Hot corrosion of materials: Fundamental studies
The DOI matches its Crossref record; 6 of the 31 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“As with the thin aqueous layer on alloys in atmospheric corrosion, this molten salt layer is a pure ionic conductor which separates the alloys from the gas phase physically [1, 19, 47].”
From A review on molten sulfate salts induced hot corrosion (2021) · cites this paper as [1]
In the citing paper
“These sulfate salts easily attach onto the surfaces of high temperature components and are melted to form a thin fused salt film at elevated temperatures.”
From A review on molten sulfate salts induced hot corrosion (2021) · cites this paper as [1]
In the citing paper
“The predominant chemical reactant involved in hot corrosion has been confirmed to be sodium sulfate (Na2SO4), due to its extraordinary stability over a wide range of temperatures and oxygen partial pressures [1, 6, 19].”
From A review on molten sulfate salts induced hot corrosion (2021) · cites this paper as [1]
In the citing paper
“The diagram demonstrates the good stability of Na2SO4 over a wide range of log and .”
From A review on molten sulfate salts induced hot corrosion (2021) · cites this paper as [1]
In the citing paper
“In the O2-SO2-SO3 environment (Eq. (1)), the solubilities of both O2 and SO2 in molten salt are poor. In contrast, SO3 can dissolve in molten salt because of the formation of pyrosulfate ions through Eq. (2) [1, 19].”
From A review on molten sulfate salts induced hot corrosion (2021) · cites this paper as [1]
2 more claims about this paper
Create a free account to see every claim other papers make about this one.
Citations
Cites
(2006) · Electrochemistry and Corrosion Science · doi:10.1007/1-4020-7860-9_10 · Cited by 1,814
The Hot Corrosion of Metals by Molten Salts
Rapp, R. A. (1981) · ECS Proceedings Volumes · doi:10.1149/198110.0159pv · Cited by 136
Self-citationDeposition and Corrosion in Gas Turbines
Billingham, J. (1974) · British Corrosion Journal · doi:10.1179/000705974798321738 · Cited by 135
Rapp, R. A. (1989) · Studies in inorganic chemistry · doi:10.1016/b978-0-444-88534-0.50016-3 · Cited by 31
Self-citationHigh temperature corrosion and protection
Colson, J. C., Strafford, K. N., & Lambertin, M. (1986) · Journal de Chimie Physique · doi:10.1051/jcp/1986830745 · Cited by 27
Solubility of CeO2 in Molten Na2SO4–10 mol% NaVO3 Salt Solution at 900°C
Zhang, Y. S. (1994) · ECS Proceedings Volumes · doi:10.1149/199413.0171pv · Cited by 2
Self-citation
Research works printed but not linked: 69
- W.T. Reid, R.C. Corey, and BJ. Cross, Trans. ASME, 67 (1945), p. 279.
- F.J. Wall and S.T. Michael, ASTM Spec. Tech. Publ. STP 421 (1967), p. 223.
- K.J. Kohl et al., J. Electrochem. Soc., 126 (1979), p. 1054.
- K.L. Luthra and H.S. Spacil, J. Electrochem. Soc., 129 (1982), p. 649.
- E.L. Simons, G.V. Browning, and H.A. Liebhafsky, Corrosion, 11 (1955), p. 505.
- A.U. Seybolt, Trans. AIME, 242 (1968), p. 1955.
- N.S. Bornstein and M.A. DeCrescente, Trans. AIME, 245 (1969), p. 583.
- N.S. Bornstein and M.A. DeCrescente, Met. Trans.,2 (1971), p. 2875.
- J.A. Goebel and F.S. Pettit, Met. Trans., 1 (1970), p. 1943.
- J.A. Goebel, F.S. Pettit, and G.W. Goward, Met. Trans., 4 (1973), p. 261.
- J. Stringer, Annual Review of Materials Sci., 7, ed. R.A. Huggins (Palo Alto, CA: Annual Review Inc., 1977), p. 449.
- J. Stringer, Materials Sci. Techn., 3 (1987), p. 482.
- F.S. Pettit and C.S. Giggins, “Hot Corrosion,” Superalloys II, ed. C.T. Sims, N.S. Stoloff, and W.C. Hagel (New York: Wiley Publ., 1987), p. 327.
- R.A. Rapp, Corrosion, 42 (1986), p. 568.
- C.O. Park and R.A. Rapp, J. Electrochem. Soc., 133 (1986), p. 1636.
- D. Inman and D.M. Wrench, Brit. Corros. J., 1 (1966), p. 246.
- D.A. Shores and R.C. John, J. Appl. Electrochem., 10 (1980), p. 275.
