Hot corrosion of materials: Fundamental studies
The DOI matches its Crossref record; 6 of the 31 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“As with the thin aqueous layer on alloys in atmospheric corrosion, this molten salt layer is a pure ionic conductor which separates the alloys from the gas phase physically [1, 19, 47].”
From A review on molten sulfate salts induced hot corrosion (2021) · cites this paper as [1]
In the citing paper
“These sulfate salts easily attach onto the surfaces of high temperature components and are melted to form a thin fused salt film at elevated temperatures.”
From A review on molten sulfate salts induced hot corrosion (2021) · cites this paper as [1]
In the citing paper
“The predominant chemical reactant involved in hot corrosion has been confirmed to be sodium sulfate (Na2SO4), due to its extraordinary stability over a wide range of temperatures and oxygen partial pressures [1, 6, 19].”
From A review on molten sulfate salts induced hot corrosion (2021) · cites this paper as [1]
In the citing paper
“The diagram demonstrates the good stability of Na2SO4 over a wide range of log and .”
From A review on molten sulfate salts induced hot corrosion (2021) · cites this paper as [1]
In the citing paper
“In the O2-SO2-SO3 environment (Eq. (1)), the solubilities of both O2 and SO2 in molten salt are poor. In contrast, SO3 can dissolve in molten salt because of the formation of pyrosulfate ions through Eq. (2) [1, 19].”
From A review on molten sulfate salts induced hot corrosion (2021) · cites this paper as [1]
2 more claims about this paper
Create a free account to see every claim other papers make about this one.
Citations
Cites
(2006) · Electrochemistry and Corrosion Science · doi:10.1007/1-4020-7860-9_10 · Cited by 1,814
The Hot Corrosion of Metals by Molten Salts
Rapp, R. A. (1981) · ECS Proceedings Volumes · doi:10.1149/198110.0159pv · Cited by 136
Self-citationDeposition and Corrosion in Gas Turbines
Billingham, J. (1974) · British Corrosion Journal · doi:10.1179/000705974798321738 · Cited by 135
Rapp, R. A. (1989) · Studies in inorganic chemistry · doi:10.1016/b978-0-444-88534-0.50016-3 · Cited by 31
Self-citationHigh temperature corrosion and protection
Colson, J. C., Strafford, K. N., & Lambertin, M. (1986) · Journal de Chimie Physique · doi:10.1051/jcp/1986830745 · Cited by 27
Solubility of CeO2 in Molten Na2SO4–10 mol% NaVO3 Salt Solution at 900°C
Zhang, Y. S. (1994) · ECS Proceedings Volumes · doi:10.1149/199413.0171pv · Cited by 2
Self-citation
Research works printed but not linked: 69
- W.T. Reid, R.C. Corey, and BJ. Cross, Trans. ASME, 67 (1945), p. 279.
- F.J. Wall and S.T. Michael, ASTM Spec. Tech. Publ. STP 421 (1967), p. 223.
- K.J. Kohl et al., J. Electrochem. Soc., 126 (1979), p. 1054.
- K.L. Luthra and H.S. Spacil, J. Electrochem. Soc., 129 (1982), p. 649.
- E.L. Simons, G.V. Browning, and H.A. Liebhafsky, Corrosion, 11 (1955), p. 505.
- A.U. Seybolt, Trans. AIME, 242 (1968), p. 1955.
- N.S. Bornstein and M.A. DeCrescente, Trans. AIME, 245 (1969), p. 583.
- N.S. Bornstein and M.A. DeCrescente, Met. Trans.,2 (1971), p. 2875.
- J.A. Goebel and F.S. Pettit, Met. Trans., 1 (1970), p. 1943.
- J.A. Goebel, F.S. Pettit, and G.W. Goward, Met. Trans., 4 (1973), p. 261.
- J. Stringer, Annual Review of Materials Sci., 7, ed. R.A. Huggins (Palo Alto, CA: Annual Review Inc., 1977), p. 449.
- J. Stringer, Materials Sci. Techn., 3 (1987), p. 482.
- F.S. Pettit and C.S. Giggins, “Hot Corrosion,” Superalloys II, ed. C.T. Sims, N.S. Stoloff, and W.C. Hagel (New York: Wiley Publ., 1987), p. 327.
- R.A. Rapp, Corrosion, 42 (1986), p. 568.
