21, t₅₀ = 11.35 min; L32 n = 2.03, t₅₀ = 11.30 min. PCL homopolymer n = 2.89, t₅₀ = 7.85 min at 42 °C; L44 n = 1.97, t₅₀ = 18.27 min; L32 n = 1.55, t₅₀ = 8.62 min; L60 n = 2.39, t₅₀ = 9.15 min at 30 °C.

Methods

  • Three PLLA-b-PCL diblock copolymers (L60¹²C40⁹, L44¹¹C56¹⁴, L32⁷C68¹⁵) plus PLLA and PCL homopolymers and solution-prepared blends were synthesized by controlled/“living” sequential block copolymerization initiated by aluminum trialkoxides and characterized by SEC and ¹H NMR.
  • Simultaneous SAXS/WAXS was performed on station 6.2 at the Daresbury Synchrotron Radiation Source (λ = 1.40 Å) using a Linkam DSC cell; DSC used a Perkin-Elmer DSC-7 at 10 °C min⁻¹; POM used thin films between cover slips, a Linkam TP-91 hot-stage, crossed polarizers, and a λ plate.
  • Sequential isothermal crystallization used a new annealing protocol: PLLA crystallized at 122 °C for 30 min, then PCL at 42 °C for 15 min; an alternate protocol used 100 °C then 30 °C. Avrami parameters were obtained by fitting DSC isothermal crystallization data.

Limitations

  • The paper states that sample susceptibility to degradation prevented longer melt annealing times that might yield better segregated structures, and that the precise origin of an additional low-q SAXS shoulder is unclear.
  • The paper notes that homopolymer analogues had somewhat higher molecular weights than the corresponding block components, but argues this would if anything increase block crystallization rates, so the observed slowing is not explained by molecular weight differences.
  • The paper states that the physical meaning of the reduced Avrami index for PLLA is difficult to explain because spherulites were observed in all cases; for PCL, the reduction is attributed to topological restrictions hindering three-dimensional growth.

Model-written summary. Check it against the paper before relying on it.

Integrity signals

Registry

Crossref · 10.1002/macp.200600085

Cites

29 of 29 references verified0 citation errors · 0 not checkable

Statistics

Nothing to recompute.