- P.P. Leblanc and R.A. Rapp, J. Electrochem. Soc., 139 (1992), p. L31.
- P.P. Leblanc and R.A. Rapp, J. Electrochem. Soc., 140 (1993), p. L41.
- D.K. Gupta and R.A. Rapp, J. Electrochem. Soc., 127 (1980), p. 2194 and 2656.
- Y.S. Zhang and R.A. Rapp, J. Electrochem. Soc., 132 (1985), p. 734 and 2498.
- Y.S. Zhang, J. Electrochem. Soc., 133 (1986), p. 655.
- P.D. Jose, D.K. Gupta, and R.A. Rapp, J. Electrochem. Soc., 132 (1985), p. 735.
- D.Z. Shi and R.A. Rapp, J. Electrochem. Soc., 133 (1986), p. 849.
- M.L. Deanhardt and K.H. Stern, J. Electrochem. Soc., 128 (1981), p. 2577.
- A.K. Misra, D.P. Whittle, and W.L. Worrell, J. Electrochem. Soc., 129 (1982), p. 1840.
- M.L. Deanhardt and K.H. Stern, J. Electrochem. Soc., 129 (1982), p. 2228.
- N.S. Jacobson and J.L. Smialek, J. Amer. Ceram. Soc., 68 (1985), p. 432.
- N.S. Jacobson, J. Amer. Ceram. Soc., 76 (1993), p. 3.
- Y.S. Hwang and R.A. Rapp,J. Electrochem. Soc., 137 (1990), p. 1276.
- Y.S. Zhang and R.A. Rapp, Corrosion, 43 (1987), p. 348.
- Y.S. Hwang and R.A. Rapp, Corrosion, 45 (1989), p. 933.
- R.A. Rapp and Y.S. Zhang, “Electrochemical Studies of Hot Corrosion of Materials,” Proc Intern. Corr. Conf. (Merida, Mexico: 1993)
- R.L. Jones, D.B. Nordman, and S.T. Gadomski, Met. Trans., 16A (1985), p. 303.
- R.L. Jones, S.R. Jones, and C.E. Williams, J. Electrochem. Soc., 132 (1985), p. 1499.
- R.L. Jones, C.E. Williams, and S.R. Jones, J. Electrochem. Soc., 133 (1986), p. 227.
- R.L. Jones and D. Mess,J. Amer. Ceram. Soc., 75 (1992), p. 1818.
- R.L. Jones, High Temp. Tech., 6 (1988), p. 187.
- M. Seiersten and P. Kofstad, Mater. Sci. Tech., 3 (1987), p. 576.
- A.S. Nagelberg, J. Electrochem. Soc., 132 (1985), p. 2502.
- F. Mansfeld and J.V. Kenkel, Corr. Sci., 16 (1976), p. 111.
- F. Mansfeld and J.V. Kenkel, Corrosion, 33 (1977), p. 238.
- R. Andresen, J. Electrochem. Soc., 126 (1979), p. 328.
- D.A. Shores and W.C. Fang,J. Electrochem. Soc., 128 (1981), p. 346.
- W.C. Fang and R.A. Rapp,J. Electrochem. Soc., 130 (1983), p. 2335.
- H. Numata, A. Nishikata, and S. Haruyama, Proc. JIMIS-3, Trans. Japan Inst. Suppl. (1983), p. 303.
- X. Zheng and R.A. Rapp,J. Electrochem. Soc., 140 (1993), p. 2857.
- H. Numata and S. Haruyama, Corrosion, 44 (1988), p. 7249.
- J. Kupper and R.A. Rapp, Werkstoffe und Korrosion, 38 (1987), p. 674.
- J.C. Nava, D.Z. Shi, and R.A. Rapp, “Electrochemical Reactions of NaVO3 and Na2CO4 Solutes in Na2SO4,” High Temperature Materials Chemistry IV (Pennington, NJ: Electrochem. Soc., 1987), p. 1.
- D.Z. Shi and R.A. Rapp, Werkstoffe und Korrosion, 41 (1990), p. 215.
- D.A. Shores, Corrosion, 31 (1975), p. 434.
- A. Rahmel, M. Schmidt, and M. Schorr, Oxid. Metals, 18 (1982), p. 195.
- W.T. Wu, A. Rahmel, Oxid. Metals, 19 (1983), p. 201.
- W.T. Wu, A. Rahmel, and M. Schorr, Oxid. Metals, 22 (1984), p. 59.
- W.T. Wu, J. Zhang, and Y. Niu, Proc 11th Intern. Cong. Mater. Corr. (Florence, Italy, April 2–6,1990), p. 1475.
- N. Otsuka and R.A. Rapp, J. Electrochem. Soc., 137 (1990), p. 46.