- C.O. Park and R.A. Rapp, J. Electrochem. Soc., 133 (1986), p. 1636.
- D. Inman and D.M. Wrench, Brit. Corros. J., 1 (1966), p. 246.
- D.A. Shores and R.C. John, J. Appl. Electrochem., 10 (1980), p. 275.
- P.P. Leblanc and R.A. Rapp, J. Electrochem. Soc., 139 (1992), p. L31.
- P.P. Leblanc and R.A. Rapp, J. Electrochem. Soc., 140 (1993), p. L41.
- D.K. Gupta and R.A. Rapp, J. Electrochem. Soc., 127 (1980), p. 2194 and 2656.
- Y.S. Zhang and R.A. Rapp, J. Electrochem. Soc., 132 (1985), p. 734 and 2498.
- Y.S. Zhang, J. Electrochem. Soc., 133 (1986), p. 655.
- P.D. Jose, D.K. Gupta, and R.A. Rapp, J. Electrochem. Soc., 132 (1985), p. 735.
- D.Z. Shi and R.A. Rapp, J. Electrochem. Soc., 133 (1986), p. 849.
- M.L. Deanhardt and K.H. Stern, J. Electrochem. Soc., 128 (1981), p. 2577.
- A.K. Misra, D.P. Whittle, and W.L. Worrell, J. Electrochem. Soc., 129 (1982), p. 1840.
- M.L. Deanhardt and K.H. Stern, J. Electrochem. Soc., 129 (1982), p. 2228.
- N.S. Jacobson and J.L. Smialek, J. Amer. Ceram. Soc., 68 (1985), p. 432.
- N.S. Jacobson, J. Amer. Ceram. Soc., 76 (1993), p. 3.
- Y.S. Hwang and R.A. Rapp,J. Electrochem. Soc., 137 (1990), p. 1276.
- Y.S. Zhang and R.A. Rapp, Corrosion, 43 (1987), p. 348.
- Y.S. Hwang and R.A. Rapp, Corrosion, 45 (1989), p. 933.
- R.A. Rapp and Y.S. Zhang, “Electrochemical Studies of Hot Corrosion of Materials,” Proc Intern. Corr. Conf. (Merida, Mexico: 1993)
- R.L. Jones, D.B. Nordman, and S.T. Gadomski, Met. Trans., 16A (1985), p. 303.
- R.L. Jones, S.R. Jones, and C.E. Williams, J. Electrochem. Soc., 132 (1985), p. 1499.
- R.L. Jones, C.E. Williams, and S.R. Jones, J. Electrochem. Soc., 133 (1986), p. 227.
- R.L. Jones and D. Mess,J. Amer. Ceram. Soc., 75 (1992), p. 1818.
- R.L. Jones, High Temp. Tech., 6 (1988), p. 187.
- M. Seiersten and P. Kofstad, Mater. Sci. Tech., 3 (1987), p. 576.
- A.S. Nagelberg, J. Electrochem. Soc., 132 (1985), p. 2502.
- F. Mansfeld and J.V. Kenkel, Corr. Sci., 16 (1976), p. 111.
- F. Mansfeld and J.V. Kenkel, Corrosion, 33 (1977), p. 238.
- R. Andresen, J. Electrochem. Soc., 126 (1979), p. 328.
- D.A. Shores and W.C. Fang,J. Electrochem. Soc., 128 (1981), p. 346.
- W.C. Fang and R.A. Rapp,J. Electrochem. Soc., 130 (1983), p. 2335.
- H. Numata, A. Nishikata, and S. Haruyama, Proc. JIMIS-3, Trans. Japan Inst. Suppl. (1983), p. 303.
- X. Zheng and R.A. Rapp,J. Electrochem. Soc., 140 (1993), p. 2857.
- H. Numata and S. Haruyama, Corrosion, 44 (1988), p. 7249.
- J. Kupper and R.A. Rapp, Werkstoffe und Korrosion, 38 (1987), p. 674.
- J.C. Nava, D.Z. Shi, and R.A. Rapp, “Electrochemical Reactions of NaVO3 and Na2CO4 Solutes in Na2SO4,” High Temperature Materials Chemistry IV (Pennington, NJ: Electrochem. Soc., 1987), p. 1.