Figures

Polarized optical micrographs during isothermal crystallization of (a) homo-PLLA, (b) homo-PCL, (c) and (d) block copolymer after 30 min at 122 8 C and after 15 min at 42 8 C.
Polarized optical micrographs during isothermal crystallization of (a) homo-PLLA, (b) homo-PCL, (c) and (d) block copolymer after 30 min at 122 8 C and after 15 min at 42 8 C.From the PDF
Image 2
From the PDF
Figure 2 DSC heating scans (at 10 8 C  min  1 ) following the cooling scans presented in Figure 1.
Figure 2 DSC heating scans (at 10 8 C  min 1 ) following the cooling scans presented in Figure 1.From the PDF
Figure 3 Melting and crystallization temperatures (obtained from the data reported in Figure 1 and 2) for the PLLA and PCL blocks within all copolymer versus PLLA composition (data points plus dashed line). The data points (without dashed line) indicate the transition temperatures for PLLA and PCL phases in the blends.
Figure 3 Melting and crystallization temperatures (obtained from the data reported in Figure 1 and 2) for the PLLA and PCL blocks within all copolymer versus PLLA composition (data points plus dashed line). The data points (without dashed line) indicate the transition temperatures for PLLA and PCL phases in the blends.From the PDF
Figure 4 Temperature profiles applied during SAXS/WAXS measurements. The solid line indicated the thermal profile applied in this work. The dashed line corresponds to the thermal program employed by us in a previous work. [16] The arrows indicate the times and temperatures selected for the presentation of specific ''time frames'' of data.
Figure 4 Temperature profiles applied during SAXS/WAXS measurements. The solid line indicated the thermal profile applied in this work. The dashed line corresponds to the thermal program employed by us in a previous work. [16] The arrows indicate the times and temperatures selected for the presentation of specific ''time frames'' of data.From the PDF
Figure 5 DSC heating scans at 10 8 C  min  1 after the main thermal program presented in Figure 4 (solid line). For the copolymer L60 12 C40 9 , line (a) indicated the heating scan after the thermal program presented in Figure 4 (solid line). Line (b) indicated the heating scan after the thermal program presented in Figure 4 (dashed line).
Figure 5 DSC heating scans at 10 8 C  min 1 after the main thermal program presented in Figure 4 (solid line). For the copolymer L60 12 C40 9 , line (a) indicated the heating scan after the thermal program presented in Figure 4 (solid line). Line (b) indicated the heating scan after the thermal program presented in Figure 4 (dashed line).From the PDF
Figure 6 WAXS data for block copolymer L32 7 C68 15 obtained starting at 190 8 C, quenching at 50 8 C  min  1 to 100 8 C where PLLA crystallizes (30 min hold), then quenching at 50 8 C  min  1 to 30 8 C (15 min hold) where PCL crystallizes (segmented line in Figure 4).
Figure 6 WAXS data for block copolymer L32 7 C68 15 obtained starting at 190 8 C, quenching at 50 8 C  min 1 to 100 8 C where PLLA crystallizes (30 min hold), then quenching at 50 8 C  min 1 to 30 8 C (15 min hold) where PCL crystallizes (segmented line in Figure 4).From the PDF
Figure 7 SAXS data for block copolymer L32 7 C68 15 obtained during the temperature ramp shown in Figure 4 (solid line). The temperature regions are indicated as: I (190 8 C); II (165 8 C); III (122 8 C) and IV (42 8 C).
Figure 7 SAXS data for block copolymer L32 7 C68 15 obtained during the temperature ramp shown in Figure 4 (solid line). The temperature regions are indicated as: I (190 8 C); II (165 8 C); III (122 8 C) and IV (42 8 C).From the PDF
Figure 8 Selected frames (indicated by arrows in Figure 4, solid line) of SAXS data for block copolymer L32 7 C68 15 .
Figure 8 Selected frames (indicated by arrows in Figure 4, solid line) of SAXS data for block copolymer L32 7 C68 15 .From the PDF
Figure 9 Normalized height of WAXS peaks for block copolymer L32 7 C68 15 from fitted Lorentzian functions: ( & ) 2 y ¼ 14.8 8 reflection of PLLA, ( * ) 110 reflection of PCL. The solid line indicates the temperature measured by the DSC instrument (Linkam) employed in the X-ray set-up. The dashed line indicates the cooling region from 122 to 42 8 C. The vertical solid line indicates the start of PCL crystallization ( t *PCL).
Figure 9 Normalized height of WAXS peaks for block copolymer L32 7 C68 15 from fitted Lorentzian functions: ( & ) 2 y ¼ 14.8 8 reflection of PLLA, ( * ) 110 reflection of PCL. The solid line indicates the temperature measured by the DSC instrument (Linkam) employed in the X-ray set-up. The dashed line indicates the cooling region from 122 to 42 8 C. The vertical solid line indicates the start of PCL crystallization ( t *PCL).From the PDF
Figure 10 WAXS (data points) and DSC (solid line) data corresponding to the isothermal crystallization of the PLLA block within copolymer L32 7 C68 15 at 122 8 C.
Figure 10 WAXS (data points) and DSC (solid line) data corresponding to the isothermal crystallization of the PLLA block within copolymer L32 7 C68 15 at 122 8 C.From the PDF
Image 12
From the PDF
Figure 11 Polarized Optical Micrographs during isothermal crystallization: (a) homoPLLA,after 8 min at 122 8 C. (b) homo-PCL, after 10 min at 42 8 C. (c) L 32 7 C68 15 after 30 min at 122 8 C. (d) L32 7 C68 15 after 15 min at 42 8 C.
Figure 11 Polarized Optical Micrographs during isothermal crystallization: (a) homoPLLA,after 8 min at 122 8 C. (b) homo-PCL, after 10 min at 42 8 C. (c) L 32 7 C68 15 after 30 min at 122 8 C. (d) L32 7 C68 15 after 15 min at 42 8 C.From the PDF
Figure 13 Selected frames (indicated by arrows in Figure 4, solid line) of SAXS data for block copolymer L44 11 C56 14 .
Figure 13 Selected frames (indicated by arrows in Figure 4, solid line) of SAXS data for block copolymer L44 11 C56 14 .From the PDF
Figure 14 Normalized height of WAXS peaks for block copolymer L44 11 C56 14 from fitted Lorentzian functions: ( & ) 2 y ¼ 14.8 8 reflection of PLLA, ( * ) 110 reflection of PCL. The solid line indicates the temperature measured by the DSC instrument (Linkam) employed in the X-ray set-up. The dashed line indicated the cooling region from 122 to 42 8 C.
Figure 14 Normalized height of WAXS peaks for block copolymer L44 11 C56 14 from fitted Lorentzian functions: ( & ) 2 y ¼ 14.8 8 reflection of PLLA, ( * ) 110 reflection of PCL. The solid line indicates the temperature measured by the DSC instrument (Linkam) employed in the X-ray set-up. The dashed line indicated the cooling region from 122 to 42 8 C.From the PDF
Figure 15 Selected frames (indicated by arrows in Figure 4, solid line) of SAXS data for block copolymer L60 12 C40 9 .
Figure 15 Selected frames (indicated by arrows in Figure 4, solid line) of SAXS data for block copolymer L60 12 C40 9 .From the PDF
Figure 16 Selected frames of SAXS data for block copolymer L60 12 C40 9 obtained during the temperature ramp shown in Figure 4 (dashed line).
Figure 16 Selected frames of SAXS data for block copolymer L60 12 C40 9 obtained during the temperature ramp shown in Figure 4 (dashed line).From the PDF
Figure 17 WAXS (data points) and DSC (solid line) data corresponding to the isothermal crystallization of PLLA block within L60 12 C40 9 copolymer at 122 8 C.
Figure 17 WAXS (data points) and DSC (solid line) data corresponding to the isothermal crystallization of PLLA block within L60 12 C40 9 copolymer at 122 8 C.From the PDF