- Y.M. Wu and R.A. Rapp, J. Electrochem. Soc., 138 (1991), p. 2683.
- G.C. Fryburg et al., J. Electrochem. Soc., 129 (1982), p. 571.
- G.C. Fryburg, F.J. Kohl, and C.A. Stearns, J. Electrochem. Soc., 131 (1984), p. 2985.
- K.L. Luthra and D.A. Shores, J. Electrochem. Soc., 127 (1980), p. 2202.
- K.L. Luthra, High Temperature Corrosion, NACE-6, ed. R.A. Rapp (Houston, TX: NACE, 1983), p. 507.
- K.L. Luthra, Met. Trans., 13A (1982), pp. 1647,1843, and 1853.
- K.L. Luthra and J.H. Wood, Thin Solid Films, 119 (1984), p. 271.
- Y.S. Zhang, L.Q. Shi, and S.T. Shih,J. Chin. Soc. Corr. Protec., 12 (1992), p. 189.
- Y.S. Zhang, X.M. Li, L.Q. Shi, and S.T. Shih, J. Chin. Soc. Corr. Protec, 11 (1991), p. 17.
- L.Q. Shi, Y.S. Zhang, and S.T. Shih, Corr. Sci., 33 (1992), p. 1427.
- L.Q. Shi, Y.S. Zhang, and S.T. Shih, Oxid. Metals, 38 (1992), p. 385.
- Y.S. Zhang, X.M. Li, T.L. Cao, and S.T. Shih, Corr. Sci. Protec Tech., 4 (1992), p. 9.
Cited by
Items 101–200 of 252
Electrochemical mechanism of hot corrosion of Bi2O3-deposited copper
Belousov, V. V. (2009) · Corrosion Science · doi:10.1016/j.corsci.2009.08.044 · Cited by 15
Catastrophic Oxidation of Copper: A Brief Review
Belousov, V. V., & Klimashin, A. A. (2012) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-012-1173-x · Cited by 16
Grégoire, B., Montero, X., Galetz, M. C., Bonnet, G., & Pedraza, F. (2023) · Corrosion Science · doi:10.1016/j.corsci.2023.111517 · Cited by 17
Corrosion Resistance of Alloy 740 as Superheater Tubing in Coal-Fired Ultra-Supercritical Boilers
Baker, B., & Smith, G. D. (2004) · NACE CORROSION Conference · doi:10.5006/c2004-04526 · Cited by 14
Matsumoto, M., Tsuchiyama, A., Miyake, A., Ito, M., Matsuno, J., Uesugi, K., Takeuchi, A., Kodama, Y., Yasutake, M., & Vaccaro, E. (2022) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2022.02.024 · Cited by 14
Gitanjaly, Singh, H., Singh, S. P., & Prakash, S. (2010) · Materials at High Temperatures · doi:10.1179/096034010x12710862884794 · Cited by 13
Müller, D., & Heuss‐Aßbichler, S. (2016) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2016.05.042 · Cited by 13
Sidhu, H. S., Sidhu, B. S., & Prakash, S. (2006) · ISIJ International · doi:10.2355/isijinternational.46.1067 · Cited by 12
Bangari, R. S., Sahu, S., & Yadav, P. C. (2018) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.2018.53 · Cited by 12
Thakare, J. G., Pandey, C., Mulik, R. S., & Mahapatra, M. M. (2019) · Materials Research Express · doi:10.1088/2053-1591/ab5265 · Cited by 12
Chen, K., Lin, J., Li, W., Zhu, W., Li, K., Yi, A., Hu, S., Chen, M., & Wang, F. (2021) · Crystals · doi:10.3390/cryst11101213 · Cited by 12
“Competing with the growth of chromium oxide, Cl− ions in the molten salt will attack the chromium oxide [33], and the reaction formula is:”
BackgroundAccelerated corrosion of MoO3-deposited copper
Klimashin, A. A., & Belousov, V. V. (2011) · Corrosion Science · doi:10.1016/j.corsci.2011.05.058 · Cited by 12
Kumar, R., Tewari, V. K., & Prakash, S. (2008) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-008-9309-2 · Cited by 12
Fan, X., Sun, R., Dong, J., Wei, L., & Wang, Q. (2020) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2020.08.068 · Cited by 12
Pourshahsavary, R., Yaghtin, A., & Hosseinabadi, N. (2023) · Materials Chemistry and Physics · doi:10.1016/j.matchemphys.2023.127406 · Cited by 11
Alam, M. S., & Das, A. K. (2023) · High Temperature Corrosion of Materials · doi:10.1007/s11085-023-10162-6 · Cited by 11
“As a result, capacity of components to transport loads declines quickly and finally leading to their catastrophic breakdown [5].”