- D.Z. Shi and R.A. Rapp, Werkstoffe und Korrosion, 41 (1990), p. 215.
- D.A. Shores, Corrosion, 31 (1975), p. 434.
- A. Rahmel, M. Schmidt, and M. Schorr, Oxid. Metals, 18 (1982), p. 195.
- W.T. Wu, A. Rahmel, Oxid. Metals, 19 (1983), p. 201.
- W.T. Wu, A. Rahmel, and M. Schorr, Oxid. Metals, 22 (1984), p. 59.
- W.T. Wu, J. Zhang, and Y. Niu, Proc 11th Intern. Cong. Mater. Corr. (Florence, Italy, April 2–6,1990), p. 1475.
- N. Otsuka and R.A. Rapp, J. Electrochem. Soc., 137 (1990), p. 46.
- Y.M. Wu and R.A. Rapp, J. Electrochem. Soc., 138 (1991), p. 2683.
- G.C. Fryburg et al., J. Electrochem. Soc., 129 (1982), p. 571.
- G.C. Fryburg, F.J. Kohl, and C.A. Stearns, J. Electrochem. Soc., 131 (1984), p. 2985.
- K.L. Luthra and D.A. Shores, J. Electrochem. Soc., 127 (1980), p. 2202.
- K.L. Luthra, High Temperature Corrosion, NACE-6, ed. R.A. Rapp (Houston, TX: NACE, 1983), p. 507.
- K.L. Luthra, Met. Trans., 13A (1982), pp. 1647,1843, and 1853.
- K.L. Luthra and J.H. Wood, Thin Solid Films, 119 (1984), p. 271.
- Y.S. Zhang, L.Q. Shi, and S.T. Shih,J. Chin. Soc. Corr. Protec., 12 (1992), p. 189.
- Y.S. Zhang, X.M. Li, L.Q. Shi, and S.T. Shih, J. Chin. Soc. Corr. Protec, 11 (1991), p. 17.
- L.Q. Shi, Y.S. Zhang, and S.T. Shih, Corr. Sci., 33 (1992), p. 1427.
- L.Q. Shi, Y.S. Zhang, and S.T. Shih, Oxid. Metals, 38 (1992), p. 385.
- Y.S. Zhang, X.M. Li, T.L. Cao, and S.T. Shih, Corr. Sci. Protec Tech., 4 (1992), p. 9.
Cited by
Hot corrosion in gas turbine components
Eliaz, N., Shemesh, G., & Latanision, R. M. (2002) · Engineering Failure Analysis · doi:10.1016/s1350-6307(00)00035-2 · Cited by 695
“In addition to their own relatively low melting point, the vanadium compounds markedly increase the solubility of the oxide when mixed with Na 2 SO 4 [17].”
BackgroundThermal Barrier Coatings—A State of the Art Review
Thakare, J. G., Pandey, C., Mahapatra, M. M., & Mulik, R. S. (2020) · Metals and Materials International · doi:10.1007/s12540-020-00705-w · Cited by 365
Gas turbine coatings – An overview
Rajendran, R. (2012) · Engineering Failure Analysis · doi:10.1016/j.engfailanal.2012.07.007 · Cited by 331
Advanced heat transfer fluids for direct molten salt line-focusing CSP plants
Bonk, A., Sau, S., Uranga, N., Hernaiz, M., & Bauer, T. (2018) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2018.02.002 · Cited by 272
Corrosion of alloys in a chloride molten salt (NaCl-LiCl) for solar thermal technologies
Gomez-Vidal, J. C., & Tirawat, R. (2016) · Solar Energy Materials and Solar Cells · doi:10.1016/j.solmat.2016.05.052 · Cited by 240
“The corrosion rate (CR) in millimeters per year can be calculated using the Stern-Geary equation through Faraday’s law [15,16]: 𝐶𝐶𝐶𝐶 = 𝜌𝜌 where K is a constant equal to 3272 [mm/(A·cm·year)], EW is the equivalent weight of the alloy [g/mole-e - ], and ρ is the alloy density [g/cm 3 ].”