Verification

Claims the paper makes

2 Valid · 0 Not valid · 24 Not checked · 91 Own results and interpretations

57 more claims

Create a free account to see all 117 claims and every source verdict.

See all claims — free account
  • Probably not a substantial claim. 30
  • It may state two separate claims as one. 28
  • The quote only partly states this claim. 7

Create a free account to see these claims.

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

2 more claims about this paper

Create a free account to see every claim other papers make about this one.

See all claims — free account

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

Each contradiction between two passages listed here was confirmed by an independent check.

3 of 3

Citations

Cites

Cited by

See all 108

Metadata

Authors
Hamley, I. W., Parras, P., Castelletto, V., Castillo, R. V., Müller, A. J., Pollet, E., Dubois, P., & Martin, C. M.
Affiliations
  • Universidad Simón Bolívar (VE)
  • University of Reading (GB)
  • Daresbury Laboratory (GB)
Corresponding author
  • Hamley, I. W.
  • Müller, A. J.
Venue
Macromolecular Chemistry and Physics
Publisher
Wiley
Published
2006-05-23
Volume
207
Issue
11
Pages
941-953
ISSN
  • 1022-1352 (ISSN-L)
  • 1521-3935
OpenAlex
W1969416531
Cited by
108
References
29
Citations by year
2026: 1 · 2025: 2 · 2023: 3 · 2022: 2 · 2021: 6 · 2020: 4 · 2019: 3 · 2018: 6 · 2017: 10 · 2016: 11 · 2015: 6 · 2014: 11 · 2013: 3 · 2012: 7
FWCI
7.93
Type
journal article
Language
en
Open access
Locations
  • Macromolecular Chemistry and Physics (publishedVersion)
  • ORBi UMONS (submittedVersion, other-oa)
Funders
Engineering and Physical Sciences Research Council
Topics
  • Physical Sciences › Materials Science › Polymers and Plastics › Polymer crystallization and properties
  • Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
  • Physical Sciences › Materials Science › Materials Chemistry › Block Copolymer Self-Assembly
Keywords
poly(L-lactic acid), polycaprolactone, diblock copolymers, sequential crystallization, spherulites, lamellar structure, crystallization kinetics, Avrami exponent, isothermal crystallization, interfacial melting, polymer blends, poly(ethylene glycol) diacrylate

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

A language model drew the claims from the paper on 2026-10-10, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).

A second model labelled each claim on 2026-10-10 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.