BackgroundYoung, D. J. (2016) · Elsevier eBooks · doi:10.1016/b978-0-08-100101-1.00008-x · Cited by 12
The influence of iron and cobalt on the type II hot corrosion behavior of NiCr model alloys
König, T., Montero, X., & Galetz, M. C. (2020) · Materials and Corrosion · doi:10.1002/maco.201911376 · Cited by 11
Tristancho-Reyes, J. L., Chacón-Nava, J. G., Ballesteros, D. Y. P., Gaona-Tiburcio, C., Gonzalez-Rodriguez, J. G., Martínez-Villafañe, A., & Almeraya-Calderón, F. (2011) · International Journal of Electrochemical Science · doi:10.1016/s1452-3981(23)15006-1 · Cited by 11
Jegadeeswaran, N., Bhat, K. U., & Ramesh, M. R. (2015) · Transactions of the Indian Institute of Metals · doi:10.1007/s12666-015-0605-x · Cited by 11
Carburization of 9 %Cr Steels in a Simulated Oxyfuel Corrosion Environment
Ōtsuka, N. (2013) · Oxidation of Metals · doi:10.1007/s11085-013-9396-9 · Cited by 11
Galedari, S. A., Jazi, M. S., Azarmi, F., & Wang, Y. C. (2017) · Materials and Corrosion · doi:10.1002/maco.201609276 · Cited by 10
Effect of SO2 on corrosion behaviour of Ni-base alloys in a simulated combustion environment
Xi, X., Zhang, J., & Young, D. J. (2024) · Corrosion Science · doi:10.1016/j.corsci.2024.112151 · Cited by 10
A New Alloy Designed for Superheater Tubing in Coal-Fired Ultra Supercritical Boilers
Baker, B. (2005) · International Symposium on Superalloys 718, 625, 706 and Various Derivatives · doi:10.7449/2005/superalloys_2005_601_611 · Cited by 10
“Perhaps incorporation of molybdenum into the trisulfate ash forming at the material surface leads to an increased corrosion rate by affecting the solubility of protective chromium oxides, as observed in Mocontaining alloys which undergo high temperature Type I hot corrosion at about 825-950°C [3,4].”
BackgroundSubramani, P., Arivazhagan, N., Selvaraj, S. K., Mancin, S., & Manikandan, M. (2022) · International Journal of Thermofluids · doi:10.1016/j.ijft.2022.100148 · Cited by 10
Hot Corrosion Behavior of Low-Pressure Cold-Sprayed CoNiCrAlY Coatings
Zhang, L. W., Ning, X., Lü, L., Wang, Q. S., & Wang, L. (2016) · Journal of Thermal Spray Technology · doi:10.1007/s11666-016-0381-0 · Cited by 10
Environmental Damage at High Temperature
(2010) · Elsevier eBooks · doi:10.1533/9780857090805.2.330 · Cited by 10
Zhang, Y., Li, X., Miao, L., Meng, X., Luo, K., Lu, J., & Cai, J. (2025) · Materials Characterization · doi:10.1016/j.matchar.2025.115795 · Cited by 10
Self-citationOxidation and hot corrosion of thermal barrier coatings (TBCs)
Zhou, C., & Song, Y. (2011) · Elsevier eBooks · doi:10.1533/9780857090829.3.193 · Cited by 10
Lyyränen, J., Jokiniemi, J. K., Kauppinen, E. I., & Silvonen, A. (2004) · Fuel Processing Technology · doi:10.1016/j.fuproc.2004.03.011 · Cited by 10
Rahimi, A., SHAMANIAN, M., & Atapour, M. (2021) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-021-05878-y · Cited by 8
Creep stress induced pit-to-crack transition of Super304H in fireside corrosion
Yang, X., Xu, Y., Fu, S., Lu, J., Huang, J., & Li, W. (2024) · Corrosion Science · doi:10.1016/j.corsci.2024.112470 · Cited by 8
Performance of MCrAlX coatings : Oxidation, Hot corrosion and Interdiffusion
Zhang, P. (2019) · Linköping studies in science and technology. Dissertations · doi:10.3384/diss.diva-161511 · Cited by 8
“There are two types of hot corrosion depending on the mechanism induced by corrosive salt: Type I at "high" temperature 850-1000 °C [114, 115] and Type II at "low" temperature below 800 °C [117, 118], as illustrated in Fig.”