Hot corrosion of some superalloys and role of high-velocity oxy-fuel spray coatings—a review
Sidhu, T. S., Agrawal, R. D., & Prakash, S. (2004) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2004.10.056 · Cited by 235
Combating hot corrosion of boiler tubes – A study
Kumar, S., Kumar, M., & Handa, A. (2018) · Engineering Failure Analysis · doi:10.1016/j.engfailanal.2018.08.004 · Cited by 207
Materials corrosion for thermal energy storage systems in concentrated solar power plants
Walczak, M., Pineda, F., Fernández, Á. G., Mata-Torres, C., & Escobar, R. A. (2018) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2018.01.010 · Cited by 197
Antunes, R. A., & de Oliveira, M. C. L. (2013) · Corrosion Science · doi:10.1016/j.corsci.2013.07.013 · Cited by 184
A review on molten sulfate salts induced hot corrosion
Hu, S., Finklea, H., & Liu, X. (2021) · Journal of Materials Science & Technology · doi:10.1016/j.jmst.2021.03.013 · Cited by 183
Water Vapor–Mediated Volatilization of High-Temperature Materials
Meschter, P. J., Opila, E. J., & Jacobson, N. S. (2013) · Annual Review of Materials Research · doi:10.1146/annurev-matsci-071312-121636 · Cited by 149
Sidhu, B. S., & Prakash, S. (2002) · Surface and Coatings Technology · doi:10.1016/s0257-8972(02)00772-7 · Cited by 146
Leyens, C., Pint, B. A., & Wright, I. G. (2000) · Surface and Coatings Technology · doi:10.1016/s0257-8972(00)00878-1 · Cited by 145
Singh, H., Sidhu, B. S., Puri, D., & Prakash, S. (2007) · Materials and Corrosion · doi:10.1002/maco.200603985 · Cited by 143
Some studies on hot corrosion performance of plasma sprayed coatings on a Fe-based superalloy
Singh, H., Puri, D., & Prakash, S. (2004) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2004.03.030 · Cited by 138
Chen, X., Zhao, Y., Gu, L., Zou, B., Wang, Y., & Cao, X. (2011) · Corrosion Science · doi:10.1016/j.corsci.2011.03.019 · Cited by 124
Vidal, J., Fernández, Á. G., Tirawat, R., Turchi, C. S., & Huddleston, W. (2017) · Solar Energy Materials and Solar Cells · doi:10.1016/j.solmat.2017.02.019 · Cited by 122
“The corrosion rate is calculated using the Stern-Geary equation through Faraday's Law as follows [27]: where CR is the corrosion rate (µm/yr), K is a constant equal to 3,272×10 3 [µm/(A cm yr)], EW is the equivalent weight of the alloy (g/ equivalent), ρ is the alloy density (g/cm 3 ), and A is the…”
Li, L., Lu, J., Liu, X., Dong, T., Zhao, X., Yang, F., & Guo, F. (2021) · Corrosion Science · doi:10.1016/j.corsci.2021.109479 · Cited by 129
Wolfe, D. E., Singh, J., Miller, R. A., Eldridge, J. I., & Zhu, D.-M. (2004) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2004.04.071 · Cited by 117
Ren, X., & Wang, F. (2006) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2005.10.042 · Cited by 101
Vidal, J., Fernández, Á. G., Tirawat, R., Turchi, C. S., & Huddleston, W. (2017) · Solar Energy Materials and Solar Cells · doi:10.1016/j.solmat.2017.03.025 · Cited by 88
Fesharaki, M. N., Razavi, R. S., Mansouri, H. A., & Jamali, H. (2018) · Optics & Laser Technology · doi:10.1016/j.optlastec.2018.09.011 · Cited by 85
Bose, S. (2007) · Elsevier eBooks · doi:10.1016/b978-075068252-7/50006-8 · Cited by 81
Sidhu, T. S., Malik, A., Prakash, S., & Agrawal, R. D. (2007) · Journal of Thermal Spray Technology · doi:10.1007/s11666-007-9106-8 · Cited by 79
Vidal, J. (2017) · npj Materials Degradation · doi:10.1038/s41529-017-0012-3 · Cited by 88
Molten salt induced corrosion of Inconel 625 superalloy in PbSO4–Pb3O4–PbCl2–Fe2O3–ZnO environment