BackgroundBordenet, B., & Boßmann, H. (2004) · Materials science forum · doi:10.4028/www.scientific.net/msf.461-464.907 · Cited by 8
Hot corrosion of alloys and coatings
Prakash, S. (2008) · Elsevier eBooks · doi:10.1533/9781845694258.1.164 · Cited by 7
Hot Corrosion Behavior of FeAl Intermetallic Compound Modified with Silver in Molten Salt Mixture
Rodriguez-Diaz, R. A., Uruchurtu, J., Molina-Ocampo, A., Porcayo-Calderón, J., Mendoza, M. E., Valdez, B. S., & Juarez-Islas, J. A. (2013) · International Journal of Electrochemical Science · doi:10.1016/s1452-3981(23)13229-9 · Cited by 8
Lyyränen, J. (2006) · Aaltodoc (Aalto University) · Cited by 9
Li, Q.-Y., Liu, F., Wang, Z., Zhao, Y.-X., Tan, L., & Huang, L. (2025) · Journal of Central South University · doi:10.1007/s11771-025-6068-2 · Cited by 7
“− Based on the Rapp-Goto model [29], the dissolution and reprecipitation of Al 2 O 3 at the oxide/salt and salt/ gas interfaces, respectively, result in the formation of sparsely acicular Al 2 O 3 structures, as evidenced in Figure 3.”
2016 Frank Newman Speller Award:Understanding High-Temperature Corrosion—Key to Energy Efficiency?
Shifler, D. A. (2016) · CORROSION · doi:10.5006/2235 · Cited by 7
Patil, A. R., & Vagge, S. T. (2023) · Strength of Materials · doi:10.1007/s11223-023-00551-2 · Cited by 7
Behaviour of thermally sprayed coating for hot corrosion applications: Review paper
Alam, M. S., Kumar, N., & Das, A. K. (2024) · Journal of Electrochemical Science and Engineering · doi:10.5599/jese.2324 · Cited by 13
“In the late 1960s, turbine makers and users learned about hot corrosion due to the severe corrosive assault that occurred in the engines of rescue planes and helicopters operating over and near seawater during the Vietnam War [3,4].”
García-Herrera, J. E., Alvarado-Orozco, J. M., Muñoz‐Saldaña, J., Garcia-Fresnillo, L., & Meier, G. H. (2015) · Oxidation of Metals · doi:10.1007/s11085-015-9586-8 · Cited by 7
Rapp, R. A. (2001) · Elsevier eBooks · doi:10.1016/b0-08-043152-6/00682-3 · Cited by 7
Self-citationÖzbek, Y. Y., Odabas, O., Binal, G., Ozgurluk, Y., & Karaoğlanlı, A. C. (2025) · Metals · doi:10.3390/met15111169 · Cited by 6
Unnervik, D., & Harada, T. (2024) · Langmuir · doi:10.1021/acs.langmuir.3c04005 · Cited by 6
Hot corrosion behavior of 304 & P91 graded composite transition joint under molten sulfate salts
Sun, T., Hu, S., Ikeuba, A. I., Wen, Y., Tan, X., Zhang, Y., Qian, H., Wang, Y., Feng, Z., Cui, B., et al. (2025) · Corrosion Science · doi:10.1016/j.corsci.2025.113033 · Cited by 6
Self-citationRocca, E., Aranda, L., Vilasi, M., & Steinmetz, P. (2004) · Materials science forum · doi:10.4028/www.scientific.net/msf.461-464.917 · Cited by 6
Garip, Y. (2026) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2026.188900 · Cited by 7
Huilgol, P., Udupa, K. R., & Bhat, K. U. (2019) · Transactions of the Indian Institute of Metals · doi:10.1007/s12666-019-01653-9 · Cited by 5
Hot Corrosion Performance of HVOF NiCr-Based Coatings in Coal/Biomass Co-fired Power Plants
Ramandhany, S., Triyono, D., Sugiarti, E., Wismogroho, A. S., Izzuddin, H., Afandi, A. M., Widayatno, W. B., Sar’i, M., Saptari, S. A., & Sundawa, R. Y. (2023) · High Temperature Corrosion of Materials · doi:10.1007/s11085-023-10208-9 · Cited by 6
Unnervik, D., & Harada, T. (2024) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.4c05337 · Cited by 5
Lyyränen, J., Jokiniemi, J. K., Kauppinen, E. I., & Silvonen, A. (2004) · Fuel Processing Technology · doi:10.1016/j.fuproc.2004.03.012 · Cited by 5
The Cyclic Hot Corrosion Behavior of Pt–Al–7%YSZ Coating
Rabieifar, A., Nategh, S., Afshar, M. R., & Najafi, H. (2020) · Oxidation of Metals · doi:10.1007/s11085-020-10006-7 · Cited by 5
Rapp, R. A., & Begum, S. (2016) · Elsevier eBooks · doi:10.1016/b978-0-12-803581-8.02723-5 · Cited by 5
Self-citationDesign and statistical analysis of plasma coatings on superalloy for gas turbine applications
Khan, M. A., Sundarrajan, S., & Natarajan, S. (2016) · Materials at High Temperatures · doi:10.1080/09603409.2016.1222051 · Cited by 6
Gitanjaly, Bala, N., Singh, H., & Prakash, S. (2015) · Surface Engineering and Applied Electrochemistry · doi:10.3103/s1068375515020040 · Cited by 5
“”[1] “During the combustion of certain low–grade fossil fuels, vanadium compounds such as NaVO3 and V2O5, may also be deposited in the salt film” [1].”
BackgroundImproving Heat Recovery In Biomass-Fired Boilers
Keiser, J. R., USDOE Office of Energy Efficiency and Renewable Energy (EERE), Sharp, W., Singbeil, D., Singh, P., Frederick, L. A., & Meyer, J. (2013) · OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) · doi:10.2172/1093743 · Cited by 7
Zhao, F., Wang, Y., Cui, X., Xiong, T., & Wang, J. (2026) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2026.133398 · Cited by 5
Characterisation of 80% Cr3c2 – 20 % (Ni-20cr) Coating and Erosion Behaviour
Bhatia, R., Singh, H., & Sidhu, B. S. (2012) · Asian Journal of Engineering and Applied Technology · doi:10.51983/ajeat-2012.1.2.2497 · Cited by 4
Yu, D., Cheng, J., Chu, Y., Zhang, H., & Zhou, X. (2025) · Anti-Corrosion Methods and Materials · doi:10.1108/acmm-03-2025-3214 · Cited by 4
Elango, D., Das, A. D., Babu, S. P. K., Natarajan, S., & Yeshitla, A. (2021) · Advances in Materials Science and Engineering · doi:10.1155/2021/8706630 · Cited by 4
RetractedChaudhary, R., Kaur, A., Bala, N., & Kansal, S. K. (2024) · High Temperature Corrosion of Materials · doi:10.1007/s11085-024-10240-3 · Cited by 4
Transmission Line Modeling Applied to Hot Corrosion of Fe-40at.pctAl in Molten LiCl–KCl
Barraza-Fierro, J. I., Espinosa-Medina, M. A., & Castaneda, H. (2015) · Metallurgical and Materials Transactions B · doi:10.1007/s11663-015-0430-y · Cited by 4
Modeling of Equilibria in Complex Cryolite Melts
Rapp, R. A., & Zhang, Y. (2005) · Monatshefte für Chemie - Chemical Monthly · doi:10.1007/s00706-005-0312-0 · Cited by 4
Self-citationA Study of Hot Corrosion Behaviour of NiAl Coatings in an Aggressive Environment
Kianicová, M., & Kafrík, J. (2015) · Diffusion and defect data, solid state data. Part B, Solid state phenomena/Solid state phenomena · doi:10.4028/www.scientific.net/ssp.226.177 · Cited by 4
“Sulphur is a principal impurity in fossil fuels, and sodium is introduced into the combustion air, usually in an aerosol originating from seawater [9, 10].”
BackgroundGoyal, G., Bala, N., Singh, H., & Prakash, S. (2014) · Oxidation of Metals · doi:10.1007/s11085-014-9476-5 · Cited by 4
Hot Corrosion Behavior of Sputtered Nanocrystalline Coating with Yttrium Addition at 900 °C
Jiang, W., Yu, P., Wang, W., Zhu, S., & Wang, F. (2014) · Materials · doi:10.3390/ma7042882 · Cited by 4
“Hot corrosion induced by salts deposition is a common phenomenon for the blades and vanes in modern gas turbines, especially in seawater environment [1–3].”