Zahrani, E. M., & Alfantazi, A. M. (2012) · Corrosion Science · doi:10.1016/j.corsci.2012.08.035 · Cited by 77
Singh, J., Vasudev, H., & Singh, S. (2020) · Materials Today: Proceedings · doi:10.1016/j.matpr.2020.01.156 · Cited by 69
Vidal, J., Noel, J., & Weber, J. (2016) · Solar Energy Materials and Solar Cells · doi:10.1016/j.solmat.2016.07.029 · Cited by 76
Grégoire, B., Oskay, C., Meißner, T. M., & Galetz, M. C. (2020) · Solar Energy Materials and Solar Cells · doi:10.1016/j.solmat.2020.110659 · Cited by 74
Garip, Y., & Ozdemir, O. (2018) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2018.11.324 · Cited by 72
Ong, T., Sarvghad, M., Lippiatt, K., Griggs, L., Ryan, H., Will, G. D., & Steinberg, T. (2020) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2020.110006 · Cited by 67
Corrosion behavior of wire arc sprayed Ni-based coatings in extreme environment
Kumar, M., Kant, S., & Kumar, S. (2019) · Materials Research Express · doi:10.1088/2053-1591/ab3bd8 · Cited by 65
Grégoire, B., Oskay, C., Meißner, T. M., & Galetz, M. C. (2020) · Solar Energy Materials and Solar Cells · doi:10.1016/j.solmat.2020.110675 · Cited by 65
The preparation and hot corrosion resistance of gradient NiCoCrAlYSiB coatings
Guo, M. H., Wang, Q. M., Ke, P. L., Gong, J., Sun, C., Huang, R. F., & Wen, L. S. (2006) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2004.12.005 · Cited by 65
Sidhu, H. S., Sidhu, B. S., & Prakash, S. (2005) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2005.07.008 · Cited by 63
Yang, Y. Q., Zhao, Y., Wen, Z., Lu, G., Pei, H., & Yue, Z. F. (2022) · Corrosion Science · doi:10.1016/j.corsci.2022.110381 · Cited by 62
High temperature oxidation performance of Ni-Cr-Ti and Ni-5Al coatings
Sharma, V., Kumar, S., Kumar, M., & Deepak, D. (2019) · Materials Today Proceedings · doi:10.1016/j.matpr.2019.11.048 · Cited by 57
Hot Corrosion of an EB-PVD Thermal-Barrier Coating System at 950°C
Leyens, C., Wright, I. G., & Pint, B. A. (2000) · Oxidation of Metals · doi:10.1023/a:1004634400479 · Cited by 56
A review on surface modification techniques
Singh, S., Kumar, S., & Khanna, V. (2023) · Materials Today Proceedings · doi:10.1016/j.matpr.2023.01.010 · Cited by 55
Corrosion Study of Selective Laser Melted IN718 Alloy upon Post Heat Treatment and Shot Peening
Mythreyi, O. V., Raja, A., Nagesha, B. K., & Jayaganthan, R. (2020) · Metals · doi:10.3390/met10121562 · Cited by 55
“The corrosion rate in mils/year (mpy) of the samples was obtained by using the Faraday law [57] in Equation (1).”
MethodHe, J., Guo, X., Qiao, Y., & Luo, F. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108948 · Cited by 54
Doolabi, M. S., Ghasemi, B., Sadrnezhaad, S. K., Habibolahzadeh, A., & Jafarzadeh, K. (2017) · Corrosion Science · doi:10.1016/j.corsci.2017.09.004 · Cited by 56
Nave, M. I., & Kornev, K. G. (2016) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-016-3888-6 · Cited by 51
Wu, N., Chen, Z., & Mao, S. X. (2005) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2005.00120.x · Cited by 51
Aung, N. N., & Liu, X. (2013) · Corrosion Science · doi:10.1016/j.corsci.2013.07.012 · Cited by 45
Rutkowski, B., Gil, A., & Czyrska‐Filemonowicz, A. (2015) · Corrosion Science · doi:10.1016/j.corsci.2015.10.030 · Cited by 45
Assessment of usability of the exploited gas turbine blade heat-resistant coatings
Bogdan, M., Błachnio, J., Spychała, J., & Zasada, D. J. (2019) · Engineering Failure Analysis · doi:10.1016/j.engfailanal.2019.07.016 · Cited by 42