BackgroundHot Corrosion In Bio Medical Waste Incinerator And Cold Spray Coatings - A Review
Kalsi, S. S. (2013) · i-manager s Journal on Material Science · doi:10.26634/jms.1.2.2451 · Cited by 4
Solubility Measurements of Fe2O3 and Cr2O3 in Fused Na2B4O7-B2O3 in Air at 1173 K
Toki, R., Doi, T., & Ōtsuka, N. (2016) · MATERIALS TRANSACTIONS · doi:10.2320/matertrans.m2015275 · Cited by 4
Chen, J., Zhou, Y., Liu, X., Li, K., Wang, A., Fu, H., Zhang, H., & Zhu, Z. (2026) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2026.186003 · Cited by 3
Zhang, D., Meng, Z., Qiao, Z., Xin, Z., & Yang, L. (2026) · npj Materials Degradation · doi:10.1038/s41529-026-00781-0 · Cited by 3
“According to the Rapp-Goto model for molten salt corrosion 43 , basic fl uxing occurs under these conditions, wherein Na ₂ O reactswith the protectiveoxides (Al ₂ O ₃ and Ta ₂ O ₅ ) to form non-protective, complex oxides (NaAlO ₂ and NaTaO ₃ ) in the intermediate layer, thereby degrading the oxide…”
Oxidation and Hot Corrosion Behaviour of Dual Phase 8YSZ + La2Zr2O7 and 8YSZ + Gd2Zr2O7 TBC Systems
Moskal, G. (2025) · Journal of Thermal Spray Technology · doi:10.1007/s11666-025-01978-6 · Cited by 3
“These studies proposed an explanation of the destruction mechanisms based on the process of mutual corrosion in oxide systems described by Rapp (Ref 86, 87), in which one of the oxides acts as an acidic medium and the other as a basic one.”
Singh, S. C. G. S. G., & TJPRC (2017) · International journal of mechanical and production engineering research and development · doi:10.24247/ijmperdaug201718 · Cited by 3
“The surface coating method has been given mo re importance to meet this challenge in the area of technology; where materials have to operate in hars h conditions of corrosive surroundings, pressure an d temperature etc [4].”
MethodFireside Corrosion in Coal- and Oil-Fired Boilers
(2006) · ASM International eBooks · doi:10.31399/asm.hb.v13c.a0004156 · Cited by 3
Enhancing Thermal Properties of Steam Turbine Blades by Coating with Nanomaterials
Ugla, A. A., Hasan, M. I., Ibrahim, Z. A., & Kamil, D. J. (2021) · Materials science forum · doi:10.4028/www.scientific.net/msf.1039.281 · Cited by 3
“The working conditions of the turbine blades, such as high-temperature corrosion[4],[5] demand that the designers employ super heat-resistant alloys of thermal fatigue[6],[7], and various studies have focused on the work temperature effect of the substantial particle erosion of bulk materials.”
BackgroundInfluence of Silicon and Chromium on the Na2SO4-Induced Hot Corrosion Behavior of Titanium Alloys
Mitoraj-Królikowska, M. (2023) · Crystals · doi:10.3390/cryst13060948 · Cited by 3
Oxidation and Hot Corrosion Studies of Laser Hybrid Welded IN617 and P91 Alloys
Paswan, S., Meena, L. K., Guguloth, K., Shariff, S. M., & Singh, R. (2023) · Transactions of the Indian Institute of Metals · doi:10.1007/s12666-023-03163-1 · Cited by 3
Hot corrosion behavior of Mo–9.0Si–8.0B
Beck, K., König, T., Case, A., Oskay, C., & Galetz, M. C. (2024) · Materials and Corrosion · doi:10.1002/maco.202414347 · Cited by 3
Singh, S., Kaur, M., Kumar, M., Singh, H., & Singh, S. (2019) · Materials Research Express · doi:10.1088/2053-1591/ab2e48 · Cited by 3
Kumar, R., Tewari, V. K., & Prakash, S. (2020) · High Temperature Materials and Processes · doi:10.1515/htmp-2020-0035 · Cited by 3
Patil, V. G., Kandaiah, S., & Somasundaram, B. (2021) · International Journal of Applied Ceramic Technology · doi:10.1111/ijac.13844 · Cited by 3
Ansari, M. S., Bansal, A., Chawla, V., & Aggarwal, V. (2021) · Surface Topography: Metrology and Properties · doi:10.1088/2051-672x/ac0171 · Cited by 2
Pei, H., Zuo, T., Wang, J. Y., Zhang, H., Wen, Z., Wen, S. F., & Yue, Z. F. (2025) · Engineering Failure Analysis · doi:10.1016/j.engfailanal.2025.110187 · Cited by 2
Kant, S. (2024) · BENTHAM SCIENCE PUBLISHERS eBooks · doi:10.2174/9789815223552124010006 · Cited by 2
Influence on Thermal Barrier Coating Delamination Behaviour of Edge Geometry
Brodin, H., Li, X.-H., & Sjoestroem, S. (2008) · Springer eBooks · doi:10.1007/1-4020-4972-2_134 · Cited by 2
“Finally the cracks will flake off due to buckling as discussed in literature [19-22].”