Bhuyan, P., Pradhan, S. K., Mitra, R., & Mandal, S. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.01.007 · Cited by 42
Type-I Hot Corrosion of Ni-Base Superalloy CM247LC in Presence of Molten Na2SO4 Film
Kumawat, M. K., Parlikar, C., Alam, M. Z., & Das, D. K. (2020) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-020-06068-6 · Cited by 41
Sheetal, Singh, A. K., Thakur, S., Pani, B., & Singh, M. (2023) · Journal of Industrial and Engineering Chemistry · doi:10.1016/j.jiec.2023.10.005 · Cited by 39
A review on protection of boiler tube steels with thermal spray coatings from hot corrosion
Singh, S., Goyal, K., & Bhatia, R. (2022) · Materials Today Proceedings · doi:10.1016/j.matpr.2022.01.219 · Cited by 39
Bose, S. (2018) · Elsevier eBooks · doi:10.1016/b978-0-12-804622-7.00005-x · Cited by 38
Singh, G., Goyal, K., & Bhatia, R. (2017) · Iranian Journal of Science and Technology Transactions of Mechanical Engineering · doi:10.1007/s40997-017-0090-4 · Cited by 38
Castable cements to prevent corrosion of metals in molten salts
Vidal, J., & Morton, E. (2016) · Solar Energy Materials and Solar Cells · doi:10.1016/j.solmat.2016.04.009 · Cited by 37
“The corrosion rates are calculated using the Stern-Geary equation through Faraday’s law [16,18]: 𝜌𝜌 where CR is the corrosion rate (mm/year), K is a constant equal to 3272 [mm/(A·cm·year)], EW is the equivalent weight of the alloy (g/mole-e), and ρ is the alloy density (g/cm 3 ).”
Prakash, S., Puri, D., & Singh, H. (2005) · ISIJ International · doi:10.2355/isijinternational.45.886 · Cited by 36
Corrosion performance of slurry aluminide coatings in molten NaCl–KCl
Grégoire, B., Oskay, C., Meißner, T. M., & Galetz, M. C. (2021) · Solar Energy Materials and Solar Cells · doi:10.1016/j.solmat.2021.110974 · Cited by 36
Kaushal, G., Singh, H., & Prakash, S. (2011) · Oxidation of Metals · doi:10.1007/s11085-011-9245-7 · Cited by 35
Sahu, J. K., Kumar, B. R., Das, S. K., Paulose, N., & Mannan, S. L. (2014) · Materials Science and Engineering A · doi:10.1016/j.msea.2014.11.016 · Cited by 32
Singh, H., Bala, N., Kaur, N., Sharma, S. K., Kim, D. Y., & Prakash, S. (2015) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2015.08.002 · Cited by 31
Dhand, D., Kumar, P., & Grewal, J. S. (2021) · Corrosion Reviews · doi:10.1515/corrrev-2020-0043 · Cited by 31
Li, S., Yang, X., Qi, H., Song, J., & Shi, D. (2018) · International Journal of Fatigue · doi:10.1016/j.ijfatigue.2018.06.035 · Cited by 29
A new solid‐state mode of hot corrosion at temperatures below 700°C
Kistler, E., Chen, W., Meier, G. H., & Gleeson, B. T. (2019) · Materials and Corrosion · doi:10.1002/maco.201810751 · Cited by 30
Young, J. (2008) · Elsevier's corrosion science series · doi:10.1016/s1875-9491(08)00008-2 · Cited by 29
High‐Temperature Oxidation and Corrosion of Intermetallics
Brady, M. P., Pint, B. A., Tortorelli, P. F., Wright, I. G., & Hanrahan, R. J. (2013) · Materials Science and Technology · doi:10.1002/9783527603978.mst0408 · Cited by 29
Rani, A., Bala, N., & Gupta, C. M. (2017) · Oxidation of Metals · doi:10.1007/s11085-017-9759-8 · Cited by 28
Behavior of Cold Spray Coating in Real Incineration Environment
Kalsi, S. S., Sidhu, T. S., Singh, H., & Karthikeyan, J. (2014) · Materials and Manufacturing Processes · doi:10.1080/10426914.2014.912319 · Cited by 28
“Rapp and Zhang [2] defined the hot corrosion as an accelerated oxidation of metal and alloy at high temperature when their surfaces are covered with molten salts of contaminants like sodium sulfate, sodium chloride, and vanadium oxide.”