BackgroundPROTECCIÓN CONTRA LA CORROSIÓN POR SALES FUNDIDAS DE UN ACERO AL CARBONO POR ROCIADO TERMICO
Arévalo, J. L. M., Metalúrgico, I., Auxiliar, P., Posada, B. A., & de Ingeniería, E. (2007) · DYNA · Cited by 2
Sequeira, C. A. C. (2018) · Wiley eBooks · doi:10.1002/9781119474371.ch15 · Cited by 2
High Temperature Electrochemistry
Sequeira, C. A. C. (2018) · Wiley eBooks · doi:10.1002/9781119474371.ch6 · Cited by 2
Texier, D. (2013) · theses.fr (ABES) · doi:10.70675/9de09720zda6dz4b35za101za6d1983868c3 · Cited by 22
Sanviemvongsak, T. (2020) · theses.fr (ABES) · doi:10.70675/12c09eedz55c0z4860z84d4z659cca161034 · Cited by 6
Corrosion in the Power Plant Industry
Dagdag, O., Haldhar, R., Thakur, A., Daoudi, W., Бериша, А., Berdimurodov, E. T., & Kim, H. (2025) · Wiley eBooks · doi:10.1002/9781394301560.ch5 · Cited by 1
Effect of W and Mo on the Hot Corrosion Behavior of Ni-Based Superalloys
Piel, D., Mondet, M., Charles, S., Juez-Lorenzo, M. D. M., Kolarik, V., & Pedraza, F. (2025) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-025-08074-y · Cited by 3
Hot Corrosion Behavior of a New Nickel-Based Superalloy TROPEA
Hunault, L., Mathieu, S., Aranda, L., Cormier, J., Lautru, J., Podor, R., & Pedraza, F. (2026) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-026-08112-3 · Cited by 1
Liu, T.-L., Wang, Y.-C., Zhang, X.-Y., Zheng, K., Yin, F.-X., Luo, Z.-C., & Sun, L.-Y. (2026) · Journal of Iron and Steel Research International · doi:10.1007/s42243-026-01738-y · Cited by 1
Hot corrosion of PtAl2-dispersed (Ni, Pt)Al coating at 900 °C: effects of PtAl2 content
Luo, H., Lu, Y., Zhang, P., Yang, Y., Ren, P., & Wang, Q. (2026) · Corrosion Communications · doi:10.1016/j.corcom.2026.03.021 · Cited by 1
Effect of Composition on the Hot Corrosion Resistance of NiAl and (Ni, Pt)Al
Leyens, C., Pint, B. A., & Wright, I. G. (2000) · NACE CORROSION Conference · doi:10.5006/c2000-00260 · Cited by 1
Life Assessment of a Sea-Recoverable Small Turbojet Engine Designated for UAV Application
Mishra, R. (2017) · Journal of Failure Analysis and Prevention · doi:10.1007/s11668-017-0284-5 · Cited by 1
“This type of corrosion is characterized by a non-uniform pitting-like attackwith small or no internal sulphidation [12, 13].”
BackgroundBallesteros, D. Y. P., Durán, H. A. E., Quintero, C. V., Cáceres, E., & Ortíz, A. (2013) · Informador Técnico · doi:10.23850/22565035.56 · Cited by 1
CONSTRUCCIÓN DE UNA CELDA ELECTROQUÍMICA PARA LA EVALUACIÓN DE LA CORROSIÓN POR SALES FUNDIDAS
Marulanda, A. J. L. (2006) · Scientia et technica · doi:10.22517/23447214.6433 · Cited by 1
Evaluating the Hot Corrosion Resistance of High Temperature Coatings for Marine Gas Turbines
Shifler, D. A. (2004) · NACE CORROSION Conference · doi:10.5006/c2004-04286 · Cited by 1
Metadata
- Authors
- Rapp, R. A., & Zhang, Y.-S.
- Affiliations
- The Ohio State University (US)
- Venue
- JOM
- Published
- 1994-12
- Volume
- 46
- Issue
- 12
- Pages
- 47-55
- ISSN
- 0148-6608 (ISSN-L)
- 1047-4838
- 1543-1851
- OpenAlex
- W2324760338
- Cited by
- 247
- References
- 31
- Citations by year
- 2026: 17 · 2025: 13 · 2024: 9 · 2023: 11 · 2022: 12 · 2021: 16 · 2020: 15 · 2019: 14 · 2018: 11 · 2017: 13 · 2016: 11 · 2015: 9 · 2014: 10 · 2013: 11 · 2012: 6
- FWCI
- 0.00
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.springer.com/tdm (tdm)
- Locations
- JOM (publishedVersion)
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Chemistry › Electrochemistry › Molten salt chemistry and electrochemical processes
- Physical Sciences › Materials Science › Metals and Alloys › Metallurgical Processes and Thermodynamics
- Keywords
- hot corrosion, sodium sulfate, electrochemical corrosion mechanism, sodium metavanadate, electrochemical polarization, corrosion kinetics, alloy corrosion
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.