BackgroundThakare, J. G., Mulik, R. S., Mahapatra, M. M., & Upadhyaya, R. (2018) · Ceramics International · doi:10.1016/j.ceramint.2018.08.217 · Cited by 27
Bhuyan, P., Sanyal, S., Mitra, R., & Mandal, S. (2022) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2022.165262 · Cited by 27
Ji, F., Wang, Z., & Wu, L. (2022) · Materials Today Communications · doi:10.1016/j.mtcomm.2022.104063 · Cited by 27
Mudgal, D., Singh, S. P., & Prakash, S. (2014) · Metallography Microstructure and Analysis · doi:10.1007/s13632-014-0182-0 · Cited by 26
“often necessitates replacement of superheater tubes as often as annually in some units [1, 2].”
BackgroundLeyens, C., Wright, I. G., & Pint, B. A. (2000) · Oxidation of Metals · doi:10.1023/a:1004698211940 · Cited by 26
High temperature corrosion-fatigue behavior of a shot peened nickel based superalloy
Li, Y., Cockings, H. L., Mignanelli, P. M., Whittaker, M. T., Cockings, B. J., Buckingham, R. C., & Bache, M. R. (2022) · Corrosion Science · doi:10.1016/j.corsci.2022.110577 · Cited by 25
Atypical decomposition processes of Sm2Zr2O7 + 8YSZ dual-phase TBCs during hot corrosion
Moskal, G., Jucha, S., Mikuśkiewicz, M., Migas, D., & Jasik, A. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108681 · Cited by 24
Bhuyan, P., Paliwal, M., Sarma, V. S., de Boer, B., Mitra, R., & Mandal, S. (2021) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2021.159499 · Cited by 25
Mishra, N. K., Mishra, S. B., & Kumar, R. S. (2014) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2014.07.089 · Cited by 24
Li, T., Zhou, Y., Li, M., & Li, Z. (2007) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2007.08.025 · Cited by 24
High‐Temperature Oxidation and Corrosion of Intermetallics
Brady, M. P., Pint, B. A., Tortorelli, P. F., Wright, I. G., & Hanrahan, R. J. (2000) · Wiley eBooks · doi:10.1002/9783527619306.ch15 · Cited by 24
Yu, Z., Lu, J., Chen, M., Wang, J., & Wang, F. (2021) · Corrosion Science · doi:10.1016/j.corsci.2021.109789 · Cited by 23
Xiang, J., Xie, F., Wu, X., Wang, S., & Li, L. (2021) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2021.127282 · Cited by 23
Mechanisms of Accelerated Oxidation of Copper in the Presence of Molten Oxides
Belousov, V. V. (2007) · Oxidation of Metals · doi:10.1007/s11085-007-9054-1 · Cited by 23
Cyclic high temperature oxidation behaviour of sputtered Cr/Al multilayer coatings on superalloy
Rahman, A., Jayaganthan, R., Prakash, S., Chawla, V., & Chandra, R. (2008) · Surface Engineering · doi:10.1179/026708408x339064 · Cited by 24
Modeling of the solubility of alumina in the NaF-AlF3 system at 1300 K
Zhang, Y., Sahai, Y., Rapp, R. A., & Gupta, S. K. (2002) · Metallurgical and Materials Transactions B · doi:10.1007/s11663-002-0015-4 · Cited by 22
Self-citationBhuyan, P., Pradhan, S. K., Mitra, R., & Mandal, S. (2021) · Materials Characterization · doi:10.1016/j.matchar.2021.111272 · Cited by 22
Effect of surface modification on the hot corrosion resistance of Inconel 718 at 700 °C
Kumar, S., Satapathy, B., Pradhan, D., & Mahobia, G. S. (2019) · Materials Research Express · doi:10.1088/2053-1591/ab1dc7 · Cited by 26
Mishra, N. K., Kumar, N., & Mishra, S. S. (2014) · Indian Journal of Materials Science · doi:10.1155/2014/453607 · Cited by 21
“Many important engineering systems operating at high temperature fail due to hot corrosion which is the main failure modes of components in the hot sections of gas turbines, boilers, and so forth [1, 2].”
BackgroundRevisiting the Inhibition of Vanadium-Induced Hot Corrosion in Gas Turbines
Rocca, E., Steinmetz, P., & Molière, M. (2003) · Journal of Engineering for Gas Turbines and Power · doi:10.1115/1.1456095 · Cited by 20
He, J., Guo, X., & Qiao, Y. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.05.010 · Cited by 21
Targhi, V. T., Omidvar, H., Hadavi, S. M. M., & Sharifianjazi, F. (2020) · Materials Research Express · doi:10.1088/2053-1591/ab6dab · Cited by 19
Hot Corrosion Behavior of Arc-Sprayed Highly Dense NiCr-Based Coatings in Chloride Salt Deposit
Qin, E., Song, Y., Ji, H. W., Huang, Q., Liu, Z., & Wu, S. (2017) · Journal of Thermal Spray Technology · doi:10.1007/s11666-017-0549-2 · Cited by 19
Development of dual sulfur oxides and oxygen solid state sensor for “in situ” measurements
Zhuiykov, S. (2000) · Fuel · doi:10.1016/s0016-2361(99)00261-6 · Cited by 18
Zhang, Y., Hu, S., Wen, Y., Ikeuba, A. I., Tan, X., Sun, T., & Liu, X. (2025) · Electrochimica Acta · doi:10.1016/j.electacta.2025.146105 · Cited by 19
Self-citationKumar, R., Tewari, V. K., & Prakash, S. (2007) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-006-9053-x · Cited by 17
Meeting materials needs in extreme naval corrosive and oxidative environments
Shifler, D. A. (2015) · Materials at High Temperatures · doi:10.1179/0960340915z.000000000115 · Cited by 16
Kumar, M., Singh, H., Singh, N., Chavan, N. M., Kumar, S., & Joshi, S. V. (2015) · Journal of Thermal Spray Technology · doi:10.1007/s11666-015-0249-8 · Cited by 16
Corrosion Behavior of Alloy 625 in PbSO4-Pb3O4-PbCl2-ZnO-10 Wt Pct CdO Molten Salt Medium
Zahrani, E. M., & Alfantazi, A. M. (2012) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-011-0996-1 · Cited by 16
Cyclic Oxidation and Hot Corrosion Behavior of Nickel–Iron-Based Superalloy
Chellaganesh, D., Khan, M. A., Jappes, J. T. W., & Sathiyanarayanan, S. (2017) · High Temperature Materials and Processes · doi:10.1515/htmp-2016-0130 · Cited by 16
Badea, T. A., Batalu, D., Constantin, N., Paraschiv, A., Pătroi, D., & Ceatra, L. C. (2022) · Materials · doi:10.3390/ma15124082 · Cited by 15
Rani, A., Bala, N., & Gupta, C. M. (2017) · Anti-Corrosion Methods and Materials · doi:10.1108/acmm-09-2016-1712 · Cited by 15
Rippy, K. C., Volk, E. K., Beers, R. A., Kozubal, E., Gauderman, K., & Vidal, J. (2022) · Energies · doi:10.3390/en15124421 · Cited by 15
Grégoire, B., Montero, X., Galetz, M. C., Bonnet, G., & Pedraza, F. (2023) · Corrosion Science · doi:10.1016/j.corsci.2023.111092 · Cited by 15
Metadata
- Authors
- Rapp, R. A., & Zhang, Y.-S.
- Affiliations
- The Ohio State University (US)
- Venue
- JOM
- Published
- 1994-12
- Volume
- 46
- Issue
- 12
- Pages
- 47-55
- ISSN
- 0148-6608 (ISSN-L)
- 1047-4838
- 1543-1851
- OpenAlex
- W2324760338
- Cited by
- 247
- References
- 31
- Citations by year
- 2026: 17 · 2025: 13 · 2024: 9 · 2023: 11 · 2022: 12 · 2021: 16 · 2020: 15 · 2019: 14 · 2018: 11 · 2017: 13 · 2016: 11 · 2015: 9 · 2014: 10 · 2013: 11 · 2012: 6
- FWCI
- 0.00
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.springer.com/tdm (tdm)
- Locations
- JOM (publishedVersion)
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Chemistry › Electrochemistry › Molten salt chemistry and electrochemical processes
- Physical Sciences › Materials Science › Metals and Alloys › Metallurgical Processes and Thermodynamics
- Keywords
- hot corrosion, sodium sulfate, electrochemical corrosion mechanism, sodium metavanadate, electrochemical polarization, corrosion kinetics, alloy corrosion
